Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STIRRING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Friction stir processing: A thermomechanical processing tool for high pressure die cast Al-alloys for vehicle light-weighting

This study uses friction stir processing (FSP) for thermomechanical processing of high-pressure die-casting (HPDC) to modify microstructure and improve mechanical properties. FSP is carried out on two different HPDC aluminum alloys: (a) general-purpose, high-iron, HPDC A380 alloy and (b) premium quality, low-iron HPDC Aural-5 alloy in thin wall, flat plate geometry. Subsequent mechanical testing shows ~30 % and ~65 % enhancement in yield strength and tensile ductility. In addition, FSP leads to ~10 times improvement in fatigue life for A380 alloy and ~70 % improvement in fracture toughness for Aural-5 alloy. These findings emphasize the capability of FSP to modify the microstructure of HPDC Al-alloys-based structural components so that they can demonstrate a good combination of strength, ductility, fracture toughness, and high fatigue properties for long-term durability and reliability.

36 MATERIALS SCIENCE↗

Three-dimensional microstructure of a friction stir welded magnesium/steel interface characterized via high-energy synchrotron X-rays

Here, the three-dimensional (3D) microstructure of a friction stir assisted scribe technique (FaST) weld interface consisting of AZ31 magnesium (Mg) alloy and zinc (Zn)-coated DP590 steel was analyzed via synchrotron micro-computed tomography (μ-CT), correlated to synchrotron x-ray diffraction, and electron microscopy. Diffraction assessment of the AZ31/Zn-coated DP590 steel interface revealed the presence of several complex Mg–Zn intermetallic phases and differences in crystalline orientation of the Mg phase at the weld interface. The 3D characterization of the synchrotron μ-CT images of the weld interface revealed: (1) the presence of AZ31 weld nugget material with iron (Fe)-rich particles; (2) the presence of a weld layer at the joining interface with Fe-rich particles; (3) the formation of a thin non-uniform layer between the weld layer and the interface of the scribed DP590 material; and (4) the presence of an Fe–Al-rich intermetallic layer and Fe-rich particles at the interface of the scribed DP590 material. This study also performed a detailed analysis of lump-like features seen in the Zn coating layer at the weld interface. A detailed 3D particle analysis of the Fe-rich particles in the AZ31 weld nugget and the weld layer at the weld interface revealed the presence of several types of particle morphologies (i.e., spherical and irregular).

36 MATERIALS SCIENCE↗

Effect of tool design and pass strategy on defect elimination and uniform, enhanced tensile properties of friction stir processed high-pressure die-cast A380 alloy

This work reports implementation of friction stir processing (FSP) to locally modify microstructure and create a defect-free processing zone with the aid of different tool designs and altering the passing strategy for two different process parameter combinations. Here, FSP is applied on high pressure die-cast (HPDC) A380 alloy, a widely used Al-Si alloy fabricated in the die casting sector for automotive and aerospace applications. However, the presence of gas and shrinkage porosity, brittle needle-shaped Fe-containing ß-FeSiAl 5 intermetallic compounds, Al-dendrites, coarse and acicular silicon particles, and large second-phase particulates have a detrimental influence on the uniformity of tensile properties across the thickness direction of an HPDC plate. FSP is able to eliminate porosity, refine microstructure and improve tensile properties. An FSP tool design and a passing strategy are identified for the best microstructure consolidation and uniform enhanced tensile properties. This study noted the importance of tool features such as scroll design and flats on tool pin and multiple pass orientation strategy to find best combination of defect-free refined microstructure and uniform tensile strength and ductility across the processing zone of HPDC Al alloys.

36 MATERIALS SCIENCE↗

Friction stir processing on a strontium modified, thin-wall, vacuum-assisted high-pressure die-cast Aural-5 alloy to improve tensile and fatigue performance

