Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SWELLING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Clay Swelling in Dry Supercritical Carbon Dioxide: Effects of Interlayer Cations on the Structure, Dynamics, and Energetics of CO 2 Intercalation Probed by XRD, NMR, and GCMD Simulations

In situ X-ray diffraction (XRD) and nuclear magnetic resonance (NMR) experiments combined with molecular dynamics simulations using the grand canonical ensemble [grand canonical molecular dynamics (GCMD)] show that the cation size, charge, and solvation energy play critical roles in determining the interlayer expansion of smectite clay minerals when exposed to dry supercritical scCO2 (scCO2) under conditions relevant to petroleum reservoirs and geological CO2 sequestration conditions. The GCMD results show that the smectite mineral, hectorite, containing interlayer alkali and alkaline earth cations with small ionic radii and high solvation energies (e.g., Na+ and Ca2+) does not intercalate CO2 and that the fully collapsed interlayer structure is the most energetically stable configuration. With Cs+ and Ba2+, the monolayer structure is the stable configuration, and CO2 should spontaneously enter the interlayer. With Cs+, there is not even an energy barrier for CO2 intercalation, in agreement with the XRD and NMR results. 13C NMR and simulations show that the average orientation of the intercalated CO2 is with their O-C-O axes parallel to the basal clay surface and that they undergo a rapid rotation about an axis perpendicular to the main molecular axis. The simulations show that the strength of the interaction between the exchangeable cation and the clay structure dominates the intercalation energetics in dry scCO2.

Loganathan, Narasimhan (ORCID:0000000302515430)↗

An energy-optimization method to study gel-swelling in confinement

Using our open-source programming environment Morpho, an energy-optimization method is developed to compute equilibrium shapes of an arbitrarily confined swollen hydrogel. The internal strains and contact forces are measured, probing its mechanics.

Joshi, Chaitanya↗

On the formation of swelling and related flaws in laser powder bed fusion

Process monitoring in laser powder bed fusion additive manufacturing can provide insights into stochastic anomalies, melt pool and plume dynamics, and part quality. Swelling, a build anomaly where overbuilt material protrudes through the powder layer after recoating, is readily detectable in post-recoat visible light images of the powder bed. Here, this work identifies several of the underlying mechanisms driving swelling formation by analyzing the influence of processing parameters, laser scan paths, and build plate locations on the presence of swelling detected in situ. Swelling near the edge of the part and swelling in the internal region of the part are shown to correlate with different process conditions. Edge and internal swelling may be driven by different phenomena, with edge swelling predominately occurring on the edge of a part facing the laser module and correlated to clusters of near-surface voids (detected with X-ray computed tomography). A larger spot size, higher laser power, and lower scan velocity also increased the presence of edge swelling. Laser spot size and scan path influenced internal swelling, which occurred preferentially with a larger spot size and in regions with large melt pools, caused by localized heat accumulation due to non-optimal processing parameters or scan path strategies. For coupons processed with a slicer-defined maximum scan vector length, swelling seldom occurred at internal vector-stripe boundaries. These results provide a mechanistic understanding of how swelling can be linked to material flaws, insight into how some instances of swelling can be avoided, and evidence supporting the use of swelling as an in situ indicator for quality assurance and part qualification.

