Molten fluid apparatus with solid non-brittle electrolyte
A battery includes a fluid negative electrode and a fluid positive electrode separated by a solid electrolyte at least when the electrodes and electrolyte are at an operating temperature. The solid electrolyte includes ions of the negative electrode material forming the fluid negative electrode and has a softness less than beta-alumina solid electrolyte (BASE) ceramics. In one example, the fluid negative electrode comprises lithium (Li), the fluid positive electrode comprises sulfur (S) and the solid electrolyte comprises lithium iodide (LiI).
PRE-COMPRESSION KOLSKY TENSION BAR TECHNIQUE FOR DYNAMIC DIRECT TENSILE CHARACTERIZATION OF BRITTLE MATERIALS
Explore the source record for details and available documents.
Molten fluid apparatus with solid non-brittle electrolyte
A battery includes a fluid negative electrode and a fluid positive electrode separated by a solid electrolyte at least when the electrodes and electrolyte are at an operating temperature. The solid electrolyte comprises a salt formed by ions of the negative electrode material forming the fluid negative electrode. In one example, the fluid negative electrode comprises lithium (Li), the fluid positive electrode comprises sulfur (S) and the solid electrolyte comprises lithium iodide (LiI).
Directionally solidified composite systems under evaluation
The directionally solidified eutectic in-situ composites being evaluated for use as turbine materials range from ductile-ductile systems, where both matrix and reinforcement are ductile, to brittle-brittle systems, where both phases are brittle. The alloys most likely to be used in gas turbine engines in the near term are the lamellar ductile-semi ductile alloys gamma prime-delta, Ni3Al-Ni3Nb and gamma/gamma prime-delta Ni,Cr,Cb,Al/Ni3Al-Ni3Nb and the fibrous ductile-brittle alloys M-MC CoTaC or NiTaC and M-M7C3(Co,Cr,Al)-(Cr,Co)7C3. The results of tests are given which indicate that gamma prime strengthened NiTaC alloys and a (Co,Cr,Al)7C3 have greater tensile strength than the strongest superalloys at temperatures up to about 600 C. The gamma prime-delta and gamma/gamma prime-delta alloys in the Ni,Al,Nb(Cr) systems have greater tensile strength than the superalloys at temperatures greater than 800 C. At low stresses fibrous carbide reinforced eutectic alloys have longer lives at high temperatures than the strongest superalloys. Lamellar delta, Ni3Nb reinforced eutectic alloys have longer lives at high temperatures than the strongest superalloys at all stresses. The experience currently being gained in designing with the brittle ceramics SiC and Si3N4 may eventually be applied to ceramic matrix eutectic in-situ composites. However, the refractory metal fiber reinforced brittle-ductile systems may find acceptance as turbine materials before the ceramic-ceramic brittle-brittle systems.
Strength and deformation properties of basaltic lava flows on planetary surfaces
Basaltic rocks are thought to constitute a volumetrically significant rock type on the Moon, Mercury, Mars, and Venus, in addition to the Earth. Spacecraft images of surfaces with known or suspected basaltic composition on these bodies, particularly on Venus, indicate that these rocks have been deformed in the brittle regime to form faults and perhaps dilatant cracks, in addition to folding and more distributed types of deformation. Predictions of brittle fracture or other types of deformation are made by comparing calculated stresses from a tectonic model to some criterion for rock strength. Common strength criteria used in the planetary science literature for near-surface deformation include a Griffith tensile-strength criterion for intact rock, a Mohr envelope for intact basalt, and a brittle strength envelope based on Byerlee's law of rock frictional resistance. However, planetary terrains of basaltic composition consist of much more than just intact basaltic rock. The aggregate basaltic material, termed the 'rock mass,' consists of both the intact rock and the associated fracture, faults, lithologic contacts, and other discontinuous surfaces. A basaltic rock mass is the relevant material for which strength properties must be defined and calculated model stresses must be compared to in order to more accurately predict brittle deformation. For example, the various strengths of a rock mass are less than that of intact material of the same composition. This means that tectonic models which compare stresses to intact failure strengths overestimate the stresses required for fracture and so underestimate the extent and magnitude of brittle deformation predicted in these models. On the other hand, rock mass shear strength can be greater than that predicted from Byerlee's law. The concept of rock mass strength is central to many engineering design studies in which calculated stresses are used to predict brittle fracture, and this experience indicates that brittle strength envelopes which assume properties for intact rock (Griffith parabolas) or sliding along a single, continuous surface (Byerlee's law) inadequately characterize the tensile, compressive, and shear strengths of rock masses. The criterion adopted here to relate stresses to rock mass fracture is based on a Griffith-type curve for tensile normal stress and a concave downward curve for compressive normal stress. It is the only available criterion that explicitly considers the weakening effects of discontinuities within the rock mass on the stress state required for fracture.
