Visualizing the SEI formation between lithium metal and solid-state electrolyte

The solid electrolyte interphase (SEI) is regarded as the most important factor affecting the durability of lithium-metal anode in all-solid-state batteries (ASSBs). Despite its significance, the nucleation and growth mechanism of SEI is not yet well understood. Here, we elucidate the thermodynamics and kinetics governing SEI formation at the Li|β-Li 3 PS 4 interface at the atomic scale via thermodynamic phase equilibrium analysis and machine-learning-potential-assisted molecular dynamics (MD) simulations. An accurate moment tensor potential using the machine-learning method is developed for a reactive model of Li|β-Li 3 PS 4 . This potential enabled us to perform large-scale MD simulations with the model size expanded to the experimental dimensions (~40 nm) while maintaining the same level of accuracy as density functional theory calculations. The results reveal a four-stage evolution process at the Li|β-Li 3 PS 4 interface, namely (i) fast ion diffusion, (ii) nucleation, (iii) Li 2 S growth, and (iv) stabilization. Notably, we demonstrate that the SEI can be categorized into crystalline and amorphous regions. The simulated SEI thickness, structure, and composition closely match experimental findings, validating the accuracy of the MD simulations. We further disclose the significant impact of ion diffusion kinetic limitations on the phase formation and crystallization of interfacial products. Furthermore, we shed light on the detailed potential energy (PE) distribution of lithium along the direction perpendicular to the interface. Finally, this information is crucial for better understanding interfacial ion mobility.

25 ENERGY STORAGE↗

Recent progress in understanding solid electrolyte interphase on lithium metal anode

Lithium (Li) metal batteries (LMBs) are among the most promising candidates of next-generation high-energy-density rechargeable batteries. Solid electrolyte interphase (SEI) on Li metal anode plays a significant role which influences the Li deposition morphology and the cycle life of LMBs. Although SEI is the most important part, a thorough understanding of SEI is inadequate. In this review, we focus on the progresses of understanding on structures, properties and influencing factors of SEI as well as efficient strategies of tailoring SEI. First, the compositions, models and recent progresses on characterizing atomic structure of SEI are summarized. Second, the properties of SEI, including electronic conduction, ionic conduction, stability and mechanical properties are elucidated. Structures and properties of SEI are greatly influenced by multiple factors such as solvent, salt, additive, solvation structure, impurity, current density, temperature, pressure and capacity utilization. Thus, interactions between these factors and SEI are comprehensively discussed. Correlations of SEI with Li deposition morphology, rate capability and cycle life are further summarized. Moreover, efficient strategies of tailoring SEI with desired properties, including in-situ SEI and ex-situ SEI are also reviewed. Despite the significant progresses that have been achieved in the researches of SEI, better understanding of SEI is still highly demand. Finally, future directions especially in-operando techniques, multi-modality approaches for characterization of SEI and artificial intelligence assisted understanding of correlation between electrolyte components and SEI properties are proposed.

Wu, Haiping↗

Final Mission and Navigation Design for the 2016 Mars InSight Mission

Project Overview: NASA’s 12th Discovery Program mission that will place a single geophysical lander on Mars to study its deep interior using seismic (tidal, marsquake, and impact), rotational, and thermal measurements -First mission to unveil the composition, structure and thermal state of martian crust, mantle and core; Rebuild of the Phoenix flight system, upgraded with Juno/GRAIL avionics -Phoenix cruise stage: 3-axis stabilized, 3.2 square meter UTJ (Ultra Triple-Junction) solar array, X-band telecom -Phoenix aeroshell (heat shield, backshell, parachute) -Phoenix lander: radar, pulsed thrusters, legs, payload deck, 5.1 square meter UTJ solar arrays, two redundant Li-ion batteries, UHF (Ultra High Frequency)/X-band telecom -Dual string: Internally or functionally-redundant equipment; Science Payload -SEIS (Seismic Experiment for Interior Structure) / CNES (Centre National d’Etudes Spatiales); Three-axis seismometry, to measure seismic waves traveling through the interior -HP3 (Heat Flow and Physical Properties Probe) / DLR (German Aerospace Center) -Subsurface heat probe, to measure the heat flux from the interior - RISE (Rotation and Interior Structure Experiment) / JPL (Jet Propulsion Laboratory) -Radiometric geodesy, to determine precession & nutation of the planet’s rotation axis. 2016 Disclaimer: The InSight launch in 2016 was suspended due to critical issues with the Seismic Experiment for Interior Structure (SEIS) instrument that could not be fixed prior to the planned launch period. This presentation and its corresponding paper represent the state of the design for the 2016 mission. No attempt has been made to reflect the latest developments. [2018 Note: InSight (Mars Lander) was later launched and arrived on Mars on Nov. 26, 2018.]