Here, this study explores the application of friction stir processing (FSP) to enhance the material properties of Sr-modified Aural-5 alloy, with a focus on improved tensile and fatigue properties. Aural-5 is a well-known vacuum-assisted high-pressure die-cast (HPDC) Al-Si7-Mg alloy used in the automotive industry to reduce vehicle weight, enhance fuel efficiency, and lower carbon emissions. This alloy modifies its material chemistry with Sr for fine fibrous networks of eutectic silicon and manganese (Mn) to reduce die soldering. It has significantly less iron (Fe) content resulting in the elimination of detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. The initial microstructure of as-received HPDC Aural-5 exhibits shrinkage porosity in the middle section, a dendritic microstructure with fibrous Al-Si eutectic colonies, a shear-band structure beneath the die-wall, large dendritic externally solidified crystals (ESCs), needle-shaped Mg 2 Si phase and significant second-phase particulates. Some of those microstructural features, such as porosity, ESCs, needle-shaped Mg 2 Si phase, and large second-phase particles, serve as initiation sites for cracks under mechanical loading, resulting in adverse effects on tensile properties, particularly ductility. FSP effectively transforms the microstructure into a wrought configuration with uniform particle distribution by eliminating porosity and disintegrating dendrites, eutectic colonies, ESCs, second-phase particles, and shear-band structures. FSP-driven microstructure modification enhances yield strength and tensile ductility by ~30% and ~35%, respectively. The fatigue life of the material in a bending mode configuration (stress ratio R = 0.1) after FSP exhibits enhancements ranging from 2.0 to 3.9 times that of the original HPDC Aural-5 alloy, depending on the applied stress level.

36 MATERIALS SCIENCE↗

Use of friction stir processing to synthesize nanocrystalline, grain boundary segregating Fe-Ti alloys

Grain boundary segregating alloys, a class of alloys designed such that nanocrystalline grain sizes are thermodynamically stabilized by the presence of high segregation energy solutes at the grain boundaries, are typically produced through geometrically limited processing techniques such as equal channel angular extrusion or thin film sputtering. Here, this study explores the use of friction stir processing (FSP) as a novel means of studying and producing these alloys using a test system of Fe-6at%Ti. Spot FSPs with a range of processing parameter sets were produced on bulk, coarse grained bars of material and optimal parameters were identified. Microscopy identified a range of processed materials which achieved nanocrystalline grains on the order of 100 nm, delineating a critical window of processing parameters which limit heat input while inducing sufficient plastic deformation for grain refinement. The finest grained nanocrystalline Fe-Ti achieved a hardness of 7.68 GPa, a significant increase in hardness over pure Fe with a similar microstructure due to increased dislocation density from FSP as well as several strengthening mechanisms produced through the presence and segregation of Ti. These results demonstrated the feasibility of using FSP to produce nanocrystalline grain boundary segregating alloys.

Fe alloys↗

Understanding the effect of friction stir processing on electrical steel: Microstructural changes and mechanical transformations

Raising Si beyond 3.5 wt% reduces core loss but embrittles electrical steels, constraining processing and application. Here we assess friction stir processing (FSP) as a solid‑state route to enable Fe–4.0 wt% Si with improved mechanical performance. Temperature‑controlled FSP with a PcBN tool produced a defect‑free processed zone. SEM/EBSD revealed dynamic recrystallization and grain refinement from an average 110 μm in the base material to ∼20 μm in the processed region, with ∼ 80% of grains < 40 μm and a reduction in high‑angle boundary fraction to ∼65% (vs >85% in the base). Comparative mechanical property analysis shows a moderate increase in yield strength in FSP samples relative to the base material, with a significant improvement in ductility (∼35–50%). Post‑fracture EBSD identified 60° twin boundaries in the base while sub-grain formation with elevated KAM in the FSP sample. Fractography revealed a shift from quasi‑cleavage in the Base-faceted planes with river patterns, steps, and occasional secondary cracks—to ductile micro void coalescence after FSP. Following FSP, the material retains soft‑magnetic behavior, with modest shifts in saturation magnetization consistent with grain refinement and stored strain, accompanied by a clear gain in formability. These results indicate that FSP provides a viable route to deploy higher‑Si electrical steels with concurrent gains in strength and ductility.

Electrical steel↗

Force reduction of friction stir welding and processing of steel

Friction stir welding and processing (FSW&P) is considered as a new fabrication method for canisters and repair of existing dry cask storage system canisters (generally made of austenitic stainless steel). Low heat input compared to fusion joining processes and grain refinement associated with low-temperature FSW&P result in a material with improved mechanical properties and equivalent generalized corrosion performance relative to the base metal. But FSW&P of austenitic stainless steel requires significant tool forge axis force to produce a weld (or a run). Exploratory runs utilizing forge axis force control were conducted to investigate the minimum force required to achieve defect-free runs. The correlation between forge axis force and resultant plunge depth was also investigated. Furthermore, detailed microstructural characterization was conducted to display the microstructural variation within the nugget zone.

