Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Recrystallized grain size”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

The effect of solute additions on the steady-state creep behavior of dispersion-strengthened aluminum.

The effect of solute additions on the steady-state creep behavior of coarse-grained dispersion-strengthened aluminum alloys was studied. Recrystallized dispersion-strengthened solid solutions were found to have stress and temperature sensitivities quite unlike those observed in single-phase solid solutions having the same composition and grain size. The addition of magnesium or copper to the matrix of a recrystallized dispersion-strengthened aluminum causes a decrease in the steady-state creep rate which is much smaller than that caused by similar amounts of solute in single-phase solid solutions. All alloys exhibited essentially a 4.0 power stress exponent in agreement with the model of Ansell and Weertman. The activation energy for steady-state creep in dispersion-strengthened Al-Mg alloys, as well as the stress dependence, was in agreement with the physical model of dislocation climb over the dispersed particles.

Reynolds, G. H.↗

An electron microscopy examination of primary recrystallization in TD-nickel.

Primary recrystallization in TD-nickel 1 in. bar has previously been regarded as the process by which the initial fine grain structure is converted to a coarse grain size (increases in grain size by 500 times) under suitable deformation and annealing conditions. This process is dependent on deformation mode. While it occurs readily after rolling transverse to the bar axis and annealing (800 C), it is completely inhibited by longitudinal rolling and swaging deformations, even for very high (1320 C) annealing temperatures. A transmission electron microscopy examination of deformation and annealing substructures indicates that primary recrystallization in TD-nickel 1 in. bar actually occurs on the sub-light optical level, to produce a grain structure similar in size to the initial fine grained state.

Petrovic, J. J.↗

Post-igneous redistribution of components in eucrites

In our analyses, we utilize a microdrilling technique that removes 40 to 100 micron diameter cores from mineral grains in thin sections analyzed by microprobe. The cores are then analyzed by INAA using the technique of Lindstrom. Three eucrites were selected for application of this analytical technique: monomict breccias Pasamonte and Stannern and unbrecciated EET90020. Pasamonte is among the most unequilibrated of the eucrites on the basis of zoning in pyroxenes and is considered to be an igneous rock not significantly affected by metamorphism. Stannern has igneous texture but its pyroxenes indicate some re-equilibration, although little, if any, recrystallization. EET90020 has a granulite texture and has been substantially recrystallized. Our sample of Pasamonte contains several clasts of different grain sizes ranging from glass to fine grained with diabasic texture containing lathy plagioclase, unexsolved pigeonite, and mesostasis. Cores were taken of the glass and from minerals and mesostases in six lithic clasts which normally allowed sampling of more than one phase per clast. Our sample of Stannern is also a breccia but with little difference in grain size between clasts and matrix. The plagioclase and pigeonite are blocky, twinned, and exsolved and coexist with a bit of mesostasis. Cores were taken of plagioclase and pigeonite with no attempt to distinguish separate clasts. EET90020 is a granular mixture of twinned plagioclase and pigeonite having rather uniform size and many triple junctions. Several cores were taken of both phases. Both clear and cloudy grains of plagioclase and pyroxene were sampled in all three eucrites.

Phinney, W. C.↗

Spatial U-Pb Age Distribution in Shock-Recrystallized Zircon – A Case Study from the Rochechouart Impact Structure, France

