Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CERAMICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Synthesis and characteristics of porous ceramic tubes: a comparison of centrifugal casting and cold isostatic pressing methods

Short porous ceramic tubes in small quantities are needed for membrane-related research and development efforts and can be synthesized by centrifugal casting (CC) or cold isostatic pressing (CIP) methods. Here, this work evaluates the characteristics of porous ceramic tubes prepared by both methods and provides a strategy for selecting the proper method for ceramic tube fabrication, depending on its application. Samarium-doped ceria (SDC) with an average crystallite size of 10 nm was synthesized by a citrate method and used to make porous SDC tubes by the CC and CIP methods under different conditions. Porous SDC tubes were prepared from an aqueous suspension of the SDC powder with polyvinyl alcohol (PVA) using a cylindrical metallic mold, centrifugated at 4000–6000 rpm, followed by sintering in 1200–1500 °C. SDC tubes were also made by the CIP method from the SDC powder placed inside a cylindrical rubber bag followed by isostatic compression at 1379 bar. The pore structure of the SDC tubes was characterized by helium permeation and liquid nitrogen Archimedes method. Due to high compression pressure giving a low porosity green tube, the CIP method with lower sintering temperature produces SDC tubes with much lower porosity and average pore size and similar tortuosity compared to the CC methods. The CIP method should be used to prepare low porosity or dense ceramic tubes, and the CC method should be used for preparing high-porosity ceramic tubes or tubes with pore gradient tube wall.

36 MATERIALS SCIENCE↗

Unravelling the sintering temperature-induced phase transformations in Ba(Fe 0.7 Ta 0.3 )O 3-δ ceramics

This work reports on the fundamental details of the crystal structure and phase transformations in Ba(Fe 0.7 Ta 0.3 )O 3-δ , the best known temperature-independent oxygen-sensing ceramic material for applications in extreme environments. Ba(Fe 0.7 Ta 0.3 )O 3-δ ceramics were synthesized using conventional solid-state ceramic reaction under variable sintering temperatures (T s = 1200–1350 °C). Combined X-ray diffraction (XRD) and high-resolution transmission electron microscopy (TEM) measurements revealed the T s -induced phase transformations and their origin in Ba(Fe 0.7 Ta 0.3 )O 3-δ . Associated with phase transformations, pseudo-cubic (PC) reflections, such as {200} PC , {211} PC , and {220} PC , exhibited distinct anomalies with increasing T s . At T s = 1200 °C, Ba(Fe 0.7 Ta 0.3 )O 3-δ stabilized in mixed orthorhombic + rhombohedral phases (Amm2 + R3m). With increasing T s (≥1250 °C), Ba(Fe 0.7 Ta 0.3 )O 3-δ ceramics stabilized in tetragonal/rhombohedral [P4mm + R3m] mixed phases, while variations in the quantity of the respective phases were observed. Because both structure and crystal chemistry play key roles in achieving enhanced performance in chemical sensing and catalytic converters, detailed understanding of the phase transformations and crystal structure of Ba(Fe 0.7 Ta 0.3 )O 3-δ ceramics, as derived in this work, will be useful to develop chemical sensors with optimum performance for high-temperature and corrosive environments.

36 MATERIALS SCIENCE↗

Field-assisted sintering and phase transition of ZnS-CaLa 2 S 4 composite ceramics

In the present study, zinc sulfide (ZnS) and calcium lanthanum sulfide (CaLa 2 S 4 , CLS) composite ceramics were consolidated via field-assisted sintering of 0.5ZnS-0.5CLS (volume ratio) composite powders at 800–1050 °C. Through sintering curve analyses and microstructural observations, it was determined that between 800 and 1000 °C, grain boundary diffusion was the main mechanism controlling grain growth for both the ZnS and CLS phases within the composite ceramics. The consolidated composite ceramics were determined to be composed of sphalerite ZnS, wurtzite ZnS and thorium phosphate CLS. The sphalerite-wurtzite phase transition of ZnS was further demonstrated to be accompanied by the formation of stacking faults and twins in the ceramics. Furthermore, it was also found that the addition of the CLS phase improved the indentation hardness of the ceramics relative to pure ZnS by homogeneous dispersion of ZnS and CLS small grains.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Entropy-Driven Structural Evolution in Ceramic Oxides

