At least 361 records · Page 20

A Comparative Study of Constitutive Characteristics and Microstructure Evolution between Uniaxial and Plane Strain Compression of an AA6061 Alloy

The hot deformation behavior of an AA6061 alloy was comparatively studied by uniaxial compression (UC) and plane strain compression (PSC) in the temperature range of 300-450 °C and strain rate range of 0.01-5 s{sup −1}. The processing maps were constructed based on a dynamic materials model, and the associated microstructures were observed. Under the same deformation conditions, the flow stress of the AA6061 alloy during PSC is higher than that during UC, which can be characterized by the Zener–Hollomon (Z) parameter in a hyperbolic sine-type equation with an activation energy Q of 175.2 kJ mol{sup −1} and 201.9 kJ mol{sup −1}, respectively. In addition, the instability domain is narrower under PSC compared to that under UC. The observed microstructures also indicate that as the Z value decreases, the tendency of dynamic recrystallization increases during PSC. The softening mechanisms in the AA6061 alloy after PSC and UC mainly consist of the dynamic recovery that is accompanied by a slight dynamic recrystallization. The optimum parameters are in the temperature range of 360-450 °C and strain rate range of 0.03-0.3 s{sup −1} for UC, and for PSC, the optimum parameters are in the temperature range of 320-400 °C and strain rate range of 0.01-0.05 s{sup −1}.

36 MATERIALS SCIENCE↗

Strengthening mechanisms, hardening/softening behavior, and microstructure evolution in an LPSO magnesium alloy at elevated temperatures

Here, rapid degradation of the mechanical properties of conventional Mg alloys with temperature precludes their wide application in industry. The LPSO (long period stacking ordered) Mg alloys, on the other hand, show considerable potential to achieve excellent high-temperature mechanical performance. In this study, a Mg-5.1Y-2.4Zn (wt.%) extrusion alloy with the microstructure comprising of α-Mg matrix and LPSO phase was prepared. It is shown that the yield strength of the alloy at 200 °C retained ~83% of the yield strength of 198 MPa at room temperature (RT). Importantly, the ductility also improved, owing to the increased non-basal slip activities at elevated temperatures. In contrast to RT and 200 °C, the alloy exhibited softening tensile behavior with an apparent loss of yield strength at 300 °C. In-situ lattice strain analysis revealed that load transfer from α-Mg to LPSO remains effective at temperatures up to 200 °C, governing the high yield strength of the alloy. The post-mortem analysis by means of electron microscopy confirmed that the LPSO phase is structurally stable at 200 °C. In particular, the high strain hardenability is rationalized by the sandwiched LPSO structures together with stacking faults serving as effective obstacles to the motion of non-basal dislocations. The load transfer effect disappears at the temperature of 300 °C, resulting in the fast deterioration of strength of the alloy. The cracking of the LPSO phase along with the recrystallizing of α-Mg grains were found to be the main causes for the softening behavior of the alloy at 300 °C.

36 MATERIALS SCIENCE↗

Friction stir welded AM50 and AZ31 Mg alloys: Microstructural evolution and improved corrosion resistance

One of the major drawbacks of Mg alloys is poor weldability, caused by porosity formation during conventional fusion welding processes. Friction Stir Welding (FSW) is promising technique in this context since it is a solid state technique. Contradicting results were published in the literature regarding the FSWed Mg alloys joint's properties. Current research was performed in order to investigate the microstructure and corrosion properties of FSWed Mg alloys, studying representatives of two commercial families: wrought AZ31-H24 and die cast AM50. It was found that in both alloys recrystallization occurred during the FSW. In AM50 the mechanism of the recrystallization was continuous, manifested by dislocation rearrangement into sub grain boundaries. In AZ31 discontinuous recrystallization had occurred through grain boundaries migration - twins rotated with respect to the matrix, turning into low angle grain boundaries. Corrosion resistance has improved during the FSW in both alloys to different extents. In the AM50 alloy, the nugget exhibited significantly higher surface potential than the base metal mainly due to the higher Al concentration in the matrix of the nugget, resulting from the dissolution of Al-enrichment and β-Mg{sub 17}Al{sub 12} phase. In the AZ31 alloy, no change in Al concentration had occurred, and the surface potential measured in the nugget was only slightly higher than in the base metal. These results underline the appropriateness of the FSW for Mg alloys since during the conventional welding deterioration of the corrosion resistance occurs. - Highlights: • Following FSW, AZ31-H24 experienced discontinuous recrystallization. • In AZ31 grain boundaries migration occurred, thus twins rotated. • In die cast AM50 continuous recrystallization occurred during the FSW. • In AM50 - dislocations rearranged into sub grain boundaries. • Corrosion resistance has improved during the FSW in both alloys to different extent.

