At least 37 records · Page 2

Development of iron phosphate ceramic waste form to immobilize radioactive waste solution

The objective of this research was to develop an iron phosphate ceramic (IPC) waste form using converter slag obtained as a by-product of the steel industry as a source of iron instead of conventional iron oxide. Both synthetic off-gas scrubber solution containing technetium-99 (or Re as a surrogate) and LiCl-KCl eutectic salt, a final waste solution from pyrochemical processing of spent nuclear fuel, were used as radioactive waste streams. The IPC waste form was characterized for compressive strength, reduction capacity, chemical durability, and contaminant leachability. Compressive strengths of the IPC waste form prepared with different types of waste solutions were 16 MPa and 19 MPa for LiCl-KCl eutectic salt and the off-gas scrubber simulant, respectively, which meet the minimum compressive strength of 3.45 MPa (500 psi) for waste forms to be accepted into the radioactive waste repository. The reduction capacity of converter slag, a main dry ingredient used to prepare the IPC waste form, was 4,136 meq/kg by the Ce(IV) method, which is much higher than those of the conventional Fe oxides used for the IPC waste form and the blast furnace slag materials. Average leachability indexes of Tc, Li, and K for the IPC waste form were higher than 6.0, and the IPC waste form demonstrated stable durability even after 63-day leaching. In addition, the Toxicity Characteristic Leach Procedure measurements of converter slag and the IPC waste form with LiCl-KCl eutectic salt met the universal treatment standard of the leachability limit for metals regulated by the Resource Conservation and Recovery Act. This study confirms the possibility of development of the IPC waste form using converter slag, showing its immobilization capability for radionuclides in both LiCl-KCl eutectic salt and off-gas scrubber solutions with significant cost savings.

converter slag↗

Glass binder development for a glass-bonded sodalite ceramic waste form

This paper discusses work to develop Na2O-B2O3-SiO2 glass binders for immobilizing LiCl-KCl eutectic salt waste in a glass-bonded sodalite waste form following electrochemical reprocessing of used metallic nuclear fuel. Here, five new glasses with high Na2O contents were designed to generate waste forms having higher sodalite contents and fewer stress fractures. The structural, mechanical, and thermal properties of the new glasses were measured using variety of analytical techniques. The glasses were then used to produce ceramic waste forms with surrogate salt waste. The materials made using the glasses developed during this study were formulated to generate more sodalite than materials made with previous baseline glasses used. The coefficients of thermal expansion for the glass phase in the glass-bonded sodalite waste forms made with the new binder glasses were closer to the sodalite phase in the critical temperature region near and below the glass transition temperature. These improvements should result in lower probability of cracking in the full-scale monolithic ceramic waste form, leading to better long-term chemical durability. Additionally, a model generated during this study for predicting softening temperature of silicate binder glasses is presented.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Self-accelerated corrosion of nuclear waste forms at material interfaces

The US plan for high-level nuclear waste includes the immobilization of long-lived radionuclides in glass or ceramic waste forms in stainless-steel canisters for disposal in deep geological repositories. Here we report that, under simulated repository conditions, corrosion could be significantly accelerated at the interfaces of different barrier materials, which has not been considered in the current safety and performance assessment models. Severe localized corrosion was found at the interfaces between stainless steel and a model nuclear waste glass and between stainless steel and a ceramic waste form. The accelerated corrosion can be attributed to changes of solution chemistry and local acidity/alkalinity within a confined space, which significantly alter the corrosion of both the waste-form materials and the metallic canisters. The corrosion that is accelerated by the interface interaction between dissimilar materials could profoundly impact the service life of the nuclear waste packages, which, therefore, should be carefully considered when evaluating the performance of waste forms and their packages. Moreover, compatible barriers should be selected to further optimize the performance of the geological repository system.

Guo, Xiaolei↗

FY16 Annual Accomplishments - Waste Form Development and Performance: Evaluation Of Ceramic Waste Forms - Comparison Of Hot Isostatic Pressed And Melt Processed Fabrication Methods

FY16 efforts were focused on direct comparison of multi-phase ceramic waste forms produced via melt processing and HIP methods. Based on promising waste form compositions previously devised at SRNL, simulant material was prepared at SRNL and a portion was sent to the Australian Nuclear Science and Technology Organization (ANSTO) for HIP treatments, while the remainder of the material was melt processed at SRNL. The microstructure, phase formation, elemental speciation, and leach behavior, and radiation stability of the fabricated ceramics was performed. In addition, melt-processed ceramics designed with different fractions of hollandite, zirconolite, perovskite, and pyrochlore phases were investigated. for performance and properties.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Charge-Coupled Substituted Garnets (Y 3-x Ca 0.5x M 0.5x )Fe 5 O 12 (M = Ce, Th): Structure and Stability as Crystalline Nuclear Waste Forms