Anomaly↗

Role of Defects in Swelling and Creep of Irradiated SiC

Silicon carbide is a promising cladding material because of its high strength and relatively good corrosion resistance. However, SiC is brittle and therefore SiC-based components need to be carefully designed to avoid cracking and failure by fracture. In design of SiC-based composites for nuclear reactor applications it is essential to take into account how mechanical properties are affected by radiation and temperature, or in other words, what strains and stresses develop in this material due to environmental conditions. While thermal strains in SiC can be predicted using classical theories, radiation-induced strains are much less understood. In particular, it is critical to correctly account for radiation swelling and radiation creep, which contribute significantly to dimensional instability of SiC under radiation. Swelling typically increases logarithmically with radiation dose and saturates at relatively low doses (damage levels of a few dpa). Consequently, swelling-induced stresses are likely to develop within a few months of operation of a reactor. Radiation-induced volume swelling in SiC can be as high as 2%, which is significantly higher than the cracking strain of 0.1% in SiC. Swelling-induced strains will lead to enormous stresses and fracture, unless these stresses can be relaxed via some other mechanism. An effective way to achieve stress relaxation is via radiation creep. Although it has been hypothesized that both radiation swelling and radiation creep are driven by formation of defect clusters, existing models for swelling and creep in SiC are limited by the lack of understanding of specific defects that form due to radiation in the range of temperatures relevant to fuel cladding in light water reactors (LWRs) (<1000°C). For example, defects that can be detected with traditional transmission electron microscopy (TEM) techniques account only for 10-45% of the swelling measured in irradiated SiC. Here, we have undertaken an integrated experimental and modeling effort to discover the previously invisible defects in irradiated SiC and to determine the contributions of these defects to radiation swelling. Knowledge of the most stable defect structures and the rate controlling processes during defect evolution is essential for development of predictive models for swelling and creep as a function of temperature and radiation dose. This research has been enabled by state-of-the-art imaging techniques, such as the aberration corrected scanning transmission electron microscopy (STEM) (FEI TITAN) closely coupled with multi-scale models of stable defect clusters and their evolution.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Cavity Swelling in Irradiated Materials

Cavity swelling, due to three-dimensional clustering of vacancies, is an undesirable isotropic volume expansion of materials under irradiation. This phenomenon occurs above stage-III recovery temperature where vacancies are mobile, between ~0.3–0.6 Tm where Tm is the absolute melting temperature. The primary mechanism for cavity swelling is “dislocation bias”, i.e., preferential absorption of interstitials by network dislocations, causing a vacancy supersaturation. Cavity swelling is highly temperature dependent and typically follows a bell-shaped curve with peak swelling occurring at an intermediate temperature. With increasing temperature, cavity size increases, and number density decreases logarithmically. With increasing dose, cavity swelling increases, but follows a hockey-stick type pattern, characterized by a low-swelling transient incubation period and then a steady-state regime. The incubation period, dominant in cavity nucleation, is dependent upon material’s chemistry and irradiation conditions such as dose rate/temperature. Cavity swelling increases linearly with dose in the steady-state regime, that is independent of chemistry and dose rate. This regime is dominated by cavity growth. Transmutation gases like He enhance cavity nucleation such that an early onset of cavity formation occurs. However, swelling magnitudes can be either increased or suppressed when He is present. Results in austenitic steels and Cu indicate that cavity swelling peaks at intermediate He/dpa ratios of ~10 appm He/dpa. The most effective method to mitigate cavity swelling is by increasing the fixed point-defect sink density, by promoting precipitation or dispersion strengthening.

Bhattacharya, Arunodaya↗

Growth-induced Donnan exclusion influences swelling kinetics in highly charged dynamic polymerization hydrogels

Polymeric gels crosslinked by DNA sequences can exploit DNA strand-displacement reactions to promote swelling through dynamic polymerization. The degree of swelling and the rate of swelling must be directly tunable to achieve the promise of programmable soft matter. Though the kinetics of the strand-displacement reaction provide insertion rates up to 10 4 /Molar/second as measured in bulk solution, DNA hydrogel swelling can take upwards of 30 h to complete. Computational modeling of the reaction-induced swelling of these gels with our recently-developed reactive electrochemomechanical theory (Zimmerman et al., 2024) suggests that their extraordinarily slow swelling is partly due to a scaling mismatch between the addition of charge and the addition of fluid volume, leading to a large transient increase in the fixed charge density. The significant increase in the gel’s fixed charge density, due to the binding of negatively charged DNA, sharply restricts the concentration of mobile hairpins through the phenomenon of Donnan charge exclusion, an effect commonly exploited in nanofiltration applications using polymeric membranes. The scaling problem is overcome when the mean additional swelling provided to the hydrogel by addition of a crosslink is above a critical value, thus the swelling outpaces the charge accumulation, leading the fixed charge density to drop and significantly accelerating the swelling process. This study shows that Donnan exclusion can explain the kinetics of DNA hydrogel swelling, and studies ways to modulate the reaction speed by either modifying the salt concentration or increasing or decreasing the number of base pairs in each DNA sequence.

