Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “steelmaking process”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Effect of Al{sub 2}O{sub 3} Addition on Mineralogical Modification and Crystallization Kinetics of a High Basicity BOF Steel Slag

Basic oxygen furnace (BOF) steel slag is a main byproduct that is produced during the converter steelmaking process. The volume instability and fast crystallization of BOF slag limits its added-value application. This article aims to understand the effect of Al{sub 2}O{sub 3} on the mineralogical modification and crystallization kinetics of a high basicity BOF steel slag. Continuous cooling transformation and time–temperature–transformation curves were constructed to determine the crystallization characteristics of BOF slag. The critical cooling rate to vitrify the slag was experimentally obtained. The crystallization sequence was clarified by integrating in situ and post-mortem observations with thermodynamic calculations. The results suggest that the addition of Al{sub 2}O{sub 3} can effectively remove free lime, decrease the melting point, and improve the glass formation ability of the high basicity BOF slag. Undercooling the slag is enhanced by increasing the cooling rate and/or adding Al{sub 2}O{sub 3}. By steering the addition of Al{sub 2}O{sub 3} and the cooling rate, BOF slag can be modified to obtain a more amorphous phase, presenting an enhanced potential to be a binder for added-value applications.

36 MATERIALS SCIENCE↗

Characteristics of Flow Field for Supersonic Oxygen Multijets with Various Laval Nozzle Structures

The Laval nozzle is used widely in steelmaking processes to increase the velocity of an oxygen jet up to approximately 2 Mach numbers. The present research is aimed at determining the effect of the Laval nozzle structure on a supersonic oxygen jet flow field. Both one-dimensional isoentropic flow theory and a characteristic-line method were used to design five-hole oxygen lances of two types and, applicable to oxygen multijets, to analyze their flow field characteristics by a series of numerical simulations and experimental studies. When compared to the conventional oxygen lance designed according to the one-dimensional isoentropic flow theory, the new oxygen lance designed with employment of the characteristic-line method is more effective in both suppressing the shock wave generation and improving the initial axial velocity of oxygen jets under the same test conditions. As a result, a larger impaction cavity was generated by the new oxygen lance and the mass transfer within oxygen, liquid slag, and molten steel was enhanced.

36 MATERIALS SCIENCE↗

Characteristics of Nozzle Clogging and Evolution of Oxide Inclusion for Al-Killed Ti-Stabilized 18Cr Stainless Steel

Characteristics of nozzle clogging and evolution of oxide inclusion were studied by sampling the deposits of submerged entry nozzle (SEN) and the molten steel in tundish during Al-killed Ti-stabilized 18Cr stainless steelmaking process. The deposits found in the clogging of SEN were mainly composed of frozen steel and inclusions. The inclusions in the deposits and tundish were both mainly (MgO-Al{sub 2}O{sub 3}){sub rich}-CaO-TiO{sub x}. The compositions of most inclusions were Liquid+Spinel or Liquid+TiSp phase. The (MgO-Al{sub 2}O{sub 3}){sub rich}-CaO inclusions that were not effectively modified by calcium treatment could be a source of clogging. By combining both the experimental results and thermodynamic calculation, (MgO-Al{sub 2}O{sub 3}){sub rich}-TiO{sub x} inclusions (TiSp inclusions) would be formed with the decreasing temperature in steel during continuous casting, which could be transported and accumulated on the inner wall of the SEN. Increasing the calcium content in the molten steel could decrease the formation of TiSp inclusions. During continuous casting, these inclusions accumulated on the inner wall of the SEN and gradually formed porous network of clog. Molten steel would gradually solidify in the porous space of the clog due to the increased residence time of the molten steel when flowing through it. The clogging gradually increased and caused the shutdown of continuous casting.

