Engineering PapersSearch

SEARCH · Engineering Papers

Results for “Slurries”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Theoretical considerations for Reaction-Formed Silicon Carbide (RFSC) formation by molten silicon infiltration into slurry-derived preforms

For reaction-formed silicon carbide (RFSC) ceramics produced by silicon melt infiltration of porous carbon preforms, equations are developed to relate the amount of residual silicon to the initial carbon density. Also, for a slurry derived preform containing both carbon and silicon powder, equations are derived which relate the amount of residual silicon in the RFSC to the relative density of the carbon in the preform and to the amount of silicon powder added to the slurry. For a porous carbon preform that does not have enough porosity to prevent choking-off of the silicon infiltration, these results show that complete silicon infiltration can occur by adding silicon powder to the slurry mixture used to produce these preforms.

Behrendt, D. R.

Investigations of Particle Velocities in a Slurry Pump Using PIV: The Tongue and Adjacent Channel Flow - Part 1

Transport of solid-liquid slurries in pipeline transport over short and medium distances is very important in many industries, including mining related processes. The particle image velocimetry technique was successfully utilized to investigate the velocities and kinetic energy fluctuations of slurry particles at the tongue region of an optically-clear centrifugal pump. The experiments were conducted using 500 micron glass beads at volumetric Concentrations of 2.5% and 5% and at pump speeds of 725 rpm and 1000 rpm. The fluctuation kinetic energy increased approximately 200% to 500% as the pump speed was increased from 725 rpm to IO00 rpm. The directional impingement mechanism is more significant at the pressure side of the blade, tongue and the casing. This mechanism becomes more important as the speed increases. This suggests that the impeller; tongue and the casing of the slurry pump can wear out quickly, especially with an increase in speed. In this paper the emphasis is on the tongue region. The random impingement mechanism caused by the fluctuation kinetic energy of the solids can play an important role on the erosion of the tongue area.

Kadambi, Jaikrishnan R.

High-Temperature Slurry Environmental Barrier Coating With Graded HfO 2 -HfSiO 4 Topcoat

Environmental barrier coatings (EBCs) have enabled the use of silicon carbide (SiC)-based ceramic matrix composites (CMCs) in gas turbine engines by protecting the underlying CMC from corrosive combustion species. Current-generation EBCs consist of a rare earth silicate topcoat and a silicon bond coat. The relatively low melting point of the silicon bond coat (1414°C) limits the upper use temperature of these coatings. To protect SiC-based CMCs at temperatures beyond that achievable by the current state-of-the-art, an oxide-based bond coat capable of withstanding temperatures of up to 1482°C has been developed at NASA Glenn Research Center. Hafnia (HfO2) is a promising EBC topcoat material due to its stability in high-temperature steam; however, its coefficient of thermal expansion (CTE) is highly anisotropic and much larger than that of SiC. In this study, a graded HfO2-HfSiO4 topcoat was deposited via a slurry process on the NASA-developed oxide-based bond coat. The oxidation resistance of this EBC system was evaluated at 1482°C in a steam cycling environment. The durability and stability of this slurry-deposited HfO2-HfSiO4 topcoat was compared to that of HfO2 deposited by plasma spray physical vapor deposition (PS-PVD).

EBC

Development of a fused slurry silicide coating for the protection of tantalum alloys

Results are reported of a research program to develop a reliable high-performance, fused slurry silicide protective coating for a tantalum-10 tungsten alloy for use at 1427 to 1538 C at 0.1 to 10 torr air pressure under cyclic temperature conditions. A review of silicide coating performance under these conditions indicated that the primary wear-out mode is associated with widening of hairline fissures in the coating. Consideration has been given to modifying the oxidation products that form on the coating surface to provide a seal for these fissures and to minimize their widening. On the basis of an analysis of the phase relationships between silica and various other oxides, a coating having the slurry composition 2.5Mn-33Ti-64.5Si was developed that is effective in the pressure range from 1 to 10 torr.

Packer, C. M.

