Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “TERNARY ALLOY SYSTEMS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Short-range order and its impact on the CrCoNi medium-entropy alloy

Traditional metallic alloys are mixtures of elements in which the atoms of minority species tend to be distributed randomly if they are below their solubility limit, or to form secondary phases if they are above it. The concept of multiple-principal-element alloys has recently expanded this view, as these materials are single-phase solid solutions of generally equiatomic mixtures of metallic elements. This group of materials has received much interest owing to their enhanced mechanical properties 1,2,3,4,5 . They are usually called medium-entropy alloys in ternary systems and high-entropy alloys in quaternary or quinary systems, alluding to their high degree of configurational entropy. However, the question has remained as to how random these solid solutions actually are, with the influence of short-range order being suggested in computational simulations but not seen experimentally 6,7 . In this paper we report the observation, using energy-filtered transmission electron microscopy, of structural features attributable to short-range order in the CrCoNi medium-entropy alloy. Increasing amounts of such order give rise to both higher stacking-fault energy and hardness. These findings suggest that the degree of local ordering at the nanometre scale can be tailored through thermomechanical processing, providing a new avenue for tuning the mechanical properties of medium- and high-entropy alloys.

36 MATERIALS SCIENCE↗

Isothermal oxidation behaviors of FeCoV and FeCoVNb alloys

The present study investigates the isothermal oxidation of two iron-cobalt based alloys at 500 deg. C for up to 5000 h. Both alloys exhibit crack-free oxide layers consist of a porosity-free iron rich outer layer and a solute rich inner layer populated with islands of solute oxides and porosities. X-ray diffraction measurements reveal the presence of MO-Fe{sub 2}O{sub 3}-type (where M=Co, Nb, and/or V) spinel structures along with Fe{sub 2}O{sub 3}. Analysis shows that the oxidation follows the parabolic rate law for both alloys with niobium containing alloy exhibiting a higher oxidation rate. Comparison of yield strengths ({sigma}{sub 0}) of oxidized specimens to those aged similarly under an inert atmosphere indicates that two competing mechanisms occur. Surface oxidation decreases the yield strength while precipitation reactions inside the iron-cobalt matrix increase the yield strength of the matrix.

36 MATERIALS SCIENCE↗

Phase stability and tensile behavior of metastable β Ti-V-Fe and Ti-V-Fe-Al alloys

Highlights: • A series of metastable β Ti-V-Fe and Ti-V-Fe-Al alloys were designed by molybdenum equivalency. • Ti-16V-Fe alloy deforms via {332}<113> twinning and stress-induced ω phase transformation. • Ti-12V-2Fe-Al and Ti-14V-2Fe-Al alloys deform via {332}<113> twinning and stress-induced α″ phase transformation. • Al addition suppresses athermal ω phase transformation in β Ti-V-Fe-Al alloys. • Fe and Al additions produce an effective solid-solution hardening for β Ti-(12-14)V-2Fe-Al alloys deformed via twinning. - Abstract: The tensile property and deformation microstructure of a series of metastable β Ti-V-Fe and Ti-V-Fe-Al alloys have been studied. The results show that although Al is an α-stabilizer element, Al addition suppresses the athermal ω phase transformation in metastable β Ti-V-Fe-Al alloys. The Ti-16V-Fe alloy plastically deforms via {332}<113> mechanical twinning and stress-induced ω phase with a special habit plane of {−5052}{sub ω}//{3-3-2}{sub β}, and the Ti-14V-2Fe-Al and Ti-12V-2Fe-Al alloys via {332}<113> twinning. The Ti-16V-2Fe, Ti-16V-2Fe-Al and Ti-16V-2Fe-2Al alloys with relatively high β phase stability plastically deforms mainly via dislocation glide. The Ti-16V-Fe, Ti-14V-2Fe-Al and Ti-12V-2Fe-Al alloys exhibit higher yield strength without loss of plasticity significantly than the binary β Ti-V alloys deformed via {332}<113> twinning due to solid-solution strengthening effect of Fe and Al elements in the alloys.

