Rapid thermal annealing of indium phosphide compound semiconductors
The rapid thermal annealing (RTA) of indium phosphide (InP) substrates using a proximity contact method and silicon nitride encapsulation is investigated. The surface conditions of the InP substrates following cleaning with procedures A and B are analyzed. Procedure A involves using an iodic acid solution to remove work-damage InP surface layers and B is a degasssing process and hydrofluoric acid solution for native oxide removal. AES, XPS, and SIMS data of the proximity contact and silicon nitride encapsulated annealed samples are examined. The data reveal that RTA using proximity contact with silicon wafers does not provide adequate protection; however, the InP sample is successfully annealed when protected by a silicon nitride encapsulant.