42 ENGINEERING↗

Very high swelling and embrittlement observed in a Fe-18Cr-10Ni-Ti hexagonal fuel wrapper irradiated in the BOR-60 fast reactor

The highest void swelling level ever observed in an operating fast reactor component has been found after irradiation in BOR-60 with swelling in Kh18H10T (Fe-18Cr-10Ni-Ti) austenitic steel exceeding 50%. At such high swelling levels the steel has reached a terminal swelling rate of ~1%/dpa after a transient that depends on both dpa rate and irradiation temperature. The transient duration at the higher irradiation temperatures is as small as 10-13 dpa depending on which face was examined. When irradiated in a fast reactor such as BOR-60 with a rather low inlet temperature, most of the swelling occurs above the core center-plane and produces a highly asymmetric swelling loop when plotted vs. dpa. Voids initially harden the alloy but as the swelling level becomes significant the elastic moduli of the alloy decreases strongly with swelling, leading to the consequence that the steel actually softens with increasing swelling. This softening occurs even as the elongation decreases as a result of void linkage during deformation. Finally, the elongation decreases to zero with further increases of swelling. This very brittle failure is known to arise from segregation of nickel to void surfaces which induces a martensitic instability leading to a zero tearing modulus and zero deformation.

Neustroev, V S↗

Swelling resistance of advanced austenitic alloy A709 and its comparison with 316 stainless steel at high damage levels

Alloy A709 is an austenitic alloy developed for power boiler applications in thermal power plants and is being considered as a candidate structural material for Generation IV reactors and fusion reactors, based especially on its increased creep strength over Type 316 stainless steel. However, improved thermal creep properties would not necessarily imply improved radiation resistance, especially with respect to void swelling. Since there are currently no neutron irradiation data on A709 to high fluences, A709 and cold-worked 316 were irradiated in the present study under identical conditions to doses between 100 and 400 peak dpa using irradiation by 3.5 MeV Fe +2 ions. The swelling behavior of 316 is well-known for both neutron and ion irradiation, thus the relative swelling behavior of A709 and 316 under ion irradiation might provide an indication of the swelling behavior of A709 in neutron irradiation environment. Swelling of A709 under ion irradiation was observed over the range of 500-600 ⁰C, peaking at 575 ⁰C. Both A709 and 316 eventually swelled at a rate of ~1 %/dpa under ion irradiation at 575 ⁰C, consistent with the swelling of 316 observed during neutron irradiation. But A709 had a significantly longer transient regime than 316 at any given dpa rate, demonstrating enhanced swelling resistance of A709 over 316 under self-ion irradiation. The swelling levels reached at 400 peak dpa were 55% and 90% for A709 and 316, respectively. The assigned local dpa levels were adjusted both temporally and spatially at each dose for swelling-induced increases in the ion range and concomitant decreases in density. The duration of the transient regimes in each alloy was also observed to increase as the local dpa rate increased, an observation also consistent with neutron irradiation behavior of 316 stainless steel.

36 MATERIALS SCIENCE↗

Antisense oligodeoxynucleotide inhibition of a swelling-activated cation channel in osteoblast-like osteosarcoma cells

By patch-clamp analysis, we have shown that chronic, intermittent mechanical strain (CMS) increases the activity of stretch-activated cation channels of osteoblast-like UMR-106.01 cells. CMS also produces a swelling-activated whole-cell conductance (Gm) regulated by varying strain levels. We questioned whether the swelling-activated conductance was produced by stretch-activated cation channel activity. We have identified a gene involved in the increase in conductance by using antisense oligodeoxynucleotides (ODN) derived from the alpha 1-subunit genes of calcium channels found in UMR-106.01 cells (alpha1S, alpha1C, and alpha1D). We demonstrate that alpha 1C antisense ODNs abolish the increase in Gm in response to hypotonic swelling following CMS. Antisense ODNs to alpha1S and alpha1D, sense ODNs to alpha1C, and sham permeabilization had no effect on the conductance increase. In addition, during cell-attached patch-clamp studies, antisense ODNs to alpha1c completely blocked the swelling-activated and stretch-activated nonselective cation channel response to strain. Antisense ODNs to alpha1S treatment produced no effect on either swelling-activated or stretch-activated cation channel activity. There were differences in the stretch-activated and swelling-activated cation channel activity, but whether they represent different channels could not be determined from our data. Our data indicate that the alpha1C gene product is involved in the Gm and the activation of the swelling-activated cation channels induced by CMS. The possibility that swelling-activated cation channel genes are members of the calcium channel superfamily exists, but if alpha1c is not the swelling-activated cation channel itself, then its expression is required for induction of swelling-activated cation channel activity by CMS.