36 MATERIALS SCIENCE↗

Dry-Sliding Tribological Properties of TiAl Alloys and Ti{sub 2}AlN/TiAl Composites at High Temperature

The dry-sliding tribological properties of TiAl alloy and its composite Ti{sub 2}AlN/TiAl were investigated comparatively in the temperature range of 25-800 °C. The wear test results showed the wear resistance of TiAl alloy and Ti{sub 2}AlN/TiAl composite from 25 to 400 °C was poor, but it improved obviously when temperature was above 600 °C. Also, 15 vol.% incorporation of Ti{sub 2}AlN particles was beneficial to improve the friction and wear properties of TiAl. Protective oxide layer generated on the wear surface of 15 vol.% Ti{sub 2}AlN/TiAl composite from 25 to 400 °C, hence, the wear resistance improved. Ti{sub 2}AlN particles played a load-carrying role and inhabited the delamination of enamel layer effectively when the temperature was above 800 °C. Overall, Ti{sub 2}AlN particles which acted as hard spots changed the state of wear surface and further provided a second phase strengthening effect, which resulted in the difference in tribological behaviors between TiAl alloy and its composite.

36 MATERIALS SCIENCE↗

Surface Condition of New γ–γ′ Co-Al-Mo-Nb and Co-Al-W Cobalt-Based Superalloys After Oxidation at 800 °C

A new type γ–γ′ Co-Al-Mo-Nb Co-based superalloys were developed due to limitations of basic Co-Al-W superalloys, related to tungsten alloying. The present study aims to characterization of new γ–γ′ Co-10Al-5Mo-2Nb (at.%) cobalt-based superalloy performance in terms of the high-temperature exposure under cyclic conditions, with particular regard to surface condition. Specimens were tested in cycles of high-temperature exposition (25, 50, 75, 100 and 150 h) in air environment at 800 °C. Detailed analysis of oxidized surfaces by scanning electron microscopy, energy-dispersive spectroscopy and x-ray diffraction was made at various intervals during testing. The cyclic oxidation behavior of new alloy was compared to the basic Co-9Al-9W (at.%) Co-based superalloy.

36 MATERIALS SCIENCE↗

Wave-Vector Filtering Effect in a Novel Magnetic Nanostructure with Zero Average Magnetic Field

We report a theoretical investigation on wave-vector filtering (WVF) effect in a magnetic nanostructure, which can be experimentally realized by depositing ferromagnetic (FM) stripes on the surface of GaAs/Al{sub x}Ga{sub 1-x}As heterostructure. An appreciable WVF effect appears in this nanosystem. The WVF efficiency is associated with structural parameters of magnetic nanostructure. Therefore, such a device can be employed as a momentum filter for nanoelectronics device applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Approaches for handling high-dimensional cluster expansions of ionic systems

Disordered multicomponent systems attract great interest due to their engineering design flexibility and subsequent rich space of properties. However, detailed characterization of the structure and atomic correlations remains challenging and hinders full navigation of these complex spaces. A lattice cluster expansion is one tool to obtain configurational and energetic resolution. While in theory a cluster expansion can be applied to any system of any dimensionality, the method has primarily been used in binary systems or ternary alloys. Here we apply cluster expansions in high-component ionic systems, setting up the largest cluster expansion ever attempted to our knowledge. In doing so, we address and discuss challenges specific to high-component ionic systems, namely charge state assignments, structural relaxations, and rank-deficient systems. We introduce practical procedures to make the fitting and analysis of complex systems tractable, providing guidance for future computational studies of disordered ionic systems.

