Extended ion pumped vacuum friction test

Boundary layer friction data under ion pumped vacuum was taken for sixteen material couples. The test series was an extension of a previous study of the effects of modified ion pumped environments. Sliding distances imposed in the present effort greatly exceeded any studied in the previous contiguous, flight or ground tests. Wear out of specific couples, in particular, thin film lubricants was noted. The behavior of the test hardware including wear out of the mechanisms was noted. As a result, the impact of test interruption was observed for several test couples. Recovery of the friction upon re-establishing sliding in vacuum was generally rapid. The results of the extended sliding study reinforce the previous conclusion that sliding distance (mechanical history) is the primary factor in establishing the force limiting boundary layer friction. General friction value under the extended sliding confirm those observed in previous orbital and the related ground test studies.

Hammel, R. L.↗

Demonstration of the Feasibility of High Temperature Bearing Lubrication From Carbonaceous Gases

Research has been conducted on silicon nitride pin-on-disk sliding contacts at temperatures of up to 520 C, and four-ball rolling contacts with silicon nitride balls and 52100 steel or silicon nitride races at 590 C. These tests were conducted in a variety of gaseous environments in order to determine the effects of simulated engine exhaust gas on the carbonaceous gas decomposition lubrication scheme. In rolling tests with steel races and exhaust gas the wear track depth was roughly half that of tests run in nitrogen gas alone. The deposition of lubricous microcrystalline graphitic carbon on the rolling surfaces, generated from the carbon monoxide within the exhaust gas mixture, was verified by microfocused Raman spectroscopy. Ten-fold reductions in rolling wear could be achieved by the exhaust gas atmosphere in cases where water vapor was removed or not present. The exhaust gas mixture alone was not found to provide any lubricating effect on silicon nitride sliding contacts, where the rate of wear greatly exceeds the rate of carbon deposition. Directed admixture of acetylene (as low as 5% of the exhaust gas flow rates), has provided reductions in both wear volume and coefficient of friction by factors of 60X and 20X respectively for sliding contacts during the initial 80 m of sliding distance. Exhaust gas atmosphere with the acetylene admixture provided 65OX reductions in steady state wear rate compared to that measured for sliding contacts in dry N2. Such acetylene admixture also augments the ability of the exhaust gas atmosphere to lubricate high-temperature rolling contacts, with up to 25-fold reductions in wear track depth compared to those measured in the presence of N2 alone. In addition to providing some lubricating benefit itself, an important potential role of the exhaust gas from rich mixtures would be to shield bearings from 02. Such shielding enables surface deposition of lubricous pyrolytic carbon from the acetylene admixture, instead of combustion, rendering feasible the continuously replenished solid lubrication of high-temperature bearing surfaces.

Blanchet, Thierry A.↗

Wear of iron and nickel in corrosive liquid environments

Friction and wear behavior of Fe and Ni sliding on aluminum oxide in aerated sulfuric acid and hydrochloric acid were investigated. The results show that the concentration of acid is an important factor in controlling the metal loss caused by wear corrosion processes in the acids. At very dilute acid concentration (10 to the -4 N), Fe behaves differently from Ni. Fe develops a soft, friable deposit, while Ni develops no corrosion layer. The formation and removal of the corrosion deposit on Fe resulted in high metal loss and coefficient of friction, as compared to the relatively low metal loss and coefficient of friction observed for Ni. At slightly higher acid concentration (10 to the -3 and 10 to the -2 N), no corrosion products were produced on both Fe and Ni. Wear of Fe and Ni was generally at a minimum. At higher acid concentration (10 to the -1 N and above), loss of Fe and Ni increased as the acid concentration increased. In sulfuric acid the maximum loss of both Fe and Ni was at 7.5 N (30%) concentration, and the metal losses of both Fe and Ni dropped markedly at 15 N (50%) and above. In hydrochloric acid, however, the Fe loss continued to increase with the increase of acid concentration, and the maximum Fe loss occurred in the most concentrated acid (12.1 N, 37%). There were variations in loss with Ni from specimen to specimen examined in hydrochloric acids (10 to the -1 N and above). The coefficient of friction for Ni increased slightly with an increase in acid concentration up to 10 to the -2 N. When corrosion started to dominate in the wear-corrosion process, the coefficient of friction decreased in both sulfuric and hydrochloric acids at 10 to the -1 N and above.

