Thickness evaluation of InGaAs/InAlAs quantum wells

This work proposes a new optoelectronic measurement of quantum well (QW) thickness and applies it to doped and undoped In{sub 0.53}Ga{sub 0.47}As/In{sub 0.52}Al{sub 0.48}As multiple-QW structures. Near-infrared spectroscopic identification of the interband optical transition at 100-300 K gave the eigenenergies of the conduction band in the QW. Evaluation of the QW thickness involved analysis of the effective mass at the corresponding eigenenergy. QW thicknesses in the range of 5.45-20.8 nm were determined in six different wafers. These thicknesses agreed well with the QW thicknesses estimated by double-crystal x-ray diffraction within almost two monolayers. This measurement was used to determine the distance of potential boundaries confining the electron wave functions.

36 MATERIALS SCIENCE↗

Influence of Ag thickness on structural, optical, and electrical properties of ZnS/Ag/ZnS multilayers prepared by ion beam assisted deposition

The structural, optical, and electrical characteristics of zinc sulfide (ZnS)/Ag/ZnS (ZAZ) multilayer films prepared by ion beam assisted deposition on k9 glass have been investigated as a function of Ag layer thickness. The characteristics of ZAZ multilayer are significantly improved up insertion of optimal Ag thickness between ZnS layers. The results show that due to bombardment of Ar ion beam, distinct Ag islands evolve into continuous Ag films at a thin Ag thickness of about 4 nm. The thinner Ag film as a thickness of 2 nm leads to high sheet resistance and low transmittance for the interface scattering induced by the Ag islands or noncontinuous films; and when the Ag thickness is over 4 nm, the ZAZ multilayer exhibits a remarkably reduced sheet resistance between 7-80 {Omega}/sq for the increase in carrier concentration and mobility of Ag layer, and a high transmittance over 90% for the interference phenomena of multilayers and low absorption and surface scattering of Ag layer. The ZAZ multilayer with 14 nm Ag film has a figure of merit up to 6.32x10{sup -2} {Omega}{sup -1}, an average transmittance over 92% and a sheet resistance of 7.1 {Omega}/sq. The results suggest that ZAZ film has better optoelectrical properties than conditional indium tin oxide single layer.

36 MATERIALS SCIENCE↗

Simultaneous measurement of ultrasonic longitudinal wave velocities and thicknesses of a two layered media in the absence of an interface echo

A measurement technique has been developed to extract the phase information of successive echoes for the simultaneous estimation of thicknesses and ultrasonic velocities of individual layers in a two layered media. The proposed method works in the absence of an interface echo and requires the total thickness of the sample to be known. Experiments have been carried out on two layered samples of white cast iron and gray cast iron with layer thickness variation in the range of 2-8 mm for total thickness variation in the range of 12-13 mm. Comparison with micrographs of a few samples confirmed the model predictions. The model is found to be sensitive to the total sample thickness but fairly insensitive to noise in the data.

36 MATERIALS SCIENCE↗

Surface roughness of MgO thin film and its critical thickness for optimal biaxial texturing by ion-beam-assisted deposition

We investigated the deposition time dependences of the in-plane grain alignment ({Delta}{phi}) and the surface roughness (w) of biaxially textured MgO thin films fabricated by ion-beam-assisted deposition (IBAD) and found a strong correlation between them. The time evolution of the surface roughness of IBAD-MgO showed an abrupt increase at the same time corresponding to the beginning of the deterioration in {Delta}{phi}. The roughness versus thickness profiles obtained under different deposition conditions with different assisting ion-beam currents collapsed to a single curve, even though the deposition rates were significantly different in each condition. This implies that the abrupt increase in roughness occurred at the same thickness--of about 4 nm--irrespective of the deposition rate. The result also indicated that the {Delta}{phi} deterioration began with the same thickness of about 4 nm. This ''critical'' thickness of about 4 nm might be related to the completion of the crystallization of the film. Further, deposition beyond the critical thickness, therefore, became merely a homoepitaxial deposition under the ''IBAD'' condition, which was far from optimal because of the ion bombardment and low temperature (no-heating), and thus {Delta}{phi} deteriorated. Based on these considerations, we propose an approach to attain a sharp texture in a IBAD-MgO-based biaxial substrate; moreover, we demonstrated this approach using a two-step deposition process.

