Multiscale Cryo Electron Microscopy Reveals Interfacial Degradation and Stabilization in Battery Electrodes

Electrochemical interfaces are dynamic systems, evolving based on their local environment and reactant surface structures. The electrode-electrolyte interface in Li-ion batteries can be protective, limiting parasitic reactions with the electrolyte to passivate the surface [1]. Additionally, this interphase has an impact on the Li-ion transport through that layer based on its composition, bonding environment, and thickness. These parameters are challenging to collect and may vary depending on the electrode surface site investigated relative to its spatial position in a coin cell. This study will detail a multiscale cryogenic electron microscopy approach where millimeter-scale cross-sections through the coin cell batteries were made using a cryogenic stage within a fs-laser plasma focused ion beam (laser PFIB) with complementary energy dispersive X-ray spectroscopy able to detect variations in the composition at electrode interfaces [2]. Microscale cross-sectioning and lamella sample preparation of battery electrodes was conducted at the Center for Integrated Nanotechnologies using a Ga-ion focused ion beam (FIB) with air-free and cryo-transfer [3], followed by nanoscale mapping of composition and bonding within the CEI through cryo-scanning transmission electron microscopy (cryo-STEM) electron energy loss spectroscopy [4]. This multiscale approach enabled identification of millimeter-scale features of a battery stack with visualization of degradation in electrodes such as cracks in cathode particles, gas evolution, and SEI evolution; microscale interfacial characteristics, such as heterogeneity in the SEI or barrier layer and identification of electrolyte networks to the electrode surfaces; and nanoscale measurement of the CEI thickness, mapping of transition metal bonding within the cathode particles to identify loss of active materials, and identification of beneficial electrolyte additives incorporated into the CEI structure. This multiscale approach allows for a statistical understanding of the primary mechanisms and parasitic degradation pathways that impact performance by limiting the ion transport pathways within Li+ batteries.

36 MATERIALS SCIENCE↗

Chemical contributions to silicon anode calendar aging are dominant over mechanical contributions

Silicon (Si) anodes are a promising candidate for increasing the energy density of lithium (Li)-ion batteries for electric vehicles. However, they have recently been identified as having poor calendar life that is insufficient for commercial needs, in addition to the well-known issue of their poor cycle life resulting from large volume expansion. Here, a specially designed protocol with variable rest periods between intermittent cycling is used to evaluate the impact of the mechanical disruption of Si and solid electrolyte interphase (SEI) from cycling on calendar aging measurements. Si was found to undergo more mechanical degradation during calendar aging with intermittent cycling than graphite. However, Si anode capacity fade was still dominated by time, especially for rest periods greater than or equal to 1 month between cycling. Postmortem dQ/dV half-cell analysis indicated this was mainly due to Li inventory loss and an increase in electrode resistance. Isothermal microcalorimetry further demonstrated that Si passivation is more disrupted than graphite passivation with intermittent cycling and suggested that there may be a chemical buildup of a detrimental species in the electrolyte, leading to a large spike in heat after the Si and SEI are disrupted by cycling.

25 ENERGY STORAGE↗

Rational Electrolyte Formulation for Sodium Metal Batteries Operating in Extremely Cold Environments

Sodium metal batteries have shown considerable potential when operated at ambient temperatures. However, their performance in cold environments is constrained by increased electrolyte resistance with decreasing temperature and dendritic sodium plating associated with unstable solid electrolyte interphase (SEI), which are primarily influenced by the electrolyte composition. In this study, we present an electrolyte formulation that remains thermally stable down to −150 °C, which not only facilitates low internal resistance but also contributes to the formation of a protective SEI under cryogenic conditions. When cycled at −40 °C at 1 mA cm −2 , the sodium metal electrode exhibits a low overpotential of only 16 mV over 750 h; even at an ultra-low temperature of −80 °C, the electrode demonstrates remarkable long-term stability with a low overpotential of 54 mV sustained over 1500 h at 0.5 mA cm −2 . Furthermore, full cell evaluations when paring with Na 3 V 2 (PO 4 ) 3 cathode reveal a high average Coulombic efficiency exceeding 99.1% and a capacity retention over 83% after 100 cycles at both −40 °C and −80 °C.