Effect of pore pressure buildup on slowness of rupture propagation
Pore fluid pressure is known to play an important role in brittle fracture initiation and propagation, yet the underlying mechanisms remain unclear. We conducted triaxial experiments on saturated porous sandstones to investigate effects of pore pressure buildup on the slowness of shear rupture propagation at different confining pressures. At low to intermediate confinements, rocks fail by brittle faulting, and pore pressure buildup causes a reduction in rock’s shear strength but does not induce measurable differences in slip behavior. When the confinement is high enough to prohibit dynamic faulting, rocks fail in the brittle-ductile transitional regime. In the transitional regime, pore pressure buildup promotes slip instability on an otherwise stably sliding fracture. Compared to those observed in the brittle regime, the slip rate, stress drop, and energy dissipated during rupture propagation with concurrent pore pressure buildup in the transitional regime are distinctively different. When decreasing confining pressure instead, the slip behavior resembles the ones of the brittle regime, emphasizing h ow the observed slowness is related to excess pore pressure beyond the effective pressure phenomenon. Analysis of the mechanical data using existing theoretical models confirms these observations. Quantitative microstructural analyses reveal that increasing pore pressure lessens the dilatancy hardening during failure, thus enhances slip along the localized zone in the transitional regime. Lastly, our experimental results suggest that pore pressure buildup induces slow slip in the transitional regime, and slip rates along a shear fracture may vary considerably depending on effective stress states.
Statistical Models of Fracture Relevant to Nuclear-Grade Graphite: Review and Recommendations
The nuclear-grade (low-impurity) graphite needed for the fuel element and moderator material for next-generation (Gen IV) reactors displays large scatter in strength and a nonlinear stress-strain response from damage accumulation. This response can be characterized as quasi-brittle. In this expanded review, relevant statistical failure models for various brittle and quasi-brittle material systems are discussed with regard to strength distribution, size effect, multiaxial strength, and damage accumulation. This includes descriptions of the Weibull, Batdorf, and Burchell models as well as models that describe the strength response of composite materials, which involves distributed damage. Results from lattice simulations are included for a physics-based description of material breakdown. Consideration is given to the predicted transition between brittle and quasi-brittle damage behavior versus the density of damage (level of disorder) within the material system. The literature indicates that weakest-link-based failure modeling approaches appear to be reasonably robust in that they can be applied to materials that display distributed damage, provided that the level of disorder in the material is not too large. The Weibull distribution is argued to be the most appropriate statistical distribution to model the stochastic-strength response of graphite.
The Effect of Prestrain Temperature on Kinetics of Static Recrystallization, Microstructure Evolution, and Mechanical Properties of Low Carbon Steel
In this research, the samples of a low carbon steel sheet were rolled up to a thickness prestrain of 67% at three different temperatures consisted of room, blue brittleness, and subzero temperature. Microhardness, SEM, and tensile tests were carried out to evaluate the static recrystallization kinetics defined by the Avrami equation, microstructural evolution, and mechanical properties. It was found that the Avrami exponent is altered with change in prestrain temperature and it achieves the value of 1 to 1. 5. Moreover, it was indicated that prestraining at subzero temperature followed by annealing at 600 °C leads to considerable enhancement in tensile properties and kinetics of static recrystallization compared to room and blue brittleness temperatures. The prestraining at blue brittleness temperature followed by annealing treatment caused, however, a higher strength and faster kinetics compared with that at room temperature. It was concluded that although from the steel ductility point of view, the blue brittleness temperature is called an unsuitable temperature, but it can be used as prestraining temperature to develop noticeable combination of strength and ductility in low carbon steel.
Microstructure and Mechanical Property Improvement in Laser-Welded TC4 Titanium Alloy and 301L Stainless Steel Joints Without Filler Metal
Pulsed laser welding of Ti alloy to stainless steel (SS) has been applied without filler metal. When the laser beam was focused on the Ti alloy–SS interface, large volumes of Ti-Fe intermetallics were formed in the joint. These Ti-Fe intermetallics were highly brittle, causing the joint to crack spontaneously after welding. The brittle coarse Ti-Fe intermetallics seriously deteriorates the joint strength of Ti alloy and SS; therefore, it is necessary to control the quantities and distributions of brittle Ti-Fe intermetallics in the joint. The amount of melted base materials was controlled by changing laser offset to control the melted proportion and thus control the quantity and distribution of brittle Ti-Fe intermetallics in weld. When laser beam was on the SS side, melting amount of Ti alloy in weld was decreased. When laser beam was on the Ti alloy side, melting amount of SS in weld was decreased. When the laser offset was 0.35 mm away from SS side, the sample realizes the effective connection between Ti alloy and SS. A compound layer was formed at the SS side with the main microstructure of β-Ti and TiFe{sub 2}. The joint fractured at the compound layer with the maximum tensile strength of 182 MPa. Microstructures and mechanical properties of joints were improved by changing laser offset.
Texture evolution and microcracking mechanisms in as-extruded and cross-rolled conditions of a 14YWT nanostructured ferritic alloy
Cr-stabilized nanostructured ferritic alloys (NFAs), dispersion strengthened by an ultra-high density of nanooxides, are attractive candidates for many nuclear energy applications due to their high-temperature strength, in-service stability and remarkable irradiation tolerance. However, typical NFA deformation processing paths lead to crystallographic texturing, formation of brittle microstructures and low toughness orientations, making fabricating components very difficult. In this paper, we characterize the dislocation-mediated deformation mechanisms that lead to the brittle texture component. The as-extruded bar is less brittle than the cross-rolled plate, which contains a large population of pre-existing cleavage microcracks. More generally, deformed ODS/NFAs are most often textured and have anisotropic low toughness orientations, even absent microcracks. However, cross-rolling produces a very high volume fraction of a plate normal {001}<110>-texture component, which constitutes the brittle cleavage system in iron. Finally, microcracks propagate along {001} low angle deformation induced subgrain boundaries in <110> directions after nucleating by the Cottrell mechanism.
Faulting of natural serpentinite: Implications for intermediate-depth seismicity
The seismic potential of serpentinites at high pressure was investigated via deformation experiments on cored natural serpentinite samples, during which micro-seismicity was monitored by recording Acoustic Emissions (AEs). Deformation was performed at pressures of 3–5 GPa, using a Deformation-DIA device, and over a wide range of temperatures, both within and outside antigorite's stability field. Below 400 °C, serpentinite deformation involves “silent” semi-brittle mechanisms, even in cases where strain localization is observed. At high temperature (i.e., above 600 °C), despite conditions propitious to dehydration embrittlement (i.e., fast strain rates and reaction kinetics), joint deformation and dehydration lead to ductile shear, without generation of AEs. Brittle behavior was observed in a narrow temperature window ca. 500 °C. In this latter case, AEs are consistently observed upon faulting and extremely sharp strain localization is observed in recovered samples. The resulting microstructures are consistent with the inverse ductile-to-brittle transition proposed by Proctor and Hirth (2016) in antigorite. This may therefore be a source of seismicity in subducting slabs at mantle pressures and temperatures from 500 to 600 °C. However, the acoustic signal observed here is orders of magnitude weaker than what is obtained at low PT conditions with brittle failure, consistently with low radiation efficiency of serpentinite faulting (Prieto et al., 2013) and suggests that other mechanisms are responsible for large intermediate-depth earthquakes. In fact, the present results are in line with a recent study (Ferrand et al., 2017), that suggests that intermediate earthquakes are likely induced by mechanical instabilities due to dehydration in partly hydrated peridotites.
Irradiation dose and temperature dependence of fracture toughness in high dose HT9 steel from the fuel duct of FFTF
To expand the knowledge base for fast reactor core materials, fracture toughness has been evaluated for high dose HT9 steel using miniature disk compact tension (DCT) specimens. The HT9 steel DCT specimens were machined from the ACO-3 fuel duct of the Fast Flux Test Facility (FFTF), which achieved high doses in the range of 3–148 dpa at 378–504 C. The static fracture resistance (J-R) tests have been performed in a servohydraulic testing machine in vacuum at selected temperatures including room temperature, 200 C, and each irradiation temperature. Brittle fracture with a low toughness less than 50 MPa pm occurred in room temperature tests when irradiation temperature was below 400 C, while ductile fracture with stable crack growth was observed when irradiation temperature was higher. No fracture toughness less than 100 MPa pm was measured when the irradiation temperature was above 430 C. It was shown that the influence of irradiation temperature was dominant in fracture toughness while the irradiation dose has only limited influence over the wide dose range 3–148 dpa. A slow decrease of fracture toughness with test temperature above room temperature was observed for the nonirradiated and high temperature (>430 *C) irradiation cases, which indicates that the ductile–brittle transition temperatures (DBTTs) in those conditions are lower than room temperature. A comparison with the collection of existing data confirmed the dominance of irradiation temperature in the fracture toughness of HT9 steels.
A multiscale microstructural approach to ductile-phase toughened tungsten for plasma-facing materials
Increasing fracture toughness and decreasing the ductile-brittle transition temperature of a tungsten-alloy has been shown to be feasible by ductile-phase toughening of tungsten. In this method, a ductile phase is included in a brittle tungsten matrix to prevent fracture propagation by crack bridging or crack deflection. This paper models the deformation behavior of ductile phase toughened tungsten materials such as tungsten-copper composites using a multiscale modeling approach that involves a microstructural dual-phase (copper-tungsten) region of interest where the constituent phases are finely discretized and are described by a continuum damage mechanics model. Large deformation, damage and fracture are allowed to occur and are modeled in this region that is connected to the adjacent homogenized elastic regions to form a macroscopic structure such as a test specimen. This paper illustrates such a multiscale modeling approach to analyze un-notched and single-edge notched (SENB) tungsten-copper composite specimens subjected to three-point bending. The predicted load-displacement responses and crack propagation patterns are compared to the corresponding experimental results to validate the model.
Investigation of the temperature-dependent failure processes in PVD Cr-coated ZIRLO nuclear fuel cladding using in situ X-ray micro-tomography imaging
In this work, an accident tolerant fuel cladding system with Cr coating deposited using physical vapour deposition (PVD) method onto commercial Optimized ZIRLO™ was studied. The cladding tubes were machined into C-rings and loaded to failure under compression with real-time synchrotron micro-X-ray computed tomography (XCT) imaging at room temperature (RT), 345 °C, 650 °C and 950 °C in argon (Ar) atmosphere. The mechanical behaviour and failure processes were found strongly temperature-dependent where the Cr coating showed brittle fracture at RT and 345 °C, ductile fracture at 650 °C and a reversion to brittle fracture at 950 °C. Nanoindentation measurements and scanning electron microscopy (SEM) imaging were conducted on the materials after high temperature testing. It was found that recrystallisation of the Cr coating occurred at elevated temperatures, which significantly affected its local properties hence the failure behaviour at different temperatures. This work represents the first in situ 3D XCT observation of progressive failure processes in PVD Cr-coated ZIRLO claddings up to 950 °C providing critical insights into its brittle-to-ductile transition (BDTT) behaviour and subsequent ductile-to-brittle reversion with the increase in temperature. Moreover, results are compared with other PVD Cr-coated Zircaloy materials from open literature; the influences of the coating microstructure and local properties on the failure stress/strain and fracture processes are discussed.