36 MATERIALS SCIENCE↗

Synthesis and characterisation of alites from reduced basic oxygen furnace slags

Basic oxygen furnace slags (BOFS) are by-products of the steelmaking process. Several researchers have studied the production of Portland cement clinker and metallic iron from BOFS via a reductive treatment. }In this study, we applied a carbothermal reduction of BOFS in a technical-scale electric arc furnace and characterised the clinker-like products. Those clinker-like non-metallic products (NMPs) had a chemical and mineralogical composition comparable to clinker for ordinary Portland cement (OPC) and contained large elongated alite crystals as major component. The pure NMPs reacted more slowly and achieved a lower degree of hydration compared with commercial OPC. }If the reactivity of the products can be further increased by employing specific adaptations, it can be used as a full clinker substitute for OPC. Nevertheless, it is also an option to use the material without further modifications as a cement component or concrete addition, which contributes to the strength development in both cases.

36 MATERIALS SCIENCE↗

Chemical and mineralogical characterizations of LD converter steel slags: A multi-analytical techniques approach

The use of LD converter steel slags (coming from Linz-Donawitz steelmaking process) as aggregates in road construction can in certain cases lead to dimensional damage due to a macroscopic swelling that is the consequence of chemical reactions. The aim of this study was to couple several analytical techniques in order to carefully undertake chemical and mineralogical characterizations of LD steel slags and identify the phases that are expected to be responsible for their instability. Optical microscopy, scanning electron microscopy and electron probe microanalyses revealed that LD steel slags mainly contain calcium silicates, dicalcium ferrites, iron oxides and lime. However, as a calcium silicate phase is heterogeneous, Raman microspectrometry and transmitted electron microscopy had to be used to characterize it more precisely. Results showed that lime is present under two forms in slag grains: some nodules observed in the matrix whose size ranges from 20 to 100 {mu}m and some micro-inclusions, enclosed in the heterogeneous calcium silicate phase whose size ranges from 1 to 3 {mu}m. It was also established that without the presence of magnesia, lime is expected to be the only phase responsible for LD steel slags instability. Nevertheless, the distribution of lime between nodules and micro-inclusions may play a major role and could explain that similar amounts of lime can induce different instabilities. Thus, it appears that lime content of LD steel slags is not the only parameter to explain their instability.

36 MATERIALS SCIENCE↗

Recycling of rubber tires in electric arc furnace steelmaking: simultaneous combustion of metallurgical coke and rubber tyres blends

The present study investigates the effect of addition of waste rubber tires on the combustion behavior of its blends with coke for carbon injection in electric arc furnace steelmaking. Waste rubber tires were mixed in different proportions with metallurgical coke (MC) (10:90, 20:80, 30:70) for combustion and pyrolysis at 1473 K in a drop tube furnace (DTF) and thermogravimetric analyzer (TGA), respectively. Under experimental conditions most of the rubber blends indicated higher combustion efficiencies compared to those of the constituent coke. In the early stage of combustion the weight loss rate of the blends is much faster compared to that of the raw coke due to the higher volatile yield of rubber. The presence of rubber in the blends may have had an impact upon the structure during the release and combustion of their high volatile matter (VM) and hence increased char burnout. Measurements of micropore surface area and bulk density of the chars collected after combustion support the higher combustion efficiency of the blends in comparison to coke alone. The surface morphology of the 30% rubber blend revealed pores in the residual char that might be attributed to volatile evolution during high temperature reaction in oxygen atmosphere. Physical properties and VM appear to have a major effect upon the measured combustion efficiency of rubber blends. The study demonstrates that waste rubber tires can be successfully co-injected with metallurgical coke in electric arc furnace steelmaking process to provide additional energy from combustion. 44 refs., 11 figs., 2 tabs.

