Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Powder Bed Fusion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Size Effects on Laser Powder Bed Fusion and Laser Powder Directed Energy Deposition GRCop-42 Alloy

Additive manufacturing (AM) plays a significant role in the fabrication of regeneratively cooled rocket engine combustion chambers, where internal channels are used to transport high pressure propellants to keep the engine from overheating. Cooling channels are designed with thin walls between the cooling and combustion sides, experiencing high thermal and mechanical stresses from large temperature gradients and internal pressures. Hence, selecting materials suited for this environment and maintaining a high-quality processing for this critical application is of utmost importance. GRCop-alloys (Cu-Cr-Nb) were developed as an ideal material for combustion chambers due to its high conductivity and high strength at temperature, being employed as a structural member for the hotwall with excellent heat transfer capabilities. GRCop-42 (Cu, 4 at% Cr, 2 at% Nb) has significantly matured using the Laser Powder Bed Fusion (L-PBF) process through microstructure, mechanical and thermophysical properties and evaluations using hot-fire testing. Additionally, Laser Powder Directed Energy Deposition (LP-DED) has demonstrated successful deposition and geometry samples using GRCop-42. While the maturation in properties has focused on bulk material properties from standard test specimens, these cannot be extrapolated to be used in thin walls, as different features (i.e., microstructure, porosity, and surface texture) have a greater effect on thin walls, especially on AM structures built using L-PBF and LP-DED. This presentation provides an overview of the effects introduced by reducing the thickness on the fabrication, microstructure, surface metrology and subsequent mechanical properties of GRCop-42 using L-PBF and LP-DED as well as future work planned for this research.

Gabriel Demeneghi↗

Quantifying Trapped Powder in Electron Beam Powder Bed Fusion

Abstract Electron beam powder bed fusion (PBF-EB) shows great potential for manufacturing complex parts including those with internal cavities for heat exchanger, manifold systems, or energy absorption purposes. PBF-EB allows for the manufacture of channel geometries without the need for support structures. Due to the nature of the powder spreading process, powder feedstock is often trapped in intentionally manufactured cavities. This trapped powder can often be difficult to remove and can disturb the intended flow of fluid through the cavity or damage downstream components in its use case. These trapped powder particles present a risk of contamination and component failure if not completely evacuated. Ti6Al4V is a choice material for aerospace applications due to its high strength to weight ratio and its composition as a nonferrous metal; however, in weight sensitive applications excess entrapped powders or powders loosely attached to the surface could cause undesirable weight increases. The inherent spreading process of PBF-EB is different than laser powder bed fusion (PBF-LB) in its operational temperature, sintering. In addition, PBF-EB is less commonly studied in literature compared to its PBF-LB counterpart, and as a result the complexity of the semi-sintered powder and its spreading behavior are not well understood. Prior work has investigated the difficulty in removing trapped powder from PBF-EB, but these studies do not address how to quantify the amount of trapped powder in the cavity. Thus, an accurate method to measure the amount of trapped powder in the cavity must be investigated. In this work, Ti6Al4V coupons were manufactured with horizontal and vertical cavities of three different sizes. Archimedes testing allows for the determination of density differences caused by porosity and trapped powders by measuring mass and volumetric dispersion. Computed tomography (CT) is well suited for segmenting the internal structure and features of a part and has been studied for applications including voids, porosity, and dross. Thus, CT was explored as a method for evaluating trapped powder content in this work. The volumetric representation of the segmentation of the reconstructed CT volume can vary greatly depending on the input filter and thresholding methods. In this study, four different types of segmentation approaches were evaluated to determine the best approach for segmenting the volume as compared to an operator labeled ground truth. The percentage density results from the Archimedes testing were compared to the volumetric percent density from the computed tomography approach. Differences in packing density between two different internal channel features were investigated. Overall, this work sought to validate the use of computed tomography for the detection of trapped powders and present a framework for volumetric segmentation.