Development and deployment of constitutive softening routines in Eulerian hydrocodes.
The state of the art in failure modeling enables assessment of crack nucleation, propagation, and progression to fragmentation due to high velocity impact. Vulnerability assessments suggest a need to track material behavior through failure, to the point of fragmentation and beyond. This eld of research is particularly challenging for structures made of porous quasi-brittle materials, such as ceramics used in modern armor systems, due to the complex material response when loading exceeds the quasi-brittle material's elastic limit. Further complications arise when incorporating the quasi-brittle material response in multi-material Eulerian hydrocode simulations. In this report, recent e orts in coupling a ceramic materials response in the post-failure regime with an Eulerian hydro code are described. Material behavior is modeled by the Kayenta material model [2] and Alegra as the host nite element code [14]. Kayenta, a three invariant phenomenological plasticity model originally developed for modeling the stress response of geologic materials, has in recent years been used with some success in the modeling of ceramic and other quasi-brittle materials to high velocity impact. Due to the granular nature of ceramic materials, Kayenta allows for signi cant pressures to develop due to dilatant plastic ow, even in shear dominated loading where traditional equations of state predict little or no pressure response. When a material's ability to carry further load is compromised, Kayenta allows the material's strength and sti ness to progressively degrade through the evolution of damage to the point of material failure. As material dilatation and damage progress, accommodations are made within Alegra to treat in a consistent manner the evolving state.
Real-Time Observation of Nanoscale Kink Band Mediated Plasticity in Ion-Irradiated Graphite: An In Situ TEM Study
Graphite IG-110 is a synthetic polycrystalline material used as a neutron moderator in reactors. Graphite is inherently brittle and is known to exhibit a further increase in brittleness due to radiation damage at room temperature. To understand the irradiation effects on pre-existing defects and their overall influence on external load, micropillar compression tests were performed using in situ nanoindentation in the Transmission Electron Microscopy (TEM) for both pristine and ion-irradiated samples. While pristine specimens showed brittle and subsequent catastrophic failure, the 2.8 MeV Au2+ ion (fluence of 4.378 × 1014 cm−2) irradiated specimens sustained extensive plasticity at room temperature without failure. In situ TEM characterization showed nucleation of nanoscale kink band structures at numerous sites, where the localized plasticity appeared to close the defects and cracks while allowing large average strain. We propose that compressive mechanical stress due to dimensional change during ion irradiation transforms buckled basal layers in graphite into kink bands. The externally applied load during the micropillar tests proliferates the nucleation and motion of kink bands to accommodate the large plastic strain. The inherent non-uniformity of graphite microstructure promotes such strain localization, making kink bands the predominant mechanism behind unprecedented toughness in an otherwise brittle material.
Directionally solidified composite systems under evaluation
The directionally solidified eutectic in-situ composites being evaluated for use as turbine materials range from ductile-ductile systems, where both matrix and reinforcement are ductile, to brittle-brittle systems, where both phases are brittle. The alloys most likely to be used in gas turbine engines in the near term are the lamellar ductile-semiductile alloys gamma prime-delta, Ni3Al-Ni3Nb and gamma/gamma prime-delta Ni,Cr,Cb,Al/Ni3Al-Ni3Nb and the fibrous ductile-brittle alloys M-MC CoTaC or NiTaC and M-M7C3(Co,Cr,Al)-(Cr,Co)7C3. Gamma-prime strengthened NiTaC alloys and a (Co,Cr,Al)-(Co,Cr)7C3 have greater tensile strength than the strongest superalloys at temperatures up to about 600 C. The gamma prime-delta and gamma/gamma prime-delta alloys in the Ni,Al,Nb(Cr) systems have greater tensile strength than the superalloys at temperatures greater than 800 C. At low stresses fibrous carbide reinforced eutectic alloys have longer lives at high temperatures than the strongest superalloys. Lamellar delta, Ni3Nb reinforced eutectic alloys have longer lives at high temperatures than the strongest superalloys at all stresses.