Prospects for coal slurry pipelines in California

The coal slurry pipeline segment of the transport industry is emerging in the United States. If accepted it will play a vital role in meeting America's urgent energy requirements without public subsidy, tax relief, or federal grants. It is proven technology, ideally suited for transport of an abundant energy resource over thousands of miles to energy short industrial centers and at more than competitive costs. Briefly discussed are the following: (1) history of pipelines; (2) California market potential; (3) slurry technology; (4) environmental benefits; (5) market competition; and (6) a proposed pipeline.

Lynch, J. F.

Critical parameters for coarse coal underground slurry haulage systems

Factors are identified which must be considered in meeting the requirements of a transportation system for conveying, in a pipeline, the coal mined by a continuous mining machine to a storage location neat the mine entrance or to a coal preparation plant located near the surface. For successful operation, the slurry haulage the system should be designed to operated in the turbulent flow regime at a flow rate at least 30% greater than the deposition velocity (slurry flow rate at which the solid particles tend to settle in the pipe). The capacity of the haulage system should be compatible with the projected coal output. Partical size, solid concentration, density, and viscosity of the suspension are if importance as well as the selection of the pumps, pipes, and valves. The parameters with the greatest effect on system performance ar flow velocity, pressure coal particle size, and solids concentration.

Maynard, D. P.

Corrosion inhibitors for water-base slurry in multiblade sawing

The use of a water-base slurry instead of the standard PC oil vehicle was proposed for multiblade sawing (MBS) silicon wafering technology. Potential cost savings were considerable; however, significant failures of high-carbon steel blades were observed in limited tests using a water-based slurry during silicon wafering. Failures were attributed to stress corrosion. A specially designed fatigue test of 1095 steel blades in distilled water with various corrosion inhibitor solutions was used to determine the feasibility of using corrosion inhibitors in water-base MBS wafering. Fatigue tests indicate that several corrosion inhibitors have significant potential for use in a water-base MBS operation. Blade samples tested in these specific corrosion-inhibitor solutions exhibited considerably greater lifetime than those blades tested in PC oil.

Chen, C. P.

Resin Powder Slurry Process for Composite Fabrication

Potentially useful process for fabrication of fiber-reinforced resinmatrix composites is powder slurry technique. Applicability of technique demonstrated using powdered resin made from thermoplastic polyimide LaRC/ TPI (thermoplastic polyimide). Use of process circumvents need for such high-cost organic solvents as N-methylpyrrolidinone and diglyme (diglycol methyl ether). Two basic slurries for LaRC/TPI powder investigated.

Mike, R. A.

Thermal certification tests of Orbiter Thermal Protection System tiles coated with KSC coating slurries

Thermal tests of Orbiter thermal protection system (TPS) tiles, which were coated with borosilicate glass slurries fabricated at Kennedy Space Center (KSC), were performed in the Radiant Heat Test Facility and the Atmospheric Reentry Materials & Structures Evaluation Facility at Johnson Space Center to verify tile coating integrity after exposure to multiple entry simulation cycles in both radiant and convective heating environments. Eight high temperature reusable surface insulation (HRSI) tiles and six low temperature reusable surface insulation (LRSI) tiles were subjected to 25 cycles of radiant heat at peaked surface temperatures of 2300 F and 1200 F, respectively. For the LRSI tiles, an additional cycle at peaked surface temperature of 2100 F was performed. There was no coating crack on any of the HRSI specimens. However, there were eight small coating cracks (less than 2 inches long) on two of the six LRSI tiles on the 26th cycle. There was practically no change on the surface reflectivity, physical dimensions, or weight of any of the test specimens. There was no observable thermal-chemical degradation of the coating either. For the convective heat test, eight HRSI tiles were tested for five cycles at a surface temperature of 2300 F. There was no thermal-induced coating crack on any of the test specimens, almost no change on the surface reflectivity, and no observable thermal-chemical degradation with an exception of minor slumping of the coating under painted TPS identification numbers. The tests demonstrated that KSC's TPS slurries and coating processes meet the Orbiter's thermal specification requirements.

Milhoan, James D.