36 MATERIALS SCIENCE↗

Elucidating reactivity regimes in cyclopentane oxidation: Jet stirred reactor experiments, computational chemistry, and kinetic modeling

This study is concerned with the identification and quantification of species generated during the combustion of cyclopentane in a jet stirred reactor (JSR). Experiments were carried out for temperatures between 740 and 1250 K, equivalence ratios from 0.5 to 3.0, and at an operating pressure of 10 atm. The fuel concentration was kept at 0.1% and the residence time of the fuel/O 2 /N 2 mixture was maintained at 0.7 s. The reactant, product, and intermediate species concentration profiles were measured using gas chromatography and Fourier transform infrared spectroscopy. The concentration profiles of cyclopentane indicate inhibition of reactivity between 850-1000 K for φ=2.0 and φ=3.0. This behavior is interesting, as it has not been observed previously for other fuel molecules, cyclic or non-cyclic. A kinetic model including both low- and high-temperature reaction pathways was developed and used to simulate the JSR experiments. The pressure-dependent rate coefficients of all relevant reactions lying on the PES of cyclopentyl + O 2 , as well as the C-C and C-H scission reactions of the cyclopentyl radical were calculated at the UCCSD(T)-F12b/cc-pVTZ-F12//M06-2X/6-311++G(d,p) level of theory. The simulations reproduced the unique reactivity trend of cyclopentane and the measured concentration profiles of intermediate and product species. Furthermore, sensitivity and reaction path analyses indicate that this reactivity trend may be attributed to differences in the reactivity of allyl radical at different conditions, and it is highly sensitive to the C-C/C-H scission branching ratio of the cyclopentyl radical decomposition.

30 DIRECT ENERGY CONVERSION↗

Studies of Low and Intermediate Temperature Oxidation of Propane up to 100 Atm in a Supercritical-Pressure Jet-Stirred Reactor

Here, the low and intermediate temperature oxidation of propane has been investigated by using a novel supercritical pressure jet stirred reactor (SP-JSR) with and without 20% CO 2 additions at fuel lean and rich conditions at 10 and 100 atm and 500–1000 K. The mole fractions of C 3 H 8 , O 2 , CO, CO 2 , CH 2 O, C 2 H 4 , CH 3 CHO, and C 3 H 6 were quantified by using a micro-gas chromatograph (µ-GC). The experiment showed that different from that of 10 atm, at 100 atm only a weak negative temperature coefficient (NTC) behavior was observed because of the significant shift of the intermediate temperature HO 2 chemistry to lower temperature. In addition, at 100 atm, existing models in literatures could successfully capture the onset temperatures of the low and intermediate chemistry, while under-predict the fuel oxidation quantitatively and fail to capture the NTC behavior between 650 and 780 K at both fuel lean and rich conditions. Similar discrepancy was observed in studies of n-butane and dimethyl ether (DME) oxidations in literatures, implying that there existed large uncertainties in hierarchy model development of fuels with low temperature chemistries at extremely high pressures. Reaction pathways and sensitivity analyses showed that RO 2 competing reactions through (P1) RO 2 = QOOH, (P2) RO 2 = C 3 H 6 + HO 2 , (P3) RO 2 + CH 2 O/HO 2 = RO 2 H + HCO / O 2 dominated the low and intermediate temperature chemistries, followed by HO 2 / H 2 O 2 chemistry at 100 atm, which differed from the dominant pathway through QOOH consumption reactions at lower pressures. Especially, P3 is a new pathway of RO 2 consumption at high pressures, which was not observed in importance at low pressures. Special attention should be paid to the accurate computations of n-C 3 H 7 O 2 / i-C 3 H 7 O 2 + CH 2 O and n-C 3 H 7 O 2 / i-C 3 H 7 O 2 + in the P3 pathway and n-C 3 H 7 O 2 / i-C 3 H 7 O 2 decomposition reactions in the P2 pathway at high pressures.