01 COAL, LIGNITE, AND PEAT↗

Activating magnetite ores for aqueous ironmaking at high current densities

Low-temperature electrochemical cells reducing iron oxides to metal in alkaline electrolytes can support fully electrified steelmaking processes. Previous studies on these cells have primarily focused on high-surface-area hematite, Fe 2 O 3 , reactants whereas attempts to reduce suspensions of magnetite, Fe 3 O 4 —one of the two feedstocks for existing ironmaking reactors—have generally been limited to low rates of reaction (<30 mA cm −2 ). Here, in this study, we control the crystalline domain size of Fe 2 O 3 and Fe 3 O 4 particles in 10 M NaOH electrolytes to study how the nanoscale morphology of oxides controls the rate of electrochemical ironmaking. Rotating-ring disk electrode measurements of Fe 2+ , in situ Raman spectroscopy of the electrode surface, and ex situ electron microscopy were consistent with a hypothesized passivation process at Fe 3 O 4 surfaces that may prevent the continuous formation of soluble intermediates. Sufficiently small (<100 nm diameter) oxide particles yielded Fe partial current densities >160 mA cm −2 , a fivefold increase relative to previously reported rates for Fe 3 O 4 suspensions and comparable to active Fe 2 O 3 . Electron microscopy revealed that electrodeposited films were composed of micron-scale crystalline Fe domains with a porous film of Fe 3 O 4 nanoparticles and supports a model where Fe is grown primarily from soluble Fe 2+ intermediates. Based on these insights, inactive blast-furnace-grade iron-oxides were transformed into high surface area nanoparticles (1.6 to 229.2 m 2 g −1 ) via reprecipitation, leading to a ninefold enhancement in faradaic efficiency and an Fe partial current density of 120 mA cm −2 . When integrated with chlor-iron cells producing reagents for reprecipitation, this approach could lead to a cost-competitive process for electrochemical ironmaking from industrially relevant feedstocks.

TEM↗

Stable, Efficient Iron Electrodeposition via Anion-Directed Control of Fe(II) Coordination

Traditional steelmaking processes consume about 7% of the world’s energy supply, with reduction of iron oxides into iron via blast furnaces representing the most energy-demanding and capital-intensive step. To economize and modularize iron reduction processes, we aim to develop an electrodeposition technique to reduce aqueous iron ions to metallic iron. However, the hydrogen reduction reaction (HER) occurs at a more positive standard reduction potential than the iron reduction reaction. In addition, aqueous Fe(II) cations easily precipitate at mildly acidic conditions (pH ≥ 3), which limits the deposition efficiency and degrades deposit quality. To address these challenges, we first search for anions that have intermediate coordination strength with Fe(II) based on the hard-soft acid-base theory, trading a slightly more negative Fe(II) reduction potential for a considerably broader pH stability range. We select citrate with predicted intermediate coordination strength, in combination with more weakly coordinating anions (e.g., SO 4 2- , Cl - ) to control the coordination structure of Fe 2+ for improved electrolyte stability and electrodeposition behavior. We find that citrate coordination stabilizes Fe 2+ -based electrolytes at higher pH conditions (4.8–5.5), significantly extending their shelf life while also suppressing HER during Fe electrodeposition by orders of magnitude. To measure Faradaic efficiencies (FE), we developed a straightforward, titration-based methodology to quantify the amount of deposited iron regardless of the rate of concurrent HER. Although coordination between citrate and Fe 2+ decreases the reduction potential of Fe(II), high FE (≥98%) was achieved at 10 mA cm -2 . FE and achievable deposition rates are tunable by both concentration and the ratio of Fe 2+ to citrate. In all cases, Raman spectroscopy and X-ray diffraction (XRD) reveal that iron deposition in citrate-containing electrolytes suppresses iron oxide/hydroxide precipitation, in contrast to deposits generated in citrate-free electrolytes. Altogether, this work demonstrates that citrate-mediated anion coordination enables high-purity iron electrodeposition with increased FE, high current density, and improved electrolyte stability. This multi-anion coordination strategy provides a versatile framework for designing stable electrolyte and efficient metal electrodeposition.

coordination↗

Solid Fuel - Oxygen Fired Combustion for Production of Nodular Reduced Iron to Reduce CO2 Emissions and Improve Energy Efficiencies

