SEARCH · Engineering Papers
Results for “isotactic polypropylene”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Understanding interfacial crystallization dynamics on carbon fiber reinforced polypropylene composite manufacturing
Reinforcing polymers with discontinuous fibers improves mechanical properties, such as strength and stiffness, and in some cases achieve isotropic properties, rendering them suitable for various engineering applications. Matrix materials are generally highly engineered thermosets (e.g. crosslinked epoxies), bonded to the fiber periphery by proprietary surface and sizing chemistries. Semicrystalline thermoplastic matrices are less utilized due to poor fiber-matrix bonding resulting in inefficient interfacial load-transfer in reinforced composites. However, flexibility with melt-processing or molding conditions can be leveraged to promote non-covalent interfacial bonding between matrix and fiber via crystallization of the matrix onto fiber surface. In the present study, we utilize a co-mingle chopped carbon and isotactic polypropylene fibers to form isotropic composites, tailoring interfacial immobilized matrix or interphase morphology to optimize performance through precise control of thermal processing/molding windows. Calorimetry and optical microscopy were employed to investigate the impact of carbon fiber at various volume fractions (10, 20, and 30 %) on isotactic polypropylene crystallization and mechanical performance. Variations in mechanical properties correspond to the structural evolution of the interfacial region and are correlated to underlying microstructural attributes using wide-angle X-ray scattering, thermal analysis, and low-field nuclear magnetic resonance spectroscopy. These results provide a practical framework for the manufacturing of thermoplastic matrix composites. In conclusion, the results presented provide a guide for the strategic optimization of interphase design, showcasing tailorable tensile strengths which outperform any isotactic polypropylene carbon fiber composites previously reported in literature.
Low gravity synthesis of polymers with controlled molecular configuration
Heterogeneous chemical systems have been studied for the synthesis of isotactic polypropylene in order to establish baseline parameters for the reaction process and to develop sensitive and accurate methods of analysis. These parameters and analytical methods may be used to make a comparison between the polypropylene obtained at one g with that of zero g (gravity). Baseline reaction parameters have been established for the slurry (liquid monomer in heptane/solid catalyst) polymerization of propylene to yield high purity, 98% isotactic polypropylene. Kinetic data for the slurry reaction showed that a sufficient quantity of polymer for complete characterization can be produced in a reaction time of 5 min; this time is compatible with that available on a sounding rocket for a zero-g simulation experiment. The preformed (activated) catalyst was found to be more reproducible in its activity than the in situ formed catalyst.
Tailoring the properties of polymers via formation of a mesophase
The combination of the control of the concentration of stereodefects in isotactic polypropylene using metallocene catalysts and the crystallization via the mesophase is a strategy to tailor the mechanical properties. Stiff materials, flexible materials, and thermoplastic elastomers can be produced depending only on the concentration of rr stereodefects. We show that in the case of isotactic polypropylene (iPP) the material properties can be finely tuned at molecular level via formation of a solid mesophase, characterized by an intermediate degree of order between amorphous and crystalline state. The effect of different degree of stereoregularity on the mesophase formation, thermal stability, morphology, is analyzed at different length scales, using different technique including wide angle X-ray scattering, atomic and optical microscopy. Different morphologies are observed depending on the stereoregularity and conditions of crystallization. In contrast to the lamellar morphology of crystals normally obtained from the melt, the solid mesophase show a nodular morphology.