33 ADVANCED PROPULSION SYSTEMS↗

Low-Temperature Oxidation of Ethylene by Ozone in a Jet-Stirred Reactor

Ethylene oxidation initiated by ozone addition (ozonolysis) is carried out in a jet-stirred reactor from 300-1000 K to explore the kinetic pathways relevant to low-temperature oxidation. The temperature dependencies of species’ mole fractions are quantified using molecular-beam mass spectrometry with electron ionization and single-photon ionization employing tunable synchrotron-generated vacuum-ultraviolet radiation. Upon ozone addition, significant ethylene oxidation is found in the low-temperature regime from 300-600 K. Here, we provide new insights into the ethylene ozonolysis reaction network via identification and quantification of previously elusive intermediates by combining experimental photoionization energy scans and ab initio threshold energy calculations for isomer identification. Specifically, the C 2 H 4 +O 3 adduct C 2 H 4 O 3 is identified as a keto-hydroperoxide (hydroperoxy-acetaldehyde, HOOCH 2 CHO) based on the calculated and experimentally observed ionization energy of 9.80 (±0.05) eV. Quantification using a photoionization cross-section of 5 Mb at 10.5 eV results in 5 ppm at atmospheric conditions which decreases monotonically with temperature until 550 K. Other hydroperoxide species, that contribute in larger amounts to the low-temperature oxidation of C 2 H 4 , like H 2 O 2 , CH 3 OOH, and C 2 H 5 OOH, are identified and their temperature-dependent mole fractions are reported. The experimental evidence for additional oxygenated species such as methanol, ketene, acetaldehyde, and hydroxy-acetaldehyde suggest multiple active oxidation routes. This experimental investigation closes the gap between ozonolysis at atmospheric and elevated temperature conditions and provides a database for future modeling.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of thread interruptions on tool pins in friction stir welding of AA6061

In this paper, effects of pin thread and thread interruptions (flats) on weld quality and process response parameters during friction stir welding (FSW) of 6061 aluminium alloy were quantified. Otherwise, identical smooth and threaded pins with zero to four flats were adopted for FSW. Weldability and process response variables were examined. Results showed that threads with flats significantly improved weld quality and reduced in-plane forces. A three-flat threaded pin led to production of defect-free welds under all examined welding conditions. Spectral analyses of in-plane forces and weld cross-sectional analysis were performed to establish correlation among pin flats, force dynamics and defect formation. Finally, the lowest in-plane force spectra amplitudes were consistently observed for defect-free welds.

42 ENGINEERING↗

Microstructure based modeling of friction stir welded joint of dissimilar metals using crystal plasticity

We report the friction stir welding (FSW) process shows promising results in joining dissimilar metals which are otherwise almost impossible to join using traditional welding techniques. Being a new technique, the deformation and the failure mechanism of the joints made by the FSW process needs to be investigated. In this work, a joint between AZ31 Mg alloy and DP590 steel is modeled using phenomenological crystal plasticity formulation on the mesoscale in the form of a representative volume element (RVE). The interface of the two materials is modeled using a cohesive zone model. A parametric study has been performed to understand the effect of grain size and interface fracture toughness as well as strength on the mechanical performance of the joint. It was found that the grain size of AZ31 Mg alloy, as well as DP590 steel, has little effect on the overall joint performance. On the other hand, interface fracture toughness and strength have a significant impact on the mechanical properties of the joint

36 MATERIALS SCIENCE↗

COUPLING SMOOTHED PARTICLE HYDRODYNAMICS WITH FINITE ELEMENT METHOD TO SIMULATE RESIDUAL STRESSES FROM FRICTION STIR PROCESSING

Friction stir processing (FSP) is a solid-state material processing technique that locally modifies the microstructure but also induces undesirable residual stresses. A robust numerical model for the FSP can help in mitigating these residual stresses. Heat source models within a finite element method (FEM) framework suffer from inaccuracies. In contrast, smoothed particle hydrodynamics (SPH) model that explicitly captures the material flow near the tool and the associated heat generation are accurate. However, the computational expense of SPH simulations can be prohibitive. In this work, we propose a coupled SPH-FEM framework. SPH is used to model the heat generation accurately near the tool and which is then inserted into to the FEM model as a heat source. To verify this proposed coupling approach, a test case is set up with typical FSP conditions and it is modeled in both SPH and SPH-FEM. The temperatures profiles were compared after the simulations have reached steady-state temperatures. The similarity of the temperature profiles from SPH-FEA and SPH validated the proposed coupling approach. This proposed approach achieves the accuracy of the SPH method while potentially retaining the low computational expense of FEM.