The current trend in the steel industry is an increase in iron and steel produced in electric arc furnaces (EAF) and a gradual decline in conventional steelmaking from taconite pellets in blast furnaces. In order to expand the opportunities for the existing iron ore mines beyond their blast furnace customer base, a new material is needed to satisfy the market demands of the emerging steel industry while utilizing the existing infrastructure and materials handling capabilities. This demand creates opportunity to convert iron ore or other iron bearing materials to Nodular Reduced Iron (NRI) in a recently designed Linear Hearth Furnace (LHF). NRI is a metallized iron product containing 98.5 to 96.0% iron and 2.5 to 4% C. It is essentially a scrap substitute with little impurity that can be utilized in a variety of steelmaking processes, especially the electric arc furnace. The objective of this project was to focus on reducing the greenhouse gas emissions (GHG) through reducing the energy intensity using specialized combustion systems, increasing production and the use of biomass derived carbon sources in this process. This research examined the use of a solid fuel-oxygen fired combustion system and compared the results from this system with both oxygen-fuel and air-fuel combustion systems. The solid pulverized fuels tested included various coals and a bio-coal produced from woody biomass in a specially constructed pilot scale torrefaction reactor at the Coleraine Minerals Research Laboratory (CMRL). In addition to combustion, the application of bio-coal was also tested as a means to produce a reducing atmosphere during key points in the fusion process, and as a reducing agent for ore conversion to metallic iron to capture the advantage of its inherent reduced carbon footprint. The results from this study indicate that the approaches taken can reduce both greenhouse gas emissions and the associated energy intensity with the Linear Hearth Furnace process for converting iron ore to metallic iron nodules. Various types of coals including a bio-coal produced though torrefaction can result in production of NRI at reduced GHG levels. The process results coupled with earlier already reported developments indicate that this process technique should be evaluated at the next level in order to develop parameter information for full scale process design. Implementation of the process to full commercialization will require a full cost production analysis and comparison to other reduction technologies and iron production alternatives. The technical results verify that high quality NRI can be produced under various operating conditions at the pilot level.

01 COAL, LIGNITE, AND PEAT↗

Zinc Removal from Basic Oxygen Steelmaking Filter Cake by Leaching with Organic Acids

The dust generated from the basic oxygen steelmaking (BOS) process is a waste material mainly containing iron that cannot be recycled owing to its high zinc content. In this study, the leaching effects of different organic acids are compared, with the aim of determining an acid that selectively leaches and removes zinc from BOS dust, so that the waste material can be recycled into ironmaking and steelmaking processes in order to substitute part of the raw materials of steelmaking. The dust used in this study was scrubbed and collected in the form of a filter cake. The acids tested were oxalic, citric, acetic, propionic, butyric, and valeric acids. Butyric acid was found to be the most effective, with a high zinc extraction level of 49.7 pct and a low iron level of only 2.5 pct. Oxalic acid was the least effective leaching reagent for both zinc and iron extractions, owing to the formation of zinc and iron oxalate precipitates following metal dissolution. The filter cake and leached residues were characterized by chemical analysis, X-ray diffraction, X-ray photoelectron spectroscopy, and scanning electron microscopy with energy dispersive spectroscpopy.

36 MATERIALS SCIENCE↗

Structure–property relations of binary ferrite melts

Molten ferrite systems are used in the smelting and refining processes in steelmaking, to reduce the loss of metals in slags and to accelerate reaction rates. Here, high-energy x-ray diffraction experiments have been performed on aerodynamically levitated molten spheres of 43BaO–57FeO X and 43SrO–57FeO X at 1873 K using laser beam heating. The composition was varied within the range of x = 1–1.5 by changing the oxygen partial pressure of the levitation gas. The corresponding x-ray pair distribution functions have been interpreted using empirical potential structure refinement (EPSR) modeling. In oxygen-rich melts (x = 1.5), our EPSR models indicate very similar structures for the different alkaline-earth liquids, with both the Ba–O and Sr–O coordination numbers to be ∼8.4 and the total Fe–O coordination numbers ∼5.7. However, our models show that in reducing environments, the Fe 3+ and Fe 2+ ions exhibit very different behaviors in the Ba- and Sr-ferrite liquids. In the Ba-ferrite melt, the Fe 3+ –O coordination number decreases from 5.7 (at x = 1.5) to 5.2 (at x = 1.07), whereas Fe 2+ –O remains constant at ∼5.0 across the same compositional range. In the Sr melts, both the Fe 2+ –O and Fe 3+ –O coordination numbers rise from ∼5.7 (at x = 1.5) to 6.3 (at x = 1.07). All models show the structures to be heterogeneous with intertwined nanometer sized clusters or channels of Ba/Sr–O and Fe–O polyhedra that grow as oxygen content is reduced. Changes in the viscosity and electrical properties are interpreted in terms of the number of bridging and non-bridging oxygens associated with FeO 4 tetrahedra and concentration of charge carriers, respectively.