36 MATERIALS SCIENCE↗

Microstructure Evolution During Controlled Solidification of “Fe{sub 2}O{sub 3}”-CaO-SiO{sub 2} Liquids in Air

The principal chemical components in iron ore sintering are Fe{sub 2}O{sub 3}, CaO, and SiO{sub 2}. This sintering process consists of three key steps: heating, holding at peak temperature, and cooling. During the cooling stage, a liquid oxide solidifies to form the final sinter microstructures. To investigate the fundamental processes taking place during the cooling of sinters, a new experimental technique has been developed that allows the stages of solidification to be determined in isolation, rather than inferred from the final microstructures. Fe{sub 2}O{sub 3}-CaO-SiO{sub 2} oxide samples of a bulk composition having a CaO/SiO{sub 2} mass ratio of 3.46 and 73.2 wt pct Fe{sub 2}O{sub 3} were cooled in air from 1623 K (1350 °C) at 2 K/s, quenched at 5 K temperature intervals from 1533 K to 1453 K (1260 °C to 1180 °C), and analyzed using Electron Probe Micro X-Ray Analysis (EPMA). During cooling, four distinct stages were observed, consisting of the phase assemblages Liquid + Hematite (I), Liquid + Hematite + C{sub 2}S(II), Liquid + C{sub 2}S + CF{sub 2}(III), and C{sub 2}S + CF{sub 2} + CF (IV). This solidification sequence differs from that predicted under equilibrium and Scheil–Gulliver Cooling. Importantly, no Silico-Ferrite of Calcium (SFC) phase was observed to form on solidification of the liquid. Based on the microstructures formed and liquid compositions, measured by EPMA, it was demonstrated that kinetic factors play a major role in determining the phases and microstructures formed under the conditions investigated.

36 MATERIALS SCIENCE↗

Thermomechanical behavior and microstructural evolution of a Ni(Pd)-rich Ni 24.3 Ti 49.7 Pd 26 high temperature shape memory alloy

We investigated the effect of thermomechanical cycling on a slightly Ni(Pd)-rich Ni 24.3 Ti 49.7 Pd 26 (near stochiometric Ni–Ti basis with Pd replacing Ni) high temperature shape memory alloy. Furthermore, aged tensile specimens (400 °C/24 h/furnace cooled) were subjected to constant-stress thermal cycling in conjunction with microstructural assessment via in situ neutron diffraction and transmission electron microscopy (TEM), before and after testing. It was shown that in spite of the slightly Ni(Pd)-rich composition and heat treatment used to precipitation harden the alloy, the material exhibited dimensional instabilities with residual strain accumulation reaching 1.5% over 10 thermomechanical cycles. This was attributed to insufficient strengthening of the material (insufficient volume fraction of precipitate phase) to prevent plasticity from occurring concomitant with the martensitic transformation. In situ neutron diffraction revealed the presence of retained martensite while cycling under 300 MPa stress, which was also confirmed by transmission electron microscopy of post-cycled samples. Neutron diffraction analysis of the post-thermally-cycled samples under no-load revealed residual lattice strains in the martensite and austenite phases, remnant texture in the martensite phase, and peak broadening of the austenite phase. The texture we developed in the martensite phase was composed mainly of those martensitic tensile variants observed during thermomechanical cycling. Presence of a high density of dislocations, deformation twins, and retained martensite was revealed in the austenite state via in-situ TEM in the post-cycled material, providing an explanation for the observed peak broadening in the neutron diffraction spectra. Despite the dimensional instabilities, this alloy exhibited a biased transformation strain on the order of 3% and a two-way shape memory effect (TWSME) strain of ~2%, at relatively high actuation temperatures.

