At least 361 records · Page 20

Formation enthalpies of LaLn'O{sub 3} (Ln'=Ho, Er, Tm and Yb) interlanthanide perovskites

High-temperature oxide melt solution calorimetry using 3Na{sub 2}O·MoO{sub 3} at 802 °C was performed for interlanthanide perovskites LaLn'O{sub 3} (Ln'=Ho, Er, Tm and Yb) and lanthanide oxides (La{sub 2}O{sub 3}, Ho{sub 2}O{sub 3}, Er{sub 2}O{sub 3}, Tm{sub 2}O{sub 3} and Yb{sub 2}O{sub 3}). The enthalpies of formation of these interlanthanide perovskites from binary lanthanide oxides at room temperature (25 °C) were determined to be −8.3±3.4 kJ/mol for LaHoO{sub 3}, −9.9±3.0 kJ/mol for LaErO{sub 3}, −10.8±2.7 kJ/mol for LaTmO{sub 3} and −12.3±2.9 kJ/mol for LaYbO{sub 3}. There is a roughly linear relationships between these enthalpy values and the tolerance factor for these and for other LaM{sup 3+}O{sub 3} (M=In, Sc, Ga, Al, Fe and Cr) perovskites, confirming that the distortion of the perovskites as results from ionic radius difference of A-site and B-site cations, is the main factor determining the stability of these compounds. - Graphical abstract: A linear relationship between the enthalpy of formation and the tolerance factor for interlanthanide LaLn'O{sub 3} (Ln'=Ho, Er, Tm, and Yb) and other LaM{sup 3+}O{sub 3} (M=In, Sc, Ga, Al, Fe and Cr) perovskites. - Highlights: • Interlanthanide perovskites were synthesized by solid state reactions. • Their enthalpies of formation were measured by oxide melt solution calorimetry. • ΔH{sub f,ox} shows a linear relationship with tolerance factor.

36 MATERIALS SCIENCE↗

Hydrogenation studies on NdScSi and NdScGe

NdScSi and NdScGe were synthesized from the elements via arc-melting and subsequent annealing. Their ordered La{sub 2}Sb type structures, with space group I4/mmm, were refined from single crystal X-ray diffractometer data: a=428.94(6) and b=1570.5(3) pm, wR2=0.0395, 309 F{sup 2} values for NdScSi and a=431.2(1) and c=1581.3(5) pm, wR2=0.1220, 227 F{sup 2} values for NdScGe, with 11 variables per refinement. Hydrogen insertion was performed on both Nd-based intermetallics by solid/gas reaction. Hydrogen uptake keeps the pristine compound space group but yields an anisotropic expansion of the unit cell with a large increase of c (≈+7%) and a slight decrease of a (≈−1.7%) parameters. Hydrogen absorption at 350 °C and under 5 bar of H{sub 2} pressure shows that the hydride NdScSiH{sub 1.48(5)} is formed. An in-situ neutron diffraction study during the deuteration of NdScSi reveals for the first time in a CeScSi-type compound, the possibility to fill two interstitial sites with deuterium atoms, leading to the composition NdScSiD{sub 1.5} for the deuteride adopting then the La{sub 2}Fe{sub 2}Se{sub 2}O{sub 3}-type structure. From magnetization measurements, we evidence that hydrogenation strongly reduces the Curie temperature of NdScSi (T{sub C}=175 K) and NdScGe (T{sub C}=194 K) since NdScSiH{sub 1.5} and NdScGeH{sub x} undergo a magnetic transition at 4 K and around 2 K, respectively. - Highlights: • Crystal structures of NdScSi and NdScGe were refined from single crystal XRD data. • The hydrogenation of NdScSi leads to the formation of the NdScSiH{sub 1.5} hydride. • NdScSiD{sub 1.5} adopts the La{sub 2}Fe{sub 2}Se{sub 2}O{sub 3}-type structure. • Hydrogenation strongly reduces the ordering temperature of both intermetallics.