Age determination of impact structures via the zircon U–Pb system remains challenging and often ambiguous due to highly variable effects of shock metamorphism on U-Pb geochronology. It is, therefore, crucial to link the observed zircon microtextures, including their temperature and pressure conditions associated with their formation, directly to the U–Pb ages preserved. Here, we analyzed three recrystallized zircon grains and one plastically deformed zircon crystal from the medium-sized Rochechouart impact structure in the northwestern Massif Central of France. For the Rochechouart impact structure the impact age (206.92 ± 0.32 Ma [40Ar/39Ar]) as well as the 2 tectono-themal history is well established making this study site ideal to test concepts about U-Pb systematics in shocked zircon and to differentiate between shock-driven age resetting and preimpact crystallization and metamorphic overprinting. Zircon microstructures were studied using scanning electron imaging, cathodoluminescence imaging, and electron backscatter diffraction (EBSD) mapping. Further, we conducted U–Pb Laser Ablation Inductively Coupled Plasma Mass Spectrometry (LA-ICP-MS) depth-profiling analysis, allowing us to interpret the resultant age data in discrete steps with increasing ablation time/depth. The U–Pb depth profiling data demonstrate that plastically strained grains are incompletely reset and preserve rim and interior age domains reflecting typical pre-impact (pre-Variscan and Variscan) regional tectonic ages. Our results also reveal that the granular crystals encountered contain microstructural evidence for “former reidite in granular neoblastic” (FRIGN) zircon, reflecting both high-pressure (⩾30GPa) and high temperature (⩾1200℃) conditions. This signifies that FRIGN zircon is now known from an additional, medium sized, impact structure further supporting the hypothesis that this impact induced microstructure is commonly preserved. In addition, FRIGN zircon has a high potential to preserve completely impact-reset crystal domains (~204 to 207 Ma) that can be identified by our combined analytical approach of U–Pb depth profiling and EBSD mapping, and thus are suitable for determining reliable impact ages

U-Pb depth profiling↗

Impact of Powder Variability on the Microstructure and Mechanical Behavior of Selective Laser Melted Alloy 718

Powder-bed additive manufacturing processes use fine powders to build parts layer-by-layer. Alloy 718 powder feedstocks for selective laser melting (SLM) additive manufacturing are produced commercially by both gas and rotary atomization and are available typically in the 10-45 or 15-45 microns size ranges. A comprehensive investigation was conducted to understand the impact of powder variability on the microstructure and mechanical behavior of SLM 718 heat treated to Aerospace Material Specification (AMS) 5664. This study included sixteen virgin powders and three once-recycled powders within the 10-45 and 15-45 microns size ranges that were obtained from seven direct source suppliers and one reseller. Although alike as highly regular spheroids, these powders showed distinct differences in composition (especially Al, C and N contents), particle size distributions, and powder features such as degree of agglomeration, fusion and surface roughness. Compositional differences expectedly had the strongest impact on microstructure. High N and C contents formed TiN-nitrides and/or (Nb,Ti,Mo)-C carbides on the grain boundaries, prevented recrystallization during heat treatment, and resulted in retained (001)-scalloped shaped grains that ranged from 19 to 41 microns in average size. In the absence of this particle pinning, the average grain size of the heat treated SLM 718 ranged from 51 microns to 90 microns. Room temperature tensile and high cycle fatigue (HCF) testing compared as-fabricated (AF) and low stress ground (LSG) surface conditions. Tensile testing revealed consistent behavior between the two surface conditions and amongst the powder lots. The finer grained SLM 718 builds displayed the lowest tensile properties. A SLM 718 build fabricated from a powder with eight times lower C content showed statistically better tensile properties presumably due to enhanced coarsening of (delta)-Ni3Nb precipitates. The specimens from once-recycled powders had slightly higher tensile strengths and slightly higher ductility compared to their virgin equivalents; once-recycling also did not substantially degrade the mean HCF life. The LSG fatigue lives agreed with conventionally manufactured 718 data, while AF lives exhibited a knock-down due to surface roughness. The fatigue lives of AF specimens were statistically equivalent across powder lots except for one and failures typically initiated at stress concentrators associated with SLM surface asperities. Fatigue testing of low stress ground specimens result in both transgranular and within facet crack initiations. More than half of the cracks initiated from these facets for the machined condition; however, these facets appeared to be within grains that were larger-than-average in size. A nitrogen-atomized powder with fine prior particles of TiN-nitrides and M(Ti,Nb,Mo)C carbides from atomization on powder surfaces resulted in the best fatigue performance with segregation of these particles to the SLM 718 grain boundaries leading to higher resistance to early-stage crack propagation. Typically the fine-grained builds with minor phases along the grain boundaries did not perform well in fatigue, whereas a larger-grain build with lower carbon content and coarser delta-Ni3Nb precipitates showed the next best HCF response. Further details of the build microstructure and its impact on tensile and fatigue behavior was considered.