36 MATERIALS SCIENCE↗

Microstructural evolution of nanostructured Ti{sub 0.7}Ni{sub 0.3}N prepared by reactive ball-milling

Graphical abstract: - Highlights: • α-Ti to β-Ti phase conversion is observed during 1 h of milling. • Ti{sub 0.7}Ni{sub 0.3}N (fcc) phase is noticed to form after 1 h of milling. • Formation time of Ti(Ni,N) phase is same as TiN phase. • Both X-ray and HRTEM microstructure characterization revealed similar results. - Abstract: Nanocrystalline stoichiometric Ti{sub 0.7}Ni{sub 0.3}N powder has been synthesized by ball-milling the α-Ti (hcp) and Ni (fcc) powders under N{sub 2} gas at room temperature. The α-Ti phase partially transforms to the transient (-Ti phase after 1 h of milling. After 5.5 h of milling, very broad reflections of Ti{sub 0.7}Ni{sub 0.3}N phase is noticed. Complete formation of Ti{sub 0.7}Ni{sub 0.3}N phase is observed after 9 h of milling. Microstructure in terms of lattice imperfections of unmilled and all ball-milled powder mixtures are primarily characterized by analyzing the X-ray powder diffraction patterns employing the Rietveld structure refinement procedure. It clearly reveals the presence of Ti{sub 0.7}Ni{sub 0.3}N phase and inclusion of nitrogen atoms into the α-Ti–Ni matrix on the way to formation of nitride phase. Microstructure of the ball milled nitride powders is also characterized by HRTEM. Particle size of Ti{sub 0.7}Ni{sub 0.3}N phase obtained from XRD method of characterization is ∼5 nm which is very close to that obtained from HRTEM.

36 MATERIALS SCIENCE↗

Use of High Magnetic Field to Control Microstructural Evolution in Metallic and Magnetic Materials

The Amendment 1, referred to as Phase 2, to the original CRADA NFE-06-00414 added tasks 3 through 7 to the original statement of work that had two main tasks that were successfully accomplished in Phase 1 of this project. In this Phase 2 CRADA extension, extensive research and development activities were conducted using high magnetic field processing effects for the purpose of manipulating microstructure in the SAE 5160 steel to refine grain size isothermally and to develop nanocrystalline spacing pearlite during continuous cooling, and to enhance the formability/forgability of the non-ferrous precipitation hardening magnesium alloy AZ90 by applying a high magnetic field during deformation processing to investigate potential magnetoplasticity in this material. Significant experimental issues (especially non-isothermal conditions evolving upon insertion of an isothermal sample in the high magnetic field) were encountered in the isothermal phase transformation reversal experiments (Task 4) that later were determined to be due to various condensed matter physics phenomenon such as the magnetocaloric (MCE) effect that occurs in the vicinity of a materials Curie temperature. Similarly the experimental deformation rig had components for monitoring deformation/strain (Task 3) that were susceptible to the high magnetic field of the ORNL Thermomagnetic Processing facility 9-T superconducting magnet that caused electronic components to fail or record erroneous (very noisy) signals. Limited experiments on developing nanocrystalline spacing pearlite were not sufficient to elucidate the impact of high magnetic field processing on the final pearlite spacing since significant statistical evaluation of many pearlite colonies would need to be done to be conclusive. Since extensive effort was devoted to resolving issues for Tasks 3 and 7, only results for these focused activities are included in this final CRADA report along with those for Task 7 (described in the Objectives Section of this report).

