Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STAINLESS STEELS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

2016 Accomplishments. Tritium aging studies on stainless steel. Forging process effects on the fracture toughness properties of tritium-precharged stainless steel

Forged austenitic stainless steels are used as the materials of construction for pressure vessels designed to contain tritium at high pressure. These steels are highly resistant to tritium-assisted fracture but their resistance can depend on the details of the forging microstructure. During FY16, the effects of forging strain rate and deformation temperature on the fracture toughness properties of tritium-exposed-and-aged Type 304L stainless steel were studied. Forgings were produced from a single heat of steel using four types of production forging equipment – hydraulic press, mechanical press, screw press, and high-energy-rate forging (HERF). Each machine imparted a different nominal strain rate during the deformation. The objective of the study was to characterize the J-Integral fracture toughness properties as a function of the industrial strain rate and temperature. The second objective was to measure the effects of tritium and decay helium on toughness. Tritium and decay helium effects were measured by thermally precharging the as-forged specimens with tritium gas at 34.5 MPa and 350°C and aging for up to five years at -80°C to build-in decay helium prior to testing. The results of this study show that the fracture toughness properties of the as-forged steels vary with forging strain rate and forging temperature. The effect is largely due to yield strength as the higher-strength forgings had the lower toughness values. For non-charged specimens, fracture toughness properties were improved by forging at 871°C versus 816°C and Screw-Press forgings tended to have lower fracture toughness values than the other forgings. Tritium exposures reduced the fracture toughness values remarkably to fracture toughness values averaging 10-20% of as-forged values. However, forging strain rate and temperature had little or no effect on the fracture toughness after tritium precharging and aging. The result was confirmed by fractography which indicated that fracture modes in the tritium-exposed specimens were similar for all forgings. Another FY16 objective was to prepare fracture toughness specimens from Types 304L and 21-6-9 stainless steel weldments and heat-affected zones (HAZ) for tritium charging.

36 MATERIALS SCIENCE↗

Effect of heat input on dissimilar welds of ultra high strength steel and duplex stainless steel: Microstructural and compositional analysis

The effect of heat input on the microstructure and compositional heterogeneity of welds of direct-quenched ultra high strength steel (Optim 960 QC) and duplex stainless steel (UNS S32205) was studied. The dissimilar welds were made using GMAW with a fully austenitic filler wire. In addition to grain coarsening in the heat affected zone (HAZ) of the ferritic side, it was found that an increase in heat input correlatively increased the proportional volume of bainitic to martensitic phases. Coarse ferritic grains were observed in the duplex HAZ. Higher heat input, however, had a beneficial effect on the nucleation of austenite in the HAZ. Heat input had a regulatory effect on grain growth within the austenitic weld and more favorable equiaxed austenite was obtained with higher heat input. On the ferritic side of the welds, macrosegregation in the form of a martensitic intermediate zone was observed for all the cooling rates studied. However, on the duplex side, macrosegregation in the fusion boundary was only noticed with higher cooling rates. Microstructural observations and compositional analysis suggest that higher heat input could be beneficial for the structural integrity of the weld despite higher heat input increasing the extent of adverse coarse grains in the HAZ, especially on the ferritic side. - Highlights: •The effect of heat input on dissimilar welds of UHSS and DSS was studied. •Transmutation of the microstructure was discussed in detail. •The influence of heat input on compositional heterogeneity of welds was described. •Higher heat input enhanced bainitic transformation on the ferritic side. •Macrosegregation was affected by the amount of heat input on the DSS side.

36 MATERIALS SCIENCE↗

SA508 low alloy steel to 316L stainless steel dissimilar metal joint made by powder metallurgy hot isostatic pressing