Abilleira, F.↗

LiH formation and its impact on Li batteries revealed by cryogenic electron microscopy

Little is known about how evolved hydrogen affects the cycling of Li batteries. Hypotheses include the formation of LiH in the solid-electrolyte interphase (SEI) and dendritic growth of LiH. Here, we discover that LiH formation in Li batteries likely follows a different pathway: Hydrogen evolved during cycling reacts to nucleate and grow LiH within already deposited Li metal, consuming active Li. We provide the evidence that LiH formed in Li batteries electrically isolates active Li from the current collector that degrades battery capacity. We detect the coexistence of Li metal and LiH also on graphite and silicon anodes, showing that LiH forms in most Li battery anode chemistries. Last, we find that LiH has its own SEI layer that is chemically and structurally distinct from the SEI on Li metal. Our results highlight the formation mechanism and chemical origins of LiH, providing critical insight into how to prevent its formation.

25 ENERGY STORAGE↗

Current Density Regulated Atomic to Nanoscale Process on Li Deposition and Solid Electrolyte Interphase Revealed by Cryogenic Transmission Electron Microscopy

Current density has been perceived to play a critical rule for controlling Li deposition morphology and solid electrolyte interphase (SEI). However, the atomic level mechanism of current density on Li deposition and the SEI remains unclear. In this work, based on cryogenic transmission electron microscopy imaging combined with energy dispersive X-ray spectroscopy and electron energy loss spectroscopy electronic structure analyses, we reveal the atomic level correlation of Li deposition morphology and SEI with current density. We discover that increasing current density leads to increased overpotential for Li nucleation and growth, leading to the transition from growth-limited to nucleation-limited mode for Li dendrite. Independence of current density, the electrochemically deposited Li metal (EDLi) exhibits crystalline whisker-like morphology. The SEI formed at low current density (0.1 mA cm -2 ) is monolithic amorphous; while, a current density of above 2 mA cm -2 leads to a mosaic structured SEI, featuring an amorphous matrix with Li 2 O and LiF dispersoids, and the thickness of the SEI increases with the increase of current density. Uniquely, the Li 2 O particles is spatially located at the top surface of the SEI, while LiF is spatially adjacent to the Li-SEI interface. These results highlight the possible tuning of crucial structural and chemical features of EDLi and SEI through altering deposit conditions and consequently direct correlation with electrochemical performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Liquid state properties of SEI components in dimethoxyethane

The solid-electrolyte interphase (SEI) layer is a critical constituent of battery technology, which incorporates the use of lithium metals. Since the formation of the SEI is difficult to avoid, the engineering and harnessing of the SEI are absolutely critical to advancing energy storage. One problem is that much fundamental information about SEI properties is lacking due to the difficulty in probing a chemically complex interfacial system. One such property that is currently unknown is the dissolution of the SEI. This process can have significant effects on the stability of the SEI, which is critical to battery performance but is difficult to probe experimentally. Here, we report the use of ab initio computational chemistry simulations to probe the solution state properties of SEI components LiF, Li 2 O, LiOH, and Li 2 CO 3 in order to study their dissolution and other solution-based characteristics. Ab initio molecular dynamics was used to study the solvation structures of the SEI with a combination of radial distribution functions, discrete solvation structure maps, and vibrational density of states, which allows for the determination of free energies. From the change in free energy of dissolution, we determined that LiOH is the most likely component to dissolve in the electrolyte followed by LiF, Li 2 CO 3 , and Li 2 O although none were favored thermodynamically. Furthermore, this indicates that dissolution is not probable, but Li 2 O would make the most stable SEI with regard to dissolution in the electrolyte.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Solid Electrolyte Interphase Architecture Determined through In Situ Neutron Scattering