NASA Discipline Musculoskeletal↗

Swell Sleeves for Testing Explosive Devices

A method of testing explosive and pyrotechnic devices involves exploding the devices inside swell sleeves. Swell sleeves have been used previously for measuring forces. In the present method, they are used to obtain quantitative indications of the energy released in explosions of the devices under test. A swell sleeve is basically a thick-walled, hollow metal cylinder threaded at one end to accept a threaded surface on a device to be tested (see Figure 1). Once the device has been tightly threaded in place in the swell sleeve, the device-and-swell-sleeve assembly is placed in a test fixture, then the device is detonated. After the explosion, the assembly is removed from the test fixture and placed in a coordinate-measuring machine for measurement of the diameter of the swell sleeve as a function of axial position. For each axial position, the original diameter of the sleeve is subtracted from the diameter of the sleeve as swollen by the explosion to obtain the diametral swelling as a function of axial position (see Figure 2). The amount of swelling is taken as a measure of the energy released in the explosion. The amount of swelling can be compared to a standard amount of swelling to determine whether the pyrotechnic device functioned as specified.

Hinkel, Todd J.↗

Measurement of kernel swelling and buffer densification in irradiated UCO and UO 2 TRISO fuel particles from AGR-2

The second Advanced Gas Reactor irradiation (AGR-2) featured UCO tristructural isotropic (TRISO)-coated particle fuel and, for comparison purposes, UO2 TRISO fuel. Particles from three UCO fuel compacts and one UO2 fuel compact were chosen for analysis of kernel swelling and buffer shrinkage. Both kernel swelling and buffer shrinkage are common elements of TRISO fuel performance models. More recently, the AGR program has determined that buffer shrinkage may impact the integrity of the inner pyrolytic carbon (IPyC) layer, which may impact SiC layer integrity (particularly during high-temperature heating tests). Therefore, measurements of buffer irradiation-induced shrinkage may be useful in improving existing models and developing new models that capture buffer-IPyC-SiC-fission product interactions observed in recent AGR post-irradiation examination (PIE). TRISO particles were mounted in epoxy, ground, polished, and imaged via optical microscopy in four separate iterations. Each of the four iterations revealed progressively deeper cross sections within the particles. Images collected from each iteration were analyzed for the circumferences/radii of the kernel, buffer, IPyC, and SiC. Spheres were fit to each set of measurements to generate spherical radii representative of the components of the fuel particle. From these radii, volumes were computed and compared to the as-fabricated volumes. UCO kernel swelling was similar among the three AGR-2 compacts ranging from approximately 28 to 32%. This is only slightly higher swelling than was measured in an earlier study of an AGR-1 compact. However, the burnup at which this swelling occurred in AGR-2 was lower than in AGR-1, indicating a faster swelling rate for the AGR-2 kernels for the irradiation conditions covered by these compacts. The AGR-2 UO2 kernel swelling was less, at 9.9%, comparable to other studies of UO2 kernel swelling. While AGR-2 UCO and UO2 kernels demonstrated different rates of swelling, the extent of buffer shrinkage was similar among the two fuel types, ranging from 24-28%. For comparison, a prior study showed that AGR-1 Compact 1-3-1 experienced 39% buffer shrinkage. A commonly-observed post-irradiation particle morphology is where the buffer pulls away from the IPyC (at least in some regions of the particle). Besides the possibility of the buffer degrading the IPyC when it pulls away from the IPyC, this gap is significant because it may also reduce heat transfer within the particle. Average AGR-2 buffer-IPyC gaps were similar for the UCO and UO2 particles, ranging from 22.2 to 26.0 µm. This is similar to what was measured for AGR-1 Compact 1-3-1.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Void swelling of conventional and composition engineered HT9 alloys after high-dose self-ion irradiation

