Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ni dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Uncovering the Critical Role of Ni on Surface Lattice Stability in Anionic Redox Active Li 1.2 Ni 0.2 Mn 0.6 O 2

Anionic redox reaction (ARR) can provide extra capacity beyond transition metal (TM) redox in lithium-rich TM oxide cathodes. Practical ARR application is much hindered by the structure instability, particularly at the surface. Oxygen release has been widely accepted as the ringleader of surficial structure instability. However, the role of TM in surface stability has been much overlooked, not to mention its interplay with oxygen release. Herein, TM dissolution and oxygen release are comparatively investigated in Li 1.2 Ni 0.2 Mn 0.6 O 2 . Ni is verified to detach from the lattice counter-intuitively despite the overwhelming stoichiometry of Mn, facilitating subsequent oxygen release of the ARR process. Intriguingly, surface reorganization occurs following regulated Ni dissolution, enabling the stabilization of the surface and elimination of oxygen release in turn. Accordingly, a novel optimization strategy is proposed by adding a relaxation step at 4.50 V within the first cycle procedure. Battery performance can be effectively improved, with voltage decay suppressed from 3.44 mV/cycle to 1.60 mV/cycle, and cycle stability improved from 66.77% to 90.01% after 100 cycles. This work provides new perspectives for clarifying ARR surface instability and guidance for optimizing ARR performance.

25 ENERGY STORAGE↗

Methanogens acquire and bioaccumulate nickel during reductive dissolution of nickelian pyrite

ABSTRACT Nickel (Ni) is a key component of the active site metallocofactors of numerous enzymes required for methanogenesis, including [NiFe]-hydrogenase, carbon monoxide dehydrogenase, and methyl CoM reductase, leading to a high demand for Ni among methanogens. However, methanogens often inhabit euxinic environments that favor the sequestration of nickel as metal-sulfide minerals, such as nickelian pyrite [(Ni,Fe)S 2 ], that have low solubilities and that are not considered bioavailable. Recently, however, several different model methanogens ( Methanosarcina barkeri , Methanococcus voltae , Methanococcus maripaludis ) were shown to reductively dissolve pyrite (FeS 2 ) and to utilize dissolution products to meet iron and sulfur biosynthetic demands. Here, using M. barkeri Fusaro, and laboratory-synthesized (Ni,Fe)S 2 that was physically isolated from cells using dialysis membranes, we show that trace nickel (<20 nM) abiotically solubilized from the mineral can support methanogenesis and limited growth, roughly fivefold less than the minimum concentration known to support methanogenesis. Furthermore, when provided direct contact with (Ni,Fe)S 2 , M. barkeri promoted the reductive dissolution of (Ni,Fe)S 2 and assimilated solubilized nickel, iron, and sulfur as its sole source of these elements. Cells that reductively dissolved (Ni,Fe)S 2 bioaccumulated approximately fourfold more nickel than those grown with soluble nickel and sulfide but had similar metabolic coupling efficiencies. While the mechanism for Ni uptake in archaeal methanogens is not known, homologs of the bacterial Nik uptake system were shown to be ubiquitous across methanogen genomes. Collectively, these observations indicate that (Ni,Fe)S 2 is bioavailable in anoxic environments and that methanogens can convert this mineral into nickel-, iron-, and sulfur-containing metalloenzymes to support methanogenesis and growth. IMPORTANCE Nickel is an essential metal, and its availability has changed dramatically over Earth history due to shifts in the predominant type of volcanism in the late Archean that limited its availability and an increase in euxinic conditions in the early Proterozoic that favored its precipitation as nickel sulfide minerals. Observations presented herein indicate that the methanogen, Methanosarcina barkeri , can acquire nickel at low concentration (<20 nM) from soluble and mineral sources. Furthermore, M. barkeri was shown to actively reduce nickelian pyrite; use dissolution products to meet their iron, sulfur, and nickel demands; and bioaccumulate nickel. These data help to explain how M. barkeri (and possibly other methanogens and anaerobes) can acquire nickel in contemporary and past anoxic or euxinic environments.