Johnstone, Brian↗

Nanoparticle-enhanced absorptivity of copper during laser powder bed fusion

We report laser powder bed fusion (LPBF) of pure copper for thermal and electrical applications is hampered by its low near-infrared absorptivity and high thermal diffusivity. These material properties make it very difficult to localize the thermal energy needed to produce high density 3D printed parts. Modification of metal powders via nanoparticle additives is a promising approach to increasing absorptivity, but the effect of nanoparticles on absorptivity and melting behavior during LPBF is not well understood. In this study, we developed an in situ calorimetry system to measure effective absorptivity during LPBF on copper substrates. We decorated copper substrates using three nanoparticle systems (CuS, TiB 2 , multilayer graphene flakes) and demonstrated an enhanced absorptivity of the decorated substrates relative to pure copper. Graphene nanoflakes resulted in the highest improved absorption relative to pure copper from 0.09 to 0.48, due to their stability at high laser scanning powers. A thermomechanical model with convective heat transfer provided confidence in the measurements by reproducing the experimental melt pool traces. Full 3D cylindrical prints demonstrated an improvement in relative density of the copper-graphene powder prints (in the range of 0.930–0.992), relative to that of as-purchased copper powder prints (in the range of 0.854–0.972). This work provides a fundamental study of nanoparticle-enabled LPBF of highly reflective metals and demonstrates a viable route for expanding the library of reliably printable metals.

36 MATERIALS SCIENCE↗

Keyhole-mode Microscopy Dataset for Laser Powder-bed Fusion Modeling

Laser powder-bed fusion (LPBF) is an additive manufacturing (AM) technology that uses high-power sintering lasers to precisely construct metal designs. Material is accumulated by selectively sintering regions of a metal powder layer to a growing structure underneath forming a 3D geometry. Certain conditions make fusion in this process to operate in "keyhole-mode," characterized by targeted materials evaporating as plasma. While keyhole-mode operations can produce deeper molten pools than that observed in "conduction-mode", this mode of operation is often undesirable, as its molten regions can collapse on themselves, encapsulating metal vapors and forming cavities. The formation of such cavities negatively affects strength and consistency of the fused materials. To identify and avoid these detrimental effects of keyhole-mode operation, considerable data collection and analysis regarding this mode of operation is needed. Therefore, under the support of the "Open Data Initiative," Lawrence Livermore National Lab is releasing a dataset for analysis of this keyhole effect, and the conditions which transition operation from conduction-mode to keyhole-mode melting. This dataset consists of 600+ micrographs from laser powder-bed single track runs, with differing cross-section angles and input parameters, operating under both normal and keyhole mode operations. This journal documents the collection, organization, and usage of this dataset.

36 MATERIALS SCIENCE↗

A Novel Additive Manufacturing Process Metric for Predicting Spatter-related Porosity in Laser Powder Bed Fusion

Components fabricated using the powder bed fusion laser beam metallic (PBF) additive manufacturing (AM) process comprise a multitude of sequential weld passes. Porosity defects resulting from weld pass inconsistencies are a concern for PBF materials and have a strong adverse effect on the mechanical properties. In an effort to understand and avoid spatter induced porosity, this work aims to provide a novel computational technique that can be used to quantify and predict the sequence-sensitive impact of spatter upon the PBF process stability and consequential porosity in as-printed material. A novel spatter impact AM model-based process metric (AM-PM) is introduced to model and quantify the impact that spatter has on the PBF process. The occurrence of spatter induced porosity is studied using thermal rise, lack of fusion, and spatter impact AM-PMs synchronized with porosity measured by high-resolution X-ray computed tomography. Six cylindrical specimens were designed to compare the AM-PM correlations with porosity across two different laser powers and three hatch scanning strategies. A point field based computational approach is shown to be effective for testing the influence of the different AM-PMs and interrogating the physical process conditions underlying the porosity formation. Further, characterization using optical metallography and scanning electron microscopy indicated that both keyhole and lack of fusion porosity correlated with the spatter impact AM-PM, which can be exploited to predict and control spatter related porosity by the hatch strategy. Efforts to predict porosity composition within PBF material should incorporate the PBF process disturbances that can result from spatter. The spatter impact AM-PM can be readily incorporated into the development of defect prediction models at the part scale.