25 ENERGY STORAGE↗

Microstructure characterization and thermal stability of TC11/Ti2AlNb joints during thermal exposure

Highlights: • Mechanical properties of TC11/Ti{sub 2}AlNb deteriorate due to coarsening of O and α{sub s}. • Thermal stability of α{sub s} phase is lower than that of O phase during exposure. • A relationship was found between the reduction of area and phase thickness. - Abstract: TC11/Ti{sub 2}AlNb welding joints undergoing hot deformation were thermally exposed at the range of 500–700 °C for 100, 200 and 500 h. In present research, typical microstructures of five different zones of the joints were investigated, fusion zone, two interfaces and two base alloys included. The microstructures of fusion zone, Ti{sub 2}AlNb-based alloy and the interface between them were characterized by the coarsening of O phase during thermal exposure, while those of TC11 alloy and the interface between it and fusion zone featured the coarsening of α{sub s} phase. The transformation from B2 to β and O phase was stifled below 600 °C and Ti{sub 2}AlNb-based alloy thus was verified to be stable at this temperature range. α{sub s} phase was stable during exposure at 500 °C. When exposed above 600 °C, α{sub s} phase coarsened by at least 52% with the extension of holding time. Due to the low thermal stability of α{sub s} phase compared with that of O phase, the fracture position of the samples tested at room temperature moved from fusion zone to TC11 alloy when temperature rose. In spite of different thermal exposure conditions, the samples tested at 300 and 500 °C all fractured at TC11 alloy for the severe coarsening of α{sub s} phase. The decrease of interfacial area resulting from the coarsening of O and α{sub s} phases facilitated the dislocation slipping and the strength of joints thus deteriorated. The mechanical properties of TC11/Ti{sub 2}AlNb joints measured at room temperature, 300 and 500 °C were all correlated with the lamellar thickness of O and α{sub s} phases.

36 MATERIALS SCIENCE↗

EBSD characterization of the eutectic microstructure in hypoeutectic Fe-C and Fe-C-Si alloys

Highlights: • EBSD investigation of eutectic cementite and austenite in as-solidified low-alloy cast iron • Crystallographically independent growth of rapidly solidified cementite/austenite eutectic • Epitaxial growth of eutectic austenite from primary dendrites • Eutectic cementite and eutectoid ferrite frequently obey Bagaryatsky or Pitsch-Petch orientation relationship. - Abstract: Hypoeutectic Fe-C and Fe-C-Si model alloys were produced at different solidification conditions. Copper mold casting yields low cooling rates promoting the formation of a eutectic microstructure, which is characterized by two morphologies: elongated cementite plates and a rod structure growing perpendicular to the plates, i.e. austenite rods in a cementite matrix. Electron beam surface remelting generates a mainly plate-like eutectic due to rapid solidification. The microstructures were characterized by light-optical microscopy and electron backscatter diffraction (EBSD). The latter allows for a spatially resolved investigation of the growth crystallography of the eutectic phases. Thereby, a possible existence of crystallographic orientations relationships between cementite and austenite within the plate-like eutectic was assessed experimentally. The eutectic phases were found to grow largely crystallographically independently. Moreover, ferrite and eutectic cementite within the decomposed eutectic microstructure frequently comply with the Bagaryatsky or the Pitsch-Petch orientation relationship. Complementary X-ray diffraction (XRD) analysis reveals a pronounced cementite {002} texture in the microstructure produced by mold casting. Characteristic changes in the lattice parameters indicate that as-cast cementite is non-stoichiometric.

36 MATERIALS SCIENCE↗

Calculation of binodals and spinodals in multicomponent alloys by different statistical methods with application to iron-copper-manganese alloys

A generalization of the pair-cluster (PC) approximation in the theory of disordered systems to multicomponent alloys is proposed. It is shown that phase equilibrium boundaries (binodals) calculated in the mean-field (MF) approximation, which is used in standard calculations of phase diagrams by the CALPHAD method, coincide with the results of rigorous calculations for dilute alloys; however, the application of these methods to calculating the boundaries of the stability region with respect to the decomposition of an alloy (spinodals) leads to large errors. At the same time, in the PC approximation, the description of all statistical properties, including binodals and spinodals, turns out to be exact for dilute alloys. The methods developed are illustrated by an example of iron-copper-manganese ternary alloys.