Benmore, Chris J. [Argonne National Laboratory (AN↗

Next Generation Metallic Iron Nodule Technology in Electric Arc Steelmaking - Phase II

The current trend in the steel industry is a gradual decline in conventional steelmaking from taconite pellets in blast furnaces, and an increasing number of alternative processes using metallic scrap iron, pig iron and metallized iron ore products. Currently, iron ores from Minnesota and Michigan are pelletized and shipped to the lower Great Lakes ports as blast furnace feed. The existing transportation system and infrastructure is geared to handling these bulk materials. In order to expand the opportunities for the existing iron ore mines beyond their blast furnace customer base, a new material is needed to satisfy the needs of the emerging steel industry while utilizing the existing infrastructure and materials handling. A recent commercial installation employing Kobe Steel’s ITmk3 process, was installed in Northeastern Minnesota. The basic process uses a moving hearth furnace to directly reduce iron oxides to metallic iron from a mixture of iron ore, coals and additives. The resulting products can be shipped using the existing infrastructure for use in various steelmaking processes. The technology reportedly saves energy by 30% over the current integrated steelmaking process and reduces emissions by more than 40%. A similar large-scale pilot plant campaign is also currently in progress using JFE Steel’s Hi-QIP process in Japan. The objective of this proposal is to build upon and improve the technology demonstrated by Kobe Steel and JFE, by further reducing cost, improving quality and creating added incentive for commercial development. This project expands previous research conducted at the University of Minnesota Duluth’s Natural Resources Research Institute and that reported by Kobe and JFE Steel. Three major issues have been identified and are addressed in this project for producing high-quality nodular reduced iron (NRI) at low cost: (1) reduce the processing temperature, (2) control the furnace gas atmosphere over the NRI, and (3) effectively use sub-bituminous coal as a reductant. From over 4000 laboratory tube and box furnace tests, it was established that the correct combination of additives, fluxes, and reductant while controlling the concentration of CO and CO2 in the furnace atmosphere (a) lowers the operating temperature, (b) decreases the use of reductant coal (c) generates less micro nodules of iron, and (d) promotes desulphurization. The laboratory scale work was subsequently verified on 12.2 m (40 ft) long pilot scale furnace. High quality NRI could be produced on a routine basis using the pilot furnace facility with energy provided from oxy-gas or oxy-coal burner technologies. Specific strategies were developed to allow the use of sub-bituminous coals both as a hearth material and as part of the reaction mixture. Computational Fluid Dynamics (CFD) modeling was used to study the overall carbothermic reduction and smelting process. The movement of the furnace gas on a pilot hearth furnace and larger simulated furnaces and various means of controlling the gas atmosphere were evaluated. Various atmosphere control methods were identified and tested during the course of the investigation. Based on the results, the appropriate modifications to the furnace were made and tested at the pilot scale. A series of reduction and smelting tests were conducted to verify the utility of the processing conditions. During this phase, the overall energy use characteristics, raw materials, alternative fuels, and the overall economics predicted for full scale implementation were analyzed. The results indicate that it should be possible to lower reaction temperatures while simultaneously producing low sulfur, high carbon NRI if the right mix chemistry and atmosphere are employed. Recommendations for moving the technology to the next stage of commercialization are presented.

Carbon↗

In-Situ Atomic-Scale Revelation of Amorphous Metallic Iron Formation during Hydrogen-Driven Reduction of Iron Oxides

