Friction and Wear Properties of As-Deposited and Carbon Ion-Implanted Diamond Films

Recent work on the friction and wear properties of as-deposited and carbon ion-implanted diamond films was reviewed. Diamond films were produced by the microwave plasma chemical vapor deposition (CVD) technique. Diamond films with various grain sizes and surface roughnesses were implanted with carbon ions at 60 keV ion energy, resulting in a dose of 1.2 x 10(exp 17) carbon ions per cm(exp 2). Various analytical techniques, including Raman spectroscopy, proton recoil analysis, Rutherford backscattering, transmission and scanning electron microscopy, X-ray photoelectron spectroscopy, and X-ray diffraction, were utilized to characterize the diamond films. Sliding friction experiments were conducted with a polished natural diamond pin in contact with diamond films in the three environments: humid air (40% relative humidity), dry nitrogen (less than 1 percent relative humidity), and ultrahigh vacuum (10(exp -7) Pa). The CVD diamond films indeed have friction and wear properties similar to those of natural diamond in the three environments. The as-deposited, fine-grain diamond films can be effectively used as self-lubricating, wear-resistant coatings that have low coefficients of friction (0.02 to 0.04) and low wear rates (10(exp -7) to lO(exp -8) mm(exp 3) N(exp -1) m(exp -1)) in both humid air and dry nitrogen. However, they have high coefficients of friction (1.5 to 1.7) and a high wear rate (10(exp -4) mm(exp 7) N(exp -1) m(exp -1)) in ultrahigh vacuum. The carbon ion implantation produced a thin surficial layer (less than 0.1 micron thick) of amorphous, non-diamond carbon on the diamond films. In humid air and dry nitrogen, the ion-implanted, fine and coarse-grain diamond films have a low coefficient of friction (around 0.1) and a low wear rate (10(exp -7) mm(exp 3) N(exp -1) m(exp-1)). Even in ultrahigh vacuum, the presence of the non-diamond carbon layer reduced the coefficient of friction of fine-grain diamond films to 0.1 or lower and the wear rate to 10(exp -6) mm(exp 3) N(exp -1) m(exp -1). Thus, the carbon ion-implanted, fine-grain diamond films can be effectively used as wear-resistant, self-lubricating coatings not only in air and dry nitrogen, but also in ultrahigh vacuum.

Miyoshi, Kazuhisa↗

Surface Chemistry, Microstructure, and Tribological Properties of Cubic Boron Nitride Films

This report deals with the surface chemistry, microstructure, bonding state, morphology, and friction and wear properties of cubic boron nitride (c-BN) films that were synthesized by magnetically enhanced plasma ion plating. Several analytical techniques - x-ray photoelectron spectroscopy, transmission electron microscopy and electron diffraction, Fourier transform infrared spectroscopy, atomic force microscopy, and surface profilometry - were used to characterize the films. Sliding friction experiments using a ball-on-disk configuration were conducted for the c-BN films in sliding contact with 440C stainless-steel balls at room temperature in ultrahigh vacuum (pressure, 10(exp -6), in ambient air, and under water lubrication. Results indicate that the boron-to-nitrogen ratio on the surface of the as-deposited c-BN film is greater than 1 and that not all the boron is present as boron nitride but a small percentage is present as an oxide. Both in air and under water lubrication, the c-BN film in sliding contact with steel showed a low wear rate, whereas a high wear rate was observed in vacuum. In air and under water lubrication, c-BN exhibited wear resistance superior to that of amorphous boron nitride, titanium nitride, and titanium carbide.

Watanabe, Shuichi↗

Friction and wear of some ferrous-base metallic glasses

Sliding friction experiments, X-ray photoelectron spectroscopy (XPS) analysis, and electron microscopy and diffraction studies were conducted with ferrous base metallic glasses (amorphous alloys) in contact with aluminum oxide at temperatures to 750 C in a vacuum. Sliding friction experiments were also conducted in argon and air atmospheres. The results of the investigation indicate that the coefficient of friction increases with increasing temperature to 350 C in vacuum. The increase in friction is due to an increase in adhesion resulting from surface segregation of boric oxide and/or silicon oxide to the surface of the foil. Above 500 C the coefficient of friction decreased rapidly. The decrease correlates with the segregation of boron nitride to the surface. Contaminants can come from the bulk of the material to the surface upon heating and impart boric oxide and/or silicon oxide at 350 C and boron nitride above 500 C. The segregation of contaminants is responsible for the friction behavior. The amorphous alloys have superior wear resistance to crystalline 304 stainless steel. The relative concentrations of the various constituents at the surfaces of the amorphous alloys are very different from the nominal bulk compositions.

