Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ZIRCONIUM 100”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Nanoindentation of ZrN Coatings on Silicon and Copper Substrates

An effective mathematical model is proposed to describe experiments on the indentation of samples with layered or functionally graded coatings. The model is based on the elastic contact problem corresponding to the penetration of a punch in a coated elastic half-space. A Berkovich indenter is considered. The results of the simulation and the experiments are compared for the indentation of two zirconium nitride (ZrN) coatings on substrates of monocrystalline (100) silicon and annealed copper. The agreement of the results is good.

42 ENGINEERING↗

ORNL Neutron Cross-Section Measurements in the Resolved Resonance Range for the NCSP

Nuclear criticality simulations test the quality and the consistency of the existing nuclear evaluated data libraries such as ENDF/B, JEFF, or JENDL. In some cases, the cross-section evaluations of those libraries are found insufficient to describe accurately criticality benchmarks. The US Nuclear Criticality Safety Program (NCSP) collaborates with the Joint Research Center (JRC) in Geel, Belgium, to perform high-resolution neutron-induced cross section measurements at the Geel Linear Accelerator (GELINA) to resolve deficiencies in nuclear data that have been emerging in criticality calculations. Problems with nuclear data include insufficient neutron energy range, missing covariances, and problems with previous experiments. For example, the use of the ENDF/B-VII.1 neutron cross section data for vanadium, cerium and zirconium in nuclear criticality safety calculations shows discrepancies between benchmark calculations measurements and demonstrates the need for reliable covariance data. For new covariances of existing data, a reevaluation of the old cross section data is needed. However, these data are in many cases no longer available. This deficit can be overcome only by obtaining new experimental data to serve as the basis of a new evaluation. Recent measurements were made of the neutron total and capture cross sections of natural vanadium and natural zirconium in the neutron energy range from 100 eV to several hundred keV. These measured data will be used to improve representation of the cross sections since most of the available evaluated data rely on old measurements.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Design and operation of a 1000 C lithium-cesium test system

A 100 kWt cesium-lithium test loop fabricated of niobium-1% zirconium for experiments on erosion and two-phase system operation at temperatures of 980 C and velocities of 150 m/s. Although operated at design temperature for 100 hours, flow instabilities in the two-phase separator interfered with the achievement of the desired mass flow rates. A modified separator was fabricated and installed in the loop to alleviate this problem.

Hays, L. G.↗

Microstructure and Mechanical Properties of W-ZrC Composites Synthesized by Reactive Melt Infiltration of Zr{sub 2}Cu into Porous Preforms from Partially Carburized W Powders

W-ZrC composites with different W contents from 48 to 73 vol.% have been synthesized by reactive melt infiltration of Zr{sub 2}Cu melt into porous preforms from partially carburized W powders at 1300 °C for 1 h in vacuum. The influences of carbon content and porosity in the preforms on microstructure and mechanical properties of W-ZrC composites are investigated. Cold isostatic pressing followed by pre-sintering process is used to produce porous preforms with suitable porosities of 53.6-47% under a pressure of 100 MPa to allow sufficient penetration of Zr{sub 2}Cu melt into the preforms. Small amounts of Cu-rich phases form in the synthesized W-ZrC composites after a complete reaction of y/2xZr{sub 2}Cu(l) + WC{sub y}(s) = y/xZrC{sub x}(s) + W(s) + y/2xCu(l). These Cu-rich phases are distributed not only at the phase boundaries of W matrix and ZrC grains, but also in the interior of ZrC{sub x} grains. With decreasing W content from 73 to 48 vol.% in the W-ZrC composites, the flexural strength and fracture toughness increase from 519 to 657 MPa and from 9.1 to 10.6 MPa m{sup 1/2}, respectively.

36 MATERIALS SCIENCE↗

The partial substitution of Y with Gd on microstructures and mechanical properties of as-cast and as-extruded Mg-10Zn-6Y-0.5Zr alloy