The transition to hydrogen as a green reductant in metal production is critical for decarbonizing the metallurgical industry, yet atomic-scale mechanisms governing reduction pathways and phase evolution remain unresolved. Using in-situ environmental transmission electron microscopy, we identify a hidden pathway that reveals dynamic formation of amorphous metallic iron (Fe) during the hydrogen-driven reduction of ferrous oxides of Fe 3 O 4 and FeO. Real-time imaging uncovers three coexisting transformation routes: (i) Fe 3 O 4 → FeO, (ii) Fe 3 O 4 → amorphous Fe, and (iii) FeO → amorphous Fe. The resulting amorphous Fe exhibits fluid-like mobility, enabling its rapid aggregation and crystallization into core-shell nanostructures, with a crystalline core enveloped by an amorphous shell. Complementary ab initio molecular dynamics simulations trace the amorphous Fe formation to interfacial strain at the metal/oxide interfaces, where large lattice mismatches destabilize the metal lattice during initial metallization. This interplay between thermodynamics and kinetics governs phase evolution: thermodynamics favors a self-limiting amorphous Fe overlayer, while rapid oxide reduction kinetics drives amorphous overgrowth. Our findings demonstrate that amorphous intermediates bypass rate-limiting crystalline steps, providing mechanistic insights to optimize H 2 -based processes for sustainable steelmaking. In conclusion, these insights bridge the gap between macroscopic process engineering and atomic-scale dynamics, with broader implications for catalysis and nanostructured material synthesis, where oxide reduction pathways critically shape functional phases and microstructures.

36 MATERIALS SCIENCE↗

Prediction of Silicon Content in a Blast Furnace via Machine Learning: A Comprehensive Processing and Modeling Pipeline

Silicon content plays an important role in determining the operational efficiency of blast furnaces (BFs) and their downstream processes in integrated steelmaking; however, existing sampling methods and first-principles models are somewhat limited in their capability and flexibility. Current data-based prediction models primarily rely on a limited set of manually selected furnace parameters. Additionally, different BFs present a diverse set of operating parameters and state variables that are known to directly influence the hot metal’s silicon content, such as fuel injection, blast temperature, and raw material charge composition, among other process variables that have their own impacts. The expansiveness of the parameter set adds complexity to parameter selection and processing. This highlights the need for a comprehensive methodology to integrate and select from all relevant parameters for accurate silicon content prediction. Providing accurate silicon content predictions would enable operators to adjust furnace conditions dynamically, improving safety and reducing economic risk. To address these issues, a two-stage approach is proposed. First, a generalized data processing scheme is proposed to accommodate diverse furnace parameters. Second, a robust modeling pipeline is used to establish a machine learning (ML) model capable of predicting hot metal silicon content with reasonable accuracy. The method employed herein predicted the average Si content of the upcoming furnace cast with an accuracy of 91% among 200 target predictions for a specific furnace provisioned by the XGBoost model. This prediction is achieved using only the past shift’s operating conditions, which should be available in real time. This performance provides a strong baseline for the modeling approach with potential for further improvement through provision of real-time features.

Chemistry↗

Interaction Between Liquid Steel and AlN Substrate Containing Al-Y-Oxides

Reactions between molten iron, molten silicon steel, and ceramic materials are of great importance from the perspective of the corrosion of refractory material in the steelmaking and continuous casting processes. Reactions between liquid steel and aluminum nitride (AlN) substrate containing Al-Y-oxides were investigated using the sessile drop method at 1833 K (1560 °C). The liquid–substrate interface was observed with the increasing holding time, and the reaction mechanism was studied. In the case of the liquid iron and the silicon steel on the AlN substrate containing Al-Y-oxides, the reaction products on the steel side of the interface between the steel and the substrate were Al-rich Al-Y-oxides and Al{sub 2}O{sub 3} particles. For silicon steel and pure AlN substrate, Al{sub 2}O{sub 3} particles were the main products. Contact angles were lower for liquid iron than for silicon steel due to the higher oxygen content in iron. In addition, the solid–liquid interfacial tension and the work of adhesion between AlN and steel were measured.

36 MATERIALS SCIENCE↗

Sustainable, Net-Zero Carbon Steelmaking Utilizing Nuclear and Renewable-based Integrated Energy Systems

Decarbonizing Steelmaking: Emissions Background Industrial processes (including power) account for 28% of global CO2 emissions dominated by steel, cement, NH3, ethylene. Steel accounts for 7% of global CO2 emissions (25% of Industrial), 2-3 Gigatonnes annually. Given long asset life and large investments in steel industry, recommend: Detailed analysis, materials R&D and pre-pilot technology integration required by 2030 to position U.S. industry for an investment decision for building first net-zero integrated steel plan Symposium site: https://www.aiche.org/cei/conferences/competitive-energy-systems/2021

08 HYDROGEN↗

Oxidation and Condensation of Zinc Fume From Zn-CO 2 -CO-H 2 O Streams Relevant to Steelmaking Off-Gas Systems