laser deposition↗

Net Shaped Component Fabrication of Refractory Metal Alloys using Vacuum Plasma Spraying

The vacuum plasma spraying (VPS) technique was employed to produce dense and net shaped components of a new tungsten-rhenium (W-Re) refractory metal alloy. The fine grain size obtained using this technique enhanced the mechanical properties of the alloy at elevated temperatures. The alloy development also included incorporation of thermodynamically stable dispersion phases to pin down grain boundaries at elevated temperatures and thereby circumventing the inherent problem of recrystallization of refractory alloys at elevated temperatures. Requirements for such alloys as related to high temperature space propulsion components will be discussed. Grain size distribution as a function of cooling rate and dispersion phase loading will be presented. Mechanical testing and grain growth results as a function of temperature will also be discussed.

Sen, S.↗

Petrography and preliminary interpretations of the crystalline breccias from the Manson M-1 core

The M-1 core was drilled on the eastern edge of the central uplift within the Manson Impact Structure in Iowa. The lower 107.9 m of the core consists of crystalline breccias. Twelve intervals of thin sections from this core have been studied for preliminary discussion. The breccias are divided into three units by matrix size and abundance. Unit 1 is characterized by a high volume fraction of matrix, and a decreasing proportion of matrix with depth. This matrix is nearly isotropic and consists of grains less than 0.005 to less than 0.02 mm in length. The matrix between 112 and 146 meters depth consists of a crystalline intergrowth of felsic and opaque minerals with or without chlorite. This was the hottest section of the core after impact, and may have undergone high temperature metamorphic recrystallization. Unit 2 is transitional between units 1 and 3, and is delineated by a rapid increase in grain size to .01-.04 mm and a decrease in matrix abundance to 10 percent. Unit 3 has a coarse, often porous matrix, whose abundance changes from about 10 percent at the top to about 2 percent at the base. Grain sizes range from 0.01-0.1 mm over this interval and coarsen with depth. Changes in the character of the matrix as well as the changes in clast lithology and abundance outlined below suggest that unit 3 is in-situ brecciated basement with injected melt and shale fragments; unit 1 is a crater veneer deposit consisting of transported basement materials and unit 2 is a mixed zone between units 1 and 3.

Bell, M. S.↗

Abnormal grain growth in TD-nickel.

Characteristics of the coarse grain transformation occurring in TD-nickel 1 in. bar under certain conditions of deformation and annealing were examined. The transformation exhibits Avrami-type kinetics, with an activation energy of 250 kcal per mole. Characteristics of untransformed regions are like those of the as-received state. The transformed grain size increases with increasing deformation and decreasing annealing temperature. The coarse grain transformation is significantly different from primary recrystallization in pure nickel. Its characteristics cannot be rationalized in terms of primary recrystallization concepts, but may be explained in terms of an abnormal grain growth description. The coarse grain transformation in TD-nickel is abnormal grain growth rather than primary recrystallization. The analysis suggests an explanation for the effect of thermomechanical history on the deformation and annealing behavior of TD-nickel.