36 MATERIALS SCIENCE↗

Note: Direct measurement of the point-to-point resolution for microns-thick specimens in the ultrahigh-voltage electron microscope

We report on a direct measurement method and results of the point-to-point resolution for microns-thick amorphous specimens in the ultrahigh-voltage electron microscope (ultra-HVEM). We first obtain the ultra-HVEM images of nanometer gold particles with different sizes on the top surfaces of the thick epoxy-resin specimens. Based on the Rayleigh criterion, the point-to-point resolution is then determined as the minimum distance between centers of two resolvable tangent gold particles. Some values of resolution are accordingly acquired for the specimens with different thicknesses at the accelerating voltage of 2 MV, for example, 18.5 nm and 28.4 nm for the 5 {mu}m and 8 {mu}m thick epoxy-resin specimens, respectively. The presented method and results provide a reliable and useful approach to quantifying and comparing the achievable spatial resolution for the thick specimens imaged in the mode of transmission electron including the scanning transmission electron microscope.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Critical thickness and strain relaxation in molecular beam epitaxy-grown SrTiO{sub 3} films

We report on the study of the critical thickness and the strain relaxation in epitaxial SrTiO{sub 3} film grown on (La{sub 0.3}Sr{sub 0.7})(Al{sub 0.65}Ta{sub 0.35})O{sub 3} (001) (LSAT) substrate using the hybrid molecular beam epitaxy approach. No change in the film's lattice parameter (both the in-plane and the out-of-plane) was observed up to a film thickness of 180 nm, which is in sharp contrast to the theoretical critical thickness of ∼12 nm calculated using the equilibrium theory of strain relaxation. For film thicknesses greater than 180 nm, the out-of-plane lattice parameter was found to decrease hyperbolically in an excellent agreement with the relaxation via forming misfit dislocations. Possible mechanisms are discussed by which the elastic strain energy can be accommodated prior to forming misfit dislocations leading to such anomalously large critical thickness.

36 MATERIALS SCIENCE↗

Thickness dependent functional properties of PbZr{sub 0.52}Ti{sub 0.48}O{sub 3}/La{sub 0.67}Sr{sub 0.33}MnO{sub 3} heterostructures

The ultra thin ferroelectric PbZr{sub 0.52}Ti{sub 0.48}O{sub 3} (PZT) films with various thicknesses ranging from 100 (P100) to 10 (P10) nm were grown on La{sub 0.67}Sr{sub 0.33}MnO{sub 3}/(LaAlO{sub 3}){sub 0.3}(Sr{sub 2}AlTaO{sub 6}){sub 0.7} (LSMO/LSAT) (001) substrates deposited by pulsed laser deposition technique. The x-ray diffraction patterns of the heterostructures show only (00l) (l = 1 and/or 2) reflections corresponding to the LSAT substrate, PZT, and LSMO layers. The atomic force microscopy studies show that the root mean square surface roughnesses of P100 and P10 films are 2.39 and 0.99 nm, respectively. An increase of both real (ε′) and imaginary (ε″) permittivities was observed when thickness of PZT increases from 10 nm to 100 nm. Temperature dependent ε′ presents an anomaly, related to ferromagnetic-metal to paramagnetic-insulator transition of the LSMO, in the range of 350–500 K. The dielectric anomalies and magnetic phase transition temperature shifted to the lower temperature values with decrease in the PZT films thicknesses. The values of the remanent polarization (P{sub r}) and coercive field (E{sub c}) of the heterostructures were in the range of 24–42 μC/cm{sup 2}–170–1300 kV/cm. An appreciable increase of saturated magnetization (M{sub s}) was observed with increase of PZT layer thickness. The average M{sub s} values of PZT/LSMO heterostructure were 170, 150, 100, and 45 emu/cm{sup 3} for 100, 50, 25, and 10 nm at 300 K, respectively. Enhancement in magnetization with increase in PZT thickness may be due to the interface effect between PZT/LSMO layers.