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Microstructure Evolution and Mechanical Properties of Large-Scale AZ80 Magnesium Alloy Billets Produced by Multitemperature Multidirectional Forging

Grain refinement is an effective method to improve the mechanical properties of magnesium (Mg) alloys. In the present research, the combination of multidirectional forging (MDF) and forward extrusion for sizing with decreasing temperature pass by pass was employed to deform as-cast AZ80 magnesium alloy billet with large size to obtain fine grains and homogeneous microstructure. It was found that with the increasing number of MDF passes, the average grain size decreases; the homogeneity of microstructures and the percentages of dynamic recrystallised grains increase simultaneously. After six-pass MDF, fine and homogeneous microstructure with an average grain size of 15 μm was achieved; however, grain refinement became very difficult with a further increase in the MDF pass number. After eight-pass MDF plus forward extrusion for sizing, excellent mechanical properties of large-scale AZ80 magnesium alloy billet were obtained. The tensile strength, the yield strength and the elongation of billet are 410 MPa, 292 MPa and 14%, respectively. Furthermore, during multitemperature MDF, the inverse of the square root of grain size and tensile yield strength fit well with the Hall–Petch relationship.

36 MATERIALS SCIENCE↗

Relationships between deformation and microstructure evolution and minimizing surface roughness after BCP processing in RRR Nb cavitites

Two strategies for improving the surface finish of niobium sheet used in superconducting radio frequency cavities were examined, using slices of single (or large-grain) material from an ingot, and equal channel angle extrusion (ECAE) preprocessing of ingot material to achieve a uniform and small grain size prior to subsequent rolling. The effect of these two processing paths on final microstructure, texture, and surface finish are discussed.

99 GENERAL AND MISCELLANEOUS↗

Competing effects of electronic and nuclear energy loss on microstructural evolution in ionic-covalent materials

Ever increasing energy needs have raised the demands for advanced fuels and cladding materials that withstand the extreme radiation environments with improved accident tolerance over a long period of time. Ceria (CeO2) is a well known ionic conductor that is isostructural with urania and plutonia-based nuclear fuels. In the context of nuclear fuels, immobilization and transmutation of actinides, CeO2 is a model system for radiation effect studies. Covalent silicon carbide (SiC) is a candidate for use as structural material in fusion, cladding material for fission reactors, and an inert matrix for the transmutation of plutonium and other radioactive actinides. Understanding microstructural change of these ionic-covalent materials to irradiation is important for advanced nuclear energy systems. While displacements from nuclear energy loss may be the primary contribution to damage accumulation in a crystalline matrix and a driving force for the grain boundary evolution in nanostructured materials, local non-equilibrium disorder and excitation through electronic energy loss may, however, produce additional damage or anneal pre-existing defect. At intermediate transit energies where electronic and nuclear energy losses are both significant, synergistic, additive or competitive processes may evolve that affect the dynamic response of materials to irradiation. The response of crystalline and nanostructured CeO2 and SiC to ion irradiation are studied under different nuclear and electronic stopping powers to describe some general material response in this transit energy regime. Although fast radiation-induced grain growth in CeO2 is evident with no phase transformation, different fluence and dose dependence on the growth rate is observed under Si and Au irradiations. While grain shrinkage and amorphization are observed in the nano-engineered 3C SiC with a high-density of stacking faults embedded in nanosize columnar grains, significantly enhanced radiation resistance is attributed to stacking faults that promote efficient point defect annihilation. Moreover, competing effects of electronic and nuclear energy loss on the damage accumulation and annihilation are observed in crystalline 4H-SiC. Systematic experiments and simulation effort are needed to understand the competitive or synergistic effects.

