Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Alloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

Understanding the role of selenium in defect passivation for highly efficient selenium-alloyed cadmium telluride solar cells

Electricity produced by cadmium telluride (CdTe) photovoltaic modules is the lowest-cost electricity in the solar industry, and now undercuts fossil fuel-based sources in many regions of the world. This is due to recent efficiency gains brought about by alloying selenium into the CdTe absorber, which has taken cell efficiency from 19.5% to its current record of 22.1%. Although the addition of selenium is known to reduce the bandgap of the absorber material, and hence increase the cell short-circuit current, this effect alone does not explain the performance improvement. Here, by means of cathodoluminescence and secondary ion mass spectrometry, we show that selenium enables higher luminescence efficiency and longer diffusion lengths in the alloyed material, indicating that selenium passivates critical defects in the bulk of the absorber layer. Here, this passivation effect explains the record-breaking performance of selenium-alloyed CdTe devices, and provides a route for further efficiency improvement that can result in even lower costs for solar-generated electricity.

14 SOLAR ENERGY↗

Superconductivity of Ta-Hf and Ta-Zr alloys: Potential alloys for use in superconducting devices

The electronic properties relevant to superconductivity are reported for bulk Ta-Hf and Ta-Zr body centered cubic alloys, in a large part to determine whether their properties are suitable for potential use in superconducting qbits. The body centered cubic unit cell sizes increase with increasing alloying. Here, the results of magnetic susceptibility, electrical resistivity, and heat capacity characterization are reported. While elemental Ta is a type I superconductor, the alloys are type II strong coupling superconductors. Although decreasing the electron count per atom is expected to increase the density of electronic states at the Fermi level and thus the superconducting transition temperature (T c ) in these systems, we find that this is not sufficient to explain the significant increases in the superconducting T c 's observed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characteristics of Molten Alloys as Anodes in Solid Oxide Fuel Cells

Molten alloys with 50-mol% In-Sb, Sn-Sb, Sb-Bi, and Sb-Pb were examined as anodes for solid oxide fuel cells at 973 K. The cells were operated in the battery mode, without added fuel, in order to understand the oxidation characteristics of these alloys at electrolyte interfaces. Cells using 50-mol% In-Sb and Sn-Sb mixtures exhibited open-circuit voltages (OCV) of 1.0 and 0.93 V, values that are identical to that of cell with pure In and Sn respectively. Also similar to the pure In and Sn anodes, the impedances of these cells were initially low but increased dramatically after drawing a small amount of charge, implying formation of In₂O₃ and SnO₂ layers at the electrolyte interface. The 50-mol% Sb-Bi cell had an OCV of 0.73 V initially, close to the OCV observed with pure Sb. The OCV remained constant until a charge identical to that required for oxidation of all the Sb had been passed, after which the OCV dropped to 0.43 V, similar to the value for pure Bi. SEM analysis of the cell after conversion of the Sb showed two distinct phases, with metallic Bi at the bottom and Sb₂O₃ at the top. The electrochemical oxidation of 50-mol% Sb-Pb alloys exhibited an OCV that changed continuously with conversion, from 0.73 V initially to 0.67 V following the addition of charge corresponding to oxidation of 120% the Sb. The total cell impedance remained low for this entire period. EDS measurements on the sectioned Sb-Pb cell suggested that both Sb and Pb were oxidized simultaneously to form a mixed oxide of Pb and Sb.