The garnet structure has been proposed as a potential crystalline nuclear waste form for accommodation of actinide elements, especially uranium (U). In this study, yttrium iron garnet (YIG) as a model garnet host was studied for the incorporation of U analogs, cerium (Ce) and thorium (Th), incorporated by a charge-coupled substitution with calcium (Ca) for yttrium (Y) in YIG, namely, 2Y 3+ = Ca 2+ + M 4+ , where M 4+ = Ce 4+ or Th 4+ . Single-phase garnets Y 3–x Ca 0.5x M 0.5x Fe 5 O 12 (x = 0.1–0.7) were synthesized by the citrate–nitrate combustion method. Ce was confirmed to be tetravalent by X-ray absorption spectroscopy and X-ray photoelectron spectroscopy. X-ray diffraction and 57 Fe–Mössbauer spectroscopy indicated that M 4+ and Ca 2+ cations are restricted to the c site, and the local environments of both the tetrahedral and the octahedral Fe 3+ are systematically affected by the extent of substitution. The charge-coupled substitution has advantages in incorporating Ce/Th and in stabilizing the substituted phases compared to a single substitution strategy. Enthalpies of formation of garnets were obtained by high temperature oxide melt solution calorimetry, and the enthalpies of substitution of Ce and Th were determined. The thermodynamic analysis demonstrates that the substituted garnets are entropically rather than energetically stabilized. This suggests that such garnets may form and persist in repositories at high temperature but might decompose near room temperature.

Guo, Xiaofeng↗

Leach Testing of Laboratory-Scale Melter Evaporator Condensate Cementitious Waste Forms

Cementitious waste forms immobilizing evaporated AP-105 off-gas condensate were used to determine radionuclide and contaminant leachability in deionized water over a 63-day period. The off-gas condensate was collected during the actual tank AP-105 low activity waste continuous laboratory-scale melter (LSM)) run performed in fiscal year 2018 and was then solidified as a cementitious waste form using the Cast Stone formulation (8 weight percent [wt%] ordinary Portland cement, 45 wt% class F fly ash, 47 wt% blast furnace slag). Here, using the U.S. Environmental Protection Agency Method 1315 leach testing procedure, the release rate of technetium 99 (Tc), iodine-129 (I), nitrate (NO 3 - ), and sodium (Na + ) from two Cast Stone specimens was measured. From these measurements, observed diffusivity values for each constituent were calculated and can be used in future iterations and maintenance of the Integrated Disposal Facility performance assessments. Furthermore, by testing Cast Stone specimens immobilizing off-gas produced while vitrifying actual tank waste, the results of this effort improve the technical defensibility of long-term waste form performance estimates for the Cast Stone formulation. Finally, 99 Tc distribution within a representative waste form at the end of the 63-day leach period as well as bulk mineralogy were determined using solid phase characterization methods.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Crystalline Ceramic Waste Forms: Comparison Of Reference Process For Ceramic Waste Form Fabrication

The research conducted in this work package is aimed at taking advantage of the long term thermodynamic stability of crystalline ceramics to create more durable waste forms (as compared to high level waste glass) in order to reduce the reliance on engineered and natural barrier systems. Durable ceramic waste forms that incorporate a wide range of radionuclides have the potential to broaden the available disposal options and to lower the storage and disposal costs associated with advanced fuel cycles. Assemblages of several titanate phases have been successfully demonstrated to incorporate radioactive waste elements, and the multiphase nature of these materials allows them to accommodate variation in the waste composition. Recent work has shown that they can be produced from a melting and crystallization process. The objective of this report is to explore the phase formation and microstructural differences between lab scale melt processing in varying gas environments with alternative densification processes such as Hot Pressing (HP) and Spark Plasma Sintering (SPS). The waste stream used as the basis for the development and testing is a simulant derived from a combination of the projected Cs/Sr separated stream, the Trivalent Actinide - Lanthanide Separation by Phosphorous reagent Extraction from Aqueous Komplexes (TALSPEAK) waste stream consisting of lanthanide fission products, the transition metal fission product waste stream resulting from the transuranic extraction (TRUEX) process, and a high molybdenum concentration with relatively low noble metal concentrations. Melt processing as well as solid state sintering routes SPS and HP demonstrated the formation of the targeted phases; however differences in microstructure and elemental partitioning were observed. In SPS and HP samples, hollandite, pervoskite/pyrochlore, zirconolite, metallic alloy and TiO 2 and Al 2 O 3 were observed distributed in a network of fine grains with small residual pores. The titanate phases that incorporate M +3 rare earth elements were observed to be distinct phases (ex. Nd 2 Ti 2 O 7 with less degree of substitution as compared to the more homogeneous melt processed samples where a high degree of substitution and variation of composition within grains was observed. Liquid phase sintering was enhanced in reducing gas environments and resulted in large (10-200 microns) irregular shaped grains along with large voids associated with the melt process; SPS and HP samples exhibited finer grain size with smaller voids. Metallic alloys were observed in the bulk of the sample for SPS and HP samples, but were found at the bottom of the crucible in melt processed trials. These results indicate that for a first melter trial, the targeted phases can be formed in air by utilizing Ti/TiO 2 additives which aid phase formation and improve the electrical conductivity. Ultimately, a melter run in reducing gas environments would be beneficial to study differences in phase formation and elemental partitioning.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Thermodynamic assessment of the hollandite high‐level radioactive waste form