Zhang, Yanwen↗

Microstructure evolution of a dissimilar junction interface between an Al sheet and a Ni-coated Cu sheet joined by magnetic pulse welding

An Al sheet and a Ni-coated Cu sheet were lap joined by using magnetic pulse welding (MPW). Tensile tests were performed on the joined sheets, and a good lap joint was achieved at a discharge energy of > 0.9 kJ. The weld interface exhibited a wavy morphology and an intermediate layer along the weld interface. Microstructure observations of the intermediate layer revealed that the Ni coating region consisted of a Ni–Al binary amorphous alloy and that the Al sheet region contained very fine Al nanograins. Ni fragments indicative of unmelted residual Ni from the coating were also observed in parts of the intermediate layer. Formation of these features can be attributed to localize melting and a subsequent high rate cooling of molten Al and Ni confined to the interface during the MPW process. In the absence of an oxide film, atomic-scale bonding was also achieved between the intermediate layer and the sheet surfaces after the collision. MPW utilises impact energy, which affects the sheet surfaces. From the obtained results, good lap joint is attributed to an increased contact area, the anchor effect, work hardening, the absence of an oxide film, and suppressed formation of intermetallic compounds at the interface. - Highlights: •Good lap joint of an Al sheet and a Ni-coated Cu sheet was achieved by using magnetic pulse welding. •A Ni–Al binary amorphous alloy was formed as an intermediate layer at weld interface. •Atomic-scale bonding was achieved between the intermediate layer and the sheet surfaces.

36 MATERIALS SCIENCE↗

Modeling and Simulation of Microstructure Evolution and Deformation in an Irradiated Environment

The ability to predict the behavior of structural components in a nuclear power plant is critical to the nuclear industry. Structural metals in the primary loop of nuclear power plants must endure challenges such as irradiation and mechanical and thermal loading, and these structural metal components must continue to function in potential transient and accident conditions throughout the operational lifetime of the power plant. This extreme operational environment changes the metal microstructure by creating additional defects. The physical interactions of dislocations with these defects govern how the metal will respond to future conditions. Therefore predicting the mechanical response of these metals requires a set of physically based and reliable models of dislocation and defect interactions. These microstructure elements include glide mobile and immobile dislocations, geometrically necessary dislocations, twinning dislocations, irradiation defects, and thermal aging defects. We present here a continuum dislocation dynamics crystal plasticity framework to capture the interaction mechanisms of these dislocations and defects, verified with a combination of benchmark problems and comparisons with experimental data for two different types of structural metals: alpha iron and nickel-based alloys. In our simulations of $\alpha$ iron we highlight the advantages of applying a Monte Carlo stochastic model of cross slip dislocation motion and show the importance of capturing the 3D nature of glide dislocation and self-interstitial atom loop radiation defect interactions. We demonstrate coupling of glide dislocations with geometrically necessary dislocations to capture the influence of lattice bending, including the sensitivity of the geometrically necessary dislocations to changes in the grain boundary angle. We further examine the interaction of glide dislocations with the twin dislocations and thermally aged defects which have been observed in a nickel-based alloy with additional models. Finally we assess the reliability of this crystal plasticity framework by comparing two dislocation glide velocity models across the range of normal operation temperatures. In successfully applying our crystal plasticity framework to multiple metals, we provide further evidence of the reliability of our approach. The results of this mechanism-based continuum dislocation dynamics crystal plasticity framework can be used to inform engineering scale models throughout the nuclear industry.

36 MATERIALS SCIENCE↗

Microstructural Evolution of NiCrBSi Coatings Fabricated by Stationary Local Induction Cladding