We demonstrate through a combination of in operando solvent exchange and depth-sensitive neutron reflectometry that the solid electrolyte interphase (SEI) formed after the initial lithiation of a silicon anode, using a standard LiPF6 ethylene carbonate/ethyl methyl carbonate electrolyte, is chemically homogeneous across the liquid-solid interface. The data show the SEI is accessible to solvent/salt exchange throughout the layer indicating the poorly bound nature of the SEI components. Further, the data indicates that P-F species, from the decomposition of the LiPF6 salt, are highly mobile and removed from the SEI with solvent exchange. Critically, the SEI layer is structurally homogenous, in contrast to the reports in the literature of an inorganic/organic bilayer, which is important to our understanding of SEI formation and chemistry.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Space Exploration Initiative and NASA Langley Research Center test facilities

The NASA Exploration Technology Program (ETP) will make possible the U.S. Space Exploration Initiative (SEI), and is structured according to mission thrusts that are based on technologies to be developed and tested or that will otherwise be utilized to support SEI. Twenty-seven technology projects have thus far been established, and NASA's Langley Research Center is responsible for six lead roles and four participating roles. This report briefly defines these ten Langley-assigned ETP technology projects, and it describes both existing and proposed test facilities capable of supporting the Center's responsibilities.

Mouring, John L.↗

A Comparison of Solid Electrolyte Interphase Formation and Evolution on Highly Oriented Pyrolytic and Disordered Graphite Negative Electrodes in Lithium–Ion Batteries

The presence and stability of solid electrolyte interphase (SEI) on graphitic electrodes is vital to the performance of lithium-ion batteries (LIBs). However, the formation and evolution of SEI remain the least understood area in LIBs due to its dynamic nature, complexity in chemical composition, heterogeneity in morphology, as well as lack of reliable in situ/operando techniques for accurate characterization. In addition, chemical composition and morphology of SEI are not only affected by the choice of electrolyte, but also by the nature of the electrode surface. While introduction of defects into graphitic electrodes has promoted their electrochemical properties, how such structural defects influence SEI formation and evolution remains an open question. In this work, utilizing nondestructive operando electrochemical atomic force microscopy (EChem-AFM) the dynamic SEI formation and evolution on a pair of representative graphitic materials with and without defects, namely, highly oriented pyrolytic and disordered graphite electrodes, are systematically monitored and compared. Complementary to the characterization of SEI topographical and mechanical changes during electrochemical cycling by EChem-AFM, chemical analysis and theoretical calculations are conducted to provide mechanistic insights underlying SEI formation and evolution. The results provide guidance to engineer functional SEIs through design of carbon materials with defects for LIBs and beyond.

25 ENERGY STORAGE↗

Cross-scale modeling and experimental integration for advancing cathode electrolyte interphase studies in high energy density lithium-ion batteries

Electrochemical interfaces are critical to the performance and durability of lithium-ion batteries (LIBs). The solid electrode-electrolyte interphase (SEI and CEI) structures that form during cycling can passivate reactive surfaces, ensuring safe operation, but also may contribute to performance degradation. Understanding the microscopic factors influencing interphase formation, growth, and evolution is essential for balanced battery design. While significant research has focused on the anode-electrolyte interphase (SEI), the cathode-electrolyte interphase (CEI) remains less explored, despite its importance in high-voltage and advanced battery technologies. Challenges in conducting in-situ or operando experiments arise from the occluded nature of these interfaces and the long timescales involved, often leading to biased interpretations. A validated multi-scale, multi-physics modeling approach, integrated with advanced characterization techniques, can effectively elucidate the intrinsic stability of electrolyte and cathode surfaces, the impact of chemical heterogeneity, and the role of microstructural features on CEI performance. In conclusion, this article reviews current modeling and simulation strategies for studying CEI in advanced LIBs and highlights opportunities for future methodological advancements and experimental integration.

Cathode-electrolyte interphase↗

Lithium oxidation and electrolyte decomposition at Li-metal/liquid electrolyte interfaces

In this work, we examine the evolution of events occurring when a Li metal surface is in contact with a 2 M solution of a Li salt in a solvent or mixture of solvents, via classical molecular dynamics simulations with a reactive force field allowing bond breaking and bond forming. The main events include Li oxidation and electrolyte reduction along with expansion of the Li surface layers forming a porous phase that is the basis for the formation of the solid-electrolyte interphase (SEI) components. Nucleation of the main SEI components (LiF, Li oxides, and some organics) is characterized. The analysis clearly reveals the details of these physical–chemical events as a function of time, during 20 nanoseconds. The effects of the chemistry of the electrolyte on Li oxidation and dissolution in the liquid electrolyte, and SEI nucleation and structure are identified by testing two salts: LiPF 6 and LiCF 3 SO 3 , and various solvents including ethers and carbonates and mixtures of them. The kinetics and thermodynamics of Li 6 F, the core nuclei in the LiF crystal, are studied by analysis of the MD trajectories, and via density functional theory calculations respectively. The SEI formed in this computational experiment is the “native” film that would form upon contact of the Li foil with the liquid electrolyte. As such, this work is the first in a series of computational experiments that will help elucidate the intricate interphase layer formed during battery cycling using metal anodes.