Joining ferritic SA508 low alloy steel (LAS) and austenitic 316 L stainless steel (SS) via powder metallurgy hot isostatic pressing (PM-HIP) was evaluated as an alternative method to welding. This study investigated the mechanical and microstructural evolutions of the bimetallic interface under different joint designs and heat treatments. Here, the direct joining of dissimilar metal alloys by PM-HIP method resulted in two designs: 1) powder SA508 to solid bar 316 L (P508–B316L) and 2) powder 316 L solid bar SA508 (P316L-B508). In both cases, P508–B316L and P316L-demonstrated satisfactory tensile strength, however, high hardness and severe depreciation in toughness were located on the bimetallic interface. The mechanisms responsible for the detrimental mechanical properties were verified. Large oxides were observed in P508–B316L due to the prior powder boundary (PPB) oxides present in SA508 powder. The intense sensitization occurred from the formation of M 23 C 6 carbides, consequently from the slow cooling after PM-HIP in P316L-B508. Post-HIP heat treatments were explored to reduce the distance of carbide formation; however, the heat treatment could not eliminate the carbides. The experimental results were compared to the diffusion couple simulation as a function of carbide formation with distance. The analysis also showed the high hardness at the bimetallic interface was primarily contributed by solid solution strengthening. In conclusion, the direct joining of P316L-B508 and P508–B316L via PM-HIP was deemed to be unfeasible, and a transitional material is necessary to impede the diffusion of carbon.

316L stainless Steel↗

Effect of microstructural and environmental variables on ductility of austenitic stainless steels

Austenitic stainless steels are used extensively in harsh environments, including for high-pressure gaseous hydrogen service. However, the tensile ductility of this class of materials is very sensitive to materials and environmental variables. While tensile ductility is generally insufficient to qualify a material for hydrogen service, ductility is an effective tool to explore microstructural and environmental variables and their effects on hydrogen susceptibility, to inform understanding of the mechanisms of hydrogen effects in metals, and to provide insight to microstructural variables that may improve relative performance. In this study, hydrogen precharging was used to simulate high-pressure hydrogen environments to evaluate hydrogen effects on tensile properties. Several austenitic stainless steels were considered, including both metastable and stable alloys. Room temperature and subambient temperature tensile properties were evaluated with three different internal hydrogen contents for type 304L and 316L austenitic stainless steels and one hydrogen content for XM-11. Significant ductility loss was observed for both metastable and stable alloys, suggesting the stability of the austenitic phase is not sufficient to characterize the effects of hydrogen. Internal hydrogen does influence the character of deformation, which drives local damage accumulation and ultimately fracture for both metastable and stable alloys. While a quantitative description of hydrogen-assisted fracture in austenitic stainless steels remains elusive, these observations underscore the importance of the hydrogen-defect interactions and the accumulation of damage at deformation length scales.

36 MATERIALS SCIENCE↗

Characterization of carbon ion implantation induced graded microstructure and phase transformation in stainless steel

Austenitic stainless steel 316L is ion implanted by carbon with implantation fluences of 1.2 × 10{sup 17} ions-cm{sup −} {sup 2}, 2.4 × 10{sup 17} ions-cm{sup −} {sup 2}, and 4.8 × 10{sup 17} ions-cm{sup −} {sup 2}. The ion implantation induced graded microstructure and phase transformation in stainless steel is investigated by X-ray diffraction, X-ray photoelectron spectroscopy and high resolution transmission electron microscopy. The corrosion resistance is evaluated by potentiodynamic test. It is found that the initial phase is austenite with a small amount of ferrite. After low fluence carbon ion implantation, an amorphous layer and ferrite phase enriched region underneath are formed. Nanophase particles precipitate from the amorphous layer due to energy minimization and irradiation at larger ion implantation fluence. The morphology of the precipitated nanophase particles changes from circular to dumbbell-like with increasing implantation fluence. The corrosion resistance of stainless steel is enhanced by the formation of amorphous layer and graphitic solid state carbon after carbon ion implantation. - Highlights: • Carbon implantation leads to phase transformation from austenite to ferrite. • The passive film on SS316L becomes thinner after carbon ion implantation. • An amorphous layer is formed by carbon ion implantation. • Nanophase precipitate from amorphous layer at higher ion implantation fluence. • Corrosion resistance of SS316L is improved by carbon implantation.