(NiFe)S2↗

Effect of chromium on corrosion resistance of Ni-Cr-Mo-Gd alloys in seawater

Neutron absorbing materials are being considered within commercial spent nuclear fuel disposal canisters to maintain nuclear subcriticality in storage. To select candidate alloys for the canisters, both neutron absorption and corrosion resistance should be considered. This work examines corrosion resistance of Ni-Cr-Mo-Gd alloys developed specifically for neutron absorption. The addition of Gd results in a secondary gadolinide phase (Ni 5 Gd) that significantly changes the corrosion properties. Testing was performed primarily in seawater at 30°C. Seawater was selected as the most prevalent terrestrial brine and is characterized by a high chloride concentration. Various electrochemical corrosion techniques were carried out to evaluate Ni-Cr-Mo-Gd alloys with different Cr compositions and investigate the role of Ni 5 Gd phase on corrosion behavior. C22 was included as a benchmark material, due to the similarity in composition and the significant corrosion data available. Here, test results showed a tendency to passivate over time which is attributed to dissolution of surface exposed Ni 5 Gd phase. Cross-sectional analysis indicated that dissolution could penetrate hundreds of micrometers deep under aggressive conditions. It was found that higher Cr variant (21.01%) showed much shallower impact, suggesting Cr prevented primary phase corrosion and thus reduced Ni 5 Gd phase dissolution. Acid pickling of the specimens showed much less dissolution for a higher Cr material and suggested some primary phase dissolution for the low Cr specimen. Acid pickled specimens showed positive shifts in the repassivation potential, suggesting increased surface passivation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Assessing Stainless Steel Compatibility in Flowing FLiBe Salt

To address the considerable interest in LiF-BeF 2 (FLiBe) compatibility for fission and fusion reactor applications, static and flowing compatibility experiments were conducted to assess the compatibility with type 316H stainless steel. In static testing at 550° and 650 °C, small mass changes were measured and posttest characterization of the FLiBe showed increased levels of Fe, Cr, Ni and Mn in the salt. Adding Be in the static salt test reduced the dissolution of Fe and Ni. Further, an initial assessment of mass transfer in flowing FLiBe without a Be addition was conducted using a monometallic 316H thermal convection loop (TCL) operated for 1000 h with a peak temperature of 650 °C. Similar to prior results in flowing FLiNaK salt, the 316H specimens exhibited small mass losses in the hot leg. Posttest characterization of the 316H specimens suggested Cr surface depletion in the hot and cold legs and possibly Fe deposition in the cold leg. To further understand this behavior, Cr and Fe dissolution was measured in static FLiBe at 550–650 °C.

316H stainless steel↗

Morphological Evolution and Dealloying During Corrosion of Ni20Cr (wt.%) in Molten FLiNaK Salts

The dealloying corrosion behavior of the FCC Ni20Cr (wt%) in molten LiF-NaF-KF (FLiNaK) salts at 600 °C under varying applied potentials was investigated. Using in-operando electrochemical techniques and a multi-modal suite of characterization methods, we connect electrochemical potential, thermodynamic stability, and electro-dissolution kinetics to the corrosion morphologies. Notably, under certain potential regimes, a micron-scale bicontinuous structure, characterized by a network of interconnected pores and ligaments riched with the composition of the more noble (MN) element, becomes prominent. At other potentials both MN and less noble (LN) elements dealloy but at different rates. The dealloying process consists of lattice and grain boundary diffusion of Cr to the metal/salt interface, interphase Cr oxidation, accompanied by surface diffusion of Ni to form interconnected ligaments. At higher potentials, the bicontinuous porous structure undergoes further surface coarsening. Concurrently, Cr(II), Cr(III), and Ni(II) begin to dissolve, with the dissolution of Ni occurring at a significantly slower rate. When solid-state transport of Cr is exceeded by the interfacial rates, dealloying depths are limited.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Heterogeneous Corrosion Pathways in Pt–Ni Nanododecahedra Revealed by In Situ Liquid Cell TEM