High-entropy ceramics, with five or more elements randomly occupying the same cation crystallographic sites, offer vast compositional diversity and unique properties for material design and applications. However, for many dissimilar elements, entropic stabilization cannot overcome the enthalpic barrier to cation substitution. As a result, most high-entropy ceramics incorporate only a few similar elements, limiting the in-depth exploration of the effect of entropy on ceramic properties. Here, we first use density functional theory to model fluorite crystal structures composed of 1-10 elements and then experimentally present practical fluorite oxide nanostructures containing 1, 3, 8, and 15 metals, as well as a record-breaking 25-element high-entropy ceramic incorporating a diverse palette of rare-earth, transition, alkaline, p-block, and noble metals. As entropy increases, structural and configurational disorder in the solid solution rises, altering structural features such as lattice distortion, crystallinity, homogeneity, defect density, and thermal stability. This research provides new insights and understanding of the role of entropy in stabilizing compositionally complex ceramics.

Liu, Shuo↗

Particle size influence on material properties of BaTiO 3 ceramics fabricated using freeze-form extrusion 3D printing

Barium titanate (BaTiO 3 ; BTO) is a well-known lead-free piezoelectric material commonly used for sensors and actuators applications. There are several traditional methods to fabricate bulk BTO ceramics; however, most of those methods have restrictions regarding being able to produce a functional and complex shape for specific application needs. Recently, additive manufacturing techniques such as binder jetting have enabled the fabrication of complex designs of piezoelectric ceramics. However, the density achieved is relatively low thus narrowing their applications. This paper presents the fabrication of high-density BaTiO 3 ceramics using Freeze-form Extrusion Fabrication (FEF). The influence on material properties for different ceramic particle size was assessed. It was found that parts printed using finer BaTiO 3 particle sizes achieved better results in terms of density, piezoelectric, and dielectric properties. For this study, the 100 nm BaTiO 3 samples achieved 85.24% density, a high piezoelectric property of 204.61pC/N and dielectric permittivity of 2551. These results demonstrated the feasibility of using FEF additive manufacturing to fabricate high-quality functional ceramics with designed geometry in a mold-free fashion.

36 MATERIALS SCIENCE↗

SRNL CRP progress report [Development of Melt Processed Ceramics for Nuclear Waste Immobilization]

A multi-phase ceramic waste form is being developed at the Savannah River National Laboratory (SRNL) for treatment of secondary waste streams generated by reprocessing commercial spent nuclear. The envisioned waste stream contains a mixture of transition, alkali, alkaline earth, and lanthanide metals. Ceramic waste forms are tailored (engineered) to incorporate waste components as part of their crystal structure based on knowledge from naturally found minerals containing radioactive and non-radioactive species similar to the radionuclides of concern in wastes from fuel reprocessing. The ability to tailor ceramics to mimic naturally occurring crystals substantiates the long term stability of such crystals (ceramics) over geologic timescales of interest for nuclear waste immobilization [1]. A durable multiphase ceramic waste form tailored to incorporate all the waste components has the potential to broaden the available disposal options and thus minimize the storage and disposal costs associated with aqueous reprocessing.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

FY2015 ceramic fuels development annual highlights

Key challenges for the Advanced Fuels Campaign are the development of fuel technologies to enable major increases in fuel performance (safety, reliability, power and burnup) beyond current technologies, and development of characterization methods and predictive fuel performance models to enable more efficient development and licensing of advanced fuels. Ceramic fuel development activities for fiscal year 2015 fell within the areas of 1) National and International Technical Integration, 2) Advanced Accident Tolerant Ceramic Fuel Development, 3) Advanced Techniques and Reference Materials Development, and 4) Fabrication of Enriched Ceramic Fuels. High uranium density fuels were the focus of the ceramic fuels efforts. Accomplishments for FY15 primarily reflect the prioritization of identification and assessment of new ceramic fuels for light water reactors which have enhanced accident tolerance while also maintaining or improving normal operation performance, and exploration of advanced post irradiation examination techniques which will support more efficient testing and qualification of new fuel systems.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Assessing the Validity of the Simplified Potential Energy Clock Model for Modeling Glass-Ceramics

