Anomalous effects of Sc substitution and processing on magnetism and structure of (Gd 1-x Sc x ) 5 Ge 4
The kinetic arrest observed in the parent Gd 5 Ge 4 gradually vanishes when a small fraction (x = 0.025, 0.05 and 0.10) of Gd is replaced by Sc in (Gd 1-x Sc x ) 5 Ge 4 , and the magnetic ground state changes from antiferromagnetic (AFM) to ferromagnetic (FM). A first order phase transition coupled with the FM-AFM transition occurs at T C = 41 K for x = 0.05 and at T C = 53 K for x = 0.10 during heating in applied magnetic field of 1 kOe, and the thermal hysteresis is near 10 K. The first-order magnetic transition is coupled with the structural Sm 5 Ge 4 -type to Gd 5 Si 4 -type transformation. The magnetization measured as a function of applied magnetic field shows sharp metamagnetic-like behavior. At the same time, the AFM to paramagnetic transition in (Gd 1 x Sc x ) 5 Ge 4 with x = 0.10, is uncharacteristically broad indicating development of strong short-range AFM correlations above the Néel temperature. Comparison of the magnetization data of bulk, powdered, and metal-varnish composite samples of (Gd 0.95 Sc 0.05 ) 5 Ge 4 shows that mechanical grinding and fabrication of a composite have little effect on the temperature of the first-order transformation, but short-range ordering and AFM/FM ratio below T C are surprisingly strongly affected.