Unraveling nanoscale corrosion pathways is essential for understanding materials degradation mechanisms and designing corrosion-resistant metal alloys. Here, in this study, we directly visualize the corrosion of Pt–Ni nanododecahedra in 0.1 M HCl using liquid cell TEM. Each nanoparticle features a Ni-rich core and a Pt-rich frame. Our observation reveals that corrosion proceeds in two distinct stages: first the Ni-rich core dissolves without forming porosity, yielding small Pt nanocrystals and transient NiCl 2 ·6H 2 O at the retreating interfaces; then the Pt-rich frame fragments into ∼5 nm Pt 3 Ni nanocrystals that subsequently dissolve uniformly, accompanied by fleeting Pt chlorides. A percolation-based theory explains the observed behaviors: The core’s ∼8% Pt lies below the Pt connectivity threshold, preventing Pt scaffold formation, whereas the frame’s 48% Ni exceeds the Ni percolation threshold and collapses. Ordered Pt 3 Ni suppresses Ni percolation, thereby enforcing uniform dissolution. These findings reveal how composition and structural ordering govern heterogeneous corrosion in Pt–Ni architectured nanoparticles.

Liquid phase TEM↗

Electrochemical stability and corrosion behavior of Ni-Cr alloy in molten LiCl-KCl salt

This study investigated the electrochemical properties and potential-dependent stability of Cr(II) and Ni(II) in a eutectic LiCl-KCl molten salt at 500 °C under an argon atmosphere using a three-electrode cell configuration with a glassy carbon working electrode, Ag/Ag + reference electrode, and graphite counter electrode. Cyclic voltammetry was employed to characterize the Cr(0)/Cr(II)/Cr(III) and Ni(0)/Ni(II) redox transitions, yielding diffusion coefficients of 0.50 (±0.01) × 10 −5 cm 2 s −1 for Cr(II) and 0.91 (±0.16) × 10 −5 cm 2 s −1 for Ni(II) at 500 °C. The redox stability domains of these species provided insight into the corrosion mechanisms of a Ni-Cr alloy (80–20 wt %) in LiCl-KCl salt. The measured open circuit potential of the alloy corresponded to the range of potentials where the Ni(0) and Cr(II) species are stable, indicating a preferential dissolution of Cr. Immersion testing of the alloy for 336 h confirmed significant Cr depletion (or Ni-enrichment) at the surface layer, corroborating Cr dealloying as the dominant corrosion reaction under open circuit conditions. Additionally, the application of a small anodic overpotential (0.11 V) resulted in selective Cr dissolution while a large anodic overpotential (0.25 V) resulted in co-dissolution of both Cr and Ni. Furthermore, these results demonstrate that the corrosion mechanisms of a Ni-Cr alloy in LiCl-KCl depend upon the applied potential, and thus the redox conditions of the molten salt should be carefully controlled in the design of a redox buffer to mitigate corrosion in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

In-Situ FTIR Detection of Transition Metal (TM)-Ion Dissolution From Cathodes in Li-Ion Batteries