Polypropylene Degradation Catalyzed by Tantalum Hydrides Supported on Sulfated Alumina
Ta–H + sites supported on sulfated aluminum oxide (SAO), [Ta(H) 2 (O–) 2 ][SAO] (1), catalyze the hydrogenolysis of isotactic polypropylene (iPP, M n = 13.3 kDa; D = 2.4; mmmm = 94%) to form low-molecular-weight branched alkanes (C 11 –C 30 ) in good yields (70%). Here, the alkanes formed lose stereochemical information originating from iPP, but residual iPP remains highly isotactic. In the presence of D 2 , similar mixtures of alkanes are formed containing –CH 3–x D x , –CHD, and –CD–. Residual iPP maintains high tacticity and incorporates deuterium primarily into –CH 3 groups of the polymer (–CH 3–x D x /–CHD–/–CD– ~10:1:0). 1 reacts with pinacolborane to form [TaH(κ 2 -H 2 BPin)(O–) 2 ][SAO] (2). At 200 °C in an iPP melt, 2 reacts to form products indicative of C–H bond activation at –CH 3 groups and internal –CH 2 – groups in iPP in a ~1:3 ratio, indicating a slight kinetic preference for C–H bond activation at internal –CH 2 – groups. 1 is more reactive toward iPP than high-density polyethylene in hydrogenolysis reactions
Influence of Magnetite Nanoparticles on the Dielectric Properties of Metal Oxide/Polymer Nanocomposites Based on Polypropylene
Structure and dielectric properties of polymer nanocomposites based on isotactic polypropylene and iron oxide (Fe{sub 3}O{sub 4}) nanoparticles are studied. Distribution of magnetite nanoparticles in a polymer matrix was studied by scanning electron microscopy (SEM, Carl Zeiss). Dielectric properties of nanocomposites were examined by means of E7-21 impedance spectrometer in the frequency range of 10{sup 2}–10{sup 6} Hz and temperature interval of 298–433 K. The frequency and temperature dependences of the dielectric permittivity ε, as well as the temperature dependence of log (ρ) were constructed. It is shown that introduction of the magnetite (Fe{sub 3}O{sub 4}) nanoparticles into a polypropylene matrix increases the dielectric permittivity of nanocomposites. An increase in the dielectric permittivity is explained by the increase in the polarization ability of nanocomposites. It is found that a decrease in the specific resistance with increasing temperature up to 318 K is associated with an increase in the ionic conductivity of nanocomposites. An increase in the resistance at temperatures higher than 358 K is due to the destruction of the crystalline phase of the polymer, as a result of which the distance between the Fe{sub 3}O{sub 4} nanoparticles increases.
One-Step Radical-Induced Synthesis of Graft Copolymers for Effective Compatibilization of Polyethylene and Polypropylene
The synthesis of copolymers from high-density polyethylene (HDPE) and isotactic polypropylene (iPP) has gained increasing attention due to their ability to improve the recycling of incompatible mixed polyolefin waste feed streams. Herein, we report a new radical grafting process that yields HDPE-g-iPP copolymers from HDPE and iPP by using a commercially available peroxide. Tensile testing of brittle 70/30 HDPE/iPP mixtures with these graft copolymers added showed promising compatibilization, improving the elongation at break of the blends from 20% up to 1080%. Detailed kinetic studies coupled with thermal and rheological characterization revealed optimized conditions for HDPE and iPP macroradical coupling and a deeper understanding of the grafting reaction. This optimization yielded HDPE-g-iPP copolymers that compatibilize HDPE and iPP blends at loadings as low as 2.5 wt %. In conclusion, the versatility of this macroradical grafting reaction was demonstrated by preparing an effective compatibilizer from untreated postconsumer waste plastics.
Improved Polypropylene Thermoformability through Polyethylene Layering
Due to its low cost, stiffness, and recyclability, isotactic polypropylene (iPP) is an excellent candidate for packaging applications. However, iPP is notoriously difficult to thermoform due to its low melt strength. The addition of just 10 thin layers of high-molecular-weight, linear low-density polyethylene (LLDPE) into iPP sheets by coextrusion significantly increased extensional viscosity and reduced sag. Both LLDPE and iPP were metallocene-catalyzed with excellent adhesion as measured in our previous work. Here, we performed a series of hot tensile tests and sheet sag measurements to determine the properties of the iPP sheet and the multilayer sheet between 130 and 180 °C. To evaluate the thermoformability of these multilayer sheets, truncated conical cups were positive vacuum formed at different temperatures and heating times, and the crush strength was measured. Cups that released easily from the mold with good shape retention and a crush strength within 80% of the maximum value were used to define a temperature–time thermoformability window. We estimated the maximum stress that occurred during the thermoforming process to be 5 MPa. Layer thicknesses before and after thermoforming were used to estimate an average strain of 0.78. The thin LLDPE layers decreased the yield stress below 5 MPa. This enabled thermoforming at sheet temperatures as low as 150 °C. The immiscible LLDPE interfaces increased extensional viscosity, which decreased sag in the multilayer sheets compared to iPP. This broadened the thermoforming range to temperatures as high as 180 °C and allowed longer heating times. These highly thermoformable, layered sheets may be recycled as iPP since they contain only 8% of LLDPE.