36 MATERIALS SCIENCE↗

An ab initio study of the electronic structure and optical properties of CdS{sub 1-x}Te{sub x} alloys

The structural, electronic and optical properties of cubic CdS{sub 1-x}Te{sub x} alloys, with Te-concentrations varying from 0% up to 100% are investigated. The calculations are based on the total-energy calculations using the full potential-linearized augmented plane wave (FP-LAPW) method. The exchange and correlation potential is treated by the generalized-gradient approximation (GGA) for the total-energy calculations, while for electronic properties in addition to that the Engel-Vosko (EV-GGA) formalism was also applied. The ground state properties for all Te-concentrations are presented. The optical dielectric constant is also determined for both the binary and their related ternary alloys. (author)

36 MATERIALS SCIENCE↗

Interface characteristics of Ti6Al4V-TiAl metal-intermetallic laminate (MIL) composites prepared by a novel hot-pack rolling

Highlights: • The Ti6Al4V/high Nb-TiAl metal-intermetallic (MIL) composite was fabricated. • The formation of γ and α{sub 2} phase at interface is diffusion controlled. • The formation of O phase at interface is due to the segregation of Nb atoms. • The Vickers hardness from Ti6Al4V to TiAl alloy shows a trend of a decrease then an increase and finally a decrease. - Abstract: Ti6Al4V (wt%)/Ti-44Al-8Nb-0.2W-0.2B-0.03Y (at.%) (high Nb-TiAl) metal–intermetallic laminate (MIL) composite with a defect-free interface was successfully prepared by hot-pack rolling and the interface microstructure was characterized by XRD, SEM, EBSD, and TEM techniques. The results showed that the interface was about 260 μm thick and consisted of four different microstructure regions. The thickness of each region was about 60–80 μm and the microstructure of the four regions consisted of acicular O, α{sub 2}, and β/B2 phases; acicular α{sub 2} phase; acicular α{sub 2} and β/B2 phases; and acicular γ, α{sub 2}, and β/B2 phases respectively. The resulting microstructure of the interface region was attributed to the interdiffusion of Ti atoms from the starting Ti6Al4V alloy layer to the high Nb-TiAl alloy layer and Al and Nb atoms from the high Nb-TiAl alloy layer to the Ti6Al4V alloy layer. The formation of acicular α{sub 2} and γ phases was diffusion-controlled and the Nb segregation at the interface caused the formation of O phase which had specific relationships with α{sub 2} and β/B2 phases. The detailed interface microstructural evolution of the Ti6Al4V/high Nb-TiAl MIL composite and the Vickers hardness of the composite are also discussed in this paper.

36 MATERIALS SCIENCE↗

A tunable amorphous p-type ternary oxide system: The highly mismatched alloy of copper tin oxide

The approach of combining two mismatched materials to form an amorphous alloy was used to synthesise ternary oxides of CuO and SnO{sub 2}. These materials were analysed across a range of compositions, and the electronic structure was modelled using density functional theory. In contrast to the gradual reduction in optical band gap, the films show a sharp reduction in both transparency and electrical resistivity with copper contents greater than 50%. Simulations indicate that this change is caused by a transition from a dominant Sn 5s to Cu 3d contribution to the upper valence band. A corresponding decrease in energetic disorder results in increased charge percolation pathways: a “compositional mobility edge.” Contributions from Cu(II) sub band-gap states are responsible for the reduction in optical transparency.

36 MATERIALS SCIENCE↗

Investigation on Tribological Properties of the Pre-oxidized Ti{sub 2}AlN/TiAl Composite

Different oxidation layers on the Ti{sub 2}AlN/TiAl substrate which was fabricated by in situ synthesis were prepared through thermal oxidation process. The microstructure, phase identification and elements distribution of the oxidation layers were analyzed. The tribological performance of pre-oxidized composites against Si{sub 3}N{sub 4} ball at 25 and 600 °C, as well as the effect of pre-oxidation layers on tribological performance was systematically investigated. The results show that, compared to Ti{sub 2}AlN/TiAl, the pre-oxidized composites present more excellent tribological properties, especially the wear resistance at 600 °C. It is a significant finding that, different from severe abrasive wear and plastic deformation of Ti{sub 2}AlN/TiAl, the tribo-films formed by the pre-oxidation layers on the worn surface of pre-oxidized composites weaken abrasive wear and suppress the development of plastic deformation to protect the underlying composite substrate from wear. Moreover, the stable cooperation on the interface between tribo-films and Si{sub 3}N{sub 4} ball results in the relatively steady friction coefficient.

