The gamma-gamma prime region of the Ni-Al-Cr-Ti-W-Mo system at 850 C
The compositional limits of gamma and gamma-prime phases in nickel-base superalloys are determined experimentally. It is found that gamma-prime had the following range of compositions for the various elements contained in this phase: 72.1 to 78.0 at.% Ni; 7.8 to 17.3 at.% Al; 1.5 to 8.9 at.% Cr; 0.3 to 13.9 at.% Ti, 0.0 to 3.9 at.% Mo, and 0.0 to 7.2 at.% W. The composition of gamma varied as follows: Ni is balanced; 1.9 to 15.4 at.% Al; 6.6 to 30.7 at.% Cr; 0.0 to 3.1 at.% Ti; 0.0 to 8.7 at.% Mo; and 0.0 to 5.0 at.% W. W additions to the gamma appeared to increase somewhat the solubility of Al in this phase. Mo and W added together decreased the solubility of Al in gamma.