Abstract Hollandite has been studied as a candidate ceramic waste form for the disposal of high‐level radioactive waste due to its inherent leach resistance and ability to immobilize alkaline‐earth metals such as Cs and Ba at defined lattice sites in the crystallographic structure. The chemical and structural complexity of hollandite‐type phases developed for high‐level waste immobilization limits the systematic experimental research that is required to understand phase development due to the large number of potential additives and compositional ranges that must be evaluated. Modeling the equilibrium behavior of the complex hollandite‐forming oxide waste system would aid in the design and processing of hollandite waste forms by predicting their thermodynamic stability. Thus, a BaO–Cs 2 O–TiO 2 –Cr 2 O 3 –Al 2 O 3 –Fe 2 O 3 –FeO–Ga 2 O 3 thermodynamic database was developed in this work according to the CALPHAD methodology. The compound energy formalism was used to model solid solution phases such as hollandite while the two‐sublattice partially ionic liquid model characterized the oxide melt. Results of model optimizations are presented and discussed including a 1473 K isothermal BaO–Cs 2 O–TiO 2 pseudo‐ternary diagram that extrapolates phase equilibrium behavior to regions not experimentally explored.

Utlak, Stephen A.↗

Epsilon Metal: A Waste Form for Noble Metals from Used Nuclear Fuel

Epsilon metal (e-metal) is the metallic phase that forms as inclusions at the grain boundaries in the UO2 fuel during reactor operation. This metal is composed of Pd, Mo, Rh, Ru, and Tc. These metallic inclusions are insoluble in strong acid and remnants of these metallic inclusions have been found in the UO2 matrix that remains from the natural reactors in Gabon that were active 1.8 billion years ago, therefore e-metal should be an excellent waste form for the immobilization of the long-lived isotopes 107Pd (6.5 ? 106 a) and 99Tc (2.13 ? 105 a), with 99Tc being the isotope of interest for repository performance. Therefore, the chemical durability of this potential waste form is assessed in this study. Typically, corrosion rates for metallic materials are measured electrochemically because they are quick, inexpensive, and can reveal the mechanism by which a metal corrodes, at least initially. However, in a repository the waste form would be subjected to slowly flowing water without an applied electrical potential over long time periods. Therefore, the corrosion rates of e-metal specimens were measured with both electrochemical tests and the single-pass flow-through test (SPFT). Potentiodynamic and potentiostatic polarization results suggest that a thin passive film exists on the alloy surface, which seems to be responsible for its high corrosion resistance. Additionally, X-Ray photoelectron spectroscopic results suggest that Pd oxides are significantly enriched in the passive film Results from the SPFT show that the dissolution rates were weakly dependent on pH. Only Mo and Re were found in solution and were used for the calculation of the dissolution rates. In general, the electrochemically determined corrosion rates agree reasonably well with the initial dissolution rate measured with the SPFT test, but they are about one or two orders of magnitude higher than the steady state rates. The causes for this discrepancy are discussed.

epsilon-metal, nuclear waste form, corrosion, sing↗

Reference Alloy Waste Form Fabrication and Initiation of Reducing Atmosphere and Reductive Additives Study on Alloy Waste Form Fabrication

This report describes the fabrication of two reference alloy waste forms, RAW-1(Re) and RAW-(Tc) using an optimized loading and heating method. The composition of the alloy materials was based on a generalized formulation to process various proposed feed streams resulting from the processing of used fuel. Waste elements are introduced into molten steel during alloy fabrication and, upon solidification, become incorporated into durable iron-based intermetallic phases of the alloy waste form. The first alloy ingot contained surrogate (non-radioactive), transition-metal fission products with rhenium acting as a surrogate for technetium. The second alloy ingot contained the same components as the first ingot, but included radioactive Tc-99 instead of rhenium. Understanding technetium behavior in the waste form is of particular importance due the longevity of Tc-99 and its mobility in the biosphere in the oxide form. RAW-1(Re) and RAW-1(Tc) are currently being used as test specimens in the comprehensive testing program investigating the corrosion and radionuclide release mechanisms of the representative alloy waste form. Also described in this report is the experimental plan to study the effects of reducing atmospheres and reducing additives to the alloy material during fabrication in an attempt to maximize the oxide content of waste streams that can be accommodated in the alloy waste form. Activities described in the experimental plan will be performed in FY12. The first aspect of the experimental plan is to study oxide formation on the alloy by introducing O 2 impurities in the melt cover gas or from added oxide impurities in the feed materials. Reducing atmospheres will then be introduced to the melt cover gas in an attempt to minimize oxide formation during alloy fabrication. The second phase of the experimental plan is to investigate melting parameters associated with alloy fabrication to allow the separation of slag and alloy components of the melt.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles: CRP T21027 1813: Processing technologies for high level waste, formulation of matrices and characterization of waste forms, Task 17208 (Final Report)

A multi-phase ceramic waste form is being developed at the Savannah River National Laboratory (SRNL) for treatment of secondary waste streams generated by reprocessing commercial spent nuclear. The envisioned waste stream contains a mixture of transition, alkali, alkaline earth, and lanthanide metals. Ceramic waste forms are tailored (engineered) to incorporate waste components as part of their crystal structure based on knowledge from naturally found minerals containing radioactive and non-radioactive species similar to the radionuclides of concern in wastes from fuel reprocessing. The ability to tailor ceramics to mimic naturally occurring crystals substantiates the long term stability of such crystals (ceramics) over geologic timescales of interest for nuclear waste immobilization [1]. A durable multi-phase ceramic waste form tailored to incorporate all the waste components has the potential to broaden the available disposal options and thus minimize the storage and disposal costs associated with aqueous reprocessing. This report summarizes results from three years of work on the IAEA Coordinated Research Project on “Processing technologies for high level waste, formulation of matrices and characterization of waste forms” (T21027), and specific task “Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles” (17208).

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles CRP T21027 1813: Processing technologies for high level waste, formulation of matrices and characterization of waste forms, Task 17208 (Final Report)

A multi-phase ceramic waste form is being developed at the Savannah River National Laboratory (SRNL) for treatment of secondary waste streams generated by reprocessing commercial spent nuclear. The envisioned waste stream contains a mixture of transition, alkali, alkaline earth, and lanthanide metals. Ceramic waste forms are tailored (engineered) to incorporate waste components as part of their crystal structure based on knowledge from naturally found minerals containing radioactive and non-radioactive species similar to the radionuclides of concern in wastes from fuel reprocessing. The ability to tailor ceramics to mimic naturally occurring crystals substantiates the long term stability of such crystals (ceramics) over geologic timescales of interest for nuclear waste immobilization. A durable multi-phase ceramic waste form tailored to incorporate all the waste components has the potential to broaden the available disposal options and thus minimize the storage and disposal costs associated with aqueous reprocessing. This report summarizes results from three years of work on the IAEA Coordinated Research Project on “Processing technologies for high level waste, formulation of matrices and characterization of waste forms” (T21027), and specific task “Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles” (17208).

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Mineral assemblage transformation of a metakaolin-based waste form after geopolymer encapsulation

Current plans for nuclear waste vitrification at the Hanford Tank Waste Treatment and Immobilization Plant (WTP) lack the capacity to treat all of the low activity waste (LAW) that is not encapsulated in the vitrified product. Fluidized Bed Steam Reforming (FBSR) is one of the supplemental technologies under consideration to fill this gap. The FBSR process results in a granular product mainly composed of feldspathoid mineral phases that encapsulate the LAW and other contaminants of concern (COCs). In order to better understand the characteristics of the FBSR product, characterization testing has been performed on the granular product as well as the granular product encapsulated in a monolithic geopolymer binder. The non-radioactive simulated tank waste samples created for use in this study are the result of a 2008 Department of Energy sponsored Engineering Scale Technology Demonstration (ESTD) in 2008. These samples were created from waste simulant that was chemically shimmed to resemble actual tank waste, and rhenium has been used as a substitute for technetium. Another set of samples was created by the Savannah River Site Bench-Scale Reformer (BSR) using a chemical shim of Savannah River Site Tank 50 waste in order to simulate a blend of 68 Hanford tank wastes. This paper presents results from coal and moisture removal tests along with XRD, SEM, and BET analyses showing that the major mineral components are predominantly sodium aluminosilicate minerals and that the mineral product is highly porous. Results also show that the materials pass the short-term leach tests: the Toxicity Characteristic Leaching Procedure (TCLP) and Product Consistency Test (PCT).

Feldspathoid Minerals↗

Evaluation of Iron‐Phosphate Glass–Ceramic Waste Form for Electrorefiner Salt Waste Simulant Dechlorinated With Phosphoric Acid

The importance of glass and glass–ceramic nuclear waste forms has been reaffirmed in recent years by the growing interest in nuclear power as a reliable energy source. Determination of processing methods for the disposal of halide-containing wastes will be essential for the advancement of nuclear technologies such as non-aqueous fuel reprocessing. Phosphate-based dechlorination and subsequent vitrification of radioactive salt waste into an iron-phosphate waste form have been identified as a potential processing scheme for electrochemical processing waste. The impact of H 3 PO 4 -based dechlorination of complex salt mixtures on the vitrification process and structure of the final iron-phosphate waste form has not yet been investigated. In this work, iron-phosphate glass–ceramics were made from simulant salt waste (48LiCl–33KCl–19NaCl mol%) dechlorinated with the H3PO4-based method. The glass-forming region was compared to that of traditionally prepared Na 2 O–Fe 2 O 3 –P 2 O 5 systems. For a candidate glass-forming composition, the processing scheme presented here was determined to favor Fe 3+ species. The O/P molar ratio was consistent for the candidate composition when dechlorinated at 400°C and 600°C in air and argon environments, indicating glass network connectivity was maintained despite variations in processing parameters. The results presented here validate processing schemes requiring iron-phosphate waste form synthesis following H 3 PO 4 -based dechlorination.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Immobilization of cesium and iodine into Cs 3 Bi 2 I 9 perovskite-silica composites and core-shell waste forms with high waste loadings and chemical durability

Cs$_3$Bi$_2$I$_9$, a defect perovskite derivative, is a potential host phase to immobilize iodine and cesium with high waste loadings. In this work, two strategies were explored to form Cs$_3$Bi$_2$I$_9$-silica composites and a core-shell structure in order to improve chemical durability of waste form materials meanwhile maintaining high waste loadings. Cs$_3$Bi$_2$I$_9$ loadings as high as 70 wt.% were incorporated into a silica matrix to form silica-ceramic composites, and 20 wt.% Cs$_3$Bi$_2$I$_9$ was encapsulated into silica to form a core–shell structure by low temperature spark plasma sintering. Chemical durability of the composite and core-shell waste forms was evaluated by semi-dynamic leaching experiments, and Cs and I were incongruently released from waste form matrices. A BiOI alteration layer formed, acting as a passivation layer to reduce the release of radionuclides. The long-term iodine release rate was low (30 mg m$^{-2}$ day$^{-1}$) for the 70 wt.%Cs$_3$Bi$_2$I$_9$–silica composite leached in deionized water at 90 °C, which can be further reduced to 5 × 10$^{-3}$ mg m$^{-2}$ day$^{-1}$ for the 20 wt.% core-shell structure. This work highlights a robust way to immobilize the highly mobile radionuclides with high waste loadings through encapsulation into durable matrices and a surface passivating mechanism that can greatly reduce the elemental transport from waste form materials and significantly enhance their chemical durability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Cold crucible induction melter studies for making glass ceramic waste forms: A feasibility assessment

Glass ceramics are being developed to immobilize fission products, separated from used nuclear fuel by aqueous reprocessing, into a stable waste form suitable for disposal in a geological repository. This work documents the glass ceramic formulation at bench scale and for a scaled melter test performed in a pilot-scale (approximately 1/4 scale) cold crucible induction melter (CCIM). Melt viscosity, electrical conductivity, and crystallization behavior upon cooling were measured on a small set of compositions to select a formulation for melter testing. Property measurements also identified a temperature range for melter operation and cooling profiles necessary to crystallize the targeted phases in the waste form. Bench scale and melter run results successfully demonstrate the processability of the glass ceramic using the CCIM melter technology.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