Petrovic, J. J.↗

Deformation and annealing response of TD-nickel chromium sheet

The deformation and annealing response of TD-nickel chromium (TD-NiCr) 0.1 inch thick sheet was examined using various cold-rolling and annealing treatments. Upon annealing (above 816 C (1500 F), the as-received material was converted from an initially ultra-fine grain size (average grain dimension 0.51 micron) to a large grain structure. Increases in grain size by a factor of 100 to 200 were observed for this transformation. However, in those material states where the large grain transformation was absent, a fine grain recrystallized structure formed upon annealing (above 732 C (1350 F)). The deformation and annealing response of TD-NiCr sheet was evaluated with respect to the processing related variables as mode and severity of deformation and annealing temperature. Results indicate that the large grain transformation, classical primary recrystallization occurs. Using selected materials produced during the deformation and annealing study, the elevated temperature tensile properties of TD-NiCr sheet were examined in the temperature range 593 C (1100 F) to 1093 C (2000 F). It was observed that the elevated temperature tensile properties of TD-NiCr sheet could be optimized by the stabilization of a large grain size in this material using the cold working and/or annealing treatments developed during the present investigation.

Kane, R. D.↗

Chondrules in Apollo 14 samples and size analyses of Apollo 14 and 15 fines.

Chondrules have been observed in several breccia samples and one fines sample returned by the Apollo 14 mission. The chondrules are formed by at least three different processes that appear to be related to large impacts: (1) crystallization of shock-melted spherules and droplets; (2) rounding of rock clasts and mineral grains by abrasion in the base surge; and (3) diffusion and recrystallization around clasts in hot base surge and fall-back deposits. In the case of the Apollo 14 samples, the large impact almost certainly is the Imbrian event. Grain size analyses of undisturbed fines samples from the Apollo 14 site and from the Apollo 15 Apennine Front are almost identical, indicating that the two localities have similar meteoroid bombardment exposure ages, approximately 3.7 x 10 to the 9th yr. This observation is consistent with the interpretation that both the Fra Mauro formation and the Apennine Front material originated as ejecta from the Imbrian event.

King, E. A., Jr.↗

The strength and ductility of polycrystalline NiAl in tension

Experiments at temperatures from 20 C to 400 C at two strain rates (.0001/s and .000005/s) establish that: (1) at room temperatures, binary and microalloyed ( 1000 ppm La, Y, Mo, Ti) NiAl shows negligible ductility, independent of grain size over the range 5 to 140 micrometers; (2) at 295 C the tensile elongation of binary 51 Ni/49 Al increases from 1% to about 5% upon decreasing the grain size to below approximately 10 micrometers; (3) similarly, at 400 C the ductility increases from about 2% to 15% upon decreasing the grain size to below 15 micrometers; (4) the ductility of fine grained (7 micrometer) binary aggregates deformed at 295 C increases from approximately 5% to 12% upon decreasing the strain rate from .0001/s to .000005/s; (5) partial recrystallization (10% to 20%) of warm extruded binary and microalloyed material imparts 1% to 2% ductility at room temperature where fully recrystallized material is brittle; (6) the yield strength obeys a Hall-Petch relationship; and (7) when ductility is not observed, fracture coincides with yielding. The mechanisms underlying the flow and fracture of NiAl are discussed in terms of the nucleation and growth of microcracks. The concept of a critical grain size is considered in the light of the results.

Schulson, E. M.↗

Mineralogical Analysis of Calcium-Aluminum-Rich Inclusions Provides Insight Into Post-Formation Processes

