Creep-rupture data for welded N-155 tubes
Creep rupture data on welded tubes for helium to air heat exchanger design
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Creep rupture data on welded tubes for helium to air heat exchanger design
Salt stress corrosion cracking effects on tensile and stress rupture properties of titanium alloy sheet
Network rupture hypothesis and molecular structure considerations used in obtaining constitutive equations for flow of polymer melts and solutions
Critical aspect ratio and stress rupture of discontinuous fiber reinforced composites
Short-time stress rupture of prestressed titanium alloys under rapid heating conditions
Knife structure for controlling rupture of shock tube diaphragms
Specialized model for analysis of creep-rupture data by minimum commitment, station function approach with general time-temperature-stress relation to include all commonly used parameters
Critical aspect ratios of copper matrix and tungsten fibers in reinforced composites from stress-rupture and tension tests
Notch sensitivity of creep-rupture properties of Waspaloy between 1000 to 1400 F
Creep rupture data analysis model based on minimum commitment station function approach, generalizing hypothesized time temperature stress relation
Critical aspect ratio of W fibers in metal matrix composites for stress rupture applications
Weld-drawn tubes of Rene 41 with 0.935 centimeter outside diameter and 0.064 centimeter wall thickness were tested to failure at temperatures from 1117 to 1233 K and internal helium pressures from 5.5 to 12.4 meganewtons per square meter. Lifetimes ranged from 5 to 2065 hours. The creep-rupture strength of the tubes was 50 percent lower than that of unwelded, thick sheet specimens, and 20 percent lower than that of unwelded, thin sheet specimens. Larson-Miller correlations and photomicrographs of some specimens are presented.
Time-dependent notch sensitivity of Waspaloy was observed at test temperatures from 1000 to 1300 deg F. Its occurrence in this range was dependent on the heat treatment. ?Overaging' eliminated the notch sensitivity. Optimum combination of smooth and notched specimen strengths for material solution treated at 1975 deg F were obtained by aging 24 hr at 1550 deg F. Necessary conditions for time-dependent notch sensitivity were (1) the notch specimen loads had to be below the approximate 0.2 percent offset yield strength; and (2 ) test data from smooth specimens had to indicate that small amounts of creep used up large fractions of creep-rupture life. No reasons were evident why these criteria will not prove applicable to other alloys.
Results from laboratory studies of hypervelocity impact against crystalline rocks, combined with estimates of the micrometeoroid flux at the lunar surface, provide a basis for calculating abrasion rates and survival times before catastrophic rupture of rocks on the lunar surface. The surface residence times observed for lunar rocks of the order of 10 m.y. (derived from the track densities of iron group nuclei) restrict the mass range of impacting particles of interest to masses less than about 1.01 gram. Extrapolation downward to smaller masses following flux distributions suggested by early satellite data and photographic meteor observations leads to absurd rates of abrasion. Consistent with the observed crater populations on the lunar rocks and with the Pegasus, Explorer, and Pioneer satellite data, the slope of the mass-flux distribution must decrease markedly for masses below 1 to .1 microgram.
Seamless Inconel 702 tubes with 0.375-in. outside diameter and 0.025-in. wall thickness were tested to failure at temperatures from 1390 to 1575 F and internal helium pressures from 700 to 1800 psi. Lifetimes ranged from 29 to 1561 hr. The creep-rupture strength of the tubes was about 70 percent lower than that of sheet specimens. Larson-Miller correlations and photomicrographs of some specimens are presented.
Seamless Hastelloy-X tubes with 0.375-in. outside diameter and 0.025-in. wall thickness were tested to failure at temperatures from 1400 to 1650 F and internal helium pressures from 800 to 1800 psi. Lifetimes ranged from 58 to 3600 hr. The creep-rupture strength of the tubes was from 20 to 40 percent lower than that of sheet specimens. Larson-Miller correlations and photomicrographs of some specimens are presented.
The mechanical properties of elastomers, including rupture and its time dependence, can be semiquantitatively predicted from nine molecular parameters which are characteristic for a given species, from the initial molecular weight of a sample before cross-linking and from the effective chain concentration (which must still be determined for each vulcanizate). Only two empirical quantities are involved - the Plazek retardation function for entanglement slippage and a related constant which serves to locate this function on the time scale. The theory leads to a new method of estimating fatigue lifetimes from short-time data.
The appearance of the terrace like fracture morphology of gaseous hydrogen induced crack growth in acicular alpha-beta titanium alloys is discussed as a function of specimen configuration, magnitude of applied stress intensity, test temperature, and hydrogen pressure. Although the overall appearance of the terrace structure remained essentially unchanged, a distinguishable variation is found in the size of the individual terrace steps, and step size is found to be inversely dependent upon the rate of hydrogen induced slow crack growth. Additionally, this inverse relationship is independent of all the variables investigated. These observations are quantitatively discussed in terms of the formation and growth of a thin hydride film along the alpha-beta boundaries and a qualitative model for hydrogen induced slow crack growth is presented, based on the film-rupture model of stress corrosion cracking.