36 MATERIALS SCIENCE↗

Anion-induced structural transformation of a sulfate-incorporated 2D Cd(II)–organic framework

A Cd(II)–organic framework {[Cd_2(tpim)_4(SO_4)(H_2O)_2]·(SO_4)·21H_2O}{sub n} (1) was synthesized by reacting CdSO{sub 4}·8/3H{sub 2}O and 2,4,5-tri(4-pyridyl)imidazole (tpim) under hydrothermal conditions. A structural analysis showed that compound 1 adopts a layered structure in which the [Cd(tpim){sub 2}]{sub n} chains are linked by sulfate anions. These 2D layers are further packed into a 3D supramolecular framework via π–π interactions. The structure contains two types of SO{sub 4}{sup 2−} anions, i.e., bridging SO{sub 4}{sup 2−} and free SO{sub 4}{sup 2−} anions, the latter of which are included in the large channels of the framework. Compound 1 exhibits interesting anion exchange behavior. In the presence of SCN{sup −} anions, both the bridging and free SO{sub 4}{sup 2−} anions in 1 were completely exchanged by SCN{sup −} ligands to form a 1D species [Cd(tpim){sub 2}(SCN){sub 2}] (1A), in which the SCN{sup –} moieties function as a monodentate ligand. On the other hand, when compound 1 was ion exchanged with N{sub 3}{sup −} anions in aqueous solution, the bridging SO{sub 4}{sup 2−} moieties remained intact, and only the free guest SO{sub 4}{sup 2−} were replaced by N{sub 3}{sup −} anions. The gas adsorption behavior of the activated compound 1 was also investigated. - Highlights: • An interesting anion-induced structural transformation of a sulfate-incorporated 2D Cd(II)–organic framework is reported. • The sulfate-incorporated 2D layer compound exhibits very different anion exchange behavior with respect to SCN{sup −} and N{sub 3}{sup −}. • Both the bridging and free SO{sub 4}{sup 2−} anions in the 2D structure were completely exchanged by SCN{sup −} ligands, resulting in the formation of a 1D species. However, in the case of N{sub 3}{sup −} anions, only the free guest SO{sub 4}{sup 2−} in the structure was replaced.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase formation and UV luminescence of Gd{sup 3+} doped perovskite-type YScO{sub 3}

Synthesis of pure and Gd{sup 3+}doped perovskite-type YScO{sub 3} was attempted by a polymerized complex (PC) method and solid state reaction (SSR) method. Crystalline phases and UV luminescence of samples were examined with varying heating temperatures. The perovskite-type single phase was not simply formed in the SSR method, as reported in some literatures, and two cubic C-type phases of starting oxide materials remained forming slightly mixed solid solutions. UV luminescence of Gd{sup 3+} doped samples increased with an increase in heating temperatures and volume of the perovskite-type phase. In contrast, a non-crystalline precursor was crystallized to a single C-type phase at 800 °C in the PC method forming a completely mixed solid solution. Then, the phase of perovskite-type YScO{sub 3} formed at 1200 °C and its single phase was obtained at 1400 °C. It was revealed that high homogeneousness of cations was essential to generate the single perovskite-phase of YScO{sub 3}. Because Gd{sup 3+} ions were also dissolved into the single C-type phase in Gd{sup 3+} doped samples, intense UV luminescence was observed above 800 °C in both C-type phase and perovskite-type phase. - Graphical abstract: A pure perovskite-type YScO{sub 3} phase was successfully synthesized by a polymerized complex (PC) method. The perovskite-type YScO{sub 3} was generated through a solid solution of C-type (Y{sub 0.5}Sc{sub 0.5}){sub 2}O{sub 3} with drastic change of morphology. The PC method enabled a preparation of the single phase of the perovskite-type YScO{sub 3} at lower temperature and in shorter heating time. Gd{sup 3+} doped perovskite-type YScO{sub 3} was found to show a strong sharp UV emission at 314 nm. - Highlights: • Pure YScO{sub 3} phase was successfully synthesized by polymerized complex (PC) method. • Pure perovskite-type YScO{sub 3} phase was generated from pure C-type (Y{sub 0.5}Sc{sub 0.5}){sub 2}O{sub 3} one. • YScO{sub 3} was obtained at lower temperature and in shorter heating time by PC method. • Perovskite-type YScO{sub 3}:Gd{sup 3+} was found to show strong sharp UV emission at 314 nm.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructural investigations on as-cast and annealed Al-Sc and Al-Sc-Zr alloys