30 DIRECT ENERGY CONVERSION↗

Film breakdown and nano-porous Mg(OH) 2 formation from corrosion of magnesium alloys in salt solutions

In this paper, small angle neutron scattering (SANS) and scanning transmission electron microscopy (STEM) were used to study film formation by magnesium alloys AZ31B (Mg-3Al-1Zn base) and ZE10A (Elektron 717, E717: Mg-1Zn + Nd, Zr) in H 2 O and D 2 O with and without 1 or 5 wt% NaCl. No SANS scattering changes were observed after 24 h D 2 O or H 2 O exposures compared with as-received (unreacted) alloy, consistent with relatively dense MgO-base film formation. However, exposure to 5 wt% NaCl resulted in accelerated corrosion, with resultant SANS scattering changes detected. The SANS data indicated both particle and rough surface (internal and external) scattering, but with no preferential size features. The films formed in 5 wt% NaCl consisted of a thin, inner MgO-base layer, and a nano-porous and filamentous Mg(OH) 2 outer region tens of microns thick. Chlorine was detected extending to the inner MgO-base film region, with segregation of select alloying elements also observed in the inner MgO, but not the outer Mg(OH) 2 . Modeling of the SANS data suggested that the outer Mg(OH) 2 films had very high surface areas, consistent with loss of film protectiveness. Finally, implications for the NaCl corrosion mechanism, and the potential utility of SANS for Mg corrosion, are discussed.

36 MATERIALS SCIENCE↗

In-situ tensile testing of single-crystal molybdenum-alloy fibers with various dislocation densities in a scanning electron microscope

In-situ tensile tests have been performed in a dual beam focused ion beam and scanning electron microscope on as-grown and prestrained single-crystal molybdenum-alloy (Mo-alloy) fibers. The fibers had approximately square cross sections with submicron edge lengths and gauge lengths in the range of 9–41 μm. In contrast to previously observed yield strengths near the theoretical strength of 10 GPa in compression tests of ~1–3-μm long pillars made from similar Mo-alloy single crystals, a wide scatter of yield strengths between 1 and 10 GPa was observed in the as-grown fibers tested in tension. Deformation was dominated by inhomogeneous plastic events, sometimes including the formation of Lüders bands. In contrast, highly prestrained fibers exhibited stable plastic flow, significantly lower yield strengths of ~1 GPa, and stress–strain behavior very similar to that in compression. A simple, statistical model incorporating the measured dislocation densities is developed to explain why the tension and compression results for the as-grown fibers are different.

36 MATERIALS SCIENCE↗

Phase Transformation Kinetics and Alloy Microsegregation in High Pressure Die Cast Magnesium Alloys (Final Report)

The primary objective of this project is to conduct a systematic, quantitative study of phase transformation kinetics and microsegregation in HPDC Mg alloys in both as-cast and heat treated conditions. These results will be used to develop and validate physics-based phase transformation kinetics micro-models that quantitatively capture microstructural evolution and microsegregation during HPDC and heat treatment of Mg alloys. Finally, this knowledge will be transferred to industry and the wider research community through these micro-models and the experimental data that will be stored in the National Institute of Standards and Technology (NIST)-DOE Energy Efficiency and Renewable Energy Advanced Automotive Cast Magnesium Alloys Repository, as well as a new repository, the University of Michigan Department of Energy Predictive Integrated Structural Materials Science (UM DOE PRISMS) Materials Commons. To accomplish these goals, a systematic and comprehensive experimental study is being combined with computational modeling and simulation.

36 MATERIALS SCIENCE↗

Effects of alloy composition in alleviating embrittlement problems associated with the tantalum alloy T-111

The causes of aging embrittlement in T-111 (Ta-8W-2Hf) and the effect of alloy modification were investigated. Results show that T-111 possesses a critical combination of tungsten and hafnium that leads to loss in ductility at -196 C after aging near 1040 C. It was found that this occurs because tungsten enhances hafnium segregation to grain boundaries, which also leads to increased susceptibility to hydrogen embrittlement. Aging embrittlement was not observed in tantalum alloys with reduced tungsten or hafnium contents; most of the alloys studied have lower strengths than T-111 and exhibit susceptibility to hydrogen embrittlement.