25 ENERGY STORAGE↗

A vision for planetary exploration

A vision for planetary exploration is proposed which combines historical perspective and current NASA studies with the realities of changing political climates, economic environments, and technological directions. The concepts of Strategic Implementation Architectures (SIA), Open System Infrastructure Standards (OSIS), and Minimum Service Level Infrastructure (MSLI) are presented in order to propose a structure for the SEI which allows the realization of incremental mission objectives, establishes an investment strategy that efficiently uses public resources, and encourages partnerships with the government. The SIA is a hypothetical master plan which will allow the implementation of the complete spectrum of envisioned system capabilities for planetary exploration. OSIS consists of standards for interconnection, interoperability, and administration. MSLI can be defined as the minimum level of services provided by the system that are not justified by profit or parochial motives.

Connolly, John F.↗

Stress- and interface-compatible red phosphorus anode for high-energy and durable sodium-ion batteries

Sodium-ion battery is a promising candidate for energy storage application, but the absence of high-capacity and low-cost anode materials significantly limit their practical specific energy and cost. Red phosphorus (RP) possesses a high theoretical specific capacity but suffers from large volume change, low electronic conductivity and unstable solid-electrolyte interphase (SEI). Herein, a hierarchical micro/nanostructured antimony-doped RP/carbon anode was developed, which demonstrate extraordinary electrochemical performance with high initial Coulombic efficiency of ~90%, high areal (~1.7 mAh cm-2) capacity together with good cycle stability and rate capability. Combined experimental and computational studies consistently revealed that such a unique structural design can dramatically accommodate the mechanical stress and moreover effectively restrain the undesired decomposition of electrolyte solvents regardless of electrolytes formulation, resulting in superior structural integrity and thin/robust SEI formation during cycling. The present finding has offered an alternative strategy for stress management and interface engineering on high-capacity alloying-based anode materials.

Liu, Xiang↗

Microscopic Observation of Solid Electrolyte Interphase Bilayer Inversion on Silicon Oxide

Silicon has been investigated in recent years as an alloying anode material to enhance gravimetric energy density in lithium-ion batteries. Although recent developments have suggested that silicon oxides exhibit improved cycling stability over pure Si, the origin of the improved cycling performance is still poorly understood. The initial solid electrolyte interphase (SEI) formation mechanisms on Si wafers with both native oxide and chemically etched thermal oxide coatings are investigated structurally, chemically, and morphologically in the nanoscale. After one electrochemical cycle, microscopy reveals that SEI formed on native SiO x features the typical SEI bilayer structure with a carbon-rich outer SEI layer and an inorganic-rich inner SEI layer. In contrast, the SEI formed on chemically etched thermal oxide shows an inversion in the structure. This work observes distinct initial SEI formation mechanisms on the HF-etched SiO 2 surface, which may be partially responsible for improved cycle life observed in SiO x -based anode materials.

25 ENERGY STORAGE↗

Fine‐Tuning Li‐Ion Solvation Structure by Enhanced Solvent‐Diluent Interactions for Long‐Cycling Lithium Metal Batteries

Achieving durable lithium (Li) metal anodes in liquid electrolytes remains challenging, primarily due to the instability of the formed solid-electrolyte interphases (SEIs). Modulating the Li-ion solvation structures is pivotal in forming a stable SEI for stabilizing Li metal anodes. Here a strategy is developed to fine-tune the Li-ion solvation structures through enhanced dipole–dipole interactions between the Li-ion-coordinated solvent and the non-Li-ion-coordinating diluent, for creating a stable SEI in the developed binary salt electrolyte. The enhanced dipole–dipole interactions weaken the coordination between Li-ions and the solvents while strengthening the interaction between Li-ions and dual anions, thereby facilitating the Li-ion transport and a robust anion-derived SEI with a distinct bilayer structure. Consequently, the developed electrolyte exhibited exceptional electrochemical performance in high energy-density Li||LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cells, with long calendar life, stable cyclability at 1 C, and reliable operation between 25 and −20 °C, and it also demonstrat remarkable cycling stability for a Li||NMC811 pouch cell with projected energy density of 402 Wh kg −1 , maintaining 80% capacity retention over 606 cycles under practical conditions.