Additive Manufacturing↗

On the formation of swelling and related flaws in laser powder bed fusion

Process monitoring in laser powder bed fusion additive manufacturing can provide insights into stochastic anomalies, melt pool and plume dynamics, and part quality. Swelling, a build anomaly where overbuilt material protrudes through the powder layer after recoating, is readily detectable in post-recoat visible light images of the powder bed. Here, this work identifies several of the underlying mechanisms driving swelling formation by analyzing the influence of processing parameters, laser scan paths, and build plate locations on the presence of swelling detected in situ. Swelling near the edge of the part and swelling in the internal region of the part are shown to correlate with different process conditions. Edge and internal swelling may be driven by different phenomena, with edge swelling predominately occurring on the edge of a part facing the laser module and correlated to clusters of near-surface voids (detected with X-ray computed tomography). A larger spot size, higher laser power, and lower scan velocity also increased the presence of edge swelling. Laser spot size and scan path influenced internal swelling, which occurred preferentially with a larger spot size and in regions with large melt pools, caused by localized heat accumulation due to non-optimal processing parameters or scan path strategies. For coupons processed with a slicer-defined maximum scan vector length, swelling seldom occurred at internal vector-stripe boundaries. These results provide a mechanistic understanding of how swelling can be linked to material flaws, insight into how some instances of swelling can be avoided, and evidence supporting the use of swelling as an in situ indicator for quality assurance and part qualification.

Anomaly↗

Heat Treatment Optimization of Laser Powder Bed Fusion Additive Manufacture C103

Laser Powder Bed Fusion (L-PBF) and Laser Powder Directed Energy Deposition (LP-DED) additive manufacture C103 is in development for propulsion applications that operate under extreme environments. The standard post-process heat treatment has called for vacuum stress relief, however, depending on the application or certification requirements hot isostatic press (HIP) may be required. Although C103 density responds well to HIP the associated grain growth results in a reduction in mechanical properties. An investigation was conducted to look at the potential benefit of leveraging HIP followed by rapid cooling to minimize grain growth. A series of heat treatment schedules varying temperature and pressure were conducted followed by microstructural and mechanical characterization.

Additive Manufacturing↗

Bending Performance of Tungsten Printed Via Laser Powder Bed Fusion With Ceramic Dispersion Modified Powder Feedstock

Additively manufactured tungsten is a candidate refractory material for high-temperature aerospace and nuclear fusion/fission applications. The printability of pure tungsten is challenged by cracking defects arising from the metal’s high brittle-to-ductile transition temperature and low solubility of interstitial impurities. Furthermore, the cast microstructure inherent to the laser powder bed fusion (L-PBF) process has limited strength compared to worked microstructures common in wrought tungsten. Aside from process-related techniques to mitigate defects and increase strength (e.g., heated build chambers, multi-laser systems, low oxygen environmental control, etc.), micro-alloying additions can positively influence tungsten printability and strength. In this work, pure tungsten L-PBF feedstock was modified with 1 wt% additions of ceramic compound nano-powders. Wrought and printed bars were evaluated in four-point bending. Flexural strength and fractography were primary means of comparison to assess the effect of the feedstock modification on printed tungsten mechanical performance.

Additive Manufacturing↗

Laser melting modes in metal powder bed fusion additive manufacturing

In laser powder bed fusion additive manufacturing of metals, extreme thermal conditions create many highly dynamic physical phenomena such as vaporization and recoil, Marangoni convection, and protrusion and keyhole instability. Collectively however, the full set of phenomena is too complicated for practical applications and, in reality, the melting modes are used as a guideline for printing. With increasing local material temperature beyond the boiling point, the mode can change from conduction to keyhole. These mode designations ignore laser-matter interaction details but in many cases are adequate to determine the approximate microstructures and hence the properties of the build. To date, no consistent, common, and coherent definitions have been agreed upon because of historic limitations in melt pool and vapor depression morphology measurements. Here, we distinguish process-based definitions of different melting modes from those based on postmortem evidence. The latter are mainly derived from the transverse cross-sections of the fusion zone, whereas the former come directly from time-resolved x-ray imaging of melt pool and vapor depression morphologies. These process-based definitions are more strict and physically sound, and they offer new guidelines for laser additive manufacturing practices and create new research directions. Further, we highlight the significance of the keyhole, which substantially enhances the laser energy absorption by the melt pool. Recent studies strongly suggest that stable-keyhole laser melting enables efficient, sustainable, and robust additive manufacturing. The realization of this scenario demands the development of multiphysics models, signal translations from morphology to other feasible signals, and in-process metrology across platforms and scales.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Optimization of stochastic feature properties in laser powder bed fusion