Introduction: Calcium-aluminum inclusions (CAIs) are cm- to mm-sized intergrowths of refractory phases found in chondritic meteorites [1]. Their mineral compositions closely match the compositions of the solids thought to condense from an extremely hot (>1500K) gas with a bulk solar composition [2-4], suggesting that CAIs were the earliest solids within the Solar System [2-4]. These inclusions provide invaluable insights into the conditions and dynamics of the early Solar System. CAIs must be transported from their formation region near the protosun to the chondrite parent-body accretion region. The nature of their journey could affect how, when, and where the secondary processes recorded in these CAIs occurred [4]. Did these secondary processes occur in the solar nebula or during accretion with the parent body, or both? How were the CAIs affected by varying thermochemical processes? To better answer these questions, we have undertaken an in-depth, textural study of the secondary alteration of select CAI samples. Methods: We chose three CAIs that experienced a range of post-formation processing to gain better understanding of secondary alteration based on previous preliminary examination [5]. Representative CAIs were chosen from NWA 5508 (CV3), NWA 12772 (CV3), and Coolidge (CL4) carbonaceous chondrites. We used scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD) techniques for detailed chemical, mineralogical, and textural analysis of the CAIs. Backscattered electron (BSE) images and X-ray elemental maps were taken of Coolidge and NWA 5508 using the Lunar and Planetary Institute (LPI) Phenom SEM. The JEOL 7900F SEM at NASA Johnson Space Center (JSC) was used to obtain energy dispersive spectroscopy (EDS) chemical maps of all samples. High resolution EBSD analysis identified the mineral phases and textures, providing key information on their nature. Based on the SEM and EBSD data, minerals of interest were selected for quantitative chemical electron probe micro-analysis (EPMA) using the JEOL JXA-8530F at NASA JSC. Results and Discussion: The EDS maps show that the NWA 5508 and NWA 12772 CAIs designated “Saguaro” and “Hoopoe” respectively [5] are enriched in calcium while the Coolidge CAI designated “Cottonwood” is aluminum and magnesium rich. Saguaro. A ~1.5cm diameter igneous Type B CAI with a rounded shape. The dominant phases are melilite, spinel, and Al-Ti pyroxene with minor anorthite. Spinel is subhedral and occurs in clusters. Some of these clusters have a circular geometry which encloses other minerals, known as a palisade structure [6] (Fig. 1). Some palisades form near perfect circles while others are more irregular in shape. Melilite in Saguaro ranges in size from coarse (>250m) to fine-grained (5-7m) and forms intergrown laths. A third of the melilite grains exhibit simple twinning about their <001> axis. The spinel palisades and twinned melilite in Saguaro suggest an igneous history, and the lack of secondary minerals suggests minimal aqueous alteration. At some point in time after the initial condensation of the minerals and formation of the inclusion, the sample was remelted and quickly solidified. The formation of the palisades is still heavily debated. One hypothesis is that the palisades are the rims of smaller CAIs that accreted early on, essentially acting as xenoliths within the larger CAIs [7]. Another hypothesis suggests an igneous origin for palisade structures [6-8] wherein the melt traps gas bubbles, and the spinel nucleates on the surface of this bubble. Based on the WDS spot analyses of 41 melilite grains using EPMA, the data suggest that the composition inside and outside the palisades is nearly identical. This finding indicates that these palisades are likely not exogenous but rather formed from melt-vapor reactions. Our results are consistent with studies by Simon and Grossman,1997 [6] and Zhang et al. (2019) [8]. Hoopoe. A ~0.5cm compact Type A CAI with an irregular shape. The dominant mineral phases are melilite, spinel, and hibonite with minor amounts of anorthite, augite, and perovskite. The melilite ranges in size from ~500 to 50µm. The larger melilite grains have simple twinning along the <001> axis like melilite in Saguaro. Melilite in Hoopoe exhibits crystal-plastic strain with misorientation dominantly about the <010> and <110> axes. Spinel shows subhedral to euhedral morphology and appears in clusters. Hibonite grains are similar to spinel in habit and size but show more plastic strain. The two minerals are often found together with one appearing to replace the other. Perovskite appears in fine grained recrystallized regions alongside fine augite and spinel. The abundant strain and deformation features in the melilite and hibonite suggest that Hoopoe experienced shock. This shock could have occurred in the nebula [9] or from an impact of another body on the parent body asteroid. The appearance of fine-grained (<10m) areas of augite, perovskite, and spinel in the dominantly coarse-grained inclusion suggest recrystallization, possibly due to the sudden increase in pressure and temperature. Cottonwood. This ~0.5cm CAI exhibits distinct mineralogy and textures suggesting a high degree of alteration. It is irregular in shape. The dominant mineral phases are spinel and anorthite with minor amounts of augite and rutile. The two main texture types can be seen in Fig. 2. The first type consists of coarse euhedral to subhedral spinel and anorthite. The second includes fine grained spinel, anorthite, rutile, and iron sulfides. Within these fine-grained regions, the anorthite grains are clustered into domains exhibiting the same crystallographic orientation. Rutile exclusively occurs with fine anorthite indicating a potential relationship between the two. Cottonwood has a clear and unbroken Wark-Lovering [10] rim (Fig. 2) on one side that consists of a sequence of spinel followed by anorthite and an outer layer of augite. The abundance of the fine-grained regions containing iron oxides and iron sulfides, secondary phases such as rutile, and oriented anorthite grains is evidence for recrystallization associated with a high degree of thermal metamorphism. The EPMA analyses on both coarse- and fine-grained spinel show that the fine spinel grains are more enriched in Cr (1-2 wt. %) than their coarse counterparts (0.1-0.5 wt. %). The data suggest thermal metamorphism drove chemical exchange of the previously refractory inclusion, introducing chromium and iron as well as sulfur, which is moderately volatile. Conclusions: The three CAIs analyzed record distinct secondary nebular and parent body processes. Saguaro melted in the nebula as seen by the twinned melilite and spinel palisades. Hoopoe experienced intense shock which deformed its melilite and recrystallized perovskite, augite, and spinel in fine-grained regions. Cottonwood shows evidence of recrystallization and chemical changes consistent with thermal metamorphism occurring after accretion into the parent-body.