Miyoshi, Kazuhisa↗

Wear of iron and nickel in corrosive liquid environments

Friction and wear behavior of Fe and Ni sliding on aluminum oxide in aerated sulfuric acid and hydrochloric acid were investigated. The results show that the concentration of acid is an important factor in controlling the metal loss caused by wear corrosion processes in the acids. At very dilute acid concentration (10 to the -4 N), Fe behaves differently from Ni. Fe develops a soft, friable deposit, while Ni develops no corrosion layer. The formation and removal of the corrosion deposit on Fe resulted in high metal loss and coefficient of friction, as compared to the relatively low metal loss and coefficient of friction observed for Ni. At slightly higher acid concentration (10 to the -3 and 10 to the -2 N), no corrosion products were produced on both Fe and Ni. Wear of Fe and Ni was generally at a minimum. At higher acid concentration (10 to the -1 N and above), loss of Fe and Ni increased as the acid concentration increased. In sulfuric acid the maximum loss of both Fe and Ni was at 7.5 N (30 percent) concentration, and the metal losses of both Fe and Ni dropped markedly at 15 N (50 percent) and above. In hydrochloric acid, however, the Fe loss continued to increase with the increase of acid concentration, and the maximum Fe loss occurred in the most concentrated acid (12.1 N, 37 percent). There were variations in loss with Ni from specimen to specimen examined in hydrochloric acids (10 to the -1 N and above). The coefficient of friction for Ni increased slightly with an increase in acid concentration up to 10 to the -2 N. When corrosion started to dominate in the wear-corrosion process, the coefficient of friction decreased in both sulfuric and hydrochloric acids at 10 to the -1 N and above.

Miyoshi, Kazuhisa↗

Sliding durability of two carbide-oxide candidate high temperature fiber seal materials in air to 900 C

A test program to determine the friction and wear properties of two complex carbide oxide ceramic fibers for high temperature sliding seal applications is described. The fibers are based on Si, C, O, and Ti or Si, C, N, and O ceramic systems. Pin on disk tests using ceramic fiber covered pins and Inconel 718 disks, were conducted in air from 25 to 900 C to evaluate potential seal materials. This testing procedure was used in a previous study of oxide ceramic fibers which were found to exhibit wear behavior based predominantly on their mechanical properties. Like the oxide fibers tested previously, these carbide oxide ceramic fibers, show an increase in friction and wear with increased test temperature. At room temperature, the wear behavior seems to be based upon mechanical properties, namely tensile strength. At 500 and especially 900 C, the fibers wear by both mechanical fracture and by oxidative type wear. Based upon post test microscopic and x ray analyses, interaction between the fiber constituents and elements transferred from the counterface, namely Ni and Cr, may have occurred enhancing the tribochemical wear process. These results are interpreted.

Dellacorte, Christopher↗

Use of Less Reactive Materials and More Stable Gases to Reduce Corrosive Wear When Lubricating with Halogenated Gases

The gases CF2Cl-CF2Cl, CF2Cl2, and CF2Br-CF2Br were used to lubricate metals, cermets, and ceramics in this study. One of the criteria for determining the effectiveness of a reactive-gas-lubricated systems is the stability of the halogen-containing gas molecule. The carbon-to-halogen bond in the ethane molecule has extremely good thermal stability superior to the methane analogs (CF2Cl2 and CF2Br2) used in earlier research. For this reason, the ethane compounds CF2Cl-CF2Cl and CF2Br-CF2Br were considered as high-temperature lubricants. Friction and wear studies were made with a hemisphere (3/16-in. rad.) rider sliding in a circumferential path on the flat surface of a rotating disk (21/2-in. diam. ). The specimens of metal alloys, cermets, and ceramics were run In an atmosphere of the various gases with a load of 1200 grams, sliding velocities from 75 to 8000 feet per minute, and temperatures from 75 to 1400 F. The gas CF2Cl-CF2Cl was found to be an effective lubricant for the cermet LT-LB (59.0 Cr, 19.0 Al2O3, 20.0 Mo, 2.0 Ti) and the ceramic Al2O3 sliding on Stellite Star J (cobalt-base alloy) at temperatures to 1400 F. The bromine-containing gas CF2Br-CF2Br was found to give friction and wear values that can be considered to be in a region of effective boundary lubrication for the cermet K175D (nickel-bonded metal carbide) sliding on the metal Hastelloy R-235 (nickel-base alloy) at temperatures to 1200 F.

Buckley, Donald H.↗

Tribolgy of selected ceramics at temperatures to 900 deg C

Results of fundamental and focused research on the tribological properties of ceramics are discussed. The basic friction and wear characteristics are given for ceramics of interest for use in gas trubine, adiabatic diesel, and Stirling engine applications. The importance of metal oxides in ceramic/metal sliding combinations is illustrated. The formulation and tribological additives are described. Friction and wear date are given for carbide and oxide-based composite coatings for temperatures to at least 900 C.