36 MATERIALS SCIENCE↗

Influence of the interface on the magnetic properties of ferromagnetic ultrathin films with various adjacent copper thicknesses

The interface and magnetic properties of two series of films with Ta(5 nm)/Fe{sub 20}Ni{sub 80}Nd{sub 0.017}(3 nm)/Cu(t nm) and Ta(5 nm)/Cu(t nm)/Fe{sub 50}Co{sub 50}Gd{sub 0.07}(3 nm)/Cu(2 nm) structures have been investigated by atomic force microscopy, vibrating sample magnetometer, and ferromagnetic resonance (FMR). The roughness of all films increases with increasing copper thickness, which causes the different grain sizes in the surface of films. The coercivity of FeCo-Gd films increases with increasing thickness of inserted Cu layer while decreases with increasing thickness of Cu capping layer for FeNi-Nd films. FMR linewidth exhibits huge dependence on the thickness of inserted Cu layer for FeCo-Gd films, increasing from 2270 to 3680 Oe, which comes from the additional contribution of effect of the two-magnon scattering. And the thickness of Cu capping layer shows also an influence on FMR linewidth of FeNi-Nd films, increasing from 190 to 320 Oe, which mainly comes from intrinsic FMR linewidth and plus minor inhomogeneous broadening. All of these extrinsic linewidth broadening are related to the interface roughness.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Thickness dependent metal-insulator transition and dimensional crossover for weak localization in Si{sub 0.02}Zn{sub 0.98}O thin films grown by pulsed laser deposition

Metal to insulator transition was observed in Si{sub 0.02}Zn{sub 0.98}O (SZO) films, grown by pulsed laser deposition on sapphire substrates, as the thicknesses of the films were reduced from ∼40 to 15 nm. The SZO film with thickness of ∼40 nm showed typical metallic behavior in temperature dependent resistivity measurements. On the contrary, the SZO film with thickness of ∼15 nm was found to exhibit strong localization where the transport at low temperature was dominated by variable range hopping conduction. In the intermediate thickness regime, quantum corrections were important and a dimensional crossover from 3D to 2D weak localization occurred in the SZO film with thickness of 20 nm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Dependency of anti-ferro-magnetic coupling strength on Ru spacer thickness of [Co/Pd]{sub n}-synthetic-anti-ferro-magnetic layer in perpendicular magnetic-tunnel-junctions fabricated on 12-inch TiN electrode wafer

We investigated the Ru spacer-thickness effect on the anti-ferro-magnetic coupling strength (J{sub ex}) of a [Co/Pd]{sub n}-synthetic-anti-ferro-magnetic layer fabricated with Co{sub 2}Fe{sub 6}B{sub 2}/MgO based perpendicular-magnetic-tunneling-junction spin-valves on 12-in. TiN electrode wafers. J{sub ex} peaked at a certain Ru spacer-thickness: specifically, a J{sub ex} of 0.78 erg/cm{sup 2} at 0.6 nm, satisfying the J{sub ex} criteria for realizing the mass production of terra-bit-level perpendicular-spin-transfer-torque magnetic-random-access-memory. Otherwise, J{sub ex} rapidly degraded when the Ru spacer-thickness was less than or higher than 0.6 nm. As a result, the allowable Ru thickness variation should be controlled less than 0.12 nm to satisfy the J{sub ex} criteria. However, the Ru spacer-thickness did not influence the tunneling-magneto-resistance (TMR) and resistance-area (RA) of the perpendicular-magnetic-tunneling-junction (p-MTJ) spin-valves since the Ru spacer in the synthetic-anti-ferro-magnetic layer mainly affects the anti-ferro-magnetic coupling efficiency rather than the crystalline linearity of the Co{sub 2}Fe{sub 6}B{sub 2} free layer/MgO tunneling barrier/Co{sub 2}Fe{sub 6}B{sub 2} pinned layer, although Co{sub 2}Fe{sub 6}B{sub 2}/MgO based p-MTJ spin-valves ex-situ annealed at 275 °C achieved a TMR of ∼70% at a RA of ∼20 Ω μm{sup 2}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electric field control of spin re-orientation in perpendicular magnetic tunnel junctions—CoFeB and MgO thickness dependence