36 MATERIALS SCIENCE↗

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating↗

Study on tempering behaviour of AISI 410 stainless steel

Martensitic stainless steels find extensive applications due to their optimum combination of strength, hardness and wear-resistance in tempered condition. However, this class of steels is susceptible to embrittlement during tempering if it is carried out in a specific temperature range resulting in significant reduction in toughness. Embrittlement of as-normalised AISI 410 martensitic stainless steel, subjected to tempering treatment in the temperature range of 673–923 K was studied using Charpy impact tests followed by metallurgical investigations using field emission scanning electron and transmission electron microscopes. Carbides precipitated during tempering were extracted by electrochemical dissolution of the matrix and identified by X-ray diffraction. Studies indicated that temper embrittlement is highest when the steel is tempered at 823 K. Mostly iron rich carbides are present in the steel subjected to tempering at low temperatures of around 723 K, whereas chromium rich carbides (M{sub 23}C{sub 6}) dominate precipitation at high temperature tempering. The range 773–823 K is the transition temperature range for the precipitates, with both Fe{sub 2}C and M{sub 23}C{sub 6} types of carbides coexisting in the material. The nucleation of Fe{sub 2}C within the martensite lath, during low temperature tempering, has a definite role in the embrittlement of this steel. Embrittlement is not observed at high temperature tempering because of precipitation of M{sub 23}C{sub 6} carbides, instead of Fe{sub 2}C, preferentially along the lath and prior austenite boundaries. Segregation of S and P, which is widely reported as one of the causes for temper embrittlement, could not be detected in the material even through Auger electron spectroscopy studies. - Highlights: • Tempering behaviour of AISI 410 steel is studied within 673–923 K temperature range. • Temperature regime of maximum embrittlement is identified as 773–848 K. • Results show that type of carbide precipitation varies with temperature of tempering. • Mostly iron rich Fe{sub 2}C carbides are present in the embrittlement temperature range. • With the precipitation of M{sub 23}C{sub 6} carbides, recovery from the embrittlement begins.

36 MATERIALS SCIENCE↗

Anomalous Annealing Response of Directed Energy Deposited Type 304L Austenitic Stainless Steel

Directed energy deposited (DED) and forged austenitic stainless steels possess dissimilar microstructures but can exhibit similar mechanical properties. In this study, annealing was used to evolve the microstructure of both conventional wrought and DED type 304L austenitic stainless steels, and significant differences were observed. In particular, the density of geometrically necessary dislocations and hardness were used to probe the evolution of the microstructure and properties. Forged type 304L exhibited the expected decrease in measured dislocation density and hardness as a function of annealing temperature. Here, the more complex microstructure–property relationship observed in the DED type 304L material is attributed to compositional heterogeneities in the solidification microstructure.

36 MATERIALS SCIENCE↗

Understanding Uranium Binding Mechanisms and Speciation on Stainless Steel - 17462

Stainless steels have been exposed to nitric acid solutions containing natural uranium under similar conditions to those found in reprocessing plants. Solution and solid analysis of the stainless steel samples has been undertaken to describe the contamination phenomenon. General corrosion of the surface was seen to take place over the month-long experiments. Contamination has been shown on all exposed surfaces. Solution analysis indicates that an equilibrium state is reached after 2 weeks exposure to the 12 M HNO{sub 3}. Surface analysis through autoradiography and X-ray absorption near edge structure (XANES) indicate that multiple mechanisms of uptake may occur and consequently concentrated regions of contamination may be produced. (authors)

36 MATERIALS SCIENCE↗

Monte Carlo simulations of Cu/Ni–Si–Mn co-precipitation in duplex stainless steels

First-Passage Kinetic Monte Carlo (FPKMC) simulations of species migration in duplex stainless steels were performed in order to establish relationships between alloy content, segregation behavior, and the formation of Ni-Si-Mn rich particles in cast duplex stainless steels during thermal aging. The Ni-Si-Mn-rich second phase forms after extended aging at reactor operating temperatures and degrades alloy properties. Simulations of Ni-Si-Mn cluster formation were validated through comparison with experimental results obtained through Atom Probe Tomography (APT) on similar alloy compositions, identifying several trends. First, Cu promotes the formation of Ni-Si-Mn clusters, but only when Ni or Mn prefer segregation to the surface of Cu particles; without the segregation of these species, the critical composition for the clusters to form was not achieved. Second, the width of precipitate-denuded zones near ?/d interfaces increases with decreasing Cu content. This finding was in strong agreement with APT results, further validating our model. Finally, our model predicts that Ni-Si-Mn cluster formation will be the most extensive when the Si:Mn ratio is approximately 1:1 and the least extensive when one of these key elements is less concentrated (Mn = 0.5 at.% or Si = 0.5 at.%). The implications of these results on how to improve alloy properties are discussed.