Here the objective of this research was to study the condensation of zinc vapor to metallic zinc and zinc oxide solid under varying environments to investigate the feasibility of in-process separation of zinc from steelmaking off-gas dusts. Water vapor content, temperature, degree of cooling, gas composition, and initial zinc partial pressure were varied to simulate the possible conditions that can occur within steelmaking off-gas systems, limited to Zn-CO 2 -CO-H 2 O gas compositions. The temperature of deposition and the effect of rapidly quenching the gas were specifically studied. A homogeneous nucleation model for applicable experiments was applied to the analysis of the experimental data. It was determined that under the experimental conditions, oxidation of zinc vapor by H 2 O or CO 2 does not occur above 1108 K (835 °C) even for highly oxidizing streams (CO 2 /CO = 40/7). Rate expressions that correlate CO 2 and H 2 O oxidation rates to gas composition, partial pressure of water vapor, temperature, and zinc partial pressure were determined to be as follows: Rate $ \left(\frac{mol}{m^2s}\right) $ = 406 exp $ \left(\frac{-50.2 kJ/mol}{RT}\right) $ (pZnpCO 2 $-$ PCO/K eq CO 2 ) $\frac{mol}{m^2 x s}$ Rate $ \left(\frac{mol}{m^2s}\right) $ = 32.9 exp $ \left(\frac{-13.7 kJ/mol}{RT}\right) $ (pZnPH 2 O $-$ PH 2 /K eq H 2 O) $\frac{mol}{m^2 x s}$. It was proven that a rapid cooling rate (500 K/s) significantly increases the ratio of metallic zinc to zinc oxide as opposed to a slow cooling rate (250 K/s). SEM analysis found evidence of heterogeneous growth of ZnO as well as of homogeneous formation of metallic zinc. The homogeneous nucleation model fit well with experiments where only metallic zinc deposited. An expanded model with rates of oxidation by CO 2 and H 2 O as shown was combined with the homogenous nucleation model and then compared with experimental data. The calculated results based on the model gave a reasonable fit to the measured data. For the conditions used in this study, the rate equations for the oxidation of zinc by carbon dioxide and water vapor as well as the homogeneous nucleation model of metallic zinc were applicable for various temperatures, zinc partial pressures, CO 2 :CO ratios, and H 2 O partial pressures.

36 MATERIALS SCIENCE↗

Improved Processing Techniques for Inclusion-Free Steel for Bearing and Mechanical Component Applications

High hardness, high carbide powder metallurgy tools steels such as M62 enable the operation of ball bearings at extremely high load and stress levels. Operation under such conditions increases the potential for rolling contact fatigue failure attributed to ceramic particle inclusions. To address this challenge, industry has sought steel made from ever increasing levels of cleanliness but the results have been uneven owing to the random nature of the occurrence of material flaws. One common approach is to rely upon careful ingot inspections prior to bearing manufacture. By selecting the cleanest portion of an ingot, it is expected that bearings relatively free from material flaws will result. This approach is not always successful because detrimental flaws that exist deep within an ingot can pass inspection undetected potentially causing subsequent failure. Recent efforts to commercialize an intermetallic material, 60NiTi, for rolling element bearings demonstrates a pathway to produce bearing steel that is free from unwanted ceramic particle inclusions. In this paper, the process used to make bearing grade ceramic-free NiTi alloys is described and applied to steelmaking. At its core, the NiTi process differs from steel making in one key aspect. NiTi alloys are made from elementally pure starting materials that are melted, blended and processed in equipment absolutely free from exposure to oxygen and ceramics ensuring a ceramic particle-free product. In contrast, the predominant method to make bearing steel is to employ a successive series of purification steps to reduce contamination levels below required thresholds. This paper describes the processes developed and applied to high carbide tool steel, M62. The resulting material and microstructures are evaluated and compared to M62 prepared by conventional powder metallurgy techniques. It is hoped that the application of materials manufacturing techniques used for fracture sensitive ceramics and intermetallic materials like NiTi can provide a pathway to Ultra-Clean, Ceramic-Inclusion free steels for rolling element bearings and other failure critical applications.

Steel↗