Ferritic/martensitic (F/M) steels are being considered as potential structural materials for next generation nuclear reactors, and variants of the alloy HT9 are some of the most promising candidates. In this study, two conventional and two composition engineered HT9 alloys were irradiated using 3.5 MeV Fe 2+ up to 600 peak displacement-per-atom (dpa) at 450 °C. Void swelling and microstructure evolution were characterized for each alloy and compared. The two conventional HT9 alloys (INL and ACO3) showed similar void swelling behavior due to their similar elemental composition and processing conditions. The INL HT9 exhibited a maximum of 2.4% swelling and the ACO3 HT9 showed a maximum of 2.8% swelling at 342 and 393 average local dpa, respectively. On the other hand, the two-composition engineered HT9 alloys with varying N contents (10 ppm for low N and 440 ppm for high N) showed disparate swelling behavior. The low N HT9 exhibited a maximum of 4.6% swelling, while the high N HT9 showed a maximum of 0.7% swelling at 342 average local dpa. Changes in the N content also affected Ni/Si rich G-phase formation. The low N HT9 showed a larger size and lower density of G-phase precipitates compared with the high N HT9 after 600 peak dpa irradiation. This study compares the void swelling behavior of the ion irradiated four current HT9 alloys to extremely high doses, with the void swelling data from neutron irradiated HT9 alloys. Furthermore, the comparison lends critical insights into how well these current alloys can withstand high neutron fluxes in future reactors, especially since the low N and high N HT9 alloys have never been exposed to such high doses before.

36 MATERIALS SCIENCE↗

Molecular Dynamics Simulation of Hydration and Swelling of Mixed-Layer Clays in the Presence of Carbon Dioxide

Swelling of clay minerals is a prime anomaly that is relevant to many problems in geoscience, oil and gas reservoirs, geophysics, and engineering. The phenomenon is even more complex when carbon dioxide is also present. Since sequestration of CO 2 in sedimentary rock has been under active consideration as a way of alleviating the increasing concerns over climate change for which CO 2 is a main culprit, studying swelling of clays minerals in the presence of CO 2 has taken on added urgency. The swelling changes the permeability and porosity of porous formations, which in turn may lead to a reactivation of dormant fractures, triggering seismic activities, and opening up new pathways for CO 2 to return to the porous formations’ surface. Although the large majority of sedimentary rocks contain various types of mixed-layer clays (MLCs) with intermixed stacking sequences of several types of distinct layers within a single crystal, the vast majority of the past experimental and computational studies of the swelling was focused on pure clays. We present the results of extensive molecular dynamics simulation of hydration and swelling of illite-montmorillonite (I-MMT) MLCs, the most common type of mixed clays, in the presence of both water and CO 2 and various combinations of interlayer cations, Na + and K + . To understand the differences with pure clays, we also report on the same phenomenon in the MMT only. At low CO 2 concentrations in Na-MMT, which has its layers’ charge concentrated in its octahedral sheet, weak ion–surface interactions result in fully hydrated ions and, therefore, more extensive swelling than in I-MMT. Without CO 2 , adsorption of the cations at the illite surface increases the hydrophobicity of its surface. Thus, in the asymmetric interlayer of I-MMT, illite with stronger surface–ion interactions causes accumulation of cations near its surface, which limits their hydration and, therefore, controls swelling of the MLCs. Further inhibition of swelling of Na-MLC can be achieved by increasing the concentration of K + in the interlayer. At higher CO 2 concentrations, however, intercalation of water and CO 2 results in a completely different behavior, since in the 2W and 3W hydration states, the hydrophobicity of the MMT surface is stronger than that of illite. Thus, the density distributions of the intercalated molecules are considerably different from that with water only, which together with disruption of the water network by CO 2 reduces the difference between the extent of swelling of the MLC and pure MMT.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Recrystallization on Gas Bubble Swelling in UMo Fuels

