Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “surface oxidation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Energy dependence of the trapping of uranium atoms by aluminum oxide surfaces

The energy dependence of the trapping probability for sputtered U-235 atoms striking an oxidized aluminum collector surface at energies between 1 eV and 184 eV was measured. At the lowest energies, approximately 10% of the uranium atoms are not trapped, while above 10 eV essentially all of them stick. Trapping probabilities averaged over the sputtered energy distribution for uranium incident on gold and mica are also presented.

Librecht, K. G.↗

Measurement of the O18 to O16 isotope ratio for characterizing oxide surface layers on LDEF samples

Calculations indicate that measurement of the O-16 to O-18 isotope ratio in oxide layers formed on the surfaces of the Long Duration Exposure Facility (LDEF) samples would provide a powerful tool for distinguishing between layers formed at high altitudes and layers formed at low altitudes, as for example during the retrieval of a satellite. In principle, this ratio may be used to date the formation of the oxide layers.

Sagalyn, Paul L.↗

Acidic attack of perfluorinated alkyl ether lubricant molecules by metal oxide surfaces

The reactions of linear perfluoropolyalkylether (PFAE) lubricants with alpha-Fe2O3 and Fe2O3-based solid superacids were studied. The reaction with alpha-Fe2O3 proceeds in two stages. The first stage is an initial slow catalytic decomposition of the fluid. This reaction releases reactive gaseous products which attach the metal oxide and convert it to FeF3. The second stage is a more rapid decomposition of the fluid, effected by the surface FeF3. A study of the inital breakdown step was performed using alpha-Fe2O3, alpha-Fe2O3 preconverted to FeF3, and sulfate-promoted alpha-Fe2O3 superacids. The results indicate that the breakdown reaction involves acidic attack at fluorine atoms on acetal carbons in the linear PFAE. Possible approaches to combat the problem are outlined.

Zehe, Michael J.↗

Acidic attack of perfluorinated alkyl ether lubricant molecules by metal oxide surfaces

The reactions of linear perfluoropolyalkylether (PFAE) lubricants with alpha-Fe203 and Fe203-based solid superacids were studied. The reaction with alpha-Fe203 proceeds in two stages. The first stage is an initial slow catalytic decomposition of the fluid. This reaction releases reactive gaseous products which attach the metal oxide and convert it to FeF3. The second stage is a more rapid decomposition of the fluid, effected by the surface FeF3. A study of the initial breakdown step was performed using alpha-Fe203, alpha-Fe203 preconverted to FeF3, and sulfate-promoted alpha-Fe203 superacids. The results indicate that the breakdown reaction involves acidic attack at fluorine atoms on acetal carbons in the linear PFAE. Possible approaches to combat the problem are outlined.

Zehe, Michael J.↗

Growth of Si spherical crystals and the surface oxidation (M-9)

Nearly 90 percent of semiconductor devices are produced with Si single crystals as the starting materials. For instance, the integrated circuits (IC), which are used in almost all electronic equipments such as TV, tape recorders, audio amplifiers, etc., are made after various processings of Si single crystal wafers. In these wafers, the same controlled amounts of impurities are added and the uniformities in their distributions are extremely important. Growth under microgravity makes it possible to eliminate the buoyancy-driven convection in the melt, which is one of the main origins of convections which results in non-uniformity of the impurity. Another source of convection is known as Marangoni convection which is driven on the free surface when a temperature gradient occurs. One of the merits of microgravity experimentation is that the detailed study of this convection becomes possible. Another important advantage of microgravity is that growth of crystals without a crucible is possible. This makes it possible to study melt growth without the strain which is usually introduced on the ground. Nevertheless, we should repeat and analyze many growth experiments in space to get reliable results. However, since in the FMPT, the time for the experiment is limited, we plan to carry out two kinds of very simple and basic experiments as the first step for the semiconductor growth experiment. In the first experiment, we use single crystal Si sphere as the starting material and as shown, this sphere is heated in the furnace at a slightly higher temperature than the melting point. After the melting front moves nearly half way to its center, the temperature is decreased to stop the melting and to start the growth from the seed for which we use the unmelted solid party of the sphere. The sphere is centered by quartz protuberances inside of the quartz crucible. There exists the possibility of temperature fluctuations being introduced when the molten sphere occasionally touches the protuberances. The total time needed for the melting and the growth processes is estimated to be 30 minutes. Infrared emission from the sphere is monitored in order to prevent the accidental loss of the central solid core. The schematical illustration of the second experient is shown. A single crystal, Si rod is used as the starting material. In the first stage, the rod is melted from one end to obtain a liquid sphere. In the second stage, the single crystal is grown by decreasing the temperature from the unmelted part of the rod which is used as the seed. The second experient somewhat resembles the Czochralski method used on the ground; however, in the space experiment, no crucible is employed and the temperature uniformity is much superior. In both experiments, phosphorous is doped to allow observation of the change in the shape of the liquid solid interface during crystal growth and the impurity striations, if any.

Nishinaga, Tatau↗

Interaction of hydrogen chloride and water with oxide surfaces. III - Titanium dioxide

The adsorption of hydrogen chloride and water vapors on five TiO2 powders in both the anatase and rutile crystalline forms was studied as a function of temperature, pressure, and outgas conditions. The adsorbents were characterized utilizing X-ray powder diffraction, scanning electron microscopy, surface area analysis, indicator method, microelectrophoresis, XPS, and infrared spectroscopy. It was found that both outgas temperature and adsorption temperature influenced the adsorption of water vapor on TiO2, while water vapor adsorption on TiO2 was completely reversible. It is argued that the number of hydroxyl groups present on the surface determines the adsorption capacity of water on the different titanium dioxides. It was found that heats of immersion in water were affected significantly by outgas temperature. Hydrogen chloride adsorption isotherms at 30 C measured on TiO2 after outgassing at 100-400 C showed that a part of the total HCl adsorbed was irreversibly adsorbed. The highest HCl adsorption capacity per unit area was exhibited by anatase, while pure rutile exhibited the lowest adsorption capacity.

Siriwardane, R. V.↗

The Role of Entrained Surface Oxides in RS-PM Aluminum Alloys on Resultant Structures and Properties

The RS-PM aluminum alloys which show less than anticipated toughness properties were studied. After eliminating negative variables such as sodium and potassium in lithium containing alloys, hydrogen in all Al alloys, and trapped impurities from the atomization processing the data pointed to fine oxides, as the primary cause of poor toughness properties. The oxide content of aluminum powders increases with: decreasing powder size, deviations from spherical powder shapes, exposure to moist atmospheres either during atomization or in subsequent powder handling, and alloy compositions which contain significant amounts of lithium, magnesium, cerium, and other reactive elements.

Grant, N. J.↗

Electrocatalytic reduction of oxygen on modified oxide surfaces

A first step which frequently occurs in the reduction of dioxygen, e.g., at the cathode of the alkaline fuel cell, is the two-electron reduction to the peroxyl ion, HO bar 2. For the efficiency of the fuel cell, this ion must be further reduced, or decomposed, to OH(-). Rate constants for HO bar 2 decomposition have been determined in 31 percent KOH at 25 C for the following catalysts in the form of suspended powders and Teflon-bonded electrodes: Pt, Au, cobalt tetrametoxyl phenyl porphyrin (CoTMPP), and La sub 0.5Pb sub 0.5MnO3. Rates were normalized to unit surface area measured by several methods as suitable. Where possible, four methods were used to measure rate constants: gasometric, oxygen probe, rotating disk electrode, and open-circuit potential decay. Steady-state polarization was also tried but was not as satisfactory. Comparisons are given for the methods in regard to reliability, applicability to the material, and convenience.

Chaffins, Scott A.↗

Composition of solar wind noble gases released by surface oxidation of a metal separate from the Weston meteorite

The paper reports on a set of experiments intended to test the feasibility of determining elemental and isotopic ratios of the noble gases and nitrogen in the solar wind in metal separates from gas-rich ordinary chondrites. Helium, neon, and argon show clear evidence of a solar wind signature, while no solar component could be identified for xenon and nitrogen. Helium, neon, and argon elemental isotopic ratios appear to depend on depth within the metal grains. The ratios derived indicate that the Weston meteorite did not acquire its solar wind gases from a recent exposure to solar wind, but more probably at a time in the past similar to or even earlier than the exposure time of Apollo 17 breccias. The Ar-36/Ar-38 ratio, in tandem with other recent determinations of this value, indicates that the solar and terrestrial values can no longer be assumed to be equivalent.

Becker, R. H.↗

Influence of mineral oil and additives on microhardness and surface chemistry of magnesium oxide (001) surface

X-ray photoelectron spectroscopy analyses and hardness experiments were conducted with cleaved magnesium oxide /001/ surfaces. The magnesium oxide bulk crystals were cleaved into specimens along the /001/ surface, and indentations were made on the cleaved surface in laboratory air, in nitrogen gas, or in degassed mineral oil with and without an additive while not exposing specimen surface to any other environment. The various additives examined contained sulfur, phosphorus, chlorine, or oleic acid. The sulfur-containing additive exhibited the highest hardness and smallest dislocation patterns evidencing plastic deformation; the chlorine-containing additive exhibited the lowest hardness and largest dislocation patterns evidencing plastic deformation. Hydrocarbon and chloride (MgCl2) films formed on the magnesium oxide surface. A chloride film was responsible for the lowest measured hardness.

Miyoshi, K.↗

Effect of nitrogen-containing plasma on adherence, friction, and wear of radiofrequency-sputtered titanium carbide coatings

Friction and wear experiments on 440C steel surfaces that were rf sputtered with titanium carbide when a small percentage of nitrogen was added to the plasma were conducted. Both X-ray photoelectron spectroscopy and X-ray diffraction were used to analyze the resultant coatings. Results indicate that the small partial pressure of nitrogen (approximately 0.5 percent) markedly improves the adherence, friction, and wear properties when compared with coatings applied to sputter-etched surfaces, oxidized surfaces, or in the presence of a small oxygen partial pressure. The improvements are related to the formation of an interface containing a mixture of the nitrides of titanium and iron, which are harder than their corresponding oxides.

Brainard, W. A.↗

Atomic Oxygen Effects on Materials

One objective of this investigation has been to offer recommendations on the selection of metal samples to be exposed to ambient atomic oxygen on the STS-8 flight presently scheduled for August 30, 1983. (These samples constitute a small subgroup of a very large group of test specimens prepared by A. Whitaker and other members of the Physical Sciences Branch for this mission.) The metals selected and prepared for STS-8 are silver, lead, copper, nickel, tungsten, molybdenum, magnesium, platinum, and alloys of FeCrAl and NiCr. Literature data are reviewed concerning the oxidation properties of these materials with a view towards understanding which oxides might be formed, the state of the oxide (surface film or volatile form), and the reaction rate. In addition, various techniques for characterizing the parent metals and the surface oxides are reviewed.

Fromhold, A. T.↗

Influence of corrosive solutions on microhardness and chemistry of magnesium oxide /001/ surfaces

X-ray photoelectron spectroscopy analyses and hardness experiments were conducted on cleaved magnesium oxide /001/ surfaces. The magnesium oxide bulk crystals were cleaved to specimen size along the /001/ surface, and indentations were made on the cleaved surface in corrosive solutions containing HCl, NaOH, or HNO3 and in water without exposing the specimen to any other environment. The results indicated that chloride (such as MgCl2) and sodium films are formed on the magnesium oxide surface as a result of interactions between an HCl-containing solution and a cleaved magnesium oxide surface. The chloride films soften the magnesium oxide surface. In this case microhardness is strongly influenced by the pH value of the solution. The lower the pH, the lower the microhardness. Sodium films, which are formed on the magnesium oxide surface exposed to an NaOH containing solution, do not soften the magnesium oxide surface.

Ishigaki, H.↗

The Rise of Oxygen and the Hydrogen Hourglass

Oxygenic photosynthesis appears to be necessary for an oxygen-rich atmosphere like Earth's. But available geological and geochemical evidence suggest that at least 200 Myr, and possibly more than 700 Myr, elapsed between the advent of oxygenic photosynthesis and the establishment of an oxygen atmosphere. The interregnum implies that at least one other necessary condition for O2 needed to be met. Here we argue that the second condition was the oxidation of the surface and crust to the point where O2 became more stable than competing reduced gases such as CH4. The cause of Earth's surface oxidation would be the same cause as it is for other planets with oxidized surfaces: hydrogen escape to space. The duration of the interregnum would have been determined by the rate of hydrogen escape and by the size of the reduced reservoir that needed to be oxidized before O2 became favored. We suggest that continental growth has been influenced by hydrogen escape, and we speculate that, if there must be an external bias to biological evolution, hydrogen escape can be that bias.

atmospheric evolution↗