Highlights: • The as-extruded Mg-10Zn-6Y-0.5Zr and Mg-10Zn-3Y-3Gd-0.5Zr alloys show bimodal microstructure and DRXed microstructure. • In addition to W phase, Icosahedral quasicrystal phase layer is observed at the surface of some W phase particles in as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt. %) alloy. • The as-extruded Mg-10Zn-6Y-0.5Zr (wt. %) alloy exhibits TYS of 341 MPa, UTS of 368 MPa and elongation to failure of 6.8%. While the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt. %) alloy shows lower TYS of 247 MPa, UTS of 330 MPa and higher elongation to failure of 19.8%. - Abstract: Mg-10Zn-6Y-0.5Zr (wt%) alloy and Mg-10Zn-3Y-3Gd-0.5Zr (wt%) alloy with medium RE content have been fabricated by conventional casting and indirect extrusion. The as-extruded Mg-10Zn-6Y-0.5Zr (wt%) alloy shows a bimodal microstructure containing dynamic recrystallized (DRXed) grains with average grain size of 2 μm and deformed regions. In addition to the fragmented W phase particle bands distributing along the extrusion direction, large amount of nano W phase and small amount of nano β{sub 2}′ phase are precipitated in the matrix. While the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt%) alloy exhibits completely dynamic recrystallized microstructure with average grain size of 3 μm. The broken W phase particles are distributed homogeneously in the matrix. Icosahedral quasicrystal phase layer is observed at the surface of some W phase particles in the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr alloy. The as-extruded Mg-10Zn-6Y-0.5Zr (wt%) alloy exhibits yield strength of 341 MPa, ultimate tensile strength of 368 MPa and elongation to failure of 6.8%. While the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt%) alloy shows lower yield strength of 247 MPa, ultimate tensile strength of 330 MPa and higher elongation to failure of 19.8%. The higher strength in the as-extruded Mg-10Zn-6Y-0.5Zr (wt%) alloy is mainly attributed to higher area fraction of unDRXed regions with strong texture and the precipitation of nano W and β{sub 2}′ phase. The fully recrystallized microstructure with weak texture and the formation of icosahedral quasicrystal phases with good coherent bond with α-Mg contribute to the good ductility of the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr alloy.

36 MATERIALS SCIENCE↗

Structure and properties of ZrN coatings deposited by high power impulse magnetron sputtering technology

Monolayer ZrN coatings were deposited exclusively by the novel high power impulse magnetron sputtering (HIPIMS) technology in an industrial scale physical vapour deposition (PVD) machine (HTC-1000-4 target system). Coatings were deposited on 1 {mu}m polished M2 high speed steel, on 304L stainless steel (SS), and on Si (100) specimens. Prior to deposition, HIPIMS plasma sustained on a zirconium (Zr) target was utilized to pretreat the specimens. Coatings were deposited at 400 deg. C in a mixed N{sub 2} and Ar atmosphere using 2 magnetrons in HIPIMS mode and at three different substrate bias voltages (U{sub bias}) keeping all other process parameters constant. The thicknesses of the coatings measured by the ball cratering technique were in the ranges of 1.84, 1.96, and 2.13 {mu}m at bias voltages of -95, -75, and -65 V, respectively, where the difference in thickness can be attributed to the resputtering effect. X-ray diffraction experiments on SS specimens revealed a dominating 111 texture for all three coatings irrespective of the bias voltage. Cross-sectional transmission electron microscopy revealed extremely dense coating structures at all bias voltages, similar to the transition zone structure (zone T) reported by Thornton. The -95 bias voltage coatings appeared extremely smooth on the top and with no dome shaped structures often associated with low ion bombardment during deposition. HIPIMS pretreatment leads to high adhesion (L{sub C}) of the coatings to the substrate. A continuous ductile perforation of the coating was observed at progressive loads greater than 65 N; however, no spallation of the coating was observed up to loads of 100 N. High values of hardness (40.4 GPa), Young's modulus (424 GPa), and compressive stress (10 GPa) were recorded for coatings deposited at -95 BV. The hardness and internal stress of the coating were found increasing with more negative bias voltages. All the coatings exhibited high dry sliding wear resistance (K{sub C}) in the range 6x10{sup -15} m{sup 3} N{sup -1} m{sup -1}. Cross-sectional transmission electron microscopy and atomic force microscopy analyses have been used to study the effect of ion bombardment obtained from HIPIMS on the structure of the coatings.

36 MATERIALS SCIENCE↗

Composite 4YSZ-Al2O3 Nanofibers Prepared by Electrospinning and Thermal Processing

The relationship between solution properties and processing parameters for novel yttria-alumina-zirconia nanofibers electrospun in a constant electric field is explored through systematic variation of precursor content and aging of the polymer gel. The upper solution viscosity and conductivity limit for electrospinning with an electric field strength of 0.84 kV/cm were ~1000 cP and ~5 mS/cm, respectively. There is a predictive relationship between volumetric flow rate and solution viscosity, conductivity, and surface tension; however, there is not a strong relationship between as-spun fiber diameters, ranging between 100 and 300 nm, and any solution property. The gelation mechanism by which aqueous polyvinylpyrollidone (PVP), zirconium acetate, and aluminum/yttrium nitrate solutions age is speculated to arise from zirconium acetate hydrolysis and polymerization, facilitating intermolecular hydrogen bonding between zirconium acetate complexes, PVP functional groups, and disassociated ionic species. The 4YSZ-Al 2 O 3 ceramic nanofiber diameters ranged between 50 and 100 nm depending on the volume percent of the ceramic phases. The annealed fibers appear amorphous and without excessive grain coarsening, indicating that a heat treatment of 1000°C for 2 hours is sufficient to produce tough, refractory nanofibrous membranes relevant for high-temperature filtration applications.