Miyoshi, K.↗

Friction and wear of some ferrous-base metallic glasses

Sliding friction experiments, X-ray photoelectron spectroscopy (XPS) analysis, and electron microscopy and diffraction studies were conducted with ferrous base metallic glasses (amorphous alloys) in contact with aluminium oxide at temperatures to 750 C in a vacuum. Sliding friction experiments were also conducted in argon and air atmospheres. The results of the investigation indicate that the coefficient of friction increases with increasing temperature to 350 C in vacuum. The increase in friction is due to an increase in adhesion resulting from surface segregation of boric oxide and/or silicon oxide to the surface of the foil. Above 500 C the coefficient of friction decreased rapidly. The decrease correlates with the segregation of boron nitride to the surface. Contaminants can come from the bulk of the material to the surface upon heating and impart boric oxide and/or silicon oxide at 350 C and boron nitride above 500 C. The segregation of contaminants is responsible for the friction behavior. The amorphous alloys have superior wear resistance to crystalline 304 stainless steel. The relative concentrations of the various constituents at the surfaces of the amorphous alloys are very different from the nominal bulk compositions.

Miyoshi, K.↗

Review of model sensor studies on Pd/SnO2(110) surfaces

Studies performed at the National Institute of Standards and Technology on the model gas sensor system, Pd/SnO2(110), are reviewed. Adsorption and interfacial effects play a primary role in the gas sensing process, as they do in catalysis. For this reason, researchers have used a variety of surface sensitive techniques in the research, including x ray and ultraviolet photoelectron spectroscopies (XPS and UPS), low energy electron diffraction (LEED), and ion scattering spectroscopy (ISS). By combining these complementary techniques with in situ gas response (conductance) measurements, researchers were able to correlate directly sensor activity with the composition and structure of the Pd/SnO2 interface. Although the intent of this work is to develop an understanding of gas sensing mechanisms, its relevance to Pt/SnO2 catalytic systems is obvious.

Fryberger, Teresa B.↗

Microscopic and Metallurgical Aspects of the Space Shuttle Columbia Accident Investigation and Reconstruction