Glass-ceramic seals may be the future of hermetic connectors at Sandia National Laboratories. They have been shown capable of surviving higher temperatures and pressures than amorphous glass seals. More advanced finite-element material models are required to enable model-based design and provide evidence that the hermetic connectors can meet design requirements. Glass-ceramics are composite materials with both crystalline and amorphous phases. The latter gives rise to (non-linearly) viscoelastic behavior. Given their complex microstructures, glass-ceramics may be thermorheologically complex, a behavior outside the scope of currently implemented constitutive models at Sandia. However, it was desired to assess if the Simplified Potential Energy Clock (SPEC) model is capable of capturing the material response. Available data for SL 16.8 glass-ceramic was used to calibrate the SPEC model. Model accuracy was assessed by comparing model predictions with shear moduli temperature dependence and high temperature 3-point bend creep data. It is shown that the model can predict the temperature dependence of the shear moduli and 3- point bend creep data. Analysis of the results is presented. Suggestions for future experiments and model development are presented. Though further calibration is likely necessary, SPEC has been shown capable of modeling glass-ceramic behavior in the glass transition region but requires further analysis below the transition region.

36 MATERIALS SCIENCE↗

Recipe for coating ceramic blades for ion trapping

The first batches of ion traps patterned and coated were processed per the standard 3-step clean, air fire, and metallization processes. The third or fourth lot using this process resulted in poorly adhering metallization. Up until this point, the standard process was used to metallize and pattern ceramic ion traps without fail. At about the 4th batch of parts something changed. After the 5th batch, the ceramic ion traps received generally came with some unknown contamination that does not come off in a standard 3-step clean (Lenium Vapor Degreaser, Acetone, IPA) and air fire (860C for 1 hour) for which this process removes the vast majority of all contamination for most ceramic metallization. This is highly unusual. Using HF + Boiling H 2 O 2 is extreme for cleaning the ceramic ion traps. The contamination was never identified and is stubborn to effectively clean. Standard as-fired ceramic should be very easy to clean as if s fired at temperatures greater than 1400°C and not much in terms of contamination should exist at these temperatures, so there must be an intermediate step/process which is imparting this contamination. It is likely a polishing compound or previous polishing contaminant, but also not easily visually distinguishable until after metallization. The halo marks observed on parts might be fingerprints (less likely) or potential polishing marks (more likely) as metallization typically doesn't cover/hide any damage or contamination, but rather quite clearly the opposite, it accentuates it. Blotchy appearances in the metallization usually indicated an adhesion issue. As a result of the fragility of the parts (yield loss due to handling) and difficulty in identifying the contamination during cleaning, we have taken a conservative approach of HF + H 2 O 2 cleaning for all batches after the contamination and adhesion issues were identified.

36 MATERIALS SCIENCE↗

Glass-Ceramic Material Modeling

Glass-ceramics are a unique class of materials in which the growth of a ceramic phase(s) may be induced in an inorganic glass resulting in a microstructurally heterogeneous material with both glass and ceramic phases. This specialized processing is often referred to as "ceramming''. A wide variety of such materials have been developed through the use of different initial glass compositions and thermomechanical processing routes and that have enabled applications in dentistry, consumer kitchenware, and telescopes mirrors. These materials may also exhibit large apparent coefficients of thermal expansion making them attractive for consideration in glass-ceramic seals. These large apparent coefficients of thermal expansion often arise from silica polymorphs, such as cristobalite, undergoing a solid-to-solid phase transformations producing additional non-linearity in the effective material response.

36 MATERIALS SCIENCE↗

Design Methods, Tools, and Data for Ceramic Solar Receivers Year 1 Continuation Report

This report describes the first year of work on a project to develop the methods, tools, and data required to analyze high temperature ceramic Concentrating Solar Power (CSP) components. This first year focused on developing the methods and data required for a time-independent assessment of potential components, focusing in particular on ceramic solar receivers. The report describes both model development and testing work focused on accomplishing this goal. Our overall conclusion is that high temperature ceramic CSP components are viable and could provide a means to overcome the expected low reliability and short service life for equivalent components constructed from Ni-based superalloys. Based on the results reported here, we recommend the project continue to Phase II which will develop more sophisticated, realistic models for time-dependent failure of ceramics operating in expected CSP component conditions and develop the time-dependent ceramic test data needed to parameterize these models, using commercial SiC as a reference material.

