Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SEI”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Visualizing the SEI formation between lithium metal and solid-state electrolyte

The solid electrolyte interphase (SEI) is regarded as the most important factor affecting the durability of lithium-metal anode in all-solid-state batteries (ASSBs). Despite its significance, the nucleation and growth mechanism of SEI is not yet well understood. Here, we elucidate the thermodynamics and kinetics governing SEI formation at the Li|β-Li 3 PS 4 interface at the atomic scale via thermodynamic phase equilibrium analysis and machine-learning-potential-assisted molecular dynamics (MD) simulations. An accurate moment tensor potential using the machine-learning method is developed for a reactive model of Li|β-Li 3 PS 4 . This potential enabled us to perform large-scale MD simulations with the model size expanded to the experimental dimensions (~40 nm) while maintaining the same level of accuracy as density functional theory calculations. The results reveal a four-stage evolution process at the Li|β-Li 3 PS 4 interface, namely (i) fast ion diffusion, (ii) nucleation, (iii) Li 2 S growth, and (iv) stabilization. Notably, we demonstrate that the SEI can be categorized into crystalline and amorphous regions. The simulated SEI thickness, structure, and composition closely match experimental findings, validating the accuracy of the MD simulations. We further disclose the significant impact of ion diffusion kinetic limitations on the phase formation and crystallization of interfacial products. Furthermore, we shed light on the detailed potential energy (PE) distribution of lithium along the direction perpendicular to the interface. Finally, this information is crucial for better understanding interfacial ion mobility.

25 ENERGY STORAGE↗

Silicon Consortium Project: No-Go on Moir Interferometry for Measuring SEI Strain as a Probe for Calendar Life Testing

Silicon is a promising candidate as a next generation anode to replace or complement graphite electrodes due to its high energy density and low lithiation potential. When silicon is lithiated, it experiences over 300% expansion which stresses the silicon as well as its solid electrolyte interphase (SEI) leading to poor performance. The use of nano-sized silicon has helped to mitigate volume expansion and stress in the silicon, yet the silicon SEI is still both mechanically and chemically unstable. Identifying the mechanical failure mechanism of the SEI will help enhance calendar and cycle life performance through improved SEI design. In situ moiré interferometry was investigated to try and track the in-plane strain in the SEI and silicon electrode for this purpose. Moiré can detect on the order of 10 nm changes in displacement and is therefore a useful tool in the measurement of strain. As the sample undergoes small deformations, large changes in the moiré fringe allow for measurements of displacement below the diffraction limit of light. Figure 1a shows how the moiré fringe changes as the sample grating deforms. As the sample contracts or expands, the frequency of the moiré fringe changes, and this change is proportional to the strain in the sample.

36 MATERIALS SCIENCE↗

Quantifying Lithium Ion Exchange in Solid Electrolyte Interphase (SEI) on Graphite Anode Surfaces

Solid Electrolyte Interphase (SEI) has been identified as the most important and least understood component in lithium-ion batteries. Despite extensive studies in the past two decades, a few mysteries remain: what is the chemical form of and degree of mobility of Li + in the interphase? What fraction of Li + is permanently immobilized in the SEI, while the rest are still able to participate in the cell reactions via the ion-exchange process with Li + in the electrolyte? This study attempted to answer, in part, these questions by using 6 Li and 7 Li-isotopes to label SEIs and electrolytes, and then quantifying the distribution of permanently immobilized and ion-exchangeable Li + with solid-state NMR and ToF-SIMS. The results showed that the majority of Li + were exchanged after one SEI formation cycle, and a complete exchange after 25 cycles. Ion exchange by diffusion based on concentration gradient in the absence of applied potential also occurred simultaneously. This knowledge will provide a foundation for not only understanding but also designing better SEIs for future battery chemistries.