36 MATERIALS SCIENCE↗

Comparative study of Sc and Er addition on microstructure, mechanical properties, and electrical conductivity of Al-0.2Zr-based alloy cables

Highlights: • The comprehensive properties of Al-0.2Zr-0.1Sc were better than those of Al-0.2Zr-0.1Er alloy cable. • The microstructures evolved from fibrous grains to equiaxed grains with increasing annealing time. • The Zener drag force increased with increasing ratio of volume fraction (F{sub V}) to average diameter F{sub V}/ d-bar . • The capability to inhibit recrystallization was as follows: Al{sub 3}(Zr, Sc) > Al{sub 3}(Zr, Er) > Al{sub 3}Zr. - Abstract: The effect of the addition of 0.1 wt% Sc and 0.1 wt% Er on the deformation microstructure, Vickers microhardness, and electrical conductivity of Al-0.2 wt% Zr-based alloy cables annealed at 400 °C for different times was investigated. The comprehensive properties of Al-0.2Zr-0.1Sc were better than those of Al-0.2Zr-0.1Er. The optimal conditions for the Al-0.2Zr-01Sc alloy cable were a microhardness of 575 MPa, an electrical conductivity of 34.5 MS/m for an annealing time of 36 h, and those for the Al-0.2Zr-0.1Er alloy cable were a microhardness of 550 MPa, an electrical conductivity of 33.6 MS/m for an annealing time of 8 h. During the annealing process, dispersed Al{sub 3}(Zr,Sc/Er) precipitates were generated, which substantially impeded recrystallization by Zener pining of grain boundaries. Based on the ratio of volume fraction (F{sub V}) to average diameter ( d-bar ) of the precipitates, their capability to inhibit recrystallization was as follows: Al{sub 3}(Zr, Sc) > Al{sub 3}(Zr, Er) > Al{sub 3}Zr. Moreover, the electrical conductivity of Al-0.2Zr-0.1Sc was better than that of Al-0.2Zr-0.1Er, probably because Sc could better inhibit recrystallization than Er, leading to fewer grain boundaries and hence lesser electron scattering.

36 MATERIALS SCIENCE↗

Realistic simulations of the AGATA Demonstrator+PRISMA Spectrometer

The performance of the AGATA Demonstrator Array coupled to the PRISMA magnetic spectrometer have been evaluated in a consistent way using detailed Monte Carlo simulations of the two devices. Results for the {sup 90}Zr+{sup 208}Pb at 560 MeV reaction are presented and discussed here, proving that the Doppler correction capabilities of the AGATA+PRISMA setup will be very close to the intrinsic energy resolution of the germanium detectors.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Determination of the direct double- β -decay Q value of Zr 96 and atomic masses of Zr 90 - 92 , 94 , 96 and Mo 92 , 94 - 98 , 100

Experimental searches for neutrinoless double-β decay offer one of the best opportunities to look for physics beyond the standard model. Detecting this decay would confirm the Majorana nature of the neutrino, and a measurement of its half-life can be used to determine the absolute neutrino mass scale. Important to both tasks is an accurate knowledge of the Q value of the double-β decay. The LEBIT Penning trap mass spectrometer was used for the first direct experimental determination of the ⁹⁶Zr double-β decay Q value: Q ββ =3355.85(15) keV. This value is nearly 7 keV larger than the 2012 Atomic Mass Evaluation [M. Wang et al., Chin. Phys. C 36, 1603 (2012)] value and one order of magnitude more precise. The 3-σ shift is primarily due to a more accurate measurement of the ⁹⁶Zr atomic mass: m(⁹⁶Zr)=95.90827735(17) u. Using the new Q value, the 2νββ-decay matrix element, |M 2ν |, is calculated. Improved determinations of the atomic masses of all other zirconium ( 90-92,94,96 Zr) and molybdenum ( 92,94-98,100 Mo) isotopes using both ¹²C₈ and ⁸⁷Rb as references are also reported.