Process parameter selection in laser powder bed fusion (LPBF) controls the as-printed dimensional tolerances, pore formation, surface quality and microstructure of printed metallic structures. Measuring the stochastic mechanical performance for a wide range of process parameters is cumbersome both in time and cost. As such, in this study, we overcome these hurdles by using high-throughput tensile (HTT) testing of over 250 dogbone samples to examine process-driven performance of strut-like small features, ~1 mm 2 in austenitic stainless steel (316 L). The output mechanical properties, porosity, surface roughness and dimensional accuracy were mapped across the printable range of laser powers and scan speeds using a continuous wave laser LPBF machine. Tradeoffs between ductility and strength are shown across the process space and their implications are discussed. While volumetric energy density deposited onto a substrate to create a melt-pool can be a useful metric for determining bulk properties, it was not found to directly correlate with output small feature performance.

316 L stainless steel↗

In situ study on radiation response of tungsten manufactured by laser powder bed fusion

Tungsten (W) produced by laser powder bed fusion (LPBF) was examined by in situ Krypton (Kr) ion irradiation at 400 °C up to 2.52 displacements per atom (dpa) to investigate its radiation response. Dislocation loops with identical Burgers vectors form aligned raft structures, inducing significant grain misorientation accumulation. Defect saturation was observed beyond 0.36 dpa, marked by constant loop density and raft spacing. WO 3 nanoparticles are found in the as-printed matrix and served as efficient defect sinks. Dislocation loops were absorbed at the W/WO 3 interface, facilitating defect annihilation and suppressing defect accumulation. In conclusion, these findings highlight the role of LPBF microstructure and oxide interfaces in mediating radiation-induced defect evolution, offering insights for designing radiation tolerant W-based materials.

Defect sink↗

Establishing an acoustic-property relationship in laser powder bed fusion with machine learning

Quality control of Laser Powder Bed Fusion (PBF-LB) additively manufactured parts is an important hurdle inhibiting the technology’s use structural applications. Acoustic monitoring of the laser powder bed fusion process can detect defects in-situ that are known to degrade mechanical properties. However, processing-structure-property (PSP) relationships are required to extrapolate from detected defects to part performance. Here, this study explores how acoustics may be a suitable signature linking processing conditions to properties, thus effectively substituting for structure in the PSP relationship. Establishing such a relationship would enable a part’s mechanical performance to be directly predicted from its acoustic signature, reducing the need for destructive testing or microstructural analysis to ensure a part will meet performance requirements. One hundred CoCrFeMnNi high entropy alloy tensile bars were printed across 13 process conditions in a series of 6 prints. The acoustic signatures of these tensile bars were used to train machine learning models to predict each part’s mechanical properties. By using both process information and acoustic information to predict mechanical properties, yield strength was predicted 18% more accurately and ductility to failure was predicted 10% more accurately than is achieved when using duplicate parts to predict part performance. Finally, individual acoustic frequencies were investigated to determine why acoustic signatures improve mechanical property predictions and the potential physical origins of these signatures. This work demonstrates how blending acoustics, process information, and machine learning can provide in-situ diagnostics of mechanical properties and improve the reliability of the PBF-LB process.

Acoustic emission↗

An experimental process parameter study on the identification of defects in additively fabricated Al6061 with laser powder bed fusion

Additively fabricated metal parts using laser powder bed fusion (L-PBF) possess sophisticated morphology due to the recurrent use of laser-induced metal powder melting and solidification. The surface and 3D morphology of these parts often include defects in the form of protrusions, depressions, pores, voids, keyholes, or cracks that are known to be influenced by laser scanning paths and layer-to-layer processing. Such inconsistent part quality hampers the extensive adoption of L-PBF. Pores and cracks are detrimental to the fatigue life of the parts and components. Quantifying and controlling part defects and optimizing processing and scanning strategy parameters adaptively in real-time through in situ monitoring systems are highly desired. This study investigates the optimization of experimental process parameters (power, scan velocity, and hatch spacing) and their effects on the cracking and porosity of Al6061 alloy using machine learning techniques. Multi-objective optimization is formulated and conducted to determine the L-PBF parameters that minimize both porosity and crack densities.

36 MATERIALS SCIENCE↗