Stephens, J. R.↗

Effects of long-term aging on ductility of the columbium alloys C-103, Cb-1Zr, and Cb-752 and the molybdenum alloy Mo-TZM

A program was conducted to determine if aging embrittlement occurs in the columbium alloys C-103, CB-1Zr, and Cb-752 or in the molybdenum alloy Mo-TZM. Results showed that aging embrittlement does not occur in C-103, Cb-1Zr, or Mo-TZM during long-term (1000 hr) aging at temperatures in the range 700 to 1025 C. In contrast, aging embrittlement did occur in the Cb-752 alloy after similar aging at 900 C. A critical combination of the solute additions W and Zr in Cb-752 led to Zr segregation at grain boundaries during long-term aging. This segregation subsequently resulted in embrittlement as indicated by an increase in the ductile-brittle transition temperature from below -1960 C to about -150 C.

Stephens, J. R.↗

Effects of alloy composition in alleviating embrittlement problems associated with the tantalum alloy T-111

The causes of aging embrittlement in T-111 (Ta-8W-2Hf) and the effects of alloy modification were investigated. Results showed that T-111 contains a critical combination of tungsten and hafnium that leads to loss of ductility at -196 C after aging near 1040 C. This appears to occur because tungsten enhances hafnium segregation to grain boundaries and this also leads to increased susceptibility to hydrogen embrittlement. Aging embrittlement was not observed in tantalum alloys with reduced tungsten or hafnium contents; however, most of the alloys studied have lower strengths than T-111 and exhibit susceptibility to hydrogen embrittlement.

Stephens, J. R.↗

Elevated temperature crack growth in aluminum alloys: Tensile deformation of 2618 and FVS0812 aluminum alloys

Understanding the damage tolerance of aluminum alloys at elevated temperatures is essential for safe applications of advanced materials. The objective of this project is to investigate the time dependent subcritical cracking behavior of powder metallurgy FVS0812 and ingot metallurgy 2618 aluminum alloys at elevated temperatures. The fracture mechanics approach was applied. Sidegrooved compact tension specimens were tested at 175, 250, and 316 C under constant load. Subcritical crack growth occurred in each alloy at applied stress intensity levels (K) of between about 14 and 25 MPa/m, well below K (sub IC). Measured load, crack opening displacement and displacement rate, and crack length and growth rate (da/dt) were analyzed with several continuum fracture parameters including, the C-integral, C (sub t), and K. Elevated temperature growth rate data suggest that K is a controlling parameter during time dependent cracking. For FVS0812, da/dt is highest at 175 C when rates are expressed as a function of K. While crack growth rate is not controlled by C (sub t) at 175 C, da/dt appears to better correlate with C (sub t) at higher temperatures. Creep brittle cracking at intermediate temperatures, and perhaps related to strain aging, is augmented by time dependent transient creep plasticity at higher temperatures. The C (sub t) analysis is, however, complicated by the necessity to measure small differences in the elastic crack growth and creep contributions to the crack opening displacement rate. A microstructural study indicates that 2618 and FVS0812 are likely to be creep brittle materials, consistent with the results obtained from the fracture mechanics study. Time dependent crack growth of 2618 at 175 C is characterized by mixed transgranular and intergranular fracture. Delamination along the ribbon powder particle boundaries occurs in FVS0812 at all temperatures. The fracture mode of FVS0812 changes with temperature. At 175 C, it is characterized as dimpled rupture, and at 316 C as mixed matrix superplastic rupture and matrix-dipersoid debonding.

Leng, Yang↗

Comparison of high temperature, high frequency core loss and dynamic B-H loops of two 50 Ni-Fe crystalline alloys and an iron-based amorphous alloy

The availability of experimental data that characterizes the performance of soft magnetic materials for the combined conditions of high temperature and high frequency is almost nonexistent. An experimental investigation was conducted over the temperature range of 23 to 300 C and frequency range of 1 to 50 kHz to determine the effects of temperature and frequency on the core loss and dynamic B-H loops of three different soft magnetic materials; and oriented grain 50Ni-50Fe alloy, a nonoriented grain 50Ni-Fe alloy, and an iron based amorphous material (Metglas 2605SC). A comparison of these materials shows that the nonoriented grain 50Ni-50Fe alloy tends to have either the lowest or next lowest core loss for all temperatures and frequencies investigated.

