Thermal fatigue and oxidation data of superalloys including directionally solidified eutectics
Thermal fatigue and oxidation data were obtained on 61 specimens, representing 15 discrete alloy compositions or fabricating techniques and three coating systems. Conventionally fabricated alloys included V57, MM 200, Rene 77, Rene 125, MM 246, MM 509, IN-738, IN-792 + Hf, and MM 200 + Hf. The directionally solidified alloys were MM 200, MM 200 single crystal, MM 200 bicrystal, cellular gamma/gamma' - delta) and lamellar gamma/gamma' - delta. The coatings systems included NiCrAlY on IN-738, In-792 + Hf, MM 200 DS, MM 200 DS single crystal, and cellular gamma/gamma' - delta and NiCrAlY/Pt on lamellar gamma/gamma' - delta. Crack initiation survival rates were recorded for all alloys, with and without coatings. All uncoated alloys, except MM 509, exhibited significant oxidation weight loss in 75,000 to 15,000 cycles. MM 509 specimens had weight losses only slightly higher than coated specimens through 7,500 cycles. All coated specimens had low weight loss.