The development of low-enriched uranium (LEU) fuels such as UMo dispersion fuels and monolithic UMo fuels is part of a global effort on nuclear nonproliferation. Although UMo fuels have the advantage of high density, excellent irradiation performance and good thermal conductivity, the volumetric swelling in irradiated metallic fuels is known to be an important design parameter because it affects not only the thermal conductivity of the fuels but also the mechanical integrity of fuel structures. Experiments also show that recrystallization dramatically affects the gas bubble swelling kinetics. A series of materials processes such as casting, mechanical rolling and thermal treatment are used in fuel fabrication. Resulting microstructure, such as grain size, porosity, and second phase, strongly depends on the material processes and process parameters. Therefore, a fundamental understanding how fabricated microstructures and irradiation conditions affect the nucleation of gas bubbles, recrystallization and gas bubble swelling kinetics is essential for optimizing material processes to obtain desired microstructure and fuel performance. Great effort has been made in the development of modeling capability for predicting gas bubble swelling kinetics and fission gas release kinetics in nuclear fuels. However, these models are based on the assumptions that the inter- and intra-granular gas bubble sizes are independent of position and only depend on time or fission density. Therefore, they are applicable to a material with uniform microstructure such as equiaxed grains with homogeneous defect distributions, homogeneous thermodynamic and kinetic properties of defects, and uniform radiation conditions. Very recently, we developed a three dimension (3D) microstructure dependent gas bubble swelling model for investigating the effect of heterogeneous microstructures and inhomogeneous thermodynamic properties of defects on gas bubble swelling in polycrystalline UMo fuels. However, the model doesn't take into account the effect of recrystallization on swelling kinetics. In this work, the spatially dependent rate theory is used to describe the evolution of interstitials and interstitial loop density. Recrystallization is described by a phase-field model with a concept of 'phase transition' when the local interstitial loop density is larger than a critical value. The intra- and inter- granular gas bubble evolution is described by the spatially dependent Booth model. A model integrating all the microstructure evolution enables one to study the effect of heterogeneous microstructures, recrystallization, and the metallic fuel thermodynamic and kinetic properties on gas bubble swelling kinetics.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

CLARITY reveals a more protracted temporal course of axon swelling and disconnection than previously described following traumatic brain injury

Abstract Diffuse axonal injury (DAI) is an important consequence of traumatic brain injury (TBI). At the moment of trauma, axons rarely disconnect, but undergo cytoskeletal disruption and transport interruption leading to protein accumulation within swellings. The amyloid precursor protein (APP) accumulates rapidly and the standard histological evaluation of axonal pathology relies upon its detection. APP+ swellings first appear as varicosities along intact axons, which can ultimately undergo secondary disconnection to leave a terminal “axon bulb” at the disconnected, proximal end. However, sites of disconnection are difficult to determine with certainty using standard, thin tissue sections, thus limiting the comprehensive evaluation of axon degeneration. The tissue‐clearing technique, CLARITY, permits three‐dimensional visualization of axons that would otherwise be out of plane in standard tissue sections. Here, we examined the morphology and connection status of APP+ swellings using CLARITY at 6 h, 24 h, 1 week and 1 month following the controlled cortical impact (CCI) model of TBI in mice. Remarkably, many APP+ swellings that appeared as terminal bulbs when viewed in standard 8‐µm‐thick regions of tissue were instead revealed to be varicose swellings along intact axons when three dimensions were fully visible. Moreover, the percentage of these potentially viable axon swellings differed with survival from injury and may represent the delayed onset of distinct mechanisms of degeneration. Even at 1‐month post‐CCI, ~10% of apparently terminal bulbs were revealed as connected by CLARITY and are thus potentially salvageable. Intriguingly, the diameter of swellings decreased with survival, including varicosities along intact axons, and may reflect reversal of, or reduced, axonal transport interruption in the chronic setting. These data indicate that APP immunohistochemistry on standard thickness tissue sections overestimates axon disconnection, particularly acutely post‐injury. Evaluating cleared tissue demonstrates a surprisingly delayed process of axon disconnection and thus longer window of therapeutic opportunity than previously appreciated. Intriguingly, a subset of axon swellings may also be capable of recovery.