Al-Sc and Al-Sc-Zr alloys containing 0.05, 0.1 and 0.5 wt.% Sc and 0.15 wt.% Zr were investigated using optical microscopy, electron microscopy and X-ray diffraction. The phase composition of the alloys and the morphology of precipitates that developed during solidification in the sand casting process and subsequent thermal treatment of the samples were studied. XRD analysis shows that the weight percentage of the Al{sub 3}Sc/Al{sub 3}(Sc, Zr) precipitates was significantly below 1% in all alloys except for the virgin Al0.5Sc0.15Zr alloy. In this alloy the precipitates were observed as primary dendritic particles. In the binary Al-Sc alloys, ageing at 470 deg. C for 24 h produced precipitates associated with dislocation networks, whereas the precipitates in the annealed Al-Sc-Zr alloys were free of interfacial dislocations except at the lowest content of Sc. Development of large incoherent precipitates during precipitation heat treatment reduced hardness of all the alloys studied. Growth of the Al{sub 3}Sc/Al{sub 3}(Sc, Zr) precipitates after heat treatment was less at low Sc content and in the presence of Zr. Increase in hardness was observed after heat treatment at 300 deg. C in all alloys. There is a small difference in hardness between binary and ternary alloys slow cooled after sand casting.

36 MATERIALS SCIENCE↗

Characterization of phase development in non-isothermally annealed mould-cast and heat-treated Al-Mn-Sc-Zr alloys

The effect of Mn addition on microstructure and mechanical properties during isochronal annealing in the temperature range of 20 deg. C - 570 deg. C of the mould-cast and heat-treated Al-Sc-Zr alloys with a various content of Mn and Zr was studied. The electrical resistometry together with the microhardness (HV0.3) measurements were compared to microstructure development. The microstructure development was examined by scanning electron microscopy, transmission electron microscopy and electron diffraction. Relative resistivity changes and the microhardness of the mould-cast and heat-treated Al-Mn-Sc-Zr alloys exhibit similar dependence on annealing temperature. Precipitation of the Al{sub 3}Sc particles is responsible for the peak microhardness in all these alloys. The microhardness decrease is slightly delayed during the isochronal annealing and during the high temperature heat treatment in the mould-cast alloy with the higher Zr-content due to a higher oversaturation of Zr. The decomposition sequence of the oversaturated solid solution of the studied Al-Mn-Sc-Zr alloys is compatible with the recently published decomposition sequence of the Al-Sc-Zr system and also with the formation of Mn,Fe-containing particles. It seems very probable that the addition of Mn does not influence the decomposition of solid solution of the ternary Al-Sc-Zr system. - Research Highlights: {yields} Al{sub 3}Sc particles are responsible for the peak microhardness in all the studied alloys. {yields} The microhardness decrease is delayed in the alloy with the higher Zr-content. {yields} The peak hardening of the heat-treated alloys is shifted to higher temperatures. {yields} Mn does not influence the decomposition sequence of the Al-Sc-Zr system.