Electrolyte↗

Electrolyte formulations for electrochemical cells containing a silicon electrode

Additives to electrolytes that enable the formation of comparatively more robust SEI films on silicon anodes. The SEI films in these embodiments are seen to be more robust in part because the batteries containing these materials have higher coulombic efficiency and longer cycle life than comparable batteries without such additives.

25 ENERGY STORAGE↗

Electrolyte formulations for electrochemical cells containing a silicon electrode

Additives to electrolytes that enable the formation of comparatively more robust SEI films on silicon anodes. The SEI films in these embodiments are seen to be more robust in part because the batteries containing these materials have higher coulombic efficiency and longer cycle life than comparable batteries without such additives. The additives preferably contain a nitrate group.

25 ENERGY STORAGE↗

Electrolyte formulations for electrochemical cells containing a silicon electrode

Additives to electrolytes that enable the formation of comparatively more robust SEI films on silicon anodes. The SEI films in these embodiments are seen to be more robust in part because the batteries containing these materials have higher coulombic efficiency and longer cycle life than comparable batteries without such additives.

Zhu, Ye↗

Nanoscale Three-Dimensional Imaging of Degradation in Composite Si-Containing Anodes

The use of silicon (Si) in next-generation lithium-ion battery (LIB) anodes has the potential to dramatically improve electrochemical performance over current LIB graphite (Gr) anodes, due to silicon’s higher specific capacity.1 However, widespread implementation of Si-containing anodes is inhibited by issues such as significant Si volume expansion during lithiation and an unstable solid-electrolyte interphase (SEI), resulting in unreliable performance and poor cycle life. Currently, composite anodes with both Si and graphite active materials are used to increase capacity and mitigate some of the limitations associated with Si. In composite electrodes with a heterogeneous distribution of components with varying electrical properties (including Si, Gr, conductive carbon additive, and binder), it is important to understand the local distribution of each component to correlate with electrochemical processes, particularly localized degradation and heterogeneous aging, and to optimize performance. To investigate Si-containing composite anodes in the nanoscale, we use scanning spreading resistance microscopy (SSRM), a form of scanning probe microscopy (SPM) that probes local electronic resistivity. By examining the intrinsic electronic resistivity contrast between the anode components, separate phases can be distinguished and understood within the composite structure.2 This work studies the effect of electrochemical cycling in two different electrolytes on component distribution and aging by comparing the electrical and structural evolution of composite Si-graphite electrodes and SEI before and after charge-discharge cycling. 1. W. J. Zhang. A review of the electrochemical performance of alloy anodes for lithium-ion batteries J. Power Sources 196 13–24 (2011). 2. C. Stetson, Z. Huey, A. Downard, Z. Li, B. To, A. Zakutayev, C.-S. Jiang, M. Al-Jassim, D. Finegan, S.-D. Han and S. DeCaluwe: Three-Dimensional Mapping of Resistivity and Microstructure of Composite Electrodes for Lithium-Ion Batteries. ACS Nano Letters Accepted (2020).

ADVANCED PROPULSION SYSTEMS↗

Avances a un ano del PR100: Resultados Preliminares del Modelzacion y Conjuntos de Datos Solares y Eolicos de Alta Resolucion

El estudio de Resiliencia y Transiciones a 100% Energia Renovable de Puerto Rico (PR100) es un estudio de 2 ano de la Oficina de Movilizacion de la Red del Departamento de Energia y seis laboratorios nacionales para analizar exhaustivamente las rutas dirigidas por las personas interesadas hacia un futuro de energia limpia en Puerto Rico. En el Ano 1 del estudio, el equipo PR100, creo y analizo los modelos que alcanzan las metas de energia renovable para Puerto Rico y los objetivos de resiliencia energetica a corto y largo plazo. Esta presentacion, que resume el progreso en el Ano 1, proporciona las consideraciones que pueden informar posibles decisiones de fondos e implementacion potenciales por parte de las agencias federales y locales clave y partes interesadas. Esta presentacion sigue a la publicacion en julio 2022 de un Informe de Seis Meses de Progreso de PR100 (en ingles y espanol), asi como webinarios publicos en febrero 2022 para lanzar el estudio y julio 2022 para presentar la actualizacion a 6 meses. Un informe final por escrito y visuales por la web seran publicados a finales del 2023. Todas las publicaciones y eventos publicos asociados con el estudio estaran disponibles en ingles y espanol. This report is also available in English https://www.nrel.gov/docs/fy23osti/85126.pdf.