The Space Shuttle Columbia was descending for a landing at the Kennedy Space Center (KSC) on February 1, 2003. Approximately 20 minutes prior to touchdown, the Columbia began disintegrating over the western United States; the majority of debris eventually impacted in eastern Texas and western Louisiana. A monumental effort eventually recovered approximately 84,000 pieces of debris, approximately 38% of the Orbiter's original dry weight. The debris was transported to KSC, where the items were catalogued and evaluated. Critical areas of interest, such as the left and right leading edge surfaces and the underside of the ship, were placed upon a grid to aid in the reconstruction. Items of interest included metallic structures, reinforced carbon-carbon composites, and ceramic heat insulation tiles. Many of the leading edge elements had re-solidified metallic deposits spattered on them. These deposits became known as slag and were one of the main focuses of the investigation. In order to help determine the sequence of events inside the left wing during the accident, the slag's composition, layering order, and directionality of deposition were studied. A myriad of analytical tests were performed in an attempt to ascertain the compositional and depositional characteristics of selected slag deposits, including the ordering of deposited layers within each individual slag deposit harvested. Initially, Scanning Electron Microscopy and Energy Dispersive X-Ray Spectroscopy (SEM/EDX) were performed to quickly characterize the overall composition of individual slag deposits: SEM utilizes a narrowlyfocused high-energy electron beam impinging upon a specimen. The incident beam excites and liberates lower energy secondary electrons, which are detected and analyzed, providing a visual representation of the sample's surface topography. EDX also relies on an incident electron beam, except an EDX unit measures X-ray energies generated by the impinging beam. Each element generates a unique X-ray signature; the EDX detector measures these discreet energies. EDX actually penetrates approximately 2 microns into the bulk of the sample. However, random examination of various portions of slag, coupled with the semiquantitative nature of the SEM/EDX analysis, did not yield convincingly pertinent data. Therefore, X-ray dot mapping was conducted, which provided more understandable data, both in terms of slag layering and composition. An X-ray dot map is generated by performing numerous EDX scans for individual elements, then compiling the scans in a visual representation. Eventually, specimens consisting of not only the slag, but of the adjacent RCC substrate as well were cross-sectioned. X-Ray dot mapping of the materialographicallymounted and -polished cross- sections provided a visual representation of both the layering sequence and compositional characteristics of the slag. Contemporaneously, Electron Spectroscopy for Chemical Analysis/X-Ray Photoelectron Spectroscopy (ESCA/XPS) and powdered X-Ray Diffraction (XRD) were performed to further characterize the deposits and to attempt to identify what, if any, compounds were present. The ESCA/XPS analysis allowed the analyst to "sputter" into the sample with an electron gun, aiding in the identification of the layering sequence. XPS uses photons, rather than electrons, which impinge upon the surface of the sample. XPS measures the electrons emitted from within the first 5 nm of the sample's surface. The XRD measures the scatter angles of incident X-rays; the angle and intensity of scatter depend upon the crystalline structure of the pulverized sample. XRD is considered a qualitative rather than quantitative technique. ESCA/XPS revealed that the final layer to deposit was predominantly carbonaceous. XRD was successful in identifying specific compounds, such as Al 2O3, Al and/or Al3 21SiO47, mullite (3(Al2)O3 -SiO2), and nickel-aluminides. Eventually, Electron MicroProbe Analysis (EMPA) was conducted on the marialographically-prepared cross- sections of selected slag deposits. Microprobe combines SEM and Wavelength Dispersive X-Ray Spectroscopy (WDS), and, like EDX, uses a narrowly-focused high-energy electron beam impinging upon a specimen to elicit, in the case of EPMA, characteristic X-rays with specific wavelengths. This quantitative, analytical tool proved the most useful in determining depositional layering and composition of the slag deposits. This information was utilized in verifying the location of the breach in the left leading edge of the wing of the Columbia.

McDaniels, Steven J.↗

Oxidation in oxygen at 900 deg and 1000 deg C of four nickel-base cast superalloys: NASA-TRW VIA, B-1900, alloy 713C, and IN-738

The oxidation at 900 and 1,000 C of four nickel-base superalloys in 1 atmosphere of slowly flowing oxygen was investigated. Thermogravimetric rate data were obtained for periods to 100 hours. The morphology and composition of the oxide scales formed after 100 hours were studied by optical microscopy, X-ray diffraction, electron microprobe, scanning electron microscopy, and X-ray photoelectron spectroscopy (ESCA). Alloys B-1900 and VIA were found to be primarily alumina formers, though probably 25 percent of their surface was covered by CR2O3-containing oxides at 900 C. Alloys 713C and IN-738 were primarily chromia formers, though the surface of 713C at 1,000 C was covered with NiO, and the surface of IN-738 at both temperatures was covered with a thin layer of TiO2.

Fryburg, G. C.↗

Optimum detection of an optical image on a photoelectric surface

The detection of an optical image in the presence of uniform background light is based on a likelihood ratio formed of the numbers of photoelectrons emitted from small elements of a photoelectric surface onto which the image is focused. When diffraction is negligible and the surface has unit quantum efficiency, this detector is equipollent with the optimum detector of the image forming light. Its performance is compared with that of the threshold detector and that of a detector basing its decisions on the total number of photoelectrons from a finite area of the image. The illuminance of the image is postulated to have a Gaussian spatial distribution. All three detectors exhibit nearly the same reliability.