Transition metal (TM) ions, commonly Ni and Mn, play a crucial role in Li-ion battery cathodes as the reaction centers for rapid redox reactions. A major challenge with TM-based cathodes is capacity degradation, particularly at higher operating voltages. This degradation is closely linked to the dissolution of TMs from the cathode materials and their subsequent deposition on the anode. This process not only modifies the surface structure of the cathode but, more significantly, alters the SEI composition on the anode [1-2]. The dissolution of TMs cations into a liquid electrolyte from cathode materials, such as Mn-ion dissolution from Mn-rich cathode (LMR), is detrimental to the cycling performance of Li-ion batteries [3-4]. Much attention has been paid to this issue but there remains a lack of characterization techniques which can detect the TM-ion dissolution from the cathode during electrochemical measurements. In our study, we use in-situ ATR-FTIR as an effective technique to probe the TM-ion dissolution from the cathode. We have first demonstrated the detrimental effects of TM ions on the electrochemical performance of Li-ion batteries by adding a small amount of TM salt (50 mM Mn(PF6)) to the electrolyte of a Li-ion coin cell with LFP and graphite electrode. We observed a rapid capacity fade after the first delithiation cycle. To investigate TM ion dissolution, we established a baseline IR spectrum for various TM solvation states (such as Mn and Ni) by measuring concentration-dependent IR spectra. This baseline spectrum helps us detect TM ion dissolution during battery cycling. In this work, we discuss in detail the effect of TM ions on the electrochemical performance of Li-ion batteries and the detection of TM ions during battery cycling using in-situ FTIR spectroscopy. We will compare TM dissolution between coated and uncoated cathodes to examine the effect of cathode coatings to mitigate degradation due to TM dissolution and cross-over from cathode to anode. References: (1) Zhan, C.; Wu, T.; Lu, J.; Amine, K. Dissolution, migration, anddeposition of transition metal ions in Li-ion batteries exemplified byMn-based cathodes - a critical review. Energy Environ. Sci. 2018, 11,243-257. (2) Jung, R.; Linsenmann, F.; Thomas, R.; Wandt, J.; Solchenbach,S.; Maglia, F.; Stinner, C.; Tromp, M.; Gasteiger, H. A. Nickel,Manganese, and Cobalt Dissolution from Ni-Rich NMC and TheirEffects on NMC622-Graphite Cells. J. Electrochem. Soc. 2019, 166,A378-A389. (3) Zhao, L.; Chenard, E.; Capraz, O. O.; Sottos, N. R.; White, S.R. Direct Detection of Manganese Ions in Organic Electrolyte by UV-Vis Spectroscopy. J. Electrochem. Soc. 2018, 165, A345-A348 (4) Zhang, Y.; Hu, A.; Xia, D.; Hwang, S.; Sainio, S.; Nordlund, D.;Michel, F. M.; Moore, R. B.; Li, L.; Lin, F. Operando characterization and regulation of metal dissolution and redeposition dynamics nearbattery electrode surface. Nat. Nanotechnol. 2023, 18, 790.

25 ENERGY STORAGE↗

Impacts of A‐Site Composition on the Cation Dissolution‐Mediated Surface Restructuring of Layered Nickelate Oxide Electrocatalysts During Alkaline Oxygen Evolution Reaction

The oxygen evolution reaction (OER) is a key anodic counter‐reaction for electrochemical production of fuels and chemicals. It is hindered by sluggish four‐electron transfer kinetics requiring highly oxidative operating potentials to achieve commercially relevant rates. NiFeO x H y electrocatalysts are among the most promising for OER in alkaline electrolytes. The Ni(OH) 2 /NiOOH redox couple has been reported as the active phase in Ni‐based electrocatalysts; however, its activity is often hindered by deactivation arising from the formation of OER‐inactive insulating species. Limited strategies exist for mitigating this deactivation. This study aims to address this by interrogating the evolution of OER active sites as a function of precatalyst composition and structural properties using a series of layered, crystalline Ni‐based Ruddlesden–Popper (RP) oxides (A 2 NiO 4+δ ). In situ evolution of the active NiO x H y surface is probed through Ni‐site OER turnover frequency analysis, and electrochemical impedance spectroscopy coupled with scanning transmission electron microscopy. We show that the stability of layered nickelate oxide electrocatalysts is governed by the dynamic competition between cation dissolution and Ni‐site reversibility, which can be tuned through the A‐site composition of RP oxides. These findings yield insights toward engineering OER oxide precatalysts that optimize the stability of in situ‐generated OER active phases.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of fluctuating redox conditions on trace metal release from wetland soils from South Carolina and stream sediments from Tennessee