datos de recursos eolicos↗

Characterization of Annealing-Induced Phase Segregation in Composite Silicon Anodes for Li-ion Batteries

Silicon (Si) anodes present a promising alternative to graphite anodes for lithium-ion batteries (LIBs), as Si has a greater specific capacity. However, one major constraint is the volumetric change of Si during lithiation that results in an unstable solid-electrolyte interphase (SEI), so Si-containing electrodes require the use of various strategies to mitigate these effects and improve performance. One such solution is the use of Si nanoparticles (NPs) that maximize the surface area to volume ratio. Here, we discuss electrodes made with Si NPs treated with polyethylene oxide (PEO) (for improving dispersion during processing), conductive carbon NPs, and P84 polyimide binder which shows significant impacts of annealing treatment on improvements of active material utilization, first cycle efficiency, and capacity retention with extensive cycling . We used air-free argon ion polishing to create electrode cross sections and imaged through the electrode thickness using atomic force microscopy (AFM)-based nano-electrical characterization of scanning spreading resistance microscopy (SSRM), nano-mechanical characterizations of contact resonance and force volume (CR-FV), and scanning electron microscopy-based energy dispersive x-ray spectroscopy (SEM-EDS). Results show that the Si and conductive carbon segregate into phases with a distinctive carbon-rich banded morphology that surrounds the Si-rich phase during annealing. In pristine electrodes, the carbon- and SEI-rich bands exhibit a higher electronic conductivity and a lower elastic modulus than the Si active material phase. These structures, as well as distinct electronic and mechanical properties, remain during cycling, suggesting an improvement of electrical conduction pathways and a mechanical strain buffer for active Si material expansion during cycling. This phase separation may be a major factor in the improvement seen in electrochemical performance due to annealing. Additionally, our nm-scale and multi-mode characterizations provide a novel route for understanding and improving energy storage devices, which is advantageous due to the highly inhomogeneous of composite electrodes in nm-mm scales.

ENERGY STORAGE↗

Semi-tubular carbon film for stable lithium metal anodes and methods of manufacture thereof

A method of forming a battery electrode by forming, on a first substrate, a polymer template comprising interconnected polymer fibers, forming, on the polymer template, a carbon coating to form a carbon-coated polymer template, removing the carbon-coated polymer template from the first substrate, subsequent to removing the carbon-coated polymer template from the first substrate, removing the polymer template from the carbon coating, and disposing the carbon coating on a second substrate. A solid electrolyte interphase layer (SEI) comprising the carbon coating produced via the method, a battery electrode comprising such an SEI layer, and a battery comprising such a battery electrode are also provided.

Ren, Zhifeng↗

Study on the Carbon Nanostructures for Nanosized Si Electrodes

Silicon (Si) has been considered as a next-generation anode material due to natural abundance, low operating potential (<0.5 V vs. Li/Li+), and high theoretical specific capacity of 4200 mAh g-1.[1] However, the electrochemical alloying reaction of Si involves large volume changes of 400% during lithiation and delithiation, causing cracking and pulverization of Si.[1] In addition, solid electrolyte interface (SEI) of Si anode experiences constant changes due to unstable SEI reactivity.[2] Considerable efforts have been made to design nanostructured Si materials to address the issues because nanostructuring can relieve the mechanical strain.[3] However, when compared to micrometer-sized active materials having sufficient electrolyte pathway through interparticle space, the nanoparticle (NP)-based electrodes tend to be densely packed. As mass loading is higher and electrode is thicker, ion transport issue can become more severe in the densely packed electrodes.[4] In this work, we will present studies on engineered porosity impacts performance in Si NP electrodes by altering carbon nanostructures. We explore the extreme limit of effectively non-porous electrodes using quasi-spherical, Si NPs, which result in densely packed electrodes when slurry is prepared with conventional carbon black. We engineer porosity using carbon nanostructures including multi-walled carbon nanotubes and carbon nanorods in place of conventional carbon black to create pore structure in Si NP-based electrodes. These experiments provide a correlation between mass loading, porosity and silicon utilization in Si NP-based electrodes. References: [1] C. K. Chan, H. Peng, G. Liu, K. Mcllwrath, X. F. Zhang, R. A. Huggins, Y. Cui, "High-performance lithium battery anodes using silicon nanowires", Nat. Nanotechnol., 2008, 3, 31, [2] J. D. McBrayer, M.-T. F. Rodrigues, M. C. Schulze, D. P. Abraham, C. A. Apblett, I. Bloom, G. M. Carroll, A. M. Coclasure, C. Fang, K. L. Harrison, G. Liu, S. D. Minteer, N. R. Neale, G. M. Veith, C. S. Johnson, J. T. Vaughey, A. K. Burrel, B. Cunningham, "Calendar aging of silicon-containing batteries", Nat. Energy, 2021, 6, 1164, [3] H. Wu, G. Zheng, N. Liu, T. J. Carney, Y. Yang, Y. Cui, "Engineering Empty space between Si Nanoparticles for Lithium-Ion Battery Anodes", Nano Lett., 2012, 12, 904, [4] X. Zhang, Z. Ju, Y. Zhu, K. J. Takeuchi, E. S. Takeuchi, A. C. Marschilok, G. Yu, "Multiscale Understanding and Architecture Design of High Energy/Power Lithium-Ion Battery Electrodes", Adv. Energy Mater., 2021, 11, 2000808