Sliney, H. E.↗

Tribology of selected ceramics at temperatures to 900 C

Results of fundamental and focused research on the tribological properties of ceramics are discussed. The basic friction and wear characteristics are given for ceramics of interest for use in gas turbine, adiabatic diesel, and Stirling engine applications. The importance of metal oxides in ceramic/metal sliding combinations is illustrated. The formulation and tribological additives are described. Friction and wear data are given for carbide and oxide-based composite coatings for temperatures to at least 900 C.

Sliney, H. E.↗

Contact solution algorithms

Two algorithms for obtaining static contact solutions are described in this presentation. Although they were derived for contact problems involving specific structures (a tire and a solid rubber cylinder), they are sufficiently general to be applied to other shell-of-revolution and solid-body contact problems. The shell-of-revolution contact algorithm is a method of obtaining a point load influence coefficient matrix for the portion of shell surface that is expected to carry a contact load. If the shell is sufficiently linear with respect to contact loading, a single influence coefficient matrix can be used to obtain a good approximation of the contact pressure distribution. Otherwise, the matrix will be updated to reflect nonlinear load-deflection behavior. The solid-body contact algorithm utilizes a Lagrange multiplier to include the contact constraint in a potential energy functional. The solution is found by applying the principle of minimum potential energy. The Lagrange multiplier is identified as the contact load resultant for a specific deflection. At present, only frictionless contact solutions have been obtained with these algorithms. A sliding tread element has been developed to calculate friction shear force in the contact region of the rolling shell-of-revolution tire model.

Tielking, John T.↗

Linear Motor With Air Slide

Improved linear actuator comprises air slide and linear electric motor. Unit exhibits low friction, low backlash, and more nearly even acceleration. Used in machinery in which positions, velocities, and accelerations must be carefully controlled and/or vibrations must be suppressed.

Johnson, Bruce G.↗

Measurement of rod seal lubrication for Stirling engine

The elastohydrodynamic behavior of sliding elastomeric seals for the Stirling engine, was analyzed using an experimental apparatus to determine the instantaneous oil film thickness throughout the cyclic reciprocating motion. Tests were conducted on two commercial elastomeric seals: a "T" seal (76 mm O.D. and 3.8 mm between backing rings) and an "O" ring (76 mm O.D. and 5.3 mm diameter). Testing conditions included seal durometers of 70 and 90, sliding velocities of 0.8, 2.0, and 3.6 m/s, and no pressure gradient across the seal. Both acrylic and aluminum cylinders were used. Measured oil film thickness profiles were compared to results of the elastohydrodynamic analysis. The comparison shows an overall qualitative agreement. Friction and oil leakage measurements were also made at these sliding speeds. The fluid used was a typical synthetic base automotive lubricant. It is concluded that this first time experimental analytical comparison for oil film thickness indicates the need for some improvements in the analytical model and in the experimental technique.

Krauter, A. I.↗

The effects of ion implantation on the tribology of perfluoropolyether-lubricated 440C stainless steel couples

The lubricating lifetime of thin films of a perfluoropolyether (PFPE) based on hexafluoropropene oxide in the presence of ion implanted 440C stainless steel is presented. Stainless steel discs, either unimplanted or implanted with N2, C, Ti, Ti + N2, or Ti + C had a thin film of PFPE (60-400 A) applied to them reproducibly (+/- 20 percent) and uniformly (+/- 15 percent) using a device developed for this study. The lifetimes of these films were quantified by measuring the number of sliding-wear cycles required to induce an increase in the friction coefficient from an initial value characteristic of the lubricated wear couple to a final, or failure value, characteristic of an unlubricated, unimplanted couple. The tests were performed in a dry nitrogen atmosphere (less than 1 percent RH) at room temperature using a 3 N normal load with a relative sliding speed of 0.05 m/s. The lubricated lifetime of the 440C couple was increased by an order of magnitude by implanting the disc with Ti. Ranked from most to least effective, the implanted species were: Ti; Ti+C; unimplanted; N2; C approximately equals Ti+N2. The mechanism postulated to explain these results involves the formation of a passivating or reactive layer which inhibits or facilitates the production of active sites. The corresponding surface microstructures induced by ion implantation, obtained using x-ray diffraction and conversion electron Mossbauer spectroscopy, ranked from most to least effective in enhancing lubricant lifetime were: amorphous Fe-Cr-Ti; amorphous Fe-Cr-Ti-C + TiC; unimplanted; epsilon-(Fe,Cr)(sub x)N, x = 2 or 3; amorphous Fe-Cr-C approximately equals amorphous Fe-Cr-Ti-N.