36 MATERIALS SCIENCE↗

Effects of Sc content on the microstructure of As-Cast Al-7 wt.% Si alloys

The effects of Sc content on the microstructure of as-cast Al-Si alloys were investigated by adding 0.05, 0.1, 0.15, 0.2, 0.25, 0.3, and 0.4 wt.% Sc to hypoeutectic Al-7 wt.% Si alloys. The results show that there are significant changes in the microstructure when the Sc content is increased to 0.15%. The volume fraction of the primary {alpha}-Al phase increased nearly monotonically with increasing Sc content in the as-cast state. As the Sc content increased, the average length of the eutectic Si in the as-cast Al-7Si-xSc alloy decreased sharply from 150 {mu}m (without Sc content) to 20 {mu}m (0.4 wt.% Sc content). The Sc atoms are concentrated in the interdendritic regions. A fish-bone structure composed of Al, Si, Sc, and Fe, which might be the Fe-rich phase precipitated on the AlSc{sub 2}Si{sub 2} (V-phase) was detected adjacent to the grain boundary by scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). - Highlights: Black-Right-Pointing-Pointer Significant changes in the microstructure when the Sc content is increased to 0.15%. Black-Right-Pointing-Pointer Volume fraction of the primary a-Al phase increased with increasing Sc content. Black-Right-Pointing-Pointer Average length of Si decreased sharply from 150 to 20 {mu}m with increasing Sc content. Black-Right-Pointing-Pointer The Sc atoms are concentrated in the interdendritic regions.

36 MATERIALS SCIENCE↗

Correlative characterization of primary Al{sub 3}(Sc,Zr) phase in an Al–Zn–Mg based alloy

Three-dimensional electron backscatter diffraction, focused ion beam, transmission electron microscopy and energy filtered transmission electron microscopy were employed to investigate the structural information of primary Al{sub 3}(Sc,Zr) phase, i.e. size, shape, element distribution and orientation relationship with the α-Al matrix. It was found that (i) most primary Al{sub 3}(Sc,Zr) phases have a cubic three-dimensional morphology, with a size of about 6–10 μm, (ii) most primary Al{sub 3}(Sc,Zr) phases are located within the α-Al matrix, and exhibit a cube to cube orientation relationship with the α-Al matrix, and (iii) a layer by layer growth was observed within primary Al{sub 3}(Sc,Zr) phases. Al, Cu, Si and Fe are enriched in the α-Al matrix between the layers of cellular eutectic Al{sub 3}(Sc,Zr) phase, while Sc, Ti and Zr are enriched in small Al{sub 3}(Sc,Zr) phases. A peritectic reaction and subsequent eutectic reaction between Al{sub 3}Sc and Al was proposed to interpret the observed layer by layer growth. This paper demonstrates that the presence of impurities (Fe, Si, Cu, Ti) in the diffusion field surrounding the growing Al{sub 3}(Sc,Zr) particle enhances the heterogeneous nucleation of Al{sub 3}(Sc,Zr) phases. - Highlights: • Most fine cubic primary Al{sub 3}(Sc,Zr) phases were observed within the α-Al matrix. • A layer by layer growth within primary Al{sub 3}(Sc,Zr) phase was observed. • A peritectic and subsequent eutectic reaction between Al{sub 3}Sc and Al was proposed. • Impurities in diffusion fields enhance heterogeneous nucleation of Al{sub 3}(Sc,Zr)

36 MATERIALS SCIENCE↗

Microstructure and transformation behavior of Ni{sub 24.7}Ti{sub 50.3}Pd{sub 25} high temperature shape-memory alloy with Sc micro-addition