Cu co-precipitation, Atom probe tomography (APT), ↗

Tritium embrittlement of austenitic stainless-steel tubing at low helium contents

Austenitic stainless steels are the standard materials for containment of hydrogen and tritium because of their resistance to mechanical property degradation in those environments. The mechanical performance of the primary containment material is critical for tritium handling, processing, and storage, thus comprehensive understanding of the processes of tritium embrittlement is an enabling capability for fusion energy. This work describes the investigation of the effects of low levels of tritium-decay-helium ingrowth on 304 L tubes. Long-term aging with tritium leads to high helium contents in austenitic stainless steels and can reduce fracture toughness by 95 %, but the details of behavior at low helium contents are not as well characterized. Here, we present results from tensile testing of tritium pre-charged 304 L tube specimens with a variety of starting microstructures that all contain a low level of helium. The results of the tritium exposed-and-aged materials are compared to previously reported results on similar specimens tested in an unexposed condition as well as the hydrogen precharged condition. Tritium precharging and aging for a short duration resulted in increased yield strengths, ultimate tensile strengths and slightly increased elongation to failure, comparable to higher concentrations of hydrogen precharging.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Gas-phase hydrogen permeation through alpha iron, 4130 steel, and 304 stainless steel from less than 100 C to near 600 C

Gas phase hydrogen permeation studies were conducted on hollow, cylindrical membranes of triply zone-refined alpha iron, AISI 304 austenitic stainless steel, and AISI-SAE 4130 steel in both the normalized (ferrite and carbide) and quenched and tempered (martensite) conditions. Membrane temperature was varied from less than 100 C to near 600 C and hydrogen pressure was varied. For one membrane material, normalized 4130 steel, gas phase hydrogen transport under both steady state and nonsteady state conditions was demonstrated to be controlled by lattice diffusion. Additionally, Sievert's law was shown to be applicable. For all membrane materials, expressions for the coefficients for hydrogen permeation were determined by analysis of steady state transport; the coefficients for diffusion were determined by the lag time technique applied to nonsteady state transport; and through a knowledge of the Sievert's constants, the subsurface equilibrium lattice hydrogen concentrations were determined.

Nelson, H. G.↗

Precipitation-site competition in duplex stainless steels: Cu clusters vs spinodal decomposition interfaces as nucleation sites during thermal aging

Competing microstructural evolution mechanisms can exist simultaneously when duplex stainless steels are operating for several decades in a high temperature service environment. Such competition between different microstructural evolution pathways can be difficult to ascertain using simple model alloy systems necessitating detailed structural and compositional analysis of phase transformation mechanisms in complex alloys Thus, in this study duplex stainless steels with complex but well understood chemistries were used to investigate the relative importance of different heterogeneous nucleation sites – specifically spinodal decomposition and Cu clustering – on precipitation of Ni-Si-Mn particles during long term thermal aging. Precipitation of Ni-Si-Mn particles in duplex stainless steels and ferritic steels during thermal aging and irradiation is known to have profound effect on mechanical properties. Using duplex stainless steels with custom modified compositions along with atom probe tomography characterization and first-passage kinetic Monte Carlo (FPKMC) simulations it is revealed that while the interface between Cr and Fe formed during spinodal decomposition can be a pathway for diffusion of Ni, Si, Mn, and Cu, it is not a site that encourages precipitation of Ni-Si-Mn rich particles. Instead, the presence of a higher concentration of Cu in these steels leads to formation of small Cu clusters with high energy interfaces that act as nucleation sites for Ni-Si-Mn particles because of its strong interaction particularly with Ni increasing the chemical driving force for precipitation. These results will help inform predictive models for the use of duplex stainless steels and other precipitation-hardened alloys for extended operation at high temperatures.

Duplex stainless steel, Thermal aging, Precipitati↗

Microstructure characteristics of LPBF&HIP fabricated graded composite transition joint between ferritic steel and austenitic stainless steel