Natural aquatic systems undergo fluctuating redox conditions due to microbial activity, varying water saturation levels, and nutrients dynamics. With fluctuating oxic and anoxic conditions, trace metals can be mobilized or sequestered in response to changes in iron and sulfur speciation and the concentrations and lability of organic carbon. We conducted a systematic laboratory-based microcosm study to examine the effect of redox fluctuations on trace metal mobility in samples collected from two different natural aquatic systems: riparian wetlands and a stream. We incubated water-saturated soils under three cycles of anoxic-oxic conditions (τanoxic:τoxic = 3) spanning 24 days and monitored the change in dissolved and bioavailable metal (copper (Cu), nickel (Ni), zinc (Zn), cobalt (Co), iron (Fe), and manganese (Mn)) concentrations. The dataset includes the results of the variation in metal concentrations due to redox fluctuations in wetland soils and stream sediments. Additionally, the variation in the bioavailable concentration of metals obtained using passive samplers based on diffuse gradient in thin-films technique is included in the dataset. We have also reported the change in the pH values and dissolved oxygen concentrations in the microcosms during the entire study of 24 days. The dataset also contains the dissolved organic carbon and sulfate concentrations, and the data on fractions of metals bound to reducible and oxidizable phases. For materials from both the wetlands and the stream, anoxic conditions favored Co and Zn release, which corresponded with the reductive dissolution of iron oxides. In contrast, dissolved Cu concentrations increased under oxic conditions for both sites and correlated positively with the release of sulfate. In wetland soils, dissolution of Fe (hydr)oxides increased Ni solubility; however, in stream sediments, Ni release occurred when sulfides or organic matter were oxidized. For stream sediments, each subsequent redox cycle increased the bioavailability of trace metals. Upon redox fluctuations in wetland soils, the bioavailability of Zn and Cu increased, whereas bioavailable Ni and Co decreased. This study illustrates that different trace metals display distinct bioavailability patterns during oxic-anoxic fluctuations in natural environments. The biogeochemical cycling of carbon and nitrogen in systems with redox fluctuations may be influenced by these patterns in trace metal availability in addition to the availability of electron donors and acceptors.

54 ENVIRONMENTAL SCIENCES↗

Dynamic Responses of Trace Metal Bioaccessibility to Fluctuating Redox Conditions in Wetland Soils and Stream Sediments

Natural aquatic systems undergo fluctuating redox conditions due to microbial activity, varying water saturation levels, and nutrients dynamics. With fluctuating redox conditions, trace metals can mobilize or sequester in response to changes in iron and sulfur speciation and the concentrations and lability of organic carbon. This study examined the effect of redox fluctuations on trace metal mobility in samples collected from two different natural aquatic systems: riparian wetlands and a stream. The wetland soils contained low sulfur and total Fe contents as compared to stream sediments. The mineral composition at both sites was dominated by quartz. We incubated water-saturated soils under three cycles of anoxic-oxic conditions (τanoxic:τoxic = 3) spanning 24 days and monitored the change in dissolved and bioavailable metal concentrations. For both natural systems, reduction of iron oxides under anoxic conditions caused Co and Zn release. In contrast, oxidation of sulfides mobilized Cu under oxic conditions in both sites. In wetland soils, dissolution of Fe (hydr)oxides increased Ni solubility; however, in stream sediments, Ni release occurred when sulfides or organic matter were oxidized. For stream sediments, each subsequent redox cycle increased the bioavailability of trace metals. Redox fluctuations in wetland soils increased bioavailable Zn and Cu and decreased bioavailable Ni and Co. This study illustrates that different trace metals display distinct bioavailability patterns during redox fluctuations in natural environments. The biogeochemical cycling of nutrients in systems with redox fluctuations may be influenced by these trace metal availability patterns in addition to the availability of electron donors and acceptors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

First-Principles Studies of Tritium Species Diffusivity Across the Interface of Nickel-Plated Zircaloy-4

In this study, we will calculate the 3H2 and 3H2O diffusion mechanism in the Ni coated layer and the dominant 3H species dissolution into the Zircaloy-4 getter. We will optimize the Ni/Zr interface and introduce Sn and O impurities. To achieve the objectives, we will perform the investigation by using spin-polarized density functional theory (DFT) methods to capture the effects of Ni magnetic properties on 3H diffusion. We will introduce NiO/Ni(OH) on the Ni side closer to the interface. Then, the 3H diffusion pathways and barriers from Ni side to the zircalory-4 will be explored. We will investigate how NiO/Ni(OH) affects the 3H diffusion across the interface.

