At least 37 records · Page 2

Substrate With Low Secondary Emissions

The present invention is directed to a method and apparatus for producing a highly -textured surface on a copper substrate -with only extremely small amounts of texture-inducing seeding or masking material. The texture-inducing seeding material is delivered to the copper substrate electrically switching the seeding material in and out of a circuit loop.

Jensen, Kenneth A.

Secondary Electron Emission Yields

The secondary electron emission (SEE) characteristics for a variety of spacecraft materials were determined under UHV conditions using a commercial double pass CMA which permits sequential Auger electron electron spectroscopic analysis of the surface. The transparent conductive coating indium tin oxide (ITO) was examined on Kapton and borosilicate glass and indium oxide on FED Teflon. The total SEE coefficient ranges from 2.5 to 2.6 on as-received surfaces and from 1.5 to 1.6 on Ar(+) sputtered surfaces with 5 nm removed. A cylindrical sample carousel provides normal incidence of the primary beam as well as a multiple Faraday cup measurement of the approximately nA beam currents. Total and true secondary yields are obtained from target current measurements with biasing of the carousel. A primary beam pulsed mode to reduce electron beam dosage and minimize charging of insulating coatings was applied to Mg/F2 coated solar cell covers. Electron beam effects on ITO were found quite important at the current densities necessary to do Auger studies.

Krainsky, I.

Effects of Surface Treatments on Secondary Electron Emission from CVD Diamond Films

Secondary electron emission (SEE) properties of polycrystalline diamond films grown by chemical vapor deposition (CVD) were measured. The total secondary yield (sigma) from as-grown samples was observed to be as high as 20 at room temperature and 48 while heating at 700 K in vacuum. Electron-beam-activated, alkali-terminated diamond films have shown stable values of sigma as high as 60 when coated with CsI and similarly high values when coated with other alkali halides. Diamond coated with BaF2 had a stable sigma of 6, but no enhancement of the SEE properties was observed with coatings of Ti or Au. Hydrogen was identified to give rise to this effect in as-grown films. However, electron beam exposure led to a reduction in sigma values as low as 2. Exposure to a molecular hydrogen environment restored sigma to its original value after degradation, and enabled stable secondary emission during electron beam exposure. Atomic hydrogen and hydrogen plasma treatments were performed on diamond/Mo samples in an attempt to increase the near-surface hydrogen concentration which might lead to increased stability in the secondary emission. Raman scattering analysis, scanning electron microscopy, and Auger electron spectroscopy (AES) confirmed that hydrogen plasma and atomic hydrogen treatments improved the quality of the CVD diamond significantly. Elastic recoil detection (ERD) showed that heating as-grown diamond targets to 7OO K, which was correlated with an increase in sigma, removed contaminants from the surface but did not drive hydrogen from the diamond bulk. ERD showed that the hydrogen plasma treatment produced an increase in the hydrogen concentration in the near-surface region which did not decrease while heating in vacuum at 700 K, but no improvement in the SEE properties was observed.

Mearini, G. T.

Secondary Electron Emission and the Exploration of Space

The emission of secondary electrons from surfaces exposed to the space plasma and radiation environment is a process of great importance to space system engineering design and operations. A spacecraft will collect charge until it reaches an equilibrium potential gov,erned by the balance of incoming electron and ion currents from the space environment with outgoing secondary, backscattered, and photoelectron currents. Laboratory measurements of secondary electron yields are an important parameter for use in spacecraft charging analyses because the magnitude and sign of the equilibrium potential depends on both the energy spectrum of electrons and ions in the space environment and the electrical properties of the surface materials (including the energy dependent secondary electron yields). Typical benign equilibrium potentials range &om a few tens of volts positive in interplanetary space to a few volts negative in low Earth orbit. However, spacecraft are known to charge to negative potentials exceeding one to ten kilovolts in some environments and anomalies or system failures due to electrostatic discharges originating from highly charged surfaces becomes a serious concern. This presentation will provide a review of the spacecraft charging process with special emphasis on the role of secondary electrons in controlling the current balance process. Charging examples will include spacecraft in Earth orbit and interplanetary space as well as dust charging on the lunar surface, a phenomenon of importance to future lunar surface operations.

Minow, Joseph I.

Role of grain size and particle velocity distribution in secondary electron emission in space plasmas

By virtue of being generally immersed in a plasma environment, cosmic dust is necessarily electrically charged. The fact that secondary emission plays an important role in determining the equilibrium grain potential has long been recognized, but the fact that the grain size plays a crucial role in this equilibrium potential, when secondary emission is important, has not been widely appreciated. Using both conducting and insulating spherical grains of various sizes and also both Maxwellian and generalized Lorentzian plasmas (which are believed to represent certain space plasmas), we have made a detailed study of this problem. In general, we find that the secondary emission yield delta increases with decreasing size and becomes very large for grains whose dimensions are comparable to the primary electron penetration depth, such as in the case of the very small grains observed at comet Halley and inferred in the interstellar medium. Moreover, we observed that delta is larger for insulators and equilibrium potentials are generally more positive when the plasma has a broad non-Maxwellian tail. Interestingly, we find that for thermal energies that are expected in several cosmic regions, grains of different sizes can have opposite charge, the smaller ones being positive while the larger ones are negative. This may have important consequences for grain accretion in polydisperse dusty space plasmas.