Microencapsulated PCM slurries for heat transfer and energy storage in spacecraft systems

The technical feasibility for providing significantly enhanced heat transport and storage as well as improved thermal control has been investigated during several Small Business Innovative Research (SBIR) programs for NASA, the United States Air Force (USAF), and the Strategic Defense Initiative Organization (SDIO) using microencapsulated phase change materials (PCMs) in both aqueous and nonaqueous two-component slurries. In the program for SDIO, novel two-component coolant fluids were prepared and successfully tested at both low (300 K) and intermediate temperatures (460 to 700 K). The two-component fluid slurries of microencapsulated PCMs included organic particles in aqueous and nonaqueous liquids, as well as microencapsulated metals that potentially could be carried by liquid metals or used as powdered heat sinks. Simulation and experimental studies showed that such active cooling systems could be designed and operated with enhancements of heat capacity that exceeded 10 times or 1000 percent that for the base fluid along with significant enhancement in the fluid's heat capacity. Furthermore, this enhancement provided essentially isothermal conditions throughout the pumped primary coolant fluid loop. The results suggest that together with much higher fluid thermal capacity, greater uniformity of temperature is achievable with such fluids, and that significant reductions in pumping power, system size, and system mass are also possible.

Colvin, David P.

Performance Comparison Between NiH2 Dry Sinter and Slurry Electrode Cells

The electrical and thermal performance of dry sinter and slurry process electrode cells manufactured for the Hubble Space Telescope (HST) batteries have been characterized for a matrix of operating conditions over the temperature range from 14 to 86 F at various charge control levels. The dry sinter process electrode cells tested are similar to the onboard HST NiH2 cells. The slurry process electrode cells were developed to be less susceptible to electrode expansion and impedance changes with life. Both cell types were impregnated by the aqueous electrochemical process. Test conditions included standard capacity tests and electrical cycling using 96-minute cycling regimens incorporating gr depth-of-discharge (DOD) cycles. The dry sinter process electrodes have higher operating capacities to 1.20V/cell, but both electrode types have similar heat dissipation for the conditions tested. The results of the testing included cyclic heat generation during a typical 96-minute cycle, operating capacity data vs. cutoff voltage to generate a temperature-compensated voltage curve, and voltage characteristics suitable to develop a voltage prediction model. Analysis of data shows differences in the discharge voltage plateaus operating conditions evaluated. This is the basis for recommended changes in the battery charge control.

Armantrout, J. D.

One-step Tape Casting of Composites via Slurry on Fiber

A process by which metal matrix composites can be made was presented. The process involves putting a powder slurry on fibers to make a precursor green tape. These green tapes are cut, stacked and hot pressed to form the fully dense composite. A computer program was presented which enables complete quantification and control of the process. Once some easily obtained properties of the slurry and its behavior are determined (such as the shrinkage from the wet to green state, and the density of the green tape) modification of the fiber spacing and blade height give the maker precise control of fiber volume fraction, and fiber architecture in the composite. The process was shown to be accurate and flexible through the production of a wide variety of volume fraction fiber composites made from a wide variety of fibers and powders. The most time consuming step of the tape casting process (other than hot pressing) was winding the fiber on the drum. The tape casting techniques developed resulted in high quality metal matrix composites, with ultimate tensile strength in the range of 215 ksi (1477 MPa), a strain at failure of 1.15 percent, and in fatigue at room temperature 0 to 120 ksi, n = 0.3 Hz, a 4-ply Ti-24Al-11Nb/SCS-6, 32 vol% fiber tape cast composite lasted 202,205 cycles with a maximum strain on the 100th cycle of 0.43 percent.

deGroh, Henry C., III

Varying Processing Parameters in the Development of Slurry-Based Oxide Bond Coat for Environmental Barrier Coatings

Silicon carbide (SiC)-based ceramic matrix composites (CMCs) are replacing nickel-base superalloys in some hot-section aircraft engine materials due to their lower density and higher working temperature. CMCs require an environmental barrier coating (EBC) for protection from corrosive combustion species. Current-generation EBCs consist of a rare earth silicate topcoat and a silicon bond coat; however, the relatively low melting point of silicon (1414°C) limits the upper use temperature of these coatings. To extend the capability of next-generation EBCs, an oxide-based bond coat capable of withstanding temperatures of up to 1480°C has been developed at NASA Glenn Research Center. In this study, the oxide-based bond coat was applied to monolithic SiC via a slurry coating process. Parameters including slurry particle size and viscosity were varied, and coating performance was evaluated after steam cycling at 1480°C. The effect of including different rare earth constituents in the bond coat was also explored.

R. I. Webster