Helstrom, C. W.↗

Effects of high energy radiation on the mechanical properties of epoxy/graphite fiber composites

Studies on the effects of high energy radiation on graphite fiber reinforced composites are summarized. Studies of T300/5208 and C6000/PMR15 composites, T300 fibers and the resin system MY720/DDS (tetraglycidyl-4,4'-diaminodiphenyl methane cured with diaminodiphenyl sulfone) are included. Radiation dose levels up to 8000 Mrads were obtained with no deleterious effects on the breaking stress or modulus. The effects on the structure and morphology were investigated using mechanical tests, electron spin resonance, X-ray diffraction, and electron spectroscopy for chemical analysis (ESCA or X-ray photoelectron spectroscopy). Details of the experiments and results are given. Studies of the fracture surfaces of irradiated samples were studied with scanning electron microscopy; current results indicate no differences in the morphology of irradiated and control samples.

Fornes, R. E.↗

Solid-State Spun Fibers from 1 mm Long Carbon Nanotube Forests Synthesized by Water-Assisted Chemical Vapor Deposition

In this work, we report continuous carbon nanotube fibers dry-drawn directly from water-assisted CVD grown forests with millimeter scale length. As-drawn nanotube fibers exist as aerogel and can be transformed into more compact fibers through twisting or densification with a volatile liquid. Nanotube fibers are characterized by scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS), Raman microscopy and wide-angle X-ray diffraction (WAXD). Mechanical behavior and electrical conductivity of the post-treated nanotube fibers are investigated.

Zhang, Shanju↗

Synthesis of polycrystalline chalcopyrite semiconductors by microwave irradiation

Polycrystalline samples of the chalcopyrites CuInS2, CuInSe2, and CuInSSe were prepared from stoichiometric mixtures of the pure elements by microwave irradiation. The reactions were performed in sealed quartz tubes in as few as 3 minutes. The products were analyzed by X-ray diffraction, scanning electron microscopy, energy dispersive X-ray analysis, and X-ray photoelectron spectroscopy. The surface morphology and shape of the particles produced by this method suggest that the products are formed from liquid melts. This method could be applied to the production of bulk chalcopyrite as sources for thin film growth.

Landry, Christopher C.↗

Changes in chemical and optical properties of thin film metal mirrors on LDEF

Thin films of the metals Cu, Ni, Pt, Au, Sn, Mo, and W deposited on fused silica flats were exposed at ambient temperature on the leading and trailing faces of the LDEF. Reflectances of these films were measured from 250 to 2500 nm and compared with controls. The exposed films were subjected to the LDEF external environment including atomic oxygen, molecular contamination, and solar ultraviolet. Major changes in optical and infrared reflectance were seen for Cu, Mo, Ni, and W films on the leading face of LDEF and are attributed to partial conversion of metal to metal oxide. Smaller changes in optical properties are seen on all films and are probably caused by thin contaminant films deposited on top of the metal. The optical measurements are correlated with film thickness measurements, x-ray photoelectron spectroscopy, optical calculations, and, in the case of Cu, with x-ray diffraction measurements. In a few cases, comparisons with results from a similar UAH experiment on STS-8 have been drawn.

Peters, Palmer N.↗

Investigation of Alpha Silicon Carbide / Carbon Fiber Proposed (2H & 6H-SiC) / C

A commercially available alpha silicon carbide coated carbon 12k fiber tow was subjected to rigorous inspection and testing. The pyrolized polyacrylonitrile (PAN) fiber had gone through a conversion process that resulted in a thin layer of SiC forming on the exterior of the fiber. The fibers? surface was characterized by x-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES) and scanning electron microscopy (SEM). Powdered x-ray diffraction (XRD) examined the bulk material properties. Transmission electron microscopy (TEM) coupled with energy-dispersive X-ray spectroscopy (EDS) examined the crystallinity of the SiC. A number of pristine samples were used to determine elongation rate and tensile strength.

Trunek, Andrew↗

Space Shuttle Columbia Post-Accident Analysis and Investigation

Although the loss of the Space Shuttle Columbia and its crew was tragic, the circumstances offered a unique opportunity to examine a multitude of components which had experienced one of the harshest environments ever encountered by engineered materials: a break up at a velocity in excess of Mach 18 and an altitude exceeding 200,000 feet (63 KM), resulting in a debris field 645 miles/l,038 KM long and 10 miles/16 KM wide. Various analytical tools were employed to ascertain the sequence of events leading to the disintegration of the Orbiter and to characterize the features of the debris. The testing and analyses all indicated that a breach in a left wing reinforced carbon/carbon composite leading edge panel was the access point for hot gasses generated during re-entry to penetrate the structure of the vehicle and compromise the integrity of the materials and components in that area of the Shuttle. The analytical and elemental testing utilized such techniques as X-Ray Diffraction (XRD), Energy Dispersive X-Ray (EDX) dot mapping, Electron Micro Probe Analysis (EMPA), and X-Ray Photoelectron Spectroscopy (XPS) to characterize the deposition of intermetallics adjacent to the suspected location of the plasma breach in the leading edge of the left wing, Fig. 1.

McDanels, Steven J.↗

Teflon FEP Analyzed After Retrieval From the Hubble Space Telescope

During the Hubble Space Telescope (HST) Second Servicing Mission, 6.8 years after the telescope was deployed in low Earth orbit, degradation of unsupported Teflon FEP (DuPont; fluorinated ethylene propylene), used as the outer layer of the multilayer insulation (MLI) blankets, was evident as large cracks on the telescope light shield. A sample of the degraded outer layer (see the photograph) was retrieved during the second servicing mission and returned to Earth for ground testing and evaluation. Also retrieved was a Teflon FEP radiator surface from a cryogen vent cover that was exposed to the space environment on the aft bulkhead of the HST. NASA Goddard Space Flight Center directed the efforts of the Hubble Space Telescope MLI Failure Review Board, whose goals included determining the FEP degradation mechanisms. As part of the investigations into the degradation mechanisms, specimens retrieved from the first and second HST servicing missions, 3.6 and 6.8 years after launch, respectively, were characterized through exhaustive mechanical, optical, and chemical testing. Testing led by Goddard included scanning electron microscopy, optical microscopy, tensile testing, solar absorptance measurements, time-of-flight secondary ion mass spectroscopy (TOF-SIMS), Fourier transform infrared microscopy (m-FTIR), attenuated total reflectance infrared microscopy (ATR/FTIR), and x-ray diffraction (XRD). The NASA Lewis Research Center contributed significantly to the analysis of the retrieved HST materials by leading efforts and providing results of bend testing, surface microhardness measurements, x-ray photoelectron spectroscopy, solid-state nuclear magnetic resonance spectroscopy, and density measurements. Other testing was conducted by Nano Instruments, Inc., and the University of Akron.

Dever, Joyce A.↗

Photoelectron spectra of the decomposition of ethylene on /110/ tungsten

The experimental apparatus used in the investigation consisted of an ultrahigh-vacuum chamber, a triple-grid, a microwave-excited resonance lamp, and an electron energy analyzer. The chemical nature of the chemisorbed species was studied, taking into account the energy distribution of photoemitted electrons, work function determinations, and low-energy electron diffraction patterns.

Plummer, E. W.↗

Optical Signal Processing: Poisson Image Restoration and Shearing Interferometry

Optical signal processing can be performed in either digital or analog systems. Digital computers and coherent optical systems are discussed as they are used in optical signal processing. Topics include: image restoration; phase-object visualization; image contrast reversal; optical computation; image multiplexing; and fabrication of spatial filters. Digital optical data processing deals with restoration of images degraded by signal-dependent noise. When the input data of an image restoration system are the numbers of photoelectrons received from various areas of a photosensitive surface, the data are Poisson distributed with mean values proportional to the illuminance of the incoherently radiating object and background light. Optical signal processing using coherent optical systems is also discussed. Following a brief review of the pertinent details of Ronchi's diffraction grating interferometer, moire effect, carrier-frequency photography, and achromatic holography, two new shearing interferometers based on them are presented. Both interferometers can produce variable shear.

Hong, Yie-Ming↗

Analysis of surfaces from the LDEF A0114, phase 2

During the reporting period, work continued on profilometry measurements of eroded and corroded sample surfaces, optical transmission measurements, analysis of the pinhole camera, and x-ray photoelectron spectroscopy (XPS) analysis of some samples. Among metal samples, copper showed some interesting new results. There were two forms of copper samples: a thin film sputter-coated on fused silica and a solid piece of OFHC copper. They were characterized by x-ray and Auger electron spectroscopies, x-ray diffraction, and high resolution profilometry. Cu 2p core level spectra were used to demonstrate the presence of Cu2O and CuO and to determine the oxidation states.