Effect of Macro- and Microstructures on Catalytic Hydrogenolysis of Polyolefins
Here, polyethylenes of varying molecular weight and branch density, as well as polypropylenes of varying molecular weight and tacticity, were catalytically converted to lower-molecular-weight liquid products to showcase how these various properties in a mixed waste plastic stream could affect the final product. A Pt nanoparticle on a strontium titanate nanocuboid (Pt/STO) catalyst was used under solvent-free conditions in the presence of 170 psi of H 2 at 300 °C for hydrogenolysis. The initial molecular weight of polyethylene was found to have a moderate effect on the yield to the final product (ranging from 55 wt% for M n ~ 7600 Da to 67 wt% for M n ~ 50,950 Da). The microstructure, defined as the length and density of branches in a polymer, of higher-molecular-weight polymers was the dominant factor in determining the yield (ranging from 67 wt% for M n ~ 50,950 Da for linear low-density polyethylene (LLDPE) with C 2 branches to 97 wt% for M n ~ 38,850 Da for LLDPE with C 6 branches). The same products (M n = C 29 –C 46 , Ð = 1.1–1.6) and distribution of undesired light gases (C 1 –C 4 ≈ 90 mol%, C 5 –C 8 ≈ 10 mol%) are obtained from conversions of PE of varying molecular weight. The tacticity of polypropylene at a given molecular weight had a significant effect on the molecular weight of the final product, while not strongly affecting conversion. Hydrogenolysis of isotactic polypropylene (iPP) produced ≈C 18 with a wider polydispersity (Ð ~ 1.4) compared to the narrow ≈C 64 (Ð ~ 1.0) and ≈C 54 (Ð ~ 1.0) products from atactic (aPP) and syndiotactic (sPP) polypropylene, respectively. The stereochemistry of the methyl groups dictates the shape and structure of the polymer in the melt, which in turn affects how the hydrocarbon chain interacts with the catalyst surface, thereby impacting the number of C–C scissions. These results show how various characteristics such as the molecular weight and structure of a waste plastic stream could affect the final product.
Size and Structure Effects of Carbon-Supported Ruthenium Nanoparticles on Waste Polypropylene Hydrogenolysis Activity, Selectivity, and Product Microstructure
Hydrogenolysis of plastic waste using Ru-based catalysts is promising for deconstructing polyolefins into lower molecular weight products. Yet, the effect of catalyst atomic structure and size on activity and product selectivity is poorly understood. Herein, we expose the effect of metal particle size and atomic structure on isotactic-polypropylene (i-PP) hydrogenolysis over Ru supported on carbon. Despite similar molecular weight distributions of solid and liquid products, their physical properties are distinct due to different chain regio-irregular CH3 sequences of steric pentads containing racemo configurations. We propose that i-PP hydrogenolysis entails an interplay of C–C bond scission and stereoisomerization. The active site’s local electronic environment and structure dictate the former, whereas polymer–catalyst surface interactions creating suitable polymer conformations control the latter. C–C scission and stereoisomerization are structure-sensitive. Small, disordered nanoclusters are effective in C–C bond scission, whereas larger metal nanoparticles promote stereoisomerization. Finally, we hypothesize that a heterogeneous distribution of metal active sites is essential for deconstruction and product (lubricant base oil) quality control.
A Vitrimer Acts as a Compatibilizer for Polyethylene and Polypropylene Blends
Polymer compatibilization plays a critical role in achieving polymer blends with favorable mechanical properties and enabling efficient recycling of mixed plastic wastes. Nonetheless, traditional compatibilization methods often require tailored designs based on the specific chemical compositions of the blends. In this study, we propose a new approach for compatibilizing polymer blends using a dynamically crosslinked polymer network, known as vitrimers. By adding a relatively small amount (1–5 w/w%) of a vitrimer made of siloxane‐crosslinked high‐density polyethylene (HDPE), we successfully compatibilized unmodified HDPE and isotactic polypropylene (iPP). The vitrimer‐compatibilized blend exhibited enhanced elongation at break (120 %) and smaller iPP domain sizes (0.4 μm) compared to the control blend (22 % elongation at break, 0.9 μm iPP droplet size). Moreover, the vitrimer‐compatibilized blend showed significantly improved microphase stability during annealing at 180 °C. This straightforward method shows promise for applications across various polymer blend systems.
A Vitrimer Acts as a Compatibilizer for Polyethylene and Polypropylene Blends
Abstract Polymer compatibilization plays a critical role in achieving polymer blends with favorable mechanical properties and enabling efficient recycling of mixed plastic wastes. Nonetheless, traditional compatibilization methods often require tailored designs based on the specific chemical compositions of the blends. In this study, we propose a new approach for compatibilizing polymer blends using a dynamically crosslinked polymer network, known as vitrimers. By adding a relatively small amount (1–5 w/w%) of a vitrimer made of siloxane‐crosslinked high‐density polyethylene (HDPE), we successfully compatibilized unmodified HDPE and isotactic polypropylene (iPP). The vitrimer‐compatibilized blend exhibited enhanced elongation at break (120 %) and smaller iPP domain sizes (0.4 μm) compared to the control blend (22 % elongation at break, 0.9 μm iPP droplet size). Moreover, the vitrimer‐compatibilized blend showed significantly improved microphase stability during annealing at 180 °C. This straightforward method shows promise for applications across various polymer blend systems.