Graded composite transition joints (GCTJs) offer a promising alternative to conventional dissimilar metal welds (DMWs) by enabling smooth compositional and microstructural transitions. However, GCTJs fabricated solely through additive manufacturing (AM) face challenges such as heat accumulation, complex parameter control, and elemental segregation. In this study, we propose a novel approach that relies on AM to design a spatially graded structure in one alloy and then employs hot isostatic pressing (HIP) as a diffusion bonding method to join it with a second alloy. Here, this method combines the flexibility of AM with the powder net-shaping advantage of HIP. Specifically, a series of closely packed austenitic stainless steel 304 conical structures were printed using laser powder bed fusion (LPBF) and then combined with ferritic steel P91 powder via HIP. By using electron backscatter diffraction (EBSD), electron probe microanalysis (EPMA), and transmission electron microscopy (TEM) techniques, the microstructure characteristics of the GCTJ of 304&P91, especially the interdiffusion zone (IDZ), have been systematically investigated. The microstructure at the interface transitions from austenite-ferrite (A+F) to austenite-martensite-ferrite (A+M+F), and finally to martensite-ferrite (M+F) due to diffusion. Additionally, the diffusion width between 304 and P91 increases with the volume fraction of P91. This unique design also ensures a gradual transition in both hardness and thermal expansion coefficient from 304 to P91, thereby enabling a smooth gradient in functional properties. Overall, this study proposes a novel approach for fabricating GCTJs and contributes to advancing design concepts in the field of dissimilar metal joining.

Additively manufacturing (AM)↗

Cold Spray Deposition of 304L Stainless Steel to Mitigate Chloride-Induced Stress Corrosion Cracking in Canisters for Used Nuclear Fuel Storage

A feasibility study of the cold spray deposition process of 304L stainless steel on 304L stainless steel substrates as a mitigation method for chloride-induced stress corrosion cracking (CISCC) has been investigated under various substrate conditions. The study is aimed at the application of this technology to mitigate CISCC that may potentially occur in or nearthe fusion welded regions of stainless steel canisters in Dry Cask Storage System (DCSS) for used nuclear fuels. Spherical gas-atomized 304L stainless steel powder, in the size range of 25 µm to 44 µm, was used as a feedstock powder for the cold spray process. The powder was deposited on four types of 304L substrates with various surface conditions: as-polished, oxidized, cold-rolled, plates with prototypical CISCC. The effects of cold spray parameters on quality of cold spray coatings were investigated. Thickness, porosity, and phases in the as-deposited materials were evaluated using scanning electron microscopy (SEM) and X-ray diffraction (XRD), and correlated with microhardness and adhesion strength measured via micro-indentation and ASTM C633 pulling test, respectively. XRD analysis of the coatings was also conducted to examine the effects of cold spray condition on residual stress state in the coating. Detailed cross-sectional examination of coating/substrate interfaces was performed with transmission electron microscopy (TEM) equipped with energy dispersive spectroscopy (EDS). Dense and continuous coatings with good adhesion strength and hardness were produced for the various substrate conditions by adjusting cold spray parameters. The results demonstrate that cold spray stainless steel coating is a viable option to provide a physical barrier against CISCC in fusion weld regions of stainless steel in corrosive chloride salt-bearing environments.

Dry Cask Storage Systems, cold spray, 304L stainle↗

Influence of Welding Strength Matching Coefficient and Cold Stretching on Welding Residual Stress in Austenitic Stainless Steel

Austenitic stainless steel is widely used in pressure vessels for the storage and transportation of liquid gases such as liquid nitrogen, liquid oxygen, and liquid hydrogen. Cryogenic pressure vessel manufacturing uses cold stretching technology, which relies heavily on welding joint performance, to construct lightweight and thin-walled vessels. Residual stress from welding is a primary factor in cases of austenitic stainless steel pressure vessel failure. In this paper, on the basis of Visual Environment 10.0 finite element simulation technology, the residual stress resulting from different welding strength matching coefficients (0.8, 1, 1.2, 1.4) for two S30408 plates welded with three-pass butt welds is calculated according to thermal elastoplastic theory. In addition, the stress field was calculated under a loading as high as 410 MPa and after the load was released. Path 1 was set to analyze stress along the welding line, and path 2 was set to analyze stress normal to the welding line. The welding strength matching coefficient strongly affected both the longitudinal residual stress (center of path 1) and the transverse residual stress (both ends of path 1) after the welding was completed. However, the coefficient had little effect on the longitudinal and transverse residual stress of path 2. Under the loading of 410 MPa, the longitudinal and transverse stress decreased and the stress distribution, with different welding strength matching coefficients, was less diverse. After the load was released, longitudinal and transverse stress distribution for both path 1 and path 2 decreased to a low level. Cold stretching could reduce the effect of residual stress to various degrees. Transverse strain along the stretching direction was also taken into consideration. The experimental results validated the reliability of the partial simulation.

36 MATERIALS SCIENCE↗