Shogrin, Bradley↗

Tribological evaluation of an Al2O3-SiO2 ceramic fiber candidate for high temperature sliding seals

A test program to determine the relative sliding durability of an alumina-silica candidate ceramic fiber for high temperature sliding seal applications is described. Pin-on-disk tests were used to evaluate the potential seal material by sliding a tow or bundle of the candidate ceramic fiber against a superalloy test disk. Friction was measured during the tests and fiber wear, indicated by the extent of fibers broken in the tow or bundle, was measured at the end of each test. Test variables studied included ambient temperatures from 25 to 900 C, loads from 1.3 to 21.2 N, and sliding velocities from 0.025 to 0.25 m/sec. In addition, the effects of fiber diameter and elastic modulus on friction and wear were measured. Thin gold films deposited on the superalloy disk surface were evaluated in an effort to reduce friction and wear of the fibers. In most cases, wear increased with test temperature. Friction ranged from 0.36 at 500 C and low velocity (0.025 m/sec) to over 1.1 at 900 C and high velocity (0.25 m/sec). The gold films resulted in satisfactory lubrication of the fibers at 25 C. At elevated temperatures diffusion of substrate elements degraded the films. These results indicate that the alumina-silica (Al2O3-SiO2) fiber is a good candidate material system for high temperature sliding seal applications. More work is needed to reduce friction.

Dellacorte, Christopher↗

Relative sliding durability of candidate high temperature fiber seal materials

The relative sliding durability behavior of six candidate ceramic fibers for high temperature sliding seal applications is reviewed and compared. Pin on disk tests were used to evaluate potential seal materials by sliding a tow or bundle of the candidate ceramic fiber against a superalloy test disk. Tests were conducted in air under a 2.65 N load, at a sliding velocity of 0.025 m/sec and at temperatures from 25 to 900 C. Friction was measured during the tests and fiber wear, indicated by the extent of fibers broken in the tow or bundle, was measured at the end of each test. For most of the fibers, friction and wear increase with test temperature. The relative fiber durability ranking correlates with tensile strength, indicating that tensile data, which is more readily available than sliding durability data, may be useful in predicting fiber wear behavior under various conditions. A dimensional analysis of the wear data shows that the fiber durability is related to a dimensionless durability ratio which represents the ratio of the fiber strength to the fiber stresses imposed by sliding. The analysis is applicable to fibers with similar diameters and elastic moduli. Based upon the results of the research program, three fiber candidates are recommended for further study as potential seal materials. They are a silicon based complex carbide-oxide fiber, an alumina-boria-silica and an aluminosilicate fiber.

Dellacorte, Christopher↗

Sliding durability of candidate seal fiber materials in hydrogen from 25 to 900 C

Sliding durability studies of candidate ceramic fibers were conducted in hydrogen to support the high temperature seal development program at NASA LeRC. Pin-on-disk tests were used to measure the friction and durability of a tow or bundle of ceramic fibers in sliding against a superalloy disk. This procedure was used previously to test candidate fibers in an air environment. The fibers based upon mullite (Al2O3-SiO2) chemistry (Nextel 550, 440, and 312) exhibited better durability in hydrogen than in air. HPZ, a complex silicon carboxynitride fiber which showed good durabilty in air, however, showed a significant loss of durability in hot hydrogen. These results are consistent with recent thermodynamic and experimental studies of ceramic compatibility with hydrogen at elevated temperatures. These research results indicate that only oxide fibers display good durability in both air and hydrogen environments. Also, simple, low cost testing in air can provide an adequate data base for initial seal material screening and selection, especially for oxide fiber candidates. The findings of this research provide critical input to the seal design team.

Dellacorte, Christopher↗

Friction and wear characteristics of wire-brush skids

The testing technique consisted of towing the skids with a ground test vehicle over asphalt and concrete surfaces at ground speeds up to 80 km/hr (50 mph) and bearing pressures up to 689 kPa (100 psi) over sliding distances up to 1585 m (5200 ft). Results indicate that the friction coefficient developed by wire brush skids is essentially independent of ground speed, is slightly increased with increasing bearing pressure, is noticeably affected by surface texture, and is not degraded by surface wetness. Skid wear is shown to increase with increasing bearing pressure and with increasing ground speed and is dependent on the nature of the surface. Runway surface damage caused by the skids was in the form of an abrasive scrubbing action rather than physical damage.