The development of induction cladding has been restricted by the complicated geometric characteristics of workpieces and the large heat-affected zone in the cladded workpieces. In this paper, three-dimensional continual local induction cladding (3D-CLIC) was proposed as a potential process to clad coating over a substrate with curved surface, and a stationary local induction cladding (SLIC) experiment was conducted as an exploratory study of 3D-CLIC. The microstructures and microhardness in the coatings were measured by SEM, EDS, XRD and microsclerometer, respectively. The results indicate that the coating is metallurgically bonded with the substrate without any defects. A compositional gradient exists in the diffusion transfer belt (DTB), and it decreases with the increase in induction heating time. The coating is mainly composed of (Fe, Ni), CrB, M{sub 7}C{sub 3}, Ni{sub 3}B, Ni{sub 3}Si and M{sub 23}C{sub 6} (M = Cr, Ni, Fe). Among the carbides, M{sub 7}C{sub 3} presents several morphologies and M{sub 23}C{sub 6} is always attached to the DTB. A special phenomenon of texture was found in the SLIC coatings. The preferred orientation in (200) crystal plane or the restrained orientation in (111) (200) crystal plane becomes more obvious as the scanning speed increases. The maximum average microhardness is 721 HV when the coating is heated for 5 s. The wear loss of different samples increases with increasing induction heating time. The longer heating time would result in higher dilution in the SLIC coatings due to the complete mixing with the substrate, thus leading to the decrease in microhardness and wear loss.

36 MATERIALS SCIENCE↗

Microstructure evolution, enhanced aging kinetics, and mechanical properties of AA7075 alloy after friction extrusion

In the present study we utilized Friction Extrusion (FE) a solid phase processing technique to produce fully consolidated dense 5 mm rods of AA7075 alloy. The combination of large shear stresses and temperatures at the tool-billet interface during the FE process resulted in the formation of dynamically recrystallized ~2.0 μm equiaxed grains and fine uniformly distributed stable η (MgZn 2 ) precipitates ~25–100 nm in size. Formation of such a microstructure resulted in lower solutionizing temperature and times (flash annealing) as compared to the conventionally extruded counterparts. Here we demonstrate for the first time that the solutionizing times for the T6 heat treatment of AA7075 can be reduced by three times using this FE process. In addition to being an energy efficient process, FE also serves to improve the performance of AA7075 alloys by retaining their strength while enhancing the ductility of the material. The tensile data for samples that were flash annealed and artificially aged after FE processing showed exceptional increase in ultimate tensile strength by over 19% and yield strength by over 59%, compared with an as-FE-processed sample.

36 MATERIALS SCIENCE↗

Passivation‐Induced Species Dynamics and Microstructural Evolution in Solid‐State Lithium–Sulfur Cathodes

Solid-state lithium–sulfur (SSLS) batteries offer high theoretical energy density, yet their practical viability is hindered by poor sulfur utilization and limited rechargeability. At the core of this challenge lies the passivating nature of Li 2 S, which restricts ionic and electronic transport, suppresses interfacial activity, and severely impedes the reversibility of electrochemical reactions. In this study, we elucidate the mechanistic origins of these limitations by resolving how charge and discharge species form, grow, and spatially evolve within the cathode microstructure under varied current densities and electrode compositions. By resolving the species distribution at the particle scale and coupling it with Raman spectroscopy and X-ray diffraction, we demonstrate how Li 2 S formation induces localized surface passivation that progressively limits electrochemical accessibility within the cathode microstructure. Sulfur utilization is found to be strongly governed by the interplay between sulfur loading, residual porosity, and interfacial architecture. High sulfur contents result in buried, electrochemically isolated domains due to poor solid electrolyte (SE) percolation, while low sulfur contents trigger SE degradation via parasitic reactions. The resulting sulfur-porosity maps delineate the mechanistic boundaries between reversible and transport-limited regimes, offering actionable design guidance for SSLS cathodes with enhanced sulfur utilization.

electrode microstructure↗

Phase equilibria and microstructure evolution in the Ni-rich region of binary Ni-Ce and ternary Ni-Ce-X (X=Al, Nb, Cr, Ti) systems at 900 °C