Paudel, Hari P.↗

The CO2 mineralization potential of New Mexico basalts and associated critical element behavior and mobility.

This presentation reports on laboratory experiments assessing the carbon dioxide (CO₂) mineralization potential of New Mexico basalts, including trachybasalt and basalt lithologies. Using simulated groundwater and controlled conditions, the study evaluates the kinetics of CO₂ sequestration, mineral saturation indices, and secondary mineral formation. It also investigates the mobility of critical and trace elements such as Ni, Zn, Cu, and Li during basalt dissolution. Results indicate that New Mexico basalts can effectively sequester CO₂ through carbonate formation, with grain size and mineral composition influencing reaction rates and elemental behavior. These findings support the viability of geologic carbon storage in mafic volcanic terrains and inform strategies for critical element recovery.

36 MATERIALS SCIENCE↗

The potential for New Mexico basalts to sequester CO 2 with a focus on critical element mobility

This study evaluates the potential of New Mexico basaltic rocks and mafic mine waste for CO₂ sequestration via mineral carbonation. Batch experiments up to 200 days at 40°C simulated CO₂-bearing fluid interactions with various crushed basaltic materials at different grain sizes. Results showed that 70–80% of injected CO₂ was mineralized, with the finest grain sizes showing the most rapid and effective drawdown. The experiments also assessed the mobility of critical metals (Cu, Ni, Zn, Co), revealing trends tied to mineral dissolution and secondary mineral formation. The findings support the dual potential of mine waste for CO₂ sequestration and critical element recovery, informing future carbon capture and resource upcycling strategies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Development of Corrosion Resistant Coatings for Structural Materials for Liquid Fueled Molten Salts Reactors Applications (Final Report)

Current structural alloys, code certified for the MSRs temperature ranges, contain high levels of chromium, making them highly susceptible to molten halide salt corrosion. One potential solution to circumvent the need for code certification of novel alloys, which is expensive and time consuming, is to design claddings that will protect the underlying code certified materials from corrosion damage during operation. In this work, we examined the corrosion of Ni and Cu electroplated, Ni and CuNi weld overlay, Mo-laser clad, and carburized claddings on SS316H for use in molten salt reactor environments. After characterization of the cladded materials (Task 1), static corrosion tests were used to assess corrosion resistance of the claddings in typical molten fluoride salts (Task 2). The corrosion tests were performed in molten FLiNaK at 700°C up to 1000 hours. Pre- and post-corrosion Scanning Electron Microscopy (SEM), energy-dispersive-spectroscopy (EDS), Transmission Electron Microscopy (TEM), X-ray Diffraction (XRD) and glow-discharge-optical-emission-spectroscopy (GDOES) were performed on cladding cross-sections and surfaces to evaluate degradation. The Cu and Ni electroplated samples, as well as the carburized samples, showed excellent corrosion resistance relative to the bare SS316H. To assess high temperature cladding stability, ageing experiments were performed at temperatures up to 900 C in inert atmosphere for the electroplated and carburized samples and a diffusion model was developed to predict long term cladding behavior (Task 3). It was found that the Cu cladding was basically insensitive to the high temperature ageing, except for small secondary phases forming at the interface. On the other hand, the Ni electroplated cladding experienced significant interdiffusion. Nevertheless, the gain in corrosion resistance for a 100μm Ni electroplated cladding is phenomenal, with more than 50% reduction in chromium dissolution from the substrate material for the first 15 years of salt exposure at 700°C. To assess radiation resistance and phase stability, high-temperature 4MeV Ni heavy ion irradiation was performed across the cladding/substrate interface up to 50 displacement-per-atom (DPA) at 500°C and 700°C to assess the phase stability and irradiation behaviors of the electroplated systems (Task 4). The Ni and Cu electroplated systems did not experience void swelling at the contrary to the SS316H substrate due to their nanocrystalline nature. Some level of recrystallization was observed in the cladding, as well as radiation induced segregation and enhanced diffusion. The interface acted as a potent sink for point defects with the presence of a void denuded zone. The mechanical properties of the claddings were assessed using thermal shock, micro-indentation, nano-indentation, and four-point bend testing experiments (Task 5). These experiments were performed on the claddings in as-received, corroded, irradiated, and thermally aged states to determine the effects of typical molten salt reactor environments on cladding integrity. No significant mass loss was observed after repeated thermal shocks. While the electroplated samples softened after high-temperature ageing, irradiation hardening compensate this effect, such that there is little different with the as-received materials. The results of these experiments suggest that the electroplated (copper/nickel) show the greatest promise for application in molten salt reactor development. These claddings prevented any chromium dissolution from occurring during the static corrosion experiments. Additionally, they demonstrated favorable properties for high temperature diffusion, phase stability, interfacial mechanical properties, and irradiation resistance. Weld-overlay cladding are also of great interest and could reach properties similar to the electroplated samples upon optimization (especially with multiple weld passes). The carburized SS316H showed excellent behavior as well, but more work needs to be done to assess their long-term stability. Finally, the Mo-laser clad system was not pursued further due to the manufacturing challenges. It is also worth noting that the Ni cladding systems should behave relatively well in terms of weldability since the Ni-weld overlay microstructure and associated corrosion rate are sound. While the NiCu weld-overlay has even lower corrosion rates than the Ni-weld overlay, more studies on welding of Cu-electroplated systems are necessary since Cu clusters are known to embrittle steels.