Chow, V. W.

Effects of secondary electron emission on charging

Laboratory charging studies using two electron sources with different energies show that the charging behaviors of typical spacecraft thermal control dielectric surface are extremely sensitive to the shape of their secondary emission curves. The results also suggest that the electron spectrum in a natural charging environment can be separated into three distinct regions (noninteracting, discharging, and charging) depending on the kinetic energy of the incident electron relative to the charged surface, and on the secondary emission characteristics of the material. To a first order approximation, the relative number of electrons in these different regions determines the potential of the charged surface. Detailed measurements of the secondary electron emission characteristics of Kapton, the effects of bulk conductivity and secondary emission on surface charging of these materials is reported.

Leung, M. S.

Textured carbon on copper: A novel surface with extremely low secondary electron emission characteristics

Experimentally determined values of true secondary electron emission and relative values of reflected primary electron yield for a range of primary electron beam energies and beam impingement angles are presented for a series of novel textured carbon surfaces on copper substrates. (All copper surfaces used in this study were oxygen-free, high-conductivity grade). The purpose of this investigation is to provide information necessary to develop high-efficiency multistage depressed collectors (MDC's) for microwave amplifier traveling-wave tubes (TWT's) for communications and aircraft applications. To attain the highest TWT signal quality and overall efficiency, the MDC electrode surface must have low secondary electron emission characteristics. While copper is the material most commonly used for MDC electrodes, it exhibits relatively high levels of secondary electron emission unless its surface is treated for emission control. The textured carbon surface on copper substrate described in this report is a particularly promising candidate for the MDC electrode application. Samples of textured carbon surfaces on copper substrates typical of three different levels of treatment are prepared and tested for this study. The materials are tested at primary electron beam energies of 200 to 2000 eV and at direct (0 deg) to near-grazing (85 deg) beam impingement angles. True secondary electron emission and relative reflected primary electron yield characteristics of the textured surfaces are compared with each other and with those of untreated copper. All the textured carbon surfaces on copper substrate tested exhibited sharply lower secondary electron emission characteristics than those of an untreated copper surface.

Curren, A. N.

Secondary-electron-emission properties of conducting surfaces with application to multistage depressed collectors for microwave amplifiers

To improve the efficiency of high power microwave tubes, low secondary electron yield electrode surface for use in depressed collectors are needed. The secondary emission characteristics of a number of materials were investigated. The materials studied were beryllium, carbon (soot and pyrolytic graphite), copper, titanium carbide, and tantalum. Both total secondary yield delta and relative reflected primary yield were measured. These measurements were made in conjunction with Auger spectroscopy so that the secondary emission characteristics could be determined as a function of surface contamination or purity. The results show that low atomic weight elements, such as beryllium and carbon, have the lowest reflected primary yield and that roughening the surface of an electrode can markedly decrease secondary yield both for delta and reflected primaries. All factors considered, a roughened pyrolytic graphite surface showed the greatest potential for use as an electrode surface in depressed collectors.

Forman, R.

Secondary electron emission properties of conducting surfaces for use in multistage depressed collectors

An Auger spectrometer in ultrahigh vacuum was used to measure the secondary emission properties of a number of candidate collector-materials including beryllium, carbon, (soot and pyrolytic graphite), copper, titanium carbide and tantalum. The advantage of the technique used is that the surface chemical constituents could be determined just before the secondary emission characteristics of the surface were measured. Pyrolytic graphite roughened by sputter etching showed the most favorable results for depressed collector use.

Forman, R.

Secondary electron emission characteristics of untreated and ion-textured titanium