Wieserman, W. R.↗

Solution chemistry effects on the stress corrosion cracking behavior of alloy 2090 (Al-Li-Cu) and alloy 2024 (Al-Cu-Mg)

The SCC initiation behavior of alloys 2090 and 2024 is examined in various NaCl-based environments. The pre-exposure and bulk/local solution chemistry effects discovered by Holroyd et al. (1986) are investigated, with emphasis on the effect of bulk solution chemistries and atmospheric CO2 on the occluded cell environment and the role of the occluded environment in the crack initiation and early-stage propagation processes. It was found that constant immersion in NaCl does not promote SCC in alloy 2090 or alloy 2024. Upon removal from NaCl, SCC is quickly facilitated, but only in the presence of atmospheric CO2. The need for CO2 is attributed to an increase in carbonate concentrations, eventually allowing passivation of blunted fissures by precipitation of Li2CO3. It is inferred that any effects due to aging are small in magnitude, relative to the effects of subtle changes in the bulk/local solution chemistries.

Moran, James P.↗

Comparison of high temperature, high frequency core loss and dynamic B-H loops of two 50 Ni-Fe crystalline alloys and an iron-based amorphous alloy

The availability of experimental data that characterize the performance of soft magnetic materials for the combined conditions of high temperature and high frequency is almost nonexistent. An experimental investigation was conducted over the temperature range of 23 to 300 C and frequency range of 1 to 50 kHz to determine the effects of temperature and frequency on the core loss and dynamic B-H loops of three different soft magnetic materials: an oriented-grain 50Ni-50Fe alloy, a nonoriented-grain 50Ni-50Fe alloy, and an iron-based amorphous material (Metglas 2605SC). A comparison of these materials shows that the nonoriented-grain 50Ni-50Fe alloy tends to have either the lowest or the next lowest core loss for all temperatures and frequencies investigated.

Wieserman, W. R.↗

Cu-Au Alloys Using Monte Carlo Simulations and the BFS Method for Alloys

Semi empirical methods have shown considerable promise in aiding in the calculation of many properties of materials. Materials used in engineering applications have defects that occur for various reasons including processing. In this work we present the first application of the BFS method for alloys to describe some aspects of microstructure due to processing for the Cu-Au system (Cu-Au, CuAu3, and Cu3Au). We use finite temperature Monte Carlo calculations, in order to show the influence of 'heat treatment' in the low-temperature phase of the alloy. Although relatively simple, it has enough features that could be used as a first test of the reliability of the technique. The main questions to be answered in this work relate to the existence of low temperature ordered structures for specific concentrations, for example, the ability to distinguish between rather similar phases for equiatomic alloys (CuAu I and CuAu II, the latter characterized by an antiphase boundary separating two identical phases).

Bozzolo, Guillermo↗

Fatigue Characterization of Alloy 10: a 1300F Disk Alloy for Small Gas Turbine Engines

A detailed fatigue characterization of Alloy 10, a high strength nickel-based disk alloy, was conducted on test coupons machined from a 'pancake' forging. Smooth bar, strain controlled fatigue testing at various R-ratios was run at representative bore, 750 F, and rim, 1300 F, temperatures. This was followed by notch fatigue testing (Kt=2) run under load control. Analysis of the fatigue data using a Smith-Watson-Topper approach and finite element analysis of the notch root was employed to understand material behavior in these tests. Smooth bar fatigue data showed a significant R-ratio dependence at either test temperature which could be accounted for using a Smith-Watson-Topper parameter (SWT). In general, fatigue life was longer at 750 F than 1300 F for a given SWT. For notch fatigue tests, life was longer at 750 F than 1300 F but only at higher stresses. This was attributed to differences in alloy strength. At lower stresses, finite element analysis suggested that convergence of fatigue life at both temperatures resulted from relaxation of stresses at the notch root in the 1300 F tests.

Gayda, John↗