Installing Controlled Stereo-Defects Yields Semicrystalline and Biodegradable Poly(3-Hydroxybutyrate) with High Toughness and Optical Clarity
Stereo-defects present in stereo-regular polymers often diminish thermal and mechanical properties, and hence suppressing or eliminating them is a major aspirational goal for achieving polymers with optimal or enhanced properties. Here, we accomplish the opposite by introducing controlled stereo-defects to semicrystalline biodegradable poly(3-hydroxybutyrate) (P3HB), which offers an attractive biodegradable alternative to semicrystalline isotactic polypropylene but is brittle and opaque. We enhance the specific properties and mechanical performance of P3HB by drastically toughening it and also rendering it with the desired optical clarity while maintaining its biodegradability and crystallinity. This toughening strategy of stereo-microstructural engineering without changing the chemical compositions also departs from the conventional approach of toughening P3HB through copolymerization that increases chemical complexity, suppresses crystal-lization in the resulting copolymers, and is thus undesirable in the context of polymer recycling and performance. More specifically, syndio-rich P3HB (sr-P3HB), readily synthesized from the eight-membered meso-dimethyl diolide, has a unique set of stereo-microstructures comprising enriched syndiotactic [rr] and no isotactic [mm] triads but abundant stereo-defects randomly distributed along the chain. This sr-P3HB material is characterized by high toughness (UT = 96 MJ/m 3 ) as a result of its high elongation at break (>400%) and tensile strength (34 MPa), crystallinity (T m = 114 degrees C), optical clarity (due to its submicron spherulites), and good barrier properties, while it still biodegrades in freshwater and soil.
SAXS Study of Reversibly Crosslinked Isotactic Polypropylene/clay Nanocomposites
A new route based on reversibly crosslinking reactive extrusion is applied for the development of iPP/clay nanocomposites. Analysis of small-angle X-ray scattering (SAXS) reflections of isotactic polypropylene (iPP)/clay nanocomposites, prepared by two different mixing and chemical crosslinking methods (i.e., conventional and in situ), is presented and results are compared with preceding wide-angle X-ray diffraction (WAXD) results. It is shown that the presence of clay significantly affects the value of long spacing in iPP, as well as the coherence length of lamellar stacks. Results show that the size of the coherently diffracting nanodomains decreases in two stages, first rapidly and then slowly as a function of increasing clay content. This can be attributed to the influence of confined iPP lamellae under the effect of rising number of clay particles. The appearance of the {gamma}-crystalline form in the crosslinked iPP/clay nanocomposites is related with the difficulty in chain folding of iPP chains introduced by the chemical crosslinking process, as well as by the presence of clay particles.
Crystallization Behavior of Isotactic Propylene-1-Hexene Random Copolymer Investigated by Time-Resolved SAXS/WAXD Techniques
The crystallization behavior of isotactic propylene-1-hexene (PH) random copolymer having 5.7% mole fraction of hexene content was investigated using simultaneous time-resolved small-angle X-ray scattering (SAXS) and wide-angle X-ray diffraction (WAXD) techniques. For this copolymer, the hexene component cannot be incorporated into the unit cell structure of isotactic polypropylene (iPP). Only {alpha}-phase crystal form of iPP was observed when samples were melt crystallized at temperatures of 40 C, 60 C, 80 C, and 100 C. Comprehensive analysis of SAXS and WAXD profiles indicated that the crystalline morphology is correlated with crystallization temperature. At high temperatures (e.g., 100 C) the dominant morphology is the lamellar structure; while at low temperatures (e.g., 40 C) only highly disordered small crystal blocks can be formed. These morphologies are kinetically controlled. Under a small degree of supercooling (the corresponding iPP crystallization rate is slow), a segmental segregation between iPP and hexene components probably takes place, leading to the formation of iPP lamellar crystals with a higher degree of order. In contrast, under a large degree of supercooling (the corresponding iPP crystallization rate is fast), defective small crystal blocks are favored due to the large thermodynamic driving force and low chain mobility.