14 SOLAR ENERGY↗

Multiscale Porous High-temperature Heat Exchanger Using Ceramic Co-extrusion

In this project, our MIT, Purdue, and GE team aims to design, model, fabricate, and test a novel high temperature, compact, and durable ceramic heat exchanger to be operated under high temperature and pressure conditions for aerospace applications. Our approach is grounded in introducing multiscale porosity, i.e., centimeter-scale channels embedded with micrometer-scale channels, into the ceramic heat exchanger to significantly improve its heat transfer performance and mechanical strength while maintaining minimal pressure losses. We first developed high-fidelity thermal-fluid-mechanical model capable of precisely capturing the heat transfer rate, temperature profile, pressure drop, and mechanical stress throughout the entire heat exchanger design. Guided by our model, we identified the optimal design parameters for the SiC heat exchanger body and manifolds. Then, we established a completed fabrication procedure to create multiscale features in the ceramic heat exchanger, including co-extrusion, lamination, burnout, and sintering. We fabricated multiple heat exchanger bodies consisting of 6 × 6 and 3 × 3 centimeter-scale channels where each individual centimeter-scale channel comprises 625 crack-free microchannels with 90 μm × 90 μm opening. Owing to the multiscale features, our fabricated heat exchanger bodies exhibited desirable mechanical strength with 156 MPa flexural strength under 1300 Celsius degree. Despite the demonstrated highly tailorable microscopic features and superior mechanical strength, we identified delamination due to the complex interaction among ceramic, polymer, and gas species can be a critical challenge to create fully defect-free heat exchanger, which requires further fundamental investigations in future works. To test the heat exchanger performance, we constructed a high-temperature and high-pressure experimental apparatus that can be safely operated under 400 Celsius degree and 4 bar. With insights gained from mechanistic modeling, material development, and detailed characterization, a cost model was finally developed to understand the market potential of the developed technology, where a cost of $43,000 Celsius degree/kW was envisioned. This project developed a transformative approach to high-performance heat exchanger design. The thermal-fluid-mechanical design approach developed in this project can serve as a generic tool to guide the design of various heat-exchangers operated under high-temperature and high-pressure conditions. The material fabrication approach established in this project can be a useful guide for ceramic processing at extreme length scales.

42 ENGINEERING↗

A Computer Design Tool for Ceramic Receivers

Gen3 solar receivers and other components will experience a combination of high temperatures and high stress caused by thermal stress and internal pressure. Under these conditions metallic components, even those manufactured from nickel-based superalloys, have poor reliability. Engineering ceramics could be a solution, as these materials have excellent high temperature strength. However, accurately assessing the reliability of a ceramic component operating in these conditions requires an entirely different approach compared to metallic materials. This paper describes the implementation of statistical models for evaluating the reliability of high temperature ceramic components in srlife – an open-source software package for estimating the life of high temperature concentrating solar power equipment. This new capability allows users to make fair comparisons between competing metallic and ceramic component designs and to accurately assess the plant efficiency and economics of ceramic solar receivers and other components.

Messner, Mark (ORCID:0000000200404385)↗

Time-Dependent Failure Assessment of Ceramic Receivers

The outlet temperature targets for Gen 3 Concentrating Solar Power (CSP) systems pose a significant challenge to the structural reliability of high temperature metallic components, including those manufactured from nickel-based superalloys. Advanced ceramics present a potential solution due to their excellent high-temperature strength. However, accurate assessment of ceramic components requires an entirely different approach compared to metallic components. This paper describes the implementation of time-dependent reliability analysis of ceramic components in srlife – an open-source software package for estimating the life of high temperature CSP components. This new capability will allow high temperature CSP designers to make fair comparisons between competing metallic and ceramic designs and accurately assess the performance of different ceramic materials for CSP receivers and other components. The current version of the tool is available at https://github.com/Argonne-National-Laboratory/srlife.

Barua, Bipul (ORCID:0000000247184113)↗

Ceramic nanostructures and methods of fabrication

Structures and methods for the fabrication of ceramic nanostructures. Structures include metal particles, preferably comprising copper, disposed on a ceramic substrate. The structures are heated, preferably in the presence of microwaves, to a temperature that softens the metal particles and preferably forms a pool of molten ceramic under the softened metal particle. A nano-generator is created wherein ceramic material diffuses through the molten particle and forms ceramic nanostructures on a polar site of the metal particle. The nanostructures may comprise silica, alumina, titania, or compounds or mixtures thereof.