25 ENERGY STORAGE↗

Alumina – Stabilized SEI and CEI in Potassium Metal Batteries

Aluminum oxide (Al 2 O 3 ) nanopowder is spin-coated onto both sides of commercial polypropene separator to create artificial solid-electrolyte interphase (SEI) and artificial cathode electrolyte interface (CEI) in potassium metal batteries (KMBs). Here, this significantly enhances the stability, including of KMBs with Prussian Blue (PB) cathodes. For example, symmetric cells are stable after 1,000 cycles at 0.5 mA/cm 2 –0.5 mAh/cm 2 and 3.0 mA/cm 2 –0.5 mAh/cm 2 . Alumina modified separators promote electrolyte wetting and increase ionic conductivity (0.59 vs. 0.2 mS/cm) and transference number (0.81 vs. 0.23). Cryo-stage focused ion beam (cryo-FIB) analysis of cycled modified anode demonstrates dense and planar electrodeposits, versus unmodified baseline consisting of metal filaments (dendrites) interspersed with pores and SEI. Alumina-modified CEI also suppresses elemental Fe crossover and reduces cathode cracking. Mesoscale modeling of metal – SEI interactions captures crucial role of intrinsic heterogeneities, illustrating how artificial SEI affects reaction current distribution, conductivity and morphological stability.

25 ENERGY STORAGE↗

SEI formation mechanisms and Li + dissolution in lithium metal anodes: Impact of the electrolyte composition and the electrolyte-to-anode ratio

The lithium metal battery is one of today's most promising high-energy-density storage devices. Its full-scale implementation depends on solving operational and safety issues intrinsic to the Li metal high reactivity leading to uncontrolled electrolyte decomposition and uneven Li deposition. In this work, we study the spontaneous formation of the solid electrolyte interphase (SEI) upon contact of Li metal with the electrolyte and describe the heterogeneous SEI morphological features. Multiple electrolyte formulations based on lithium bis(fluorosulfonyl)imide (LiFSI), dimethoxyethane (DME), dimethyl carbonate (DMC), 1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) and bis(2,2,2-trifluoroethyl) ether (BTFE) are used. Findings include the description of the SEI evolution from dispersed LiO, LiS, LiN, and LiF clusters to a continuous and compact inorganic phase in which the LiO and LiF content depend on the presence of fluorine diluents. Further, the role of the DME ether solvent helping the growth of a “wet-SEI” is compared to that of the highly unstable carbonate DMC, which decomposes into complex radical oligomers that might contribute to further electrolyte decomposition. The impact of the electrolyte-to-anode ratio on LiFSI decomposition is highlighted. Finally, we suggest the existence of a critical LiFSI concentration and electrolyte-to-anode ratio that could potentially balance the rate of electrolyte depletion and lithium consumption.

25 ENERGY STORAGE↗

A Modified Sand’s Time Incorporating Li-Ion Transport Across the SEI: Basis for Understanding Li Dendrite Formation and Li-Metal Battery Electrolyte Selection

Abstract Understanding the initiation of lithium dendrites remains elusive, largely due to the intricate role of the solid electrolyte interphase (SEI) which forms on the Li surface during electrodeposition. Many studies have utilized the classical Sand’s equation to estimate the onset time when lithium dendrites begin to form. The Sand’s equation provides the time when the cation (Li+) concentration at the electrode-electrolyte interface approaches zero under diffusion-limited conditions in galvanostatic Li electrodeposition. However, recent experimental studies have revealed that the observed lithium dendrite onset time deviates considerably from the Sand’s time. Here, we show that this deviation from classical theory is likely due to the transport of Li+ ions through the SEI - a transport limitation that is much more dominant in controlling dendrite formation. We develop a ‘modified’ Sand's equation, incorporating the SEI layer and the diffusional transport across it to predict Li dendrite onset times. To validate this approach, we conducted Li electrodeposition experiments at various current densities using two distinct organic electrolytes. Analysis of the results demonstrates that the modified Sand's equation provides a more accurate prediction of dendrite onset times, highlighting the importance of incorporating SEI into transport models of Li plating in next-generation rechargeable Li-metal batteries.

Ma, Yuanman (ORCID:0000000200444811)↗

Quantifying SEI Reaction Rate in the Presence and Absence of Mn 2+

In this work, a methodology utilizing potentiostatic holds is developed for measuring side-reaction rates at graphite (Gr) electrodes. The influence of Mn 2+ on parasitic reactions is evaluated in the presence of various preformed solid-electrolyte interphases (SEI). Gr SEI preformation was carried out using vinylene carbonate (VC) or lithium difluoro(oxalato)borate (LiDFOB) as an additive. In addition, a highly fluorinated electrolyte, free of traditional non-fluorinated organic carbonates, was used. Parasitic current increases were observed for all preformed Gr SEIs when Mn 2+ was present. Of the preforming electrolytes, the VC-derived SEI showed the lowest parasitic currents both with and without Mn 2+ .

Tornheim, Adam [Argonne National Laboratory (ANL),↗

Interdependence of Support Wettability - Electrodeposition Rate- Sodium Metal Anode and SEI Microstructure

Here, this study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm -2 , 0.5–3 mA cm -2 ) representative of commercially relevant mass loading in anode-free sodium metal battery (AF-SMBs) are analyzed. Synchrotron X-ray nanotomography and grazing-incidence wide-angle X-ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo-FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te-Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

36 MATERIALS SCIENCE↗

The Effect of Artificial SEIs on Lithium Metal Anode Morphology and Conductivity

Lithium metal has often been termed the “holy grail” of battery technology, due to its high capacity (2,061 mAh/cm3) and low electrochemical potential (-3.04 V vs. SHE). However, lithium’s beneficially low potential also causes it to be highly reactive in the presence of organic solvents, making it difficult to harness the high energy capabilities for rechargeable batteries. Common failure of lithium metal batteries occurs by rapid dendrite growth leading to a hazardous short-circuit. Various methods have been brought forth to better understand the fundamental mechanisms of lithium metal batteries, as well as modifications made to better stabilize lithium metal. A common route of modification is done through interface engineering, with attempts to artificially provide a stable, homogeneous solid-electrolyte interface (SEI). The stability of the SEI has direct effects on the heterogeneity of the electrode surface, which initiates a waterfall effect of for progressive reactions such as dendrite growth, dead lithium accumulation, and electrolyte consumption. This work aims to produce a mixed LiI-LiF artificial SEI to improve ionic conductivity while retaining a high elastic modulus.

25 ENERGY STORAGE↗

Interdependence of Support Wettability ‐ Electrodeposition Rate‐ Sodium Metal Anode and SEI Microstructure

Abstract This study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm −2 , 0.5–3 mA cm −2 ) representative of commercially relevant mass loading in anode‐free sodium metal battery (AF‐SMBs) are analyzed. Synchrotron X‐ray nanotomography and grazing‐incidence wide‐angle X‐ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo‐FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te−Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

Lo, Chang‐An↗

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

Abstract The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high‐energy‐density sodium metal batteries. Herein, a hybrid SEI layer containing Li‐species is dexterously constructed on the surface of sodium metal anode. Li‐containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite‐free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra‐high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Xia, Li [State Key Laboratory of Physical Chemistr↗

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high-energy-density sodium metal batteries. Herein, a hybrid SEI layer containing Li-species is dexterously constructed on the surface of sodium metal anode. Li-containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite-free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra-high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Diffusion kinetic↗

Materials Data on Nb(SeI)2 by Materials Project

Nb(SeI)2 crystallizes in the monoclinic C2/m space group. The structure is two-dimensional and consists of one Nb(SeI)2 sheet oriented in the (0, 0, 1) direction. Nb5+ is bonded in a 8-coordinate geometry to four Se+1.50- and four equivalent I1- atoms. There are two shorter (2.64 Å) and two longer (2.66 Å) Nb–Se bond lengths. There are two shorter (3.00 Å) and two longer (3.01 Å) Nb–I bond lengths. There are two inequivalent Se+1.50- sites. In the first Se+1.50- site, Se+1.50- is bonded in a 2-coordinate geometry to two equivalent Nb5+ atoms. In the second Se+1.50- site, Se+1.50- is bonded in a 2-coordinate geometry to two equivalent Nb5+ atoms. I1- is bonded in a distorted water-like geometry to two equivalent Nb5+ atoms.