25 ENERGY STORAGE↗

Long cycle and calendar life of Si-based Li-ion batteries enabled by localized high-concentration electrolytes and their surprising water tolerance

Silicon-based anodes promise an increase in energy density for Li-ion batteries, yet they suffer from a poor calendar life. Researchers have posited that fluorinated lithium salt forms reactive side products that destroy the solid electrolyte interphase (SEI), even without cycling. HF is one such reactive side product formed from trace water contamination in the electrolyte. Some electrolytes, such as localized high concentration electrolytes (LHCEs) may improve cell stability in highly reactive systems, such as Li metal and Si. In the present study, LHCEs containing 200-300 ppm of water retained up to 8% greater capacity (1200-1300 mAh/g Si) in calendar life tests over 200 days compared to dried electrolytes (< 20 ppm water). Calendar aging took place at 100% state of charge. Cells with 200-300 ppm water performed comparably to cells with 20 ppm water in cycle life tests (900-1000 mAh/g Si) . Even adding 1000 ppm water did not lead to rapid capacity fade in cells undergoing cycle life tests. Nano-FTIR spectroscopy revealed chemical and structural differences in the SEI for cells with 1000 ppm water compared to 200-300 ppm water. The SEI differences, including increased Li2O concentration, may have contributed to improved calendar life. This research reveals the capabilities of LHCEs to improve the calendar and cycle life of Si-based Li-ion batteries, despite the presence of a highly reactive contaminant.

25 ENERGY STORAGE↗

Impact of dual-layer solid-electrolyte interphase inhomogeneities on early-stage defect formation in Si electrodes

While intensive efforts have been devoted to studying the nature of the solid-electrolyte interphase (SEI), little attention has been paid to understanding its role in the mechanical failures of electrodes. Here we unveil the impact of SEI inhomogeneities on early-stage defect formation in Si electrodes. Buried under the SEI, these early-stage defects are inaccessible by most surface-probing techniques. With operando full field diffraction X-ray microscopy, we observe the formation of these defects in real time and connect their origin to a heterogeneous degree of lithiation. This heterogeneous lithiation is further correlated to inhomogeneities in topography and lithium-ion mobility in both the inner- and outer-SEI, thanks to a combination of operando atomic force microscopy, electrochemical strain microscopy and sputter-etched X-ray photoelectron spectroscopy. Our multi-modal study bridges observations across the multi-level interfaces (Si/LixSi/inner-SEI/outer-SEI), thus offering novel insights into the impact of SEI homogeneities on the structural stability of Si-based lithium-ion batteries. Severe structural deformation during (de)lithiation is the main factor limiting the stability of Si anodes in Li-ion batteries. Here, a multi-modal approach is used to visualize these deformations in their early-stage and link them to inhomogeneities in the dual-layer solid-electrolyte interphase.

25 ENERGY STORAGE↗

Investigation of the Electrode-Electrolyte Interphase in Ester-Based Electrolytes in NCM523/Graphite Cells

The use of methyl acetate (MA) and methyl propionate (MP) as co-solvents in carbonate/LiPF 6 electrolytes have been investigated in LiNi 0.5 Co 0.2 Mn 0.3 O 2 (NCM523)/graphite cells to improve electrochemical performance at low temperature (−20 °C). Consistent with previous investigations, improved low temperature performance was observed with all electrolyte formulations containing esters. Detailed ex situ surface analysis of the surface films generated with the ester-based electrolytes containing electrolyte additives reveal significant changes to the SEI on graphite upon cycling at moderately elevated temperature (45 °C). In the presence of vinylene carbonate (VC) lithium plating is observed upon cycling at low temperature (−20 °C) which leads to a thicker solid electrolyte interface (SEI) upon cycling at 45 °C. Incorporation of fluoroethylene carbonate (FEC) as an electrolyte additive results in the generation of a thin SEI and alters the structure of the surface film on the NCM523 cathode resulting in stable cycling over a wide temperature range.

Rodrigo, Nuwanthi D. (ORCID:0000000343129536)↗