carbon nanostructure↗

Sulfur Solutions: Advancing High Voltage and High Energy Lithium Batteries with Organosulfur Electrolytes

Achieving energy densities exceeding 350 Wh kg -1 while operating at elevated voltages (>4.5 V vs Li/Li + ) is attainable through judicious selection of electrochemical pairs at the cathode and anode. However, current state-of-the-art electrolytes exhibit limited stability when exposed to systems operating at or above 4.3 V. This limitation contributes to the degradation of electrode materials and raises critical safety concerns, impeding the commercialization of such systems. Consequently, there has been a notable surge in research efforts aimed at developing innovative electrolyte compositions capable of supporting high-voltage lithium-ion batteries (LIBs). A substantial portion of this research has focused on the family of organosulfur molecules, which possess high oxidative stability. Organosulfur salts also facilitate the formation of dense, ionically conductive solid electrolyte interfaces (SEI) and demonstrate excellent solubility. This article provides a comprehensive overview of the field of organosulfur electrolyte components for their applications in energy storage, encompassing solvents, alternative conducting salts, and additives. It emphasizes the idea that the deliberate design of electrolyte compositions is instrumental in controlling electrode passivation, with organosulfur-based structures historically proving advantageous in every aspect of the electrolyte. Crucially, it should be noted that many of these components are commercially available, holding significant implications for industrial applications.

25 ENERGY STORAGE↗

High Energy Density and Stable Three-Dimensionally Structured Se-Loaded Bicontinuous Porous Carbon Battery Electrodes

Here, 3D structured Se-loaded bicontinuous porous carbon (BPC) electrodes were fabricated through colloidal templating of BPC followed by pulsed-voltage Se electrodeposition. The resultant electrodes were found to deliver a specific capacity of 665 mA h g -1 at a rate of 0.1 C, near the theoretical value for Se. When a vinylene carbonate containing electrolyte was utilized, the capacity fade over 500 cycles at 1 C rate was as small as a few percent. Impedance measurements and physical characterization of cycled electrodes indicated the exceptionally stable cycling performance was possibly due to vinylene carbonate resulting in formation of a stable SEI during cycling. Along with cycling stability, the rate performance of the 3D Se/BPC electrodes was also good. Due to the bicontinuous structure of carbonaceous current collector at rates as high as 5 C, the deliverable capacity was about 300 mA h g -1 .

25 ENERGY STORAGE↗

Valuation of Anode Materials for High-Performance Lithium Batteries: From Graphite to Lithium Metal and Beyond

Lithium-ion batteries have revolutionized energy storage, yet advanced technologies such as electric vehicles and eVTOLs demand even higher performance and safety. Anodes, the negative electrodes, are crucial in enhancing batteries’ safety, lifespan, and fast-charging capabilities. This review paper comprehensively evaluates the progression of anode materials from traditional graphite to advanced anodes like lithium metal. Graphite anodes, with a capacity of 372 mAh g −1 , enabled the first commercial lithium-ion batteries, but future applications require higher energy densities and fast-charging capabilities. Emerging anode materials, including alloying, and conversion types, as well as lithium metal, offer significantly higher capacities, with lithium metal offering a theoretical capacity of 3 860 mAh g −1 . However, these advanced anodes face challenges such as volume expansion, high surface reactivity, sluggish Li+ kinetics, and unstable lithium deposition morphologies. Here, this review critically examines the electrochemical performance, interfacial properties, mechanical attributes, and stability issues of various anode materials. It further discusses solid electrolyte interphase (SEI) formation, strategies for enhancing interface stability, and the requirements of anodes for solid-state batteries. Additionally, the review explores potential solutions for limitations with each anode type, highlights innovative anode-free architectures, and evaluates the current and future trends of battery anode industries. Ultimately, this paper aims to guide the development of high-performance anode materials, paving the way for the next generation of efficient, reliable lithium batteries.