Weber, Maura T.↗

Radiation-induced Swelling and Microcracking in SiC Cladding for LWRs

After the Fukushima accident in 2011, SiC has attracted considerable attention as a potential material for fuel cladding that can offer increased accident tolerance in light water reactors (LWRs) compared to zircaloy cladding. Existing measurements on nuclear grade SiC/SiC composites made of high-purity, stoichiometric SiC have already shown very good radiation tolerance in various harsh environments. However, there are a number of challenges that need to be addressed before SiC composites can be successfully used in LWR technologies. One of them is irradiation-induced swelling, which can lead to development of significant stresses in the matrix, followed by microcracking and subsequent release of fission products. Models of irradiation-induced swelling had been largely empirical and therefore they cannot be used to predict the microstructural dependence of microcracking. Existing models are also limited by the lack of understanding of defects that form due to irradiation in the range of temperatures relevant to fuel cladding in LWRs (<1000°C). Many of the defects in this regime of temperature are too small to be detected with traditional transmission electron microscopy (TEM) techniques. In fact the defects observed in traditional TEM account only for 10-45% of the swelling measured in irradiated SiC. Here, we developed a multi-scale simulation methodology combined with state of the art experimental imaging techniques based on aberration corrected scanning transmission electron microscopy (STEM) to provide a scientific basis for predictive models of radiation swelling and microcracking in SiC. Specifically, we have developed a phase field fracture model that predicts microcrack initiation and growth in polycrystalline SiC. The model accounts for single crystal anisotropy, including anisotropy in the elastic constants and anisotropic surface energy. It also considers the reduced fracture strength of grain boundaries. The model was implemented using the MARMOT mesoscale nuclear materials tool. We have parameterized the model for SiC using molecular dynamics simulation results. The model has been verified using single crystal, bicrystal, and polycrystal examples. Swelling model has also been developed based on cluster dynamics simulations of defect evolution in SiC. We found that point defects and small defect clusters have a significant contribution to swelling. This finding is important because point defects and very small defect clusters are not visible in experiments (e.g., in TEM). Combined modeling and experiments can bring critical insights into how swelling depends on irradiation conditions and the microstructure. In situ nanoindentation tests and ex situ nanoindentation tests were performed on assynthesized 3C-SiC and 3C-SiC irradiated under different radiation conditions. Without radiation, bend contour movement and residual bend contours after indentation demonstrate some room temperature plastic flow and residual plastic deformation. Plastic deformation recovery is also observed on unirradiated samples during unloading. Radiation-induced embrittlement is demonstrated by differences in crack geometry in in situ tests, and is consistent with ex situ test results. Failure by single, straight, cracks indicates decreased fracture toughness due to irradiation in 3C-SiC. Future work includes coupling of the swelling and fracture models and development of a master equation that can be used in the BISON code.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Analysis and prediction of ocean swell using instrumented buoys

During the period 20-23 September 1990, the remnants of Supertyphoon Flo moved into the central North Pacific Ocean with sustained wind speeds of 28 m/s. The strong wind and large fetch area associated with this storm generated long-period swell that propagated to the west coast of North America. National Data Buoy Center moored-buoy stations, located in a network that ranged from the Gulf of Alaska to the California Bight, provided wave spectral estimates of the swell from this storm. The greatest dominant wave periods measured were approximately 20-25 s, and significant wave heights measured ranged from 3 to 8 m. Wave spectra from an array of three nondirectional buoys are used to find the source of the long-period swell. Directional wave spectra from a heave-pitch-roll buoy are also used to make an independent estimate of the source of the swell. The ridge-line method, using time-frequency contour plots of wave spectral energy density, is used to determine the time of swell generation, which is used with the appropriate surface pressure analysis to infer the swell generation area. The diagnosed sources of the swell are also compared with nowcasts from the Global Spectral Ocean Wave Model of the Fleet Numerical Oceanography Center. A simple method of predicting the propagation of ocean swell, by applying a simple kinematic model of wave propagation to the estimated point and time source, is demonstrated.

Mettlach, Theodore↗