The equilibrium compositions of all phases in the Ni-rich region of binary Ni-Ce and ternary Ni-Ce-X (X=Al, Nb, Cr, Ti) systems at 900 °C were determined experimentally through isothermal annealing for up to 500 h and compared with currently available computational thermodynamic descriptions. Additionally, the study examined how adding a third element to the binary system affects the microstructure by analyzing changes in the volume fraction of the intermetallic phase in the eutectic region. It was observed that Nb and Ti addition lowered the intermetallic fraction in the eutectic region while Al and Cr addition did the opposite. The fraction of intermetallic phase in the eutectic region is very important because it contributes to extreme brittleness of these alloys. Also, Al, Nb and Ti addition promoted different precipitates upon annealing when added in sufficient amounts. The collected data on composition and phase equilibria provides crucial information for improving the thermodynamic assessments of the binary and ternary alloy systems.

energy dispersive spectrometry↗

Elucidating microstructural evolution and hardness variation across friction self-piercing riveted Al-7055 using synchrotron X-ray scattering and advanced microscopy techniques

Friction self-piercing riveting (FSPR) is a unique hybrid joining technique that combines the advantages of mechanical interlocking, frictional heat, and solid-state joining (if metallurgically compatible) to produce crack free joints in high strength and/or low-ductility alloys at room temperature. Here, in the current study, Al-7055 sheets were joined using FSPR for lightweight automotive applications and significant microhardness variations were observed across the joint cross-section. A detailed microstructural characterization at multiple length scales was carried out using advanced electron microscopy and X-ray scattering techniques to provide a fundamental understanding of the process-structure-property relationships. The relative contributions of microstructural characteristics at various length scales (i.e., grain size, dislocation density, solute concentration, precipitate nature) to strengthening were estimated using existent formulations (i.e., Hall-Petch, Taylor, precipitate bypass/shear equations) and correlated to the observed microhardness values across different regions. Small-angle X-ray scattering and scanning transmission electron microscopy revealed significant changes in the size and volume fraction of precipitate species, i.e., GP-I Zones, η′, and Mg/Zn solute co-clusters, depending on the process region. It was observed that the dissolution of the small η′/GP-I zones (T ∼ 150–200 °C) in the heat-affected zone were the key reason for the hardness drop. Further, it was shown that solid-solution, dislocation, grain size and solute co-cluster strengthening played a key role in the thermo-mechanically affected zone and grain-refined zone (GRZ). Finally, these observations were leveraged along with the Zener-Holloman relationship and grain size in the GRZ to estimate the peak joining temperature of the GRZ (∼ 350 °C) near the steel rivet.

aluminum 7xxx alloy↗

Interfacial microstructure evolution and weld formation during ultrasonic welding of Al alloy to Cu

Highlights: • Surface oxide layer was fractured and dispersed around the weld interface during ultrasonic welding of Al alloy to Cu. • Mechanical mixing around the weld interface was caused by compressive deformation with ultrasonic vibration. • Once micro-bonds were generated between Al and Cu, shear deformation occurred around the weld interface. • Enhanced Cu diffusion into Al in the severely deformed region significantly contributed to the weld formation. - Abstract: Dissimilar welds of Al alloy 1050 to Cu were prepared via ultrasonic spot welding in order to understand the formation of welds and interfacial microstructures. To observe oxide layer behavior at the weld interface, the anodized Al alloy 1050 was also welded to Cu. Mechanical mixing and material flow during ultrasonic welding broke and dispersed the oxide layers into the Al matrix. This material flow is attributed to compressive deformation that occurred due to ultrasonic vibrations. Direct bonding in the Al/Cu region increased with welding time. Once micro-bonds were generated between Al and Cu, the Al matrix in the vicinity of the weld interface was severely deformed in the direction of the ultrasonic vibrations. Consequently, a recrystallized microstructure with shear texture was formed in the Al matrix. Deformation heating and severe shear deformation formed Al{sub 2}Cu intermetallic compound layers at the weld interface. The growth rate of the Al{sub 2}Cu layer was much faster than had previously been estimated based upon the peak temperature and ultrasonic welding heating time. This is likely due to the increased rate of Cu diffusion into Al in the severely deformed region.