V E Burnette↗

Simulation of possible regolith optical alteration effects on carbonaceous chondrite meteorites

As the spectral reflectance search continues for links between meteorites and their parent body asteroids, the effects of optical surface alteration processes need to be considered. We present the results of an experimental simulation of the melting and recrystallization that occurs to a carbonaceous chondrite meteorite regolith powder upon heating. As done for the ordinary chondrite meteorites, we show the effects of possible parent-body regolith alteration processes on reflectance spectra of carbonaceous chondrites (CC's). For this study, six CC's of different mineralogical classes were obtained from the Antarctic Meteorite Collection: two CM meteorites, two CO meteorites, one CK, and one CV. Each sample was ground with a ceramic mortar and pestle to powders with maximum grain sizes of 180 and 90 microns. The reflectance spectra of these powders were measured at RELAB (Brown University) from 0.3 to 2.5 microns. Following comminution, the 90 micron grain size was melted in a nitrogen controlled-atmosphere fusion furnace at an approximate temperature of 1700 C. The fused sample was immediately held above a flow of nitrogen at 0 C for quenching. Following melting and recrystallization, the samples were reground to powders, and the reflectance spectra were remeasured. The effects on spectral reflectance for a sample of the CM carbonaceous chondrite called Murchison are shown.

Clark, Beth E.↗

Petrology of fine-grained rock fragments and petrologic implications of single crystal from the Luna 20 soil.

Only fine-grained rocks are present in the Luna 20 samples, and coarser-grained rocks are represented by fragments of single crystals. A petrologic study has been made of 47 fine-grained crystalline rocks, microbreccias, and glassy aggregates. In addition, a total of 33 single crystals of pyroxene, plagioclase, olivine, and spinel, in the size range from 125 to 500 microns, have been examined using electron microprobe and single-crystal X-ray diffraction techniques. The most abundant fine-grained crystalline rocks in the samples examined are recrystallized anorthositic norite and anorthositic troctolite. Gabbroic rocks, anorthosite, and KREEP basalt are present but not common. Most of the single crystals of pyroxene and plagioclase could have been derived from coarser-grained noritic, troctolitic, and anorthositic rocks. However, three of the 14 pyroxene crystals, and two of the five olivine crystals have Fe/(Fe + Mg) contents greater than 0.45 and are believed to have been derived from mare basalts or related rocks.

Cameron, K. L.↗

Shock induced magnetic effects in fine particle iron dispersions

Magnetic effects associated with shock induced transformation of fcc antiferromagnetic iron precipitates in polycrystalline copper disks at levels up to 5 GPa in weak magnetic fields (H not greater than 0.5 Oe) were investigated. The demagnetization and anisotropy associated with second order transition, the effects of plastic deformation in imparting magnetic anisotropy and magnetic hardening, and the influence of post shock thermal transients on magnetization associated with recovery, recrystallization and grain growth were studied. It was found that on the microsecond time scale of the shock induced first order transformation, the field sense is recorded in the transformed iron particles. For a given particle size the degree of transformation of fcc iron depends on the level of the shock. For a given shock level the resultant magnetic properties depend on the particle size distribution, with maximum effects noted in specimens with 400 to 600 A particles.

Wasilewski, P. J.↗

Deposition rate and substrate temperature effects on the structure and properties of bulk-sputtered OFHC Cu and Cu-0.15Zr

Bulk-sputtered OFHC Cu and Cu-0.15 Zr used as inner walls of advanced regeneratively cooled thrust chambers are evaluated as to microstructure, surface topography, and fractography. It is found that under conditions of low substrate temperature, crystallite size and openness of the structure increase with increasing deposition rate for both materials. At elevated temperatures, an equiaxed ductile structure of OFHC Cu is produced only at low deposition rates; at higher deposition rate, open structures are observed with recrystallized equiaxed grains within large poorly bonded crystallites. The Cu-0.15 Zr alloy sputtered from the hollow cathode using a diode discharge shows open-type structures for all conditions evaluated. The use of a triode discharge in generating a dense non-voided structure of Cu-0.15 Zr is discussed.

Hecht, R. J.↗

The Sm-Nd systematics of silicate inclusions in iron meteorites: Results from Caddo (IAB)

The timing of events leading to the formation of silicate-rich and metal-rich regions in planetesimals remains an important problem in the study of planetary formation and differentiation in the early solar system. The IAB irons are especially important as they are considered to represent a magmatic differentiation series. Iron meteorites present a particular challenge for chronological studies, due to the relative paucity of phases serving as hosts for radioactive parent-daughter nuclides. Recent work using the Re-Os system, following on the pioneering work by Herr et al. and Luck and Allegre, appears promising, but investigators up to now have concentrated on whole rock isochrons. Silicate clasts enclosed within iron meteorites can provide information about the chronology and thermal history of irons. Extensive work on Rb-Sr, K-Ar, and I-Xe has been reported on silicate inclusions in iron meteorites. We report the initial results from our Sm-Nd study of an inclusion with the Caddo IAB iron, the first Sm-Nd isotopic study of a silicate clast embedded within an iron meteorite. Our results include measurements of the standard long-lived Sm-147/Nd-143 (tau = 152 AE) system, as well as the shorter-lived SM-146/Nd-142 (tau = 0.149 AE) system, which has been shown to be very useful in deciphering the history of the early solar system. The Caddo silicate clast was described by Palme et al., who kindly provided us with a major part of the inclusion. The inclusion is coarse-grained consisting predominantly of olivine, clinopyroxene, and plagioclase, with lesser amounts of orthopyroxene, Fe-Ni metal, sulfide, and phosphate. The relatively large grain size (up to 3 mm) and 120 degree grain boundaries suggest extensive metamorphism at high temperatures. Based on study of a thin section, there is evidence for metal invading along grain boundaries in some regions of the inclusion, suggesting that the Fe-Ni metal was molten when the silicate clast was incorporated. Metamorphic recrystallization may have occurred during this event.

Stewart, Brian W.↗

Deformation and annealing response of TD-nickel chromium

The recrystallization and grain growth processes occurring in TD-NiCr were examined with respect to deformation severity, annealing time, and temperature. Results indicated that two different annealing responses of TD-NiCr are possible, depending on the initial state and processing history prior to annealing. As-received sheet showed a dramatic increase in grain size with decreasing annealing temperature, whereas sheet prior-annealed at 1316 C for 1 hr exhibited very little variation with subsequent annealing temperature.

Kane, R. D.↗