Gulyuz, K.↗

Oxidation Behavior of Zirconium Diboride Nanoparticles

The products of oxidation of ZrB{sub 2} powders with average particle sizes of ~100 and ~30 nm by atmospheric oxygen under isothermal conditions and during heating have been characterized by thermal analysis, X-ray diffraction, scanning electron microscopy, IR frustrated total internal reflection spectroscopy, energy dispersive X-ray analysis, and elemental analysis. The oxidation onset has been observed at 594 and 396°C, respectively. Oxidation at temperatures of ≥800°C leads to the formation of boron oxide and monoclinic ZrO{sub 2}, independent of the particle size of ZrB{sub 2}. The reaction rate constants for the oxidation of ZrB{sub 2} nanoparticles ~100 and ~30 nm in size have been determined to be 0.03, 0.15, and 0.31 h{sup –1} at 600, 650, and 700°C and 0.11, 0.35, and 0.81 h{sup –1} at 500, 600, and 700°C, respectively. The apparent activation energies for the oxidation of the ZrB{sub 2} nanoparticles ~100 and ~30 nm in size are 161 ± 4 and 62 ± 3 kJ/mol, respectively, as evaluated from the temperature dependence of the rate constants at the above temperatures.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Concept Feasibility Report for Electroplating Zirconium onto Uranium Foil - Year 2

The Fuel Fabrication Capability within the U.S. High Performance Research Reactor Conversion Program is funded through the National Nuclear Security Administration (NNSA) NA-26 (Office of Material Management and Minimization). An investigation was commissioned to determine the feasibility of using electroplating techniques to apply a coating of zirconium onto depleted uranium/molybdenum alloy (U-10Mo). Electroplating would provide an alternative method to the existing process of hot roll-bonding zirconium foil onto the U-10Mo fuel foil during the fabrication of fuel elements for high-performance research reactors. The objective of this research was to develop a reproducible and scalable plating process that will produce a uniform, 25 μm thick zirconium metal coating on U-10Mo foil. In previous work, Pacific Northwest National Laboratory (PNNL) established a molten salt electroplating apparatus and protocol to plate zirconium metal onto molybdenum foil (Coffey 2015). During this second year of the research, PNNL furthered this work by moving to the U-10Mo alloy system (90 percent uranium:10 percent molybdenum). The original plating apparatus was disassembled and re-assembled in a laboratory capable of handling low-level radioactive materials. Initially, the work followed the previous year’s approach, and the salt bath composition was targeted at the eutectic composition (LiF:NaF:ZrF4 = 26:37:37 mol%). Early results indicated that the formation of uranium fluoride compounds would be problematic. Other salt bath compositions were investigated in order to eliminate the uranium fluoride production (LiF:NaF = 61:39 mol% and LiF:NaF:KF = 46.5:11.5:42 mol% ). Zirconium metal was used as the crucible for the molten salt. Three plating methods were used—isopotential, galvano static, and pulsed plating. The molten salt method for zirconium metal application provided high-quality plating on molybdenum in PNNL’s previous work. A key advantage of this approach is that plating can be performed under conditions that would greatly reduce the quantity of intermetallics that form at the interface between the zirconium and U-10Mo; unlike roll bonding, the molten salt plating approach would allow for complete coverage of the U-10Mo foil with zirconium. When utilizing the experimental parameters developed for zirconium plating onto molybdenum, a uranium fluoride reaction product was formed at the Zr/U-10Mo interface. By controlling the initial plating potential, the uranium fluoride could be prevented; however, the targeted zirconium thickness (25 ±12.5 μm) could not be achieved while maintaining 100% coverage.

36 MATERIALS SCIENCE↗

Blending as an In-Tank Waste Processing Strategy: Year 1 Progress Report

The Hanford Site stores approximately 56 million gallons of radioactive legacy defense waste in underground tanks. Direct feed of southeast quadrant tank waste to a high-level waste treatment facility is currently being explored to accelerate tank treatment activities. This study seeks to de-risk waste transfers by favorably altering the resuspension and critical velocities of wastes through strategic waste blending. Wastes rich in aluminum- and zirconium-bearing solids pose significant risks due to their high settled strength and density. A series of tests explores how solid phase particle size and suspending phase chemistry alter waste transport properties, quantified through the just-suspended mixing speed (NJS), for pure and blended aluminum- and zirconium-bearing waste solid simulants. The study utilizes a range of gibbsites (three sizes spanning 10 to 90 µm) and zirconia solids (three sizes spanning 10 to 100 µm). As expected, the NJS of pure solids largely follows predictions based on literature correlations; blends of gibbsite and zirconium-bearing solids of differing particle sizes exhibit NJS maxima attributed to dense packing of the mixed-size settled solids. The findings of this study will assist in developing strategies to optimize the transport of waste solids for the safe and efficient delivery of tank waste.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Methods to increase solid solution zirconium in aluminum alloys

A method of making an aluminum alloy containing zirconium includes heating a first composition comprising aluminum to a first temperature of greater than or equal to about 580° C. to less than or equal to about 800° C. The method further includes adding a second composition including a copper-zirconium compound to the first composition to form a third composition. The copper-zirconium compound of the second composition has a molar composition of greater than or equal to about 41% zirconium to less than or equal to about 67% zirconium and a balance of copper. The method also includes solidifying the third composition at a cooling rate of greater than or equal to about 0.1° C./second to less than or equal to about 100° C./second to a second temperature less than or equal to a solidus temperature and decomposing the copper-zirconium compound at a third temperature of less than or equal to about 715° C.

36 MATERIALS SCIENCE↗

Experimental verification of a crystal plasticity-based simulation framework for predicting microstructure and geometric shape changes: Application to bending and Taylor impact testing of Zr

This paper is concerned with experimental verification of a recently developed multi-scale simulation framework for plastic deformation of metallic materials from quasi-static to impact deformation conditions. The framework is a visco-plastic self-consistent (VPSC) polycrystalline model embedded in an implicit finite element method (FE-VPSC) to provide a microstructure-sensitive constitutive response at each material point. Each material point of the FEM model is a polycrystalline aggregate with crystallographic deformation mechanisms operating at the single crystal scale with their evolving activity based on a dislocation density-based hardening law and texture. Four beams and three cylinders machined in different orientations from a textured plate of high-purity zirconium are tested quasi-statically in 4-point bending and at speeds of 100 m/s, 170 m/s and 243 m/s during Taylor impact tests, respectively. The variation in dimensional changes resulting from different sample orientations in the plate with respect to loading directions is measured for each sample. Moreover, texture and twinning characterization is performed using electron backscattered diffraction (EBSD). The deformation processes and underlying evolution of microstructure are successfully simulated using the FE-VPSC framework. In doing so, the model parameters are optimized and validated across a broad range of strain rates and temperatures. Simulation results in terms of geometrical changes and microstructural evolution are compared with the experimental measurements. The model predicts anisotropic material flow resulting from the hard-to-deform crystallographic directions, the development of gradients in texture and twinning through the geometries, tension–compression asymmetry, as well as the extent of plasticity under impact.

42 ENGINEERING↗

Investigation of heat transfer in zirconium potassium perchlorate at low temperature: A study of the failure mechanism of the NASA standard initiator

The objective of this work was to study the reasons for the failure of pyrotechnic initiators at very low temperatures (10 to 100 K). A two-dimensional model of the NASA standard initiator was constructed to model heat transfer from the electrically heated stainless steel bridgewire to the zirconium potassium perchlorate explosive charge and the alumina charge cup. Temperature dependent properties were used in the model to simulate initiator performance over a wide range of initial temperatures (10 to 500 K). A search of the thermophysical property data base showed that pure alumina has a very high thermal conductivity at low temperatures. It had been assumed to act as a thermal insulator in all previous analyses. Rapid heat transfer from the bridgewire to the alumina at low initial temperatures was shown to cause failure of the initiators if the wire did not also make good contact with the zirconium potassium perchlorate charge. The mode is able to reproduce the results of the tests that had been conducted to investigate the cause for failure. It also provides an explanation for previously puzzling results and suggests simple design changes that will increase reliability at very low initial temperatures.

Varghese, Philip L.↗

Neutrinoless double-β decay and nuclear transition matrix elements

Within mechanisms involving the light Majorana neutrinos, squark-neutrino, Majorons, sterile neutrinos and heavy Majorana neutrino, nuclear transition matrix elements for the neutrinoless (β{sup −}β{sup −}){sub 0ν} decay of {sup 96}Zr, {sup 100}Mo, {sup 128,130}Te and {sup 150}Nd nuclei are calculated by employing the PHFB approach. Effects due to finite size of nucleons, higher order currents, short range correlations, and deformations of parent as well as daughter nuclei on the calculated matrix elements are estimated. Uncertainties in nuclear transition matrix elements within long-ranged mechanisms but for double Majoron accompanied (β{sup −}β{sup −}ϕϕ){sub 0ν} decay modes are 9%–15%. In the case of short ranged heavy Majorona neutrino exchange mechanism, the maximum uncertainty is about 35%. The maximum systematic error within the mechanism involving the exchange of light Majorana neutrino is about 46%.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