NiTiPd shape-memory alloys (SMAs) are potential functional materials for use as solid-state actuators in the temperature range 100–250 °C. The present study investigates the effect of 1.0 at.% Sc micro-addition to Ni{sub 24.7}Ti{sub 50.3}Pd{sub 25} alloy, Sc replacing either Ti or Ni. Results show that all the three alloys studied have stable transformation behavior on stress-free thermal cycling and hence, are suitable for cyclic actuation applications. However, the addition of Sc to NiTiPd alloy leads to decrease of transformation temperatures, the magnitude of decrease being greater for the alloy with Sc replacing Ni. The martensite finish (M{sub f}) temperature of 181 °C for the NiTiPd alloy decreased to 139 °C for Sc replacing Ti and 83 °C for Sc replacing Ni. Also, the indentation modulus of NiTiPdSc (Sc replacing Ni) alloy is found to be significantly low compared to the other alloys. Analysis indicates that the observed differences in the alloy properties are related to the solubility of Sc in the NiTiPd matrix. While the quaternary NiTiPdSc alloy, Sc replacing Ti, has a single phase microstructure, the alloy with Sc replacing Ni shows the presence of Sc-rich and TiPd-type second phases in the microstructure. TEM examination revealed that the TiPd-type phase has a distinct rod-like morphology (30–50 nm) arranged in a grid-like structure. The transformation and indentation behavior of the alloys is elucidated using thermodynamic calculations of frictional energy and an electronic structure based analysis. - Highlights: • TEM of Ni{sub 23.7}Ti{sub 50.3}Pd{sub 25}Sc{sub 1} showed distinct grid of TiPd-type phase nanorods < 50 nm. • Stress-free thermal cycling of all the three alloys showed stable transformation behavior. • Ni{sub 24.7}Ti{sub 49.3}Pd{sub 25}Sc{sub 1} and Ni{sub 23.7}Ti{sub 50.3}Pd{sub 25}Sc{sub 1} showed single and multiphase structures. • Sc micro-addition (1 at.%) to Ni{sub 24.7}Ti{sub 50.3}Pd{sub 25} alloy decreased TTs significantly. • Ni{sub 23.7}Ti{sub 50.3}Pd{sub 25}Sc{sub 1} exhibited lower modulus of 67 GPa to 85 GPa of Ni{sub 24.7}Ti{sub 50.3}Pd{sub 25}.

36 MATERIALS SCIENCE↗

Microstructural development of electron beam processed Al-3Ti-1Sc alloy under different electron beam scanning speeds

A systematic study has been made of the microstructural development in as-cast 30 mm thick Al-3Ti-1Sc (wt%) plate samples that were processed by electron beam (EB) melting at different scanning speeds of 3, 5, 8, 12, 15 and 20 mm/s. The composition of the alloy is designed to capitalize on the potential for significantly extended solubility values of both Sc and Ti in Al when cooled at high cooling rates. The resulting microstructures are characterised using transmission electron microscopy (TEM) and other analytical means, assisted with Thermo-Calc predictions and Vicker's microhardness measurements. EB scanning speed plays a key role in determining the phase formation and microstructural development in the Al-3Ti-1Sc alloy when the beam is applied an accelerating voltage of 50 kV and a current of 30 μA. The major microstructural features in the re-solidified zone include (i) the formation of the primary tetragonal Al{sub 3}(Ti,Sc) phases and their retention or subsequent transformation to stable cubic Al{sub 3}(Ti,Sc) phases; (ii) the complete suppression of the primary tetragonal Al{sub 3}(Ti,Sc) phases at the scanning speed of 20 mm/s; and (iii) the formation of cubic Al{sub 3}(Ti,Sc) precipitates in the α(Al) matrix supersaturated with both Sc and Ti. These experimental findings are informative for both EB processing of Al-Ti-Sc alloys and the design of new Al alloys for additive manufacturing processes.

36 MATERIALS SCIENCE↗

Effects of friction stir processing and minor Sc addition on the microstructure, mechanical properties, and damping capacity of 7055 Al alloy

Highlights: • Good mechanical and damping properties were obtained in the 7055 after FSP and Sc addition. • The strengthening and damping mechanisms of FSP 7055(-Sc) were analyzed. • FSP and Sc addition were found to be strategy of preparing 7xxx alloys with well damping and mechanical properties. - Abstract: This study investigated the effects of friction stir processing (FSP) and addition of 0.25% (mass ratio) Sc on the microstructure, mechanical properties, and damping capacity of AA 7055 alloy. Microstructure analyses revealed that a low tool rotation rate of 300 rpm effectively inhibited the grain coarsening in the recrystallization of the alloy during FSP. Sc addition prevented the coarsening of grains and precipitated η phase and the annihilation of dislocations in the FSP AA 7055 alloy. After being subjected to FSP at 300 rpm, the AA 7055 alloy containing Sc exhibited good mechanical and damping properties, which were mainly attributed to the fine recrystallized grain structure, fine precipitated η phase, and large number of nano-sized Al{sub 3}(Sc, Zr) particles located at the grain boundaries and dislocations. This work provides an effective strategy for preparing commercial Al alloys with excellent damping capacity and mechanical properties.

36 MATERIALS SCIENCE↗

Effect of trace amounts of added Sc on microstructure and mechanical properties of 2055 aluminum alloy

Highlights: • Effect of trace Sc on microstructure and mechanical properties in 2055 Al-alloy was investigated. • T{sub 1} is the main strengthening phase in Sc free and Sc added 2055 alloy at the aging temperature of 175°C and 200°C. • The refinement of T{sub 1} by Sc addition depends on the aging temperature. • Mechanical properties were deteriorated by Sc at the aging temperature of 175°C and improved at 200°C aging treatment. - Abstract: The effects of Sc additions and isothermal aging on the microstructure and mechanical properties of 2055 aluminum alloy have been investigated. The isothermal aging temperatures investigated were 175 °C and 200 °C. Results show that the aging temperature does not affect the type of precipitates in both Sc-free and Sc-added 2055 Al alloys. While remarkable changes in the size and number density of T{sub 1} (Al{sub 2}CuLi) precipitates have been observed. For samples aged at 175 °C for 8 h, the average length of T{sub 1} precipitates was increased from 39.9 nm to 45.6 nm, the number density decreased from 5.77 × 10{sup 22} m{sup −3} to 3.68 × 10{sup 22} m{sup −3} after Sc addition. On the contrary, when samples were aged at 200 °C for 8 h, the length decreased from 59.89 nm to 43.32 nm and number density increased from 2.13 × 10{sup 22} m{sup −3} to 3.00 × 10{sup 22} m{sup −3} by adding trace Sc. Slight deterioration of tensile strength and yield strength with higher ductility was founded at the aging temperature of 175 °C for 8 h due to the larger size and lower number density of T{sub 1} precipitates along with the formation of a W (AlCuSc) phase during the casting or homogenization processes. When aging temperature increased to 200 °C, tensile strength and yield strength were significantly improved by Sc addition without losing ductility. Highly dense fine T{sub 1} precipitates take responsible for the strength improvement, and to some extent it compensated the strength loss caused by the formation of W phase. A “vacancy-prison” mechanism was adopted to explain the effect of Sc additions on the precipitation of T{sub 1} phase as a function of aging temperature.

36 MATERIALS SCIENCE↗

Effects of Nb and Ta additions on the strength and coarsening resistance of precipitation-strengthened Al-Zr-Sc-Er-Si alloys

Highlights: • Nb and Ta micro-additions are made to a dilute Al-Er-Sc-Zr-Si alloys. • Zr-enriched primary L1{sub 2} precipitates form on solidification. • Secondary L1{sub 2} precipitates form on aging, and show improved coarsening resistance. • Nb and Ta are enriched at the secondary nanoprecipitate/matrix interface. • Micro-additions of Nb and Ta have similar effects as V, previously studied. - Abstract: A dilute Al-0.07Zr-0.02Sc-0.005Er-0.06Si (at.%) alloy was microalloyed with 0.08 at.% Nb or Ta. Atom-probe tomography reveals that, upon aging, Nb and Ta partition to the coherent L1{sub 2}-Al{sub 3}(Zr,Sc,Er) nanoprecipitates (with average concentrations of 0.2 and 0.08 at.%, respectively), with both segregating at the matrix/nanoprecipitate heterophase interface. This is consistent with the Nb- and Ta-modified alloys exhibiting, as compared to the unmodified alloy: (i) higher peak microhardness, from a higher nanoprecipitate volume fraction and/or lattice parameter mismatch; and (ii) improved aging resistance, from slower nanoprecipitate coarsening due to the small diffusivities of niobium and tantalum in aluminum. Analogous results were previously reported for a V-modified alloy.

36 MATERIALS SCIENCE↗

Influence of Sc content on the microstructure and mechanical properties of cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy

Highlights: • The grain size was continuously reduced with the increasing Sc content. • No evidence for the formation of the Cu-rich and Sc-containing W phase was observed. • Sc addition could promote the precipitation of S′ in the absence of pre-age stretch. • Sc addition would reduce the growth rate of δ′ and δ′-PFZs. • The highest combinations of strength and ductility were obtained in cast Al-Li alloys. - Abstract: In this work, the influence of Sc content on the microstructure and mechanical properties of cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy was investigated. It was found that the grain size of As-cast alloy was significantly reduced in steps with the increase of Sc addition, accompanied by the arising and increasing of cubic primary Al{sub 3}(Sc, Zr) phases. No evidence for the presence of the ternary W (Al{sub 8−x}Cu{sub 4+x}Sc) phase was obtained. The volume fraction of nanoscale Al{sub 3}(Sc, Zr) dispersoids was improved with the increase of Sc content, and the presence of Sc was observed to refine the S′ (Al{sub 2}CuMg) morphology during ageing. The addition of Sc lowered the growth rates of δ′ (Al{sub 3}Li) particles and δ′-Precipitate-free zones (δ′-PFZs) of the base alloy. The tensile property results showed that, with the increasing Sc content and ageing times, the yield strength (YS) and ultimate tensile strength (UTS) were continuously increased, and the highest elongation of 6.0% was obtained in the 0.2Sc-containing alloy aged for 32 h at 175 °C. The results indicated that the optimal Sc addition in cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy was 0.2 wt%.

36 MATERIALS SCIENCE↗

Microstructural analysis of undoped and moderately Sc-doped TiO2 anatase nanoparticles using Scherrer equation and Debye function analysis

Highlights: • UV light sensitive undoped and moderate Sc-doped anatase nanocrystallites were prepared without post-synthesis annealing. • Elongated nanocrystallites were found by Scherrer equation and Debye Function Analysis applied to XRD data and also HRTEM. • 4 at.% Sc doping reduced the amount of Ti vacancies by half. • Doping showed ~0.3% growth of lattice parameters. - Abstract: UV light sensitive undoped and moderate (4 at.%) Sc-doped anatase nanocrystallites were prepared by an efficient and environmentally benign method based on homogeneous hydrolysis of TiOSO{sub 4} and Sc{sub 2}(C{sub 2}O{sub 4}){sub 3.5}H{sub 2}O aqueous solutions using urea as a precipitation agent, without post-synthesis calcination or annealing. X-ray diffraction study of the obtained powders revealed single phase anatase in both samples. Two different methods were applied to estimate the anatase crystallite size and shape from the X-ray diffraction data. The first one is based on the more conventional Scherrer equation (as implanted in GSAS-II program) while the second one is based on Debye function analysis (as implanted in DUBUSSY suite version 2.2), which is considered to be more adequate for nanocrystallites. Although each program has its own shape models, both methods indicated similar results of elongated nanocrystallite geometry for Sc-doped TiO{sub 2}: (i) GSAS-II confirmed ellipsoid shape with equatorial size of 5.1(0) nm and axial size of 6.8(0), (ii) DEBUSSY suite 2.2 showed cylinder shape with diameter of equivalent circle in the ab-plane, D{sub ab} = 4.9(1.0) nm and crystallite length along the c-axis, L{sub c} = 5.4(3.2) nm. For the undoped TiO{sub 2} sample, equatorial size of 5.5(0) nm and axial size of 7.3(0) nm for the ellipsoid shape was determined according to GSAS-II, while D{sub ab} = 5.5(1.3) nm and L{sub c} = 6.0(2.2) nm for the cylinder shape was determined by DEBUSSY suite 2.2. These outcomes were found to corroborate with HRTEM analysis. Doping with 4 at.% Sc caused ~0.3% growth of lattice parameters from a = 3.7979 [4] Å, c = 9.4995 [9] Å for the undoped sample to a = 3.8110 [7] Å, c = 9.5274 [16] Å for the moderately Sc doped sample, while reduction in the Ti vacancies by half was confirmed by both methods. The introducing of Sc as electronically active secondary species into the crystal lattice of TiO{sub 2} can greatly alter its optical absorption. The incorporation of Sc into the crystal lattice of TiO{sub 2} favors the substitution of Ti, as both have approximately the same ionic size, and generates surface oxygen vacancies which can act as trapping center for the photogenerated electrons and reduce the recombination of electron–hole pairs. We can expect Sc doped TiO{sub 2} nanomaterials to have applications as effective photocatalysts for selective photocatalytic oxidation of various environmental organic pollutants.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Comparative study of Sc and Er addition on microstructure, mechanical properties, and electrical conductivity of Al-0.2Zr-based alloy cables

Highlights: • The comprehensive properties of Al-0.2Zr-0.1Sc were better than those of Al-0.2Zr-0.1Er alloy cable. • The microstructures evolved from fibrous grains to equiaxed grains with increasing annealing time. • The Zener drag force increased with increasing ratio of volume fraction (F{sub V}) to average diameter F{sub V}/ d-bar . • The capability to inhibit recrystallization was as follows: Al{sub 3}(Zr, Sc) > Al{sub 3}(Zr, Er) > Al{sub 3}Zr. - Abstract: The effect of the addition of 0.1 wt% Sc and 0.1 wt% Er on the deformation microstructure, Vickers microhardness, and electrical conductivity of Al-0.2 wt% Zr-based alloy cables annealed at 400 °C for different times was investigated. The comprehensive properties of Al-0.2Zr-0.1Sc were better than those of Al-0.2Zr-0.1Er. The optimal conditions for the Al-0.2Zr-01Sc alloy cable were a microhardness of 575 MPa, an electrical conductivity of 34.5 MS/m for an annealing time of 36 h, and those for the Al-0.2Zr-0.1Er alloy cable were a microhardness of 550 MPa, an electrical conductivity of 33.6 MS/m for an annealing time of 8 h. During the annealing process, dispersed Al{sub 3}(Zr,Sc/Er) precipitates were generated, which substantially impeded recrystallization by Zener pining of grain boundaries. Based on the ratio of volume fraction (F{sub V}) to average diameter ( d-bar ) of the precipitates, their capability to inhibit recrystallization was as follows: Al{sub 3}(Zr, Sc) > Al{sub 3}(Zr, Er) > Al{sub 3}Zr. Moreover, the electrical conductivity of Al-0.2Zr-0.1Sc was better than that of Al-0.2Zr-0.1Er, probably because Sc could better inhibit recrystallization than Er, leading to fewer grain boundaries and hence lesser electron scattering.

36 MATERIALS SCIENCE↗

Template-free solution approach to synthesize CdS dendrites with SCN based ionic liquid

Highlights: {yields} Template-free solution approach to synthesize CdS hierarchical dendrites. {yields} The 1-butyl-3-methlyimidazole thiocyanate ([BMIM][SCN]) plays doubly functional roles in the progress. {yields} The CdS hierarchical dendrites exhibit a more intense emission at 710 nm belongs to infrared band. -- Abstract: Cadmium sulfide dendrites were synthesized by a facile hydrothermal treatment from CdCl{sub 2} and ionic liquid 1-butyl-3-methlyimidazole thiocyanate acted both as sulfur source and surfactant. The product was characterized by means of X-ray powder diffraction and scanning electron microscopy. X-ray powder diffraction studies indicated that the product was well-crystallized hexagonal phase of CdS, and the scanning electron microscopy images showed that the obtained powders consisted of a wealth of well-defined CdS dendritic microstructures with a pronounced trunk and highly ordered branches. The UV-Vis and photoluminescence spectroscopy measurements were taken as well. The possible formation mechanism of CdS dendrites was simply proposed in the end.

36 MATERIALS SCIENCE↗