smoothed particle hydrodynamics, Finite Element Me↗

Impact of tool wear on joint strength in friction stir spot welding of DP 980 steel

Friction stir spot welding has been shown to be a viable method of joining ultra high strength steel (UHSS), both in terms of joint strength and process cycle time. However, the cost of tooling must be reasonable in order for this method to be adopted as an industrial process. Recently a new tool alloy has been developed, using a blend of PCBN and tungsten rhenium (W-Re) in order to improve the toughness of the tool. Wear testing results are presented for two of these alloys: one with a composition of 60% PCBN and 40% W-Re, and one with 70% PCBN and 30% W-Re. The sheet material used for all wear testing was 1.4 mm DP 980. Lap shear testing was used to show the relationship between tool wear and joint strength. The Q70 tool provided the best combination of wear resistance and joint strength.

36 MATERIALS SCIENCE↗

Fatigue Behaviour of Magnesium to Steel Dissimilar Friction Stir Lap Joints

A short study has been conducted to assess the performance of friction stir welded Mg/steel joints under dynamic loads. The major mode of failure was found to be top Mg sheet fracture. Crack initiation is noted to have taken place at the Mg/steel interface. The fatigue life of the joints is found to be significantly different than the fatigue data of the Mg alloy obtained from the literature. The reasons behind such a difference have been examined in this work.

36 MATERIALS SCIENCE↗

Effect of tool pin features on process response variables during friction stir welding of dissimilar aluminum alloys

In this article, the effect of pin features and orientation/placement of the materials on advancing side were investigated for friction stir welding (FSW) of dissimilar aluminum alloys AA2050 and AA6061. Pins for FSW were produced with a 2.12 mm pitch thread having three flats/flutes. Three sets of rotational speed/welding speed were used to perform a series of welds in a butt joint arrangement. The results show that, joint quality, process response variables and welding temperature are highly affected by pin features and material orientation in FSW. Defect free joints with effective material transportation in the weld nugget zone were obtained when welding was performed with AA2050 on the advancing side. The tool also encounters less in-plane reaction force for welding with 2050 on the advancing side. Pin with thread+3 flats produces quality welds at low rotational and travel speed regardless of the location of alloys on advancing or retreating side.

36 MATERIALS SCIENCE↗

Modeling Induction Stirring and Particle Tracking in Molten Uranium

Two independent numerical models have been developed to simulate the behavior of carbon impurities in molten uranium metal. Informed by experimental parameters, one model was created using the commercial software Star-CCM+ and compared with another developed using open-source codes, including OpenFOAM, Finite Element Method Magnetics (FEMM) and a First Passage Kinetic Monte Carlo (FPKMC) approach. The target experimental system features a 404g uranium metal charge containing an average carbon concentration of 139 ppm which was melted in a vacuum induction furnace at 1400° C then resolidified. The microstructures of the uranium and its impurities before and after melting have been characterized and reported separately. Prior to simulating the uranium-carbon system described, the numerical models were validated using a previously published nonradioactive experimental system to ensure agreement with expected output values. Focus has been placed on modeling velocity fields under induction stirring and impurity particle trajectories.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructural, Corrosion, and Mechanical Characterization of Friction Stir Welded Al 6022-to-ZEK100 Mg Joints

Friction stir welded (FSW) aluminum–magnesium lightweight vehicle joints have gained significant interest due to their high strength-to-weight ratio. In this work, the corrosion resistance of this material is analyzed through electrochemical tests, which include open circuit potential (OCP) inspection and potentiodynamic polarization (PD) scanning. Weight loss measurements tested the corrosion rate of the FSW weld through cyclic corrosion testing (CCT) according to the standard SAEJ 2334. Mechanical properties were also investigated, including lap-shear strength, micro- and nano-hardness mapping, and true stress–strain curves as a function of local processing history. The electrochemical results indicate that the center weld zone’s corrosion property stays between the two base alloys. Indentation-based testing demonstrated that the weld zone behaves differently from base alloys. Lap shear strength surprisingly did not drop much even after eight weeks of cyclic corrosion tests, indicating that the joint did not allow any ingress of the electrolyte.

36 MATERIALS SCIENCE↗