Alloying anodes↗

Ultrahigh coulombic efficiency electrolyte enables Li||SPAN batteries with superior cycling performance

Raising the coulombic efficiency of lithium metal anode cycling is the deciding step in realizing long-life rechargeable lithium batteries. Here, we designed a highly concentrated salt/ether electrolyte diluted in a fluorinated ether: 1.8 M LiFSI in DEE/BTFE (diethyl ether/bis(2,2,2-trifluoroethyl)ether), which realized an average coulombic efficiency of 99.37% at 0.5 mA cm -2 and 1 mAh cm -2 for more than 900 cycles. This electrolyte also maintained a record coulombic efficiency of 98.7% at 10 mA cm -2 , indicative of its ability to provide fast-charging with high cathode loadings. Morphological studies reveal dense, dendrite free Li depositions after prolonged cycling, while surface analyses confirmed the formation of a robust LiF-rich SEI layer on the cycled Li surface. Moreover, we discovered that this ether-based electrolyte is highly compatible with the low-cost, high-capacity SPAN (Sulfurized polyacrylonitrile) cathode, where the constructed Li||SPAN cell exhibited reversible cathode capacity of 579 mAh g -1 and no capacity decay after 1200 cycles. A cell where a high areal loading SPAN electrode (>3.5 mAh cm -2 ) is paired with only onefold excess Li was constructed and cycled at 1.75 mA cm -2 , maintaining a coulombic efficiency of 99.30% for the lithium metal. Computational simulations revealed that at saturation, the Li-FSI complex forms contact ion pairs, with a first solvation shell comprising DEE molecules, and a second solvation shell with a mix of DEE/BTFE. This study provides a path to enable high energy density Li||SPAN batteries with stable cycling.

36 MATERIALS SCIENCE↗

Detecting onset of lithium plating during fast charging of Li-ion batteries using operando electrochemical impedance spectroscopy

Electrochemical plating of Li metal on the graphite electrode is the key limitation behind slow charging times of Li-ion batteries (LIBs) in electric vehicles (EVs). Currently, electrochemical methods to detect the onset of Li plating while a battery is fast charging are sparse. In this study, we use operando electrochemical impedance spectroscopy to reliably detect the onset of Li plating on graphite electrodes in three-electrode LIBs. An increase in the graphite solid-electrolyte interface (SEI) resistance indicates that Li plating has occurred. By cross-validating with a highly sensitive ex situ chemical titration, we determine that this technique can detect very small amounts of plated Li (<0.6% of the graphite electrode's capacity). We also offer physical explanations for the observed impedance behavior. Finally, we show that this technique can be applied to standard two-electrode LIB systems, making the method an important step toward safely implementing fast charging protocols for LIBs in EVs.

25 ENERGY STORAGE↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Understanding the Effect of Cathode Composition on the Interface and Crosstalk in NMC/Si Full Cells

Crosstalk between the cathode and the anode in lithium-ion batteries has a great impact on performance, safety, and cycle lifetime. Still, no report exists for a systematic investigation on crosstalk behavior in silicon (Si)-based cells as a function of transition metal composition in cathodes. We studied the effect of crosstalk on degradation of Si-rich anodes in full cells with different cathodes having the same crystal structure but different transition metal compositions, such as LiNi 1/3 Mn 1/3 Co 1/3 O 2 (NM111), LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532), and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811). We found that the transition metal composition in cathodes, especially Mn ion concentration, significantly affects electrolyte decomposition reactions, even from very early cycles. This change causes differences in the solid electrolyte interphase (SEI) chemistry of each aged Si sample. As a result, each of the aged Si samples has a different electrochemistry, in terms of initial Coulombic efficiency and the mechanism of capacity fade.

25 ENERGY STORAGE↗