Experimentally determined values of true secondary electron emission and relative values of reflected primary electron yield are presented for untreated (simply machined) and ion-textured, high-purity titanium over ranges of primary electron beam energies and beam impingement angles. The purpose of the investigation was to explore the feasibility of using titanium as electrode material in the multistage depressed collectors (MDC's) used in microwave amplifier traveling wave tubes (TWT's) for space communications and aircraft applications. Because of its relatively low density and thermal expansion characteristics and relatively high strength, thermal emissivity, and melting temperature, titanium presents itself as a possible candidate for the MDC electrode application. A detailed description of the method of ion texturing the titanium is included. Although the ion-treated surface considered in this study is not presented as being optimum from the standpoint of secondary electron emission suppression, it nevertheless serves to demonstrate that the surface can be modified by this procedure to significantly reduce these emission characteristics relative to those of the untreated surface. Further studies can reasonably be expected to produce surfaces with even lower secondary emission characteristics. The titanium surface were tested at primary electron beam energies of 200 to 2000 eV and at direct (0 deg) to near-grazing (85 deg) beam impingement angles. True secondary electron emission and relative reflected primary electron yield characteristics of the surfaces were compared with each other and with textured titanium surface exhibited secondary electron emission characteristics sharply lower than those exhibited by untreated titanium or copper. Clearly, then, in consideration of the secondary electron emission suppression of ion-textured titanium along with its other favorable physical properties, it must be included as a potential candidate for use as MDC electrode material in some applications.

Curren, Arthur N.

Determination of secondary electron emission characteristics of lunar soil samples

A procedure is described for the determination of the 'apparent crossover voltage', i.e. the value of the primary (bombarding) electron energy at which an insulating sample surface changes the average sign of its charge. This apparent crossover point is characteristic of the secondary emission properties of insulating powders such as the lunar soil samples. Lunar core samples from well-defined, distinct soil layers are found to differ significantly in their secondary emission properties. This observation supports the suggestion that soil layers were deposited by an electrostatic transport process.

Gold, T.

Process reduces secondary resonant emission in electronic components

Process reduces secondary electron emission in coaxial connector and in waveguides in the atmosphere. The assembly is placed in a vacuum chamber and is gradually vented to the atmosphere. It is exposed to high voltage, argon gas, and a hydrocarbon gas during the process.

Erpenbach, H.

Study of the Effects of the Electric Field on Charging Measurements on Individual Micron-size Dust Grains by Secondary Electron Emissions

The dust charging by electron impact is an important dust charging process in Astrophysical, Planetary, and the Lunar environments. Low energy electrons are reflected or stick to the grains charging the dust grains negatively. At sufficiently high energies electrons penetrate the grain leading to excitation and emission of electrons referred to as secondary electron emission (SEE). Available theoretical models for the calculation of SEE yield applicable for neutral, planar or bulk surfaces are generally based on Sternglass Equation. However, viable models for charging of individual dust grains do not exist at the present time. Therefore, the SEE yields have to be obtained by some experimental methods at the present time. We have conducted experimental studies on charging of individual micron size dust grains in simulated space environments using an electrodynamic balance (EDB) facility at NASA-MSFC. The results of our extensive laboratory study of charging of individual micron-size dust grains by low energy electron impact indicate that the SEE by electron impact is a very complex process expected to be substantially different from the bulk materials. It was found that the incident electrons may lead to positive or negative charging of dust grains depending upon the grain size, surface potential, electron energy, electron flux, grain composition, and configuration. In this paper we give a more elaborate discussion about the possible effects of the AC field in the EDB on dust charging measurements by comparing the secondary electron emission time-period (tau (sub em) (s/e)) with the time-period (tau (sub ac) (ms)) of the AC field cycle in the EDB that we have briefly addressed in our previous publication.

Tankosic, D.

Beam impingement angle effects on secondary electron emission characteristics of textured pyrolytic graphite

Experimentally determined values of true secondary electron emission and relative values of reflected primary electron yield for untreated and ion-textured pyrolytic graphite over a range of primary electron energy levels and electron beam impingement angles are presented. Information required to develop high efficiency multistage depressed collectors (MDC's) for microwave amplifier traveling-wave tubes for space communication and aircraft applications is provided. To attain the highest possible MDC efficiencies, the electrode surfaces must have low secondary electron emission characteristics. Pyrolytic graphite, a chemically vapor-deposited material, is a particularly promising candidate for this application. The pyrolytic graphite surfaces studied were tested over a range of primary electron beam energies and beam impingement angles from 200 to 2000 eV and direct (0 deg) to near-grazing angles (85 deg), respectively. Surfaces both parallel to and normal to the planes of material deposition were examined. The true secondary electron emission and reflected primary electron yield characteristics of the pyrolytic graphite surfaces are compared to those of sooted control surfaces.

Curren, A. N.

Secondary electron emission from a charged dielectric in the presence of normal and oblique electric fields

The secondary electron emission coefficient was obtained for a FEP-Teflon dielectric charged with monoenergetic electrons normally incident upon the surface of the specimen. Measurements of secondary emission coefficient were done for normal and oblique incidence with different primary beam energies in the presence of normal and oblique electric fields. A collimated probing beam was directed to different points on the surface of the specimen and the released or accumulated charge was monitored using an electrometer. The measured data for different probing beam energies, different impact points and different angles of incidence were plotted vs. impact energy and impact point. Data analyzed by computer simulations to find the potential distribution on the surface of the specimen and the electric field around it, is presented and discussed.

Javidi, B.