36 MATERIALS SCIENCE↗

A Carboranyl Electrolyte Enabling Highly Reversible Sodium Metal Anodes via a “Fluorine‐Free” SEI

Abstract Realization of practical sodium metal batteries (SMBs) is hindered due to lack of compatible electrolyte components, dendrite propagation, and poor understanding of anodic interphasial chemistries. Chemically robust liquid electrolytes that facilitate both favorable sodium metal deposition and a stable solid‐electrolyte interphase (SEI) are ideal to enable sodium metal and anode‐free cells. Herein we present advanced characterization of a novel fluorine‐free electrolyte utilizing the [HCB 11 H 11 ] 1− anion. Symmetrical Na cells operated with this electrolyte exhibit a remarkably low overpotential of 0.032 V at a current density of 2.0 mA cm −2 and a high coulombic efficiency of 99.5 % in half‐cell configurations. Surface characterization of electrodes post‐operation reveals the absence of dendritic sodium nucleation and a surprisingly stable fluorine‐free SEI. Furthermore, weak ion‐pairing is identified as key towards the successful development of fluorine‐free sodium electrolytes.

Tomich, Anton W.↗

A Carboranyl Electrolyte Enabling Highly Reversible Sodium Metal Anodes via a “Fluorine-Free” SEI

Realization of practical sodium metal batteries (SMBs) is hindered due to lack of compatible electrolyte components, dendrite propagation, and poor understanding of anodic interphasial chemistries. Chemically robust liquid electrolytes that facilitate both favorable sodium metal deposition and a stable solid-electrolyte interphase (SEI) are ideal to enable sodium metal and anode-free cells. Herein we present advanced characterization of a novel fluorine-free electrolyte utilizing the [HCB 11 H 11 ] 1- anion. Symmetrical Na cells operated with this electrolyte exhibit a remarkably low overpotential of 0.032 V at a current density of 2.0 mA cm -2 and a high coulombic efficiency of 99.5 % in half-cell configurations. Additionally, surface characterization of electrodes post-operation reveals the absence of dendritic sodium nucleation and a surprisingly stable fluorine-free SEI. Furthermore, weak ion-pairing is identified as key towards the successful development of fluorine-free sodium electrolytes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Unravelling fast-charging degradation in NMC/Gr pouch cells: Lithium plating and SEI properties

As fast-charging technology expands across the electric vehicle and emerging energy-storage applications, understanding its impact on battery performance and longevity is critical. In this study, 1.8 Ah LiNi 0.6 Mn 0.2 Co 0.2 O 2 /graphite pouch cells were charged at various charging rates (0.5C, 2C, 4C, and 6C) to investigate the degradation mechanisms. Our results showed that well-designed NMC/Gr pouch cells could reach over 1000 cycles with a 2C charging rate, while only reaching around 500 cycles with 4C and 6C charging rates. Fast-charging effects on NMC and graphite electrodes were obtained through a series of post-mortem characterizations, including electrochemical impedance spectroscopy (EIS), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS). Although higher charging rates cause pulverization of NMC secondary particles, the dominant degradation mechanism driving the fading of fast-charging-related performance lies in the graphite anode, where lithium plating and LiF-rich solid electrolyte interphase (SEI) formation result in Li inventory loss and impedance growth. The postmortem results suggest that the formation of a LiF-rich SEI, which exacerbates anode impedance and some irreversible Li + ion loss, is likely driven by the substantial decomposition of PF 6 − during fast charging, an effect often overlooked in smaller laboratory-scale studies.

Luo, Mei [Argonne National Laboratory (ANL), Argon↗

Understanding the Role of SEI Layer in Low-Temperature Performance of Lithium-Ion Batteries

Low-temperature electrolytes (LTEs) have been considered as one of the most challenging aspects for the wide adoption of lithium-ion batteries (LIBs) since the SOA electrolytes cannot sufficiently support the redox reactions at LT resulting in dramatic performance degradation. Although many attempts have been taken by employing various noncarbonate solvent electrolytes, there was a lack of fundamental understanding of the limiting factors for low-temperature operations (e.g., -20 to -40 degrees C). Here, the crucial role of the solid-electrolyte-interface (SEI) in LIB performance at low temperature using a butyronitrile (BN)-based electrolyte was demonstrated. These results suggested that an additive formed SEI with low resistance and low charge transfer dictates the LT performance in terms of capacity and cycle life, presenting a useful guideline in designing new electrolytes to address the LT issue.

25 ENERGY STORAGE↗