36 MATERIALS SCIENCE↗

Effect of Aluminum Addition on the Evolution of Microstructure, Crystallographic Texture and Mechanical Properties of Single Phase Hexagonal Close Packed Mg-Li Alloys

In the present investigation, an effort has been made to understand the effect of aluminum addition to α Mg-Li alloys. The corresponding composition Mg-4Li-xAl (x = 0, 2, 4 and 6 wt.%) alloys have been prepared by stir casting route under an argon environment. Extrusion was carried out at 300 °C with the extrusion ratio of 15:1. Significant grain refinement was observed after extrusion. X-ray diffraction-based investigation of the cast and extruded alloys showed the presence of intermetallic compounds such as Mg{sub 17}Al{sub 12} and AlLi in the Al-rich alloys namely, Mg-4Li-xAl (x = 4 and 6 wt.%). These precipitates were also present in the extruded plus annealed samples, indicating the stability of the precipitates at high temperature. The bulk x-ray texture measurement revealed a crystallographic texture where the c-axis of the h.c.p crystals was perpendicular to the extrusion direction (ED) for extruded sample. A texture transition was observed on annealing. The c-axis was oriented parallel to the ED. Mechanical properties of the cast, extruded and extruded plus annealed material illustrate that the addition of Al led to enhancement in hardness, yield strength and ultimate tensile strength.

36 MATERIALS SCIENCE↗

Fabrication and Mechanical Properties of In Situ Synthesized Ti{sub 2}AlN/TiAl Composite

TiAl matrix composites reinforced with Ti{sub 2}AlN were fabricated by in situ reactive method of powder metallurgy. Microstructures, bending properties at room temperature and compressive properties at elevated temperatures were investigated in contrast with those of TiAl alloy. The results reveal that the microstructure of TiAl matrix is significantly refined due to the synthesis of Ti{sub 2}AlN. 15 vol.%Ti{sub 2}AlN/TiAl exhibits excellent bending properties at room temperature, with bending strength of 753 MPa and fracture strain of 0.74%, which are 24.3 and 19.7% higher than those of TiAl alloy. The compressive strength of Ti{sub 2}AlN/TiAl is markedly improved in comparison to that of TiAl alloy at elevated temperatures. Noticeably, the compressive strength of 15 and 35 vol.%Ti{sub 2}AlN/TiAl increases by 67.4 and 58.7% at 1000 °C, respectively. The remarkable enhancement of mechanical performance is mainly due to the noteworthy refinement of TiAl matrix and the efficient obstruction of Ti{sub 2}AlN particles to crack propagation, as well as the effective load-carrying role of Ti{sub 2}AlN with high elastic modulus.

36 MATERIALS SCIENCE↗

Estimation of the band gap of a series of new thermoelectric materials

The band gap E{sub g} of a number of new thermoelectric materials, such as skutterudites, clathrates, Heusler phases, (Ge,Sn,Pb)(Te,Se)]{sub m}[(Bi,Sb){sub 2}(Te,Se){sub 3}]{sub n} (m, n = 0, 1, 2…) ternary alloys, and others is estimated. Estimations are performed using Goldsmid-Sharp’s formula E{sub g} = 2e|α{sub max}|T{sub max}, Vegard’s rule E{sub g} = (mE{sub g}{sup A} + nE{sub g}{sup B})/(m + n), and the empirical dependence T{sub max} = f(E{sub g}) (A and B denote the corresponding binary alloys, T{sub max} is the temperature corresponding to the thermoelectric-power maximum |α{sub max}| or the thermoelectric figure of merit (ZT){sub max}, and e is the elementary charge). It is shown that the empirical dependence E{sub g} = f(T{sub max}) gives the most accurate estimates of E{sub g} for difference classes of thermoelectric materials.

36 MATERIALS SCIENCE↗