23 records · Page 2

Effect of Chemical Composition on the Microstructure and Tribological Properties of Sn-Based Alloys

This article presents the test results of two bearing alloys on a tin matrix, differing in the content of alloy additions. Microscopic tests were performed using scanning electron microscopy, along with Brinell hardness tests and tests of tribological properties in the conditions of technical dry friction and wet friction using a TU-32 oil. Additionally, wear mechanisms were analyzed depending on the process conditions. The results indicate better tribological properties of the B82 alloy, with a higher content of antimony compared to the B89 alloy. This alloy contains more precipitates of hard phase β—SnSb, which both influence the level of the mechanical properties and determine the tribological properties. Additionally, it was proven that using the TU-32 oil as a lubricant practically eliminates adhesive wear, and the post-friction surfaces for both alloys are of a similar nature.

36 MATERIALS SCIENCE↗

A Study on the Microstructures and Properties of Selective Laser Melted Babbitt Metals

Babbitt metal cubes were prepared by means of selected laser melting (SLM) process using Sn—11% Sb—6% Cu alloy powders; their microstructures were studied using optical microscope (OM), SEM, EDS, XRD and DSC; and their mechanical properties were tested using Vickers hardness and tensile methods. The results show that fully dense Babbitt metal components can be prepared by using appropriate SLM process parameters and an interlayer staggered laser scanning strategy. Anisotropy characteristics appear in both the microstructure and mechanical properties of SLM-Babbitt cubic specimens. The average hardness was in the range of 32.5 HV0.05 to 35.3 HV0.05. Both tensile strength and elongation were somewhat higher in a direction parallel to the laser scanning speed (Y axis) than in a direction perpendicular to the laser scanning speed (X axis). The strengthening mechanism is suggested to include solid solution strengthening of oversaturated Sb in the Sn matrix, as well as dispersion strengthening of finely dispersed SnSb and Cu{sub 6}Sn{sub 5} particles. The overgrown acicular Cu{sub 6}Sn{sub 5} phases at low laser scanning speeds and void formation at higher laser scanning speeds seriously deteriorate the mechanical properties of the SLM-Babbitt specimens.

36 MATERIALS SCIENCE↗

Microstructural Coarsening Kinetics and Mechanical Property Changes in Long-Term Aged Sn–Pb–Sb Solder Joints

Tin-lead-antimony (50Sn–47Pb–3Sb wt.%) soldered assemblies were mechanically tested approximately 30 years after initial production and found to have solder joints of reduced strength. The microstructure of this solder alloy exhibits a ternary eutectic structure with Sn-rich, Pb-rich, and SnSb phases. Accelerated aging was performed to evaluate solder microstructural coarsening and associated strength of laboratory solder joints to correlate these properties to the “naturally aged” solder joints. Isothermal aging was conducted at room temperature, 55, 70, 100, and 135 °C and aging times that ranged from 0.1 to 365 days. The coarsening kinetics of the Pb-rich phase were determined through optical microscopy and image analysis methods established in previous studies on binary Sn–Pb solder. A kinetic equation was developed with time exponent n of 0.43 and activation energy of 24000 J/mol, suggesting grain boundary diffusion or other fast diffusion pathways controlling the microstructural evolution. Compression testing and Vickers microhardness showed significant strength loss within the first 20–30 days after soldering; then, the microstructure and mechanical properties changed more slowly over long periods of time. Further, by combining accelerated aging data and the microstructure-based kinetics, strength predictions were made that match well with the properties of the actual soldered assemblies naturally aged for 30 years. However, aging at the highest temperature of 135 °C produced anomalous behavior suggesting that extraneous aging mechanisms are active. Therefore, data obtained at this temperature or higher should not be used. Overall, the combined microstructural and mechanical property methods used in this study confirmed that the observed reduction in strength of ~ 30-year-old solder joints can be accounted for by the microstructural coarsening that takes place during long-term solid-state aging.

36 MATERIALS SCIENCE↗

High-pressure Raman spectroscopy of phase change materials

We used high-pressure Raman spectroscopy to study the evolution of vibrational frequencies of the phase change materials (PCMs) Ge{sub 2}Sb{sub 2}Te{sub 5}, GeSb{sub 2}Te{sub 4}, and SnSb{sub 2}Te{sub 4}. We found that the critical pressure for triggering amorphization in the PCMs decreases with increasing vacancy concentration, demonstrating that the presence of vacancies, rather than differences in the atomic covalent radii, is crucial for pressure-induced amorphization in PCMs. Compared to the as-deposited amorphous phase, the pressure-induced amorphous phase has a similar vibrational spectrum but requires much lower laser power to transform into the crystalline phase, suggesting different kinetics of crystallization, which may have implications for applications of PCMs in non-volatile data storage.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

On the tin impurity in the thermoelectric compound ZnSb: Charge-carrier generation and compensation

The technique for measuring the Hall coefficient and electrical conductivity in the thermal cycling mode is used to study the effect of the Sn impurity on the microstructure and properties of pressed ZnSb samples. Tin was introduced as an excess component (0.1 and 0.2 at %) and as a substitutional impurity for Zn and Sb atoms in a concentration of (2–2.5) at % The temperature dependences of the parameters of lightly doped samples are fundamentally like similar curves for ZnSb with 0.1 at % of Cu. The highest Hall concentration, 1.4 × 10{sup 19} cm{sup –3} at 300 K, is obtained upon the introduction of 0.1 at % of Sn; the dimensionless thermoelectric figure of merit attains its maximum value of 0.85 at 660 K. The experimental data are discussed under the assumption of two doping mechanisms, which are effective in different temperature ranges, with zinc vacancies playing the decisive role of acceptor centers. In two ZnSb samples with SnSb and ZnSn additives, the charge-carrier compensation effect is observed; this effect depends on temperature and markedly changes with doping type. As in p-type A{sup IV}–B{sup VI} materials with a low Sn content, hole compensation can be attributed to atomic recharging Sn{sup 2+} → Sn{sup 4+}. Types of compensating complexes are considered.

36 MATERIALS SCIENCE↗