36 MATERIALS SCIENCE↗

Optimizing a chemical cleaning protocol to determine the nickel isotopic composition of ancient seawater from carbonates

Reconstructing the ancient marine cycle of Ni, a trace metal in the oceans essential to enzymes regulating the C, N, and O cycles, would inform how Ni bioavailability shaped early life. The Ni isotopic composition of seawater (δ 60 Ni SW ) through time could provide insight, but this approach requires sedimentary archives that faithfully record δ 60 Ni SW . Carbonates are an often-used record of seawater chemistry, but contaminants could bias the measured δ 60 Ni of bulk sediment. To isolate the true carbonate-bound δ 60 Ni signal, we optimized a chemical cleaning protocol designed to minimize non‑carbonate Ni contributions and maximize carbonate recovery. We analyzed ODP Site 1007 sediments and evaluated oxidative and reductive pre-cleaning steps and carbonate dissolution protocols. Our results show that only reductive cleaning significantly altered the subsequent carbonate leachate composition, lowering Ni/Ca ratios by up to 60% and δ 60 Ni values by as much as 0.4 ‰. In contrast, δ 60 Ni values were largely insensitive to premature carbonate dissolution during pre-cleaning or to partial leaching of silicates during carbonate dissolution, even at higher acid molarities or longer reaction times. We recommend an evidence-based protocol that removes hydro-soluble salts and clays, applies reductive cleaning and oxidative cleaning for certain sample compositions, and dissolves carbonate using 0.5 M acetic acid, adjusted to pH 5. Using these results, we infer a ∼ 0.9 ‰ Ni isotopic fractionation between chemically cleaned deep-water carbonates (+0.4 ± 0.1 ‰) and deep seawater. This method development is a key step toward accurately reconstructing ancient marine Ni cycles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Protonation Stimulates the Layered to Rock Salt Phase Transition of Ni‐Rich Sodium Cathodes

Abstract Protonation of oxide cathodes triggers surface transition metal dissolution and accelerates the performance degradation of Li‐ion batteries. While strategies are developed to improve cathode material surface stability, little is known about the effects of protonation on bulk phase transitions in these cathode materials or their sodium‐ion battery counterparts. Here, using NaNiO 2 in electrolytes with different proton‐generating levels as model systems, a holistic picture of the effect of incorporated protons is presented. Protonation of lattice oxygens stimulate transition metal migration to the alkaline layer and accelerates layered‐rock‐salt phase transition, which leads to bulk structure disintegration and anisotropic surface reconstruction layers formation. A cathode that undergoes severe protonation reactