Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLIC COMPOUNDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Microstructure and mechanical properties of resistance-spot-welded joints for A5052 aluminum alloy and DP 600 steel

The microstructure and mechanical properties of resistance-spot-welded A5052 aluminum alloy and DP 600 dual-phase steel joint were studied. The fusion zone (FZ) and heat-affected zone (HAZ) of DP 600 exhibited lath martensite and ferrite-martensite structures, respectively. The microstructure of FZ and HAZ in the A5052 side was composed of cellular crystals and the boundary region of FZ exhibited a columnar crystal morphology. A Fe{sub 2}Al{sub 5} intermetallic compound (IMC) layer with 3.3 μm thickness was found adjacent to the DP 600 side, whereas a needle-shaped Fe{sub 4}Al{sub 13} IMC layer with length of 0.67 μm to 15.8 μm was found adjacent to the aluminum alloy side. The maximum tensile shear load of the A5052/DP 600 joint was 5.5 KN, with a corresponding molten nugget diameter of 6.3 mm. The fracture morphology of the optimized A5052/DP 600 joint was mainly an elongated dimple fracture accompanied by cleavage fracture. - Highlights: •A5052 and DP 600 with large gaps in properties were investigated by RSW. •The microstructures of RSW joints in DP 600/A5052 were examined detailedly. •The micro/macro-characteristics and strength relations of joints were analyzed.

36 MATERIALS SCIENCE↗

Electromigration-induced back stress in critical solder length for three-dimensional integrated circuits

Because of the miniaturization of electronic devices, the reliability of electromigration has become a major concern when shrinking the solder dimensions in flip-chip joints. Fast reaction between solders and electrodes causes intermetallic compounds (IMCs) to form, which grow rapidly and occupy entire joints when solder volumes decrease. In this study, U-grooves were fabricated on Si chips as test vehicles. An electrode-solder-electrode sandwich structure was fabricated by using lithography and electroplating. Gaps exhibiting well-defined dimensions were filled with Sn3.5Ag solders. The gaps between the copper electrodes in the test sample were limited to less than 15 μm to simulate microbumps. The samples were stressed at various current densities at 100 °C, 125 °C, and 150 °C. The morphological changes of the IMCs were observed, and the dimensions of the IMCs were measured to determine the kinetic growth of IMCs. Therefore, this study focused on the influence of back stress caused by microstructural evolution in microbumps.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Comparison of the magnetic properties of GeMn thin films through Mn L-edge x-ray absorption

X-ray absorption spectroscopy of epitaxial GeMn thin films reveals an experimentally indistinguishable electronic configuration of Mn atoms incorporated in Ge{sub 1?x}Mn{sub x} nanoclusters and in precipitates of the intermetallic compound Mn{sub 5}Ge{sub 3}, respectively. However, the average magnetic response of thin films containing Ge{sub 1?x}Mn{sub x} nanoclusters is lower than the response of films containing Mn{sub 5}Ge{sub 3} precipitates. This reduced magnetic response of Ge{sub 1?x}Mn{sub x} nanoclusters is explained in terms of a fraction of Mn atoms being magnetically inactive due to antiferromagnetic coupling or the presence of structural disorder. A determination of the role of magnetically inactive Mn atoms in the self-assembly of the thermodynamically metastable Ge{sub 1?x}Mn{sub x} nanoclusters seems to be an essential ingredient for an enhanced control of this promising high Curie temperature magnetic semiconductor.

36 MATERIALS SCIENCE↗

Hf{sub 3}Fe{sub 4}Sn{sub 4} and Hf{sub 9}Fe{sub 4−x}Sn{sub 10+x}: Two stannide intermetallics with low-dimensional iron sublattices

This article reports two new Hf-rich intermetallics synthesized using Sn flux: Hf{sub 3}Fe{sub 4}Sn{sub 4} and Hf{sub 9}Fe{sub 4−x}Sn{sub 10+x}. Hf{sub 3}Fe{sub 4}Sn{sub 4} adopts an ordered variant the Hf{sub 3}Cu{sub 8} structure type in orthorhombic space group Pnma with unit cell edges of a=8.1143(5) Å, b=8.8466(5) Å, and c=10.6069(6) Å. Hf{sub 9}Fe{sub 4−x}Sn{sub 10+x}, on the other hand, adopts a new structure type in Cmc2{sub 1} with unit cell edges of a=5.6458(3) Å, b=35.796(2) Å, and c=8.88725(9) Å for x=0. It exhibits a small amount of phase width in which Sn substitutes on one of the Fe sites. Both structures are fully three-dimensional and are characterized by pseudo one- and two-dimensional networks of Fe–Fe homoatomic bonding. Hf{sub 9}Fe{sub 4−x}Sn{sub 10+x} exhibits antiferromagnetic order at T{sub N}=46(2) K and its electrical transport behavior indicates that it is a normal metal with phonon-dictated resistivity. Hf{sub 3}Fe{sub 4}Sn{sub 4} is also an antiferromagnet with a rather high ordering temperature of T{sub N}=373(5) K. Single crystal resistivity measurements indicate that Hf{sub 3}Fe{sub 4}Sn{sub 4} behaves as a Fermi liquid at low temperatures, indicating strong electron correlation. - Graphical abstract: Slightly different growth conditions in Sn flux produce two new intermetallic compounds: Hf{sub 3}Fe{sub 4}Sn{sub 4} and Hf{sub 9}Fe{sub 4−x}Sn{sub 10+x}. - Highlights: • Single crystals of both Hf{sub 3}Fe{sub 4}Sn{sub 4} and Hf{sub 9}Fe{sub 4−x}Sn{sub 10+x} were grown using Sn flux. • The crystal structures were determined using single crystal X-ray diffraction. • The Fe moments in Hf{sub 3}Fe{sub 4}Sn{sub 4} display AFM order below T{sub N}=373 K. • The Fe moments in Hf{sub 9}Fe{sub 4−x}Sn{sub 10+x} display AFM order below T{sub N}=46 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Studies of LaSn{sub 3} as a negative electrode for lithium ion batteries.

The intermetallic compound LaSn{sub 3} has been explored as a possible negative electrode for lithium-ion batteries. A combination of experiment and density functional theory calculations provides evidence that the structure is intolerant to lithium insertion and that the electrochemical reaction occurs via a displacement mechanism. Experiment shows that approximately six Li react initially with LaSn{sub 3}; calculated energetics suggest that during the reaction La{sub 3}Sn{sub 5} and lithiated tin are formed and that the electrode operates by delithiation and relithiation of the Sn particles within an inert lanthanum-tin matrix. LaSn{sub 3} electrodes provide a reversible specific capacity of 200-250 mAh/g, whereas In-substituted electrodes that form a solid solution with LaSn{sub 3}, such as LaSn{sub 2.7}In{sub 0.3}, yield a slightly lower capacity.

74 ATOMIC AND MOLECULAR PHYSICS↗

KINETIC STUDY OF AGING IN A URANIUM-TITANIUM EUTECTOID ALLOY USING THERMOELECTRIC POWER MEASUREMENT

Considerable attention has been given to the study of microstructure evolution and mechanical properties of dilute U-Ti alloys. A typical procedure of heat treatment of the eutectoid uranium-titanium alloy consists of solution treatment in the {gamma} phase, obtaining of soft {alpha}{sup '} martensitic metastable structure by water quenching to room temperature and precipitation hardening by aging at 300-550 deg. C. Depending on employed temperature and time the aging results in GP zone formation through the precipitation reaction {alpha}{sup '}{yields}{alpha}+{delta}. The {delta} phase is a hexagonal U{sub 2}Ti intermetallic compound, responsible for the significant increase in the level of the micro-strain in the metastable {alpha}{sup '} matrix. Thermoelectric power (TEP) measurements have recently gained a growing attention for the characterization of metallurgical properties in steels and other alloys. These measurements, which are based on the Seebeck effect, are sensitive to changes in the electronic structure of the material as result of various metallurgical processes. In the current research, TEP measurement technique was applied as a non destructive assessment technique to characterize the aging kinetics of the quenched uranium-titanium binary alloy. Good correlation has been found between measured TEP, micro-strain evolution, as obtained by using XRD, and hardness values at different heat treatment stages. A reasonable explanation of the correlation between the crystallography changes, micro-strain, TEP measurements and properties is presented.

36 MATERIALS SCIENCE↗

Refill Friction Stir Spot Welding Dissimilar Al/Mg Alloys

Dissimilar Al/Mg alloys were joined by refill friction stir spot welding (RFSSW) in this work. The effect of sleeve plunge depth on microstructure and mechanical properties of the joints was studied. The results showed that sound joint can be obtained at sleeve plunge depth of 2.4 mm. Intermetallic compounds (IMCs) layer, formed by the liquid eutectic phase, were observed at both the sleeve-affected zone and joint center. The IMC at the pin-affected zone was thicker than that at the sleeve-affected zone because of its flow characteristic. Less liquid eutectic phase formed during RFSSW when joint using Mg as the upper sheet because the oxide layer on the Al sheet was hard to break, resulting to thinner IMC layer. The maximum load of 3.6 kN was obtained at 2.6 mm when the Al alloys served as the upper sheet, and the maximum failure of 3.6 kN was also obtained at 2.4 mm when the Mg alloys served as the upper sheet. The RFSSW joint presented shear fracture mode. The XRD patterns showed that the IMC of Al{sub 3}Mg{sub 2} and Al{sub 12}Mg{sub 17} formed inside the joint.

36 MATERIALS SCIENCE↗

The Y{sub 5−x}Mg{sub 24+x}(1.08(4)≤x≤1.30(1)) series and a ternary derivative Ce{sub 6.9}Y{sub 12.5(7)}Mg{sub 92.2}: A comparison of their crystal and electronic structures

The Y{sub 5−x}Mg{sub 24+x} series and a ternary derivative, Ce{sub 0.36}Y{sub 0.64(2)}Mg{sub 4.76}, have been synthesized using high-temperature methods and characterized by both powder and single crystal X-ray diffraction. The Y{sub 5−x}Mg{sub 24+x} series upon quenching from 580 °C crystallizes over the range 1.08(4)≤x≤1.30(1) in the cubic α-Mn structure type (I4{sup ¯}3m, Z=2, Pearson symbol cI58) with mixed occupancy of Y and Mg at the 8c site. As Mg content increases, the corresponding lattice parameter a increases from 11.2337(6) Å for Y{sub 3.92(4)}Mg{sub 25.08} to 11.256(2) Å for Y{sub 3.70(1)}Mg{sub 25.30}. Attempts to replace Y atoms with larger, isovalent Ce atoms yielded Ce{sub 6.9}Y{sub 12.5(7)}Mg{sub 92.2}(=Ce{sub 0.36}Y{sub 0.64(2)}Mg{sub 4.76}), which adopts a defect Sm{sub 11}Cd{sub 45} structure type (F4{sup ¯}3m, Z=8, Pearson symbol cF446.4), with a lattice parameter a=22.443(2) Å that is nearly twice larger than those of the Y{sub 5−x}Mg{sub 24+x} series. The complex crystal structure of this ternary derivative can be described as an ordered, body-centered cubic packing of four chemically and structurally distinctive “nested-polyhedra,” two 27-atom and two 29-atom, α-Mn units. Electronic structure calculations show nearly free electron like behavior, but with a distinctive pseudogap in the density of states curve for the ternary system. - Graphical abstract: Reported is the Mg-rich intermetallic compounds Y{sub 5−x}Mg{sub 24+x} series adopting the cubic α-Mn type structure and its complex ternary derivative Ce{sub 6.9}Y{sub 12.5}Mg{sub 92.2} crystallized in a defect Sm{sub 11}Cd{sub 45} type structure with a nearly twice larger lattice parameter than those of the Y{sub 5−x}Mg{sub 24+x} series. Electronic structure calculations show nearly free electron like behavior, but with a distinctive pseudogap in the density of states curve for the ternary system. Highlights: • The Y{sub 5−x}Mg{sub 24+x} series and Ce{sub 6.9}Y{sub 12.5}Mg{sub 92.2} have been synthesized. • Ce{sub 6.9}Y{sub 12.5}Mg{sub 92.2} is seen as a body-centered cubic packing of “nested-polyhedra”. • Electronic structures show nearly free electron like behavior.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Comparative study of surface modification and D retention between beryllium and beryllides under high flux plasma exposure

The microstructures and deuterium (D) retention properties were investigated for beryllium intermetallic compounds (beryllides), such as Be 12 Ti and Be 12 V, compared to pure beryllium (Be), exposed to high density pure D and helium (He) mixed plasmas. TEM cross-sectional observations revealed the formation of cone structures on the Be surface exposed to the plasmas at a moderate temperature of 573 K. The crystal structure of the cones and the mass loss caused by the plasma exposure implied that the cone structures were generated by sputtering. The Ti or V surface enrichment was observed on both beryllides with no cone structures developed. TDS measurements indicated that He seeding to D plasma caused a ~ 4 times reduction of the D retention for both beryllides, while no reduction was observed for Be. As a result, the beryllide samples exposed to D + He mixture plasmas showed a lower total D retention than in Be.

Hydrogen retention↗

Surface Modification of High-Carbon Steel Using Fiber Laser and Its Thermal, Microstructural and Tribological Analysis

In this study, surface modification of high-carbon steel was carried out using 2 kW fiber laser and thermal, microstructural and tribological characterizations were performed. The process parameters selected for laser surface treatment were laser power (600-1500 W) and scan speed (3000-4500 mm/min). Infrared pyrometer was used to record the surface temperature during the process. The metallographic analysis was carried out using an optical microscope to find the depth and width of the laser-treated zone. Scanning electron microscopy and energy-dispersive spectroscopy were performed to reveal the microstructure and compositional changes taking place in the laser-treated zone. It was observed that the dendritic growth took place from the top surface toward the center of the laser-treated zone. The amount of dendritic growth can be related to the maximum surface temperature generated during the process. XRD analysis indicated the formation of some intermetallic compounds and phase shifts taking place in the laser-treated zone. Residual stress analysis was performed to analyze the amount of stress accumulation in the laser-treated zone. When the temperature cycle was analyzed, it was found that the melting of the steel resulted in the formation of a surface under compressive stress while the non-melt hardened zone developed a surface under tensile stress. The maximum Vickers microhardness value achieved was about 958.8 HV{sub 0.5} for 1500 W power and 3000 mm/min scan speed. Scratch test was performed on the laser-treated track, and it was found that the hardened zone showed better tribological properties with respect to the parent material. Finally, it was observed that the surface roughness value increased with higher heat input probably due to high rate of oxide formation as well as due to the presence of martensite in the laser-treated zone.

36 MATERIALS SCIENCE↗

Pulsed TIG Welding–Brazing of Aluminum–Stainless Steel with an Al-Cu Twin Hot Wire

A TIG welding–brazing process with a twin aluminum hot wire technique was utilized to control the heat input, improve the joint formation, suppress the interfacial intermetallic compounds (IMCs) and increase the joint strength, thereby creating reliable joints between an aluminum alloy and stainless steel with an ER2319 filler. Twin wires with reasonable diameters and filling modes led to a satisfactory weld of parent metals with varying thicknesses. By the hot wire technique, the reasonable range of the welding current was extended and the thickness of the interfacial IMC at the seam bottom was reduced. In addition, both the tensile strength and stability of the joints increased compared with a cold wire. The IMC consisted of θ-(Fe,Cu){sub 4}Al{sub 13} and minor Cr{sub 0.7}Fe{sub 0.3}Al{sub 6}, and the precipitated phases in the weld were Al{sub 2}Cu and Al{sub 2}CuMg. With an increasing welding current, the IMC thickness significantly increased, while the joint strength decreased. The fracture positions of the joints varied with the corresponding welding currents.

36 MATERIALS SCIENCE↗

Depressing effect of 0.1 wt.% Cr addition into Sn-9Zn solder alloy on the intermetallic growth with Cu substrate during isothermal aging

In this paper, the effect of 0.1 wt.% Cr addition into Sn-9Zn lead-free solder alloys on the growth of intermetallic compound (IMC) with Cu substrate during soldering and subsequent isothermal aging was investigated. During soldering, it was found that 0.1 wt.% Cr addition did not contribute to forming the IMC, which was verified as the same phase structure as the IMC for Sn-9Zn/Cu. However, during solid-state isothermal aging, the IMC growth was remarkably depressed by 0.1 wt.% Cr addition in the Sn-9Zn solder, and this effect tended to be more prominent at higher aging temperature. The activation energy for IMC growth was determined as 21.2 kJ mol{sup -1} and 42.9 kJ mol{sup -1} for Sn-9Zn/Cu and Sn-9Zn-Cr/Cu, respectively. The reduced diffusion coefficient was confirmed for the 0.1Cr-containing solder/Cu. Energy-dispersive X-ray mapping and point analysis also showed ZnCr phase existing in solder matrix, which can reduce diffusion rate of Zn atoms.

36 MATERIALS SCIENCE↗

On the formation mechanism of solid-solution Cu-to-Cu joints in the Cu/Ni/Ga/Ni/Cu system

Highlights: • The mechanism of Cu/(Ni,Cu,Ga)/Cu solid-solution joint formation is elaborated. • Ga is the dominant diffusion species in the Cu/Ni/Ga/Ni/Cu bonding system. • Loose and columnar Ni{sub 3}Ga{sub 7} layer is formed by the (001)-textured Ni/Ga reactions. • Cu significantly accelerates the growth of Ni{sub 3}Ga{sub 7} layer by enhancing Ga diffusion. • Supersaturated Cu in Ni{sub 2}Ga{sub 3} phase promotes the formation of the final fcc phase. - Abstract: Copper (Cu)-to-Cu interconnection is crucial in electronic packaging for applications ranging from three-dimensional integrated circuits to die-attachment in wide band-gap devices. Solid-solution phases are innate with better ductility and electrical and thermal conductivity over intermetallic compounds, which are brittle, electrical resistant, and unstable; yet are commonly seen in electronic joints. The desired solid-solution Cu-to-Cu joints have recently been demonstrated using transient-liquid-phase bonding with gallium (Ga) as the filler material to bond Cu substrates with electroplated nickel (Ni) as under-bump-metallurgy. The Cu/Ni/Ga/Ni/Cu couples can fully transform into the Cu/face-centered cubic (fcc)-(Ni,Cu,Ga)/Cu solid-solution joints. However, why and how the solid-solution joints were formed remains unclear. Here we proposed the formation mechanism of the fcc-(Ni,Cu,Ga) solid-solution joints based on five sets of Cu-Ni-Ga couples, namely the Ni/Ga, Ni/Cu/Ga, Ni/Ni/Ga, (Cu,Ni)/Ga, and Cu/Ni/Ni{sub 3}Ga{sub 7}/Ni{sub 3}Ga{sub 7}/Ni/Cu reactions. The roles of each element in the Cu-Ga-Ni interactions as well as the reaction progressions are elaborated.

36 MATERIALS SCIENCE↗

In Situ SEM Observations of Fracture Behavior of Laser Welded–Brazed Al/Steel Dissimilar Joint

Laser welding–brazing of 6061-T6 aluminum alloy to DP590 dual-phase steel with Al-Si12 flux-cored filler wire was performed. The microstructure at the brazing interface was characterized. Fracture behavior was observed and analyzed by in situ scanning electron microscope. The microstructure of the brazing interface showed that inhomogeneous intermetallic compounds formed along the thickness direction, which had a great influence on the crack initiation and propagation. In the top region, the reaction layer at the interface consisted of scattered needle-like Fe(Al,Si){sub 3} and serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the middle region, the compound at the interface was only serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the bottom region, the interface was composed of lamellar-shaped Fe{sub 1.8}Al{sub 7.2}Si. The cracks were first detected in the bottom region and propagated from bottom to top along the interface. At the bottom region, the crack initiated and propagated along the Fe{sub 1.8}Al{sub 7.2}Si/weld seam interface during the in situ tensile test. When the crack propagated into the middle region, a deflection of crack propagation appeared. The crack first propagated along the steel/Fe{sub 1.8}Al{sub 7.2}Si interface and then moved along the weld seam until the failure of the joint. The tensile strength of the joint was 146.5 MPa. Some micro-cracks were detected at Fe(Al,Si){sub 3} and the interface between the steel substrate and Fe(Al,Si){sub 3} in the top region while the interface was still connected.

36 MATERIALS SCIENCE↗

Thermodynamic insights into the intricate magnetic phase diagram of EuAl 4

The tetragonal intermetallic compound EuAl 4 hosts an exciting variety of low-temperature phases. In addition to a charge density wave below 140 K, four ordered magnetic phases are observed below 15.4 K. Recently, a skyrmion phase was proposed based on Hall effect measurements under a c-axis magnetic field. Here, we present a detailed investigation of the phase transitions in EuAl 4 under c-axis magnetic field. Our dilatometry, heat-capacity, DC magnetometry, AC magnetic susceptibility, and resonant ultrasound spectroscopy measurements reveal three magnetic phase transitions not previously reported. The first key result is a detailed H ∥ [001] magnetic phase diagram mapping the seven phases we observe. Second, we identify a high-field phase, phase VII, which directly corresponds to the region were skyrmions have been previously suggested. Our results provide guidance for future studies exploring the complex magnetic interactions and spin structures in EuAl 4 .

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Discovery of Cu 3 Pb

Here, materials discovery enables both realization and understanding of new, exotic, physical phenomena. An emerging approach to the discovery of novel phases is high–pressure synthesis within diamond anvil cells, thereby enabling in–situ monitoring of phase formation. Now, the discovery via high–pressure synthesis of the first intermetallic compound in the Cu–Pb system, Cu 3 Pb is reported. Cu 3 Pb is notably the first structurally characterized mid– to late–first–row transition–metal plumbide. The structure of Cu 3 Pb can be envisioned as a direct mixture of the two elemental lattices. From this new framework, we gain insight into the structure as a function of pressure and hypothesize that the high–pressure polymorph of lead is a possible prerequisite for the formation of Cu 3 Pb. Crucially, electronic structure computations reveal band crossings near the Fermi level, suggesting that chemically doped Cu 3 Pb could be a topologically nontrivial material.

36 MATERIALS SCIENCE↗

A Low-Cost Lightweight Entropic Alloy with High Strength

In this study, a series of lightweight Al–Mg system entropic alloys containing Zn, Cu, and Si were designed based on the order/disorder or entropy, and eutectic concepts. The alloys of Al{sub 58.5}Mg{sub 31.5}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 63}Mg{sub 27}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 66.7}Mg{sub 23.3}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 80}Mg{sub 14}Zn{sub 2.7}Cu{sub 2.7}Si{sub 0.6}; Al{sub 85}Mg{sub 10.5}Zn{sub 2.025}Cu{sub 2.025}Si{sub 0.45}; and Al{sub 90}Mg{sub 7}Zn{sub 1.35}Cu{sub 1.35}Si{sub 0.3} were prepared by induction melting under a high-purity argon atmosphere and then casted into stainless steel molds. The microstructures which were tested in the as-cast state exhibited multiphases and contained apparent volume fractions of intermetallic compounds and solid solutions. Then, the compressive mechanical properties of the alloys were measured, and high fracture strengths of 577, 677, 590, 498, 814, and 794 MPa, respectively, were determined. Strong hardening phenomena were observed in the Al{sub 80}Mg{sub 14}Zn{sub 2.7}Cu{sub 2.7}Si{sub 0.6}, Al{sub 85}Mg{sub 10.5}Zn{sub 2.025}Cu{sub 2.025}Si{sub 0.45}, and Al{sub 90}Mg{sub 7}Zn{sub 1.35}Cu{sub 1.35}Si{sub 0.3} alloys at room temperature, with amazing plasticity percentages of 13.8, 24.8, and 32.7%, respectively. The property differences in the lightweight alloys were analyzed using the following parameters: the critical values of the enthalpy of mixing; atomic size differences; ratio of entropy to enthalpy; valence electron concentration (VEC); and Pauling electronegativity difference. Finally, three of the aforementioned parameters (atomic size difference, enthalpy of mixing, and Pauling electronegativity difference) were regarded in this study as the crucial rules for the lightweight multicomponent alloys.

36 MATERIALS SCIENCE↗