We report an investigation of electric-field (EF) control of spin re-orientation as functions of the thicknesses of CoFeB free layer (FL) and MgO layer in synthetic-antiferromagnetic pinned magnetic tunnel junctions with perpendicular magnetic anisotropy. It is found that the EF modulates the coercivity (Hc) of the FL almost linearly for all FL thicknesses, while the EF efficiency, i.e., the slope of the linearity, increases as the FL thickness increases. This linear variation in Hc is also observed for larger MgO thicknesses (≥1.5 nm), while the EF efficiency increases only slightly from 370 to 410 Oe nm/V when MgO thickness increases from 1.5 to 1.76 nm. We have further observed the absence of quasi-DC unipolar switching. We discuss its origin and highlight the underlying challenges to implement the EF controlled switching in a practical magnetic memory.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electrocaloric properties of ferroelectric-paraelectric superlattices controlled by the thickness of paraelectric layer in a wide temperature range

As functions of the paraelectric layer thickness, misfit strain and temperature, the electrocaloric properties of ferroelectric-paraelectric superlattices are investigated using a time-dependent Ginzburg-Landau thermodynamic model. Ferroelectric phase transition driven by the relative thickness of the superlattice is found to dramatically impact the electrocaloric response. Near the phase transition temperature, the magnitude of the electrocaloric effect is maximized and shifted to lower temperatures by increasing the relative thickness of paraelectric layer. Theoretical calculations also imply that the electrocaloric effect of the superlattices depends not only on the relative thickness of paraelectric layer but also on misfit strain. Furthermore, control of the relative thickness of paraelectric layer and the misfit strain can change availably both the magnitude and the temperature sensitivity of the electrocaloric effect, which suggests that ferroelectric-paraelectric superlattices may be promising candidates for use in cooling devices in a wide temperature range.

36 MATERIALS SCIENCE↗

General analytical approach for sound transmission loss analysis through a thick metamaterial plate

We report theoretically and numerically on the sound transmission loss performance through a thick plate-type acoustic metamaterial made of spring-mass resonators attached to the surface of a homogeneous elastic plate. Two general analytical approaches based on plane wave expansion were developed to calculate both the sound transmission loss through the metamaterial plate (thick and thin) and its band structure. The first one can be applied to thick plate systems to study the sound transmission for any normal or oblique incident sound pressure. The second approach gives the metamaterial dispersion behavior to describe the vibrational motions of the plate, which helps to understand the physics behind sound radiation through air by the structure. Computed results show that high sound transmission loss up to 72 dB at 2 kHz is reached with a thick metamaterial plate while only 23 dB can be obtained for a simple homogeneous plate with the same thickness. Such plate-type acoustic metamaterial can be a very effective solution for high performance sound insulation and structural vibration shielding in the very low-frequency range.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Thickness effect on magnetocrystalline anisotropy of Co/Pd(111) films: A density functional study

In this study, we carried out first-principles calculations on magnetocrystalline anisotropy (MCA) of Co/Pd thin films by adopting two different systems of (i) n-Co/3-Pd and (ii) n-Pd/3-Co. In one system, we vary the thickness of Co layer, fixing the thickness of the Pd layer to 3-monolayers, and in the other system vice versa. MCA is mainly governed by the surface and interface Co atoms, while contributions from other Co atoms are smaller. MCA energy (E{sub MCA}) of the Co/Pd thin film shows oscillatory behavior with the thickness of the Co layer, but is insensitive to the thickness of the Pd layer. In particular, the n-Co/3-Pd films of n = 2, 4, and 6 exhibit strong perpendicular MCA of about 1 meV. Our results suggest that controlling the thickness of the Co layer in Co/Pd (111) is crucial in achieving strong perpendicular MCA.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Thickness- and temperature-dependent magnetodynamic properties of yttrium iron garnet thin films

The magnetodynamical properties of nanometer-thick yttrium iron garnet films are studied using ferromagnetic resonance as a function of temperature. The films were grown on gadolinium gallium garnet substrates by pulsed laser deposition. First, we found that the damping coefficient increases as the temperature increases for different film thicknesses. Second, we found two different dependencies of the damping on film thickness: at room temperature, the damping coefficient increases as the film thickness decreases, while at T = 8 K, we find the damping to depend only weakly on the thickness. We attribute this behavior to an enhancement of the relaxation of the magnetization by impurities or defects at the surfaces.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Thickness-dependent blue shift in the excitonic peak of conformally grown ZnO:Al on ion-beam fabricated self-organized Si ripples

Al-doped ZnO (AZO) thin films of thicknesses 5,10, 15, 20, and 30 nm were deposited on 500 eV argon ion-beam fabricated nanoscale self-organized rippled-Si substrates at room temperature and are compared with similar films deposited on pristine-Si substrates (without ripples). It is observed that morphology of self-organized AZO films is driven by the underlying substrate morphology. For instance, for pristine-Si substrates, a granular morphology evolves for all AZO films. On the other hand, for rippled-Si substrates, morphologies having chain-like arrangement (anisotropic in nature) are observed up to a thickness of 20 nm, while a granular morphology evolves (isotropic in nature) for 30 nm-thick film. Photoluminescence studies reveal that excitonic peaks corresponding to 5–15 nm-thick AZO films, grown on rippled-Si templates, show a blue shift of 8 nm and 3 nm, respectively, whereas the peak shift is negligible for 20-nm thick film (with respect to their pristine counter parts). The observed blue shifts are substantiated by diffuse reflectance study and attributed to quantum confinement effect, associated with the size of the AZO grains and their spatial arrangements driven by the anisotropic morphology of underlying rippled-Si templates. The present findings will be useful for making tunable AZO-based light-emitting devices.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

HfO{sub 2} dielectric thickness dependence of electrical properties in graphene field effect transistors with double conductance minima

We investigate the electrical properties in back-gated graphene field effect transistors (GFETs) with SiO{sub 2} dielectric and different thickness of high-k HfO{sub 2} dielectric. The results show that transform characteristic (I{sub ds}–V{sub gs}) curves of GFETs are uniquely W-shaped with two charge neutrality point (left and right) in both SiO{sub 2} and HfO{sub 2} dielectric (SiO{sub 2}-GFETs and HfO{sub 2}-GFETs). The gate voltage reduces drastically in HfO{sub 2}-GFETs compared with that in SiO{sub 2}-GFETs, and it becomes much smaller with the decline of HfO{sub 2} thickness. The left charge neutrality point in I{sub d}–V{sub g} curves of all HfO{sub 2}-GFETs is negative, compared to the positive ones in SiO{sub 2}-GFETs, which means that there exists n-doping in graphene with HfO{sub 2} as bottom dielectric. We speculate that this n-doping comes from the HfO{sub 2} layer, which brings fixed charged impurities in close proximity to graphene. The carrier mobility is also researched, demonstrating a decreasing trend of hole mobility in HfO{sub 2}-GFETs contrast to that in SiO{sub 2}-GFETs. In a series of HfO{sub 2}-GFETs with different HfO{sub 2} dielectric thickness, the hole mobility shows a tendency of rise when the thickness decreases to 7 nm. The possible reason might be due to the introduced impurities into HfO{sub 2} film from atomic layer deposition process, the concentration of which varies from the thickness of HfO{sub 2} layer.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Optimization of barrier layer thickness in MgSe/CdSe quantum wells for intersubband devices in the near infrared region

The authors report the optimization of MgSe barrier thickness in CdSe/MgSe multiple quantum well structures and its effect on structural, optical qualities and intersubband (ISB) transition characteristics. Three samples with the MgSe thicknesses of 2 nm, 3 nm, and 4 nm were grown on InP substrates by molecular beam epitaxy. X-ray diffraction and photoluminescence measurements showed that the thinner the MgSe barrier thickness the better the structural quality. However, ISB absorption was only observed in the sample with a MgSe thickness of 3 nm. Failing to observe ISB absorption in the sample with a thicker MgSe barrier (≥4 nm) is due to the deteriorated material quality while the missing of ISB transition in the sample with thinner barrier (≤2 nm) is due to the tunneling of electrons out of the CdSe wells. The optimized MgSe barrier thickness of around 3 nm is found to be able to suppress the electron tunneling while maintaining a good material quality of the overall structure.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