36 MATERIALS SCIENCE↗

Use of additives to improve microstructures and fracture resistance of silicon nitride ceramics

A high-strength, fracture-resistant silicon nitride ceramic material that includes about 5 to about 75 wt-% of elongated reinforcing grains of beta-silicon nitride, about 20 to about 95 wt-% of fine grains of beta-silicon nitride, wherein the fine grains have a major axis of less than about 1 micron; and about 1 to about 15 wt-% of an amorphous intergranular phase comprising Si, N, O, a rare earth element and a secondary densification element. The elongated reinforcing grains have an aspect ratio of 2:1 or greater and a major axis measuring about 1 micron or greater. The elongated reinforcing grains are essentially isotropically oriented within the ceramic microstructure. The silicon nitride ceramic exhibits a room temperature flexure strength of 1,000 MPa or greater and a fracture toughness of 9 MPa-m.sup.(1/2) or greater. The silicon nitride ceramic exhibits a peak strength of 800 MPa or greater at 1200 degrees C. Also included are methods of making silicon nitride ceramic materials which exhibit the described high flexure strength and fracture-resistant values.

36 MATERIALS SCIENCE↗

Fuel cell integral bundle assembly including ceramic open end seal and vertical and horizontal thermal expansion control

A plurality of integral bundle assemblies contain a top portion with an inlet fuel plenum and a bottom portion containing a base support, the base supports a dense, ceramic air exhaust manifold having four supporting legs, the manifold is below and connects to air feed tubes located in a recuperator zone, the air feed tubes passing into the center of inverted, tubular, elongated, hollow electrically connected solid oxide fuel cells having an open end above a combustion zone into which the air feed tubes pass and a closed end near the inlet fuel plenum, where the open end of the fuel cells rest upon and within a separate combination ceramic seal and bundle support contained in a ceramic support casting, where at least one flexible cushion ceramic band seal located between the recuperator and fuel cells protects and controls horizontal thermal expansion, and where the fuel cells operate in the fuel cell mode and where the base support and bottom ceramic air exhaust manifolds carry from 85% to all of the weight of the generator.

42 ENGINEERING↗

Experimental Determination of the Speciation, Partitioning, and Release of Perrhenate as a Chemical Surrogate for Pertechnetate from a Sodalite-Bearing Multiphase Ceramic Waste Form

A key component to closing the nuclear fuel cycle is the storage and disposition of nuclear waste in geologic systems. Multiphase ceramic waste forms have been studied extensively as a potential host matrix for nuclear waste. Understanding the speciation, partitioning, and release behavior of radionuclides immobilized in multiphase ceramic waste forms is a critical aspect of developing the scientific and technical basis for nuclear waste management. In this study, we evaluated a sodalite-bearing multiphase ceramic waste form (i.e., fluidized-bed steam reform sodium aluminosilicate [FBSR NAS] product) as a potential host matrix for long-lived radionuclides, such as technetium (99Tc). The FBSR NAS material consists primarily of nepheline (ideally NaAlSiO4), anion-bearing sodalites (ideally M8[Al6Si6O24]X2, where M refers to alkali and alkaline earth cations and X refers to monovalent anions), and nosean (ideally Na8[AlSiO4]6SO4). Bulk x-ray absorption fine structure analysis of the multiphase ceramic waste form, suggest rhenium (Re) is in the Re(VII) oxidation state and has partitioned to a Re-bearing sodalite phase (most likely a perrhenate sodalite Na8[Al6Si6O24](ReO4)2). Rhenium was added as a chemical surrogate for 99Tc during the FBSR NAS synthesis process. The weathering behavior of the FBSR NAS material was evaluated under hydraulically unsaturated conditions with deionized water at 90 C. The steady-state Al, Na, and Si concentrations suggests the weathering mechanisms are consistent with what has been observed for other aluminosilicate minerals and include a combination of ion exchange, network hydrolysis, and the formation of an enriched-silica surface layer or phase. The steady-state S and Re concentrations are within an order of magnitude of the nosean and perrhenate sodalite solubility, respectively. The order of magnitude difference between the observed and predicted concentration for Re and S may be associated with the fact that the anion-bearing sodalites contained in the multiphase ceramic matrix are present as mixed-anion sodalite phases. These results suggest the multiphase FBSR NAS material may be a viable host matrix for long-lived, highly mobilie radionuclides which is a critical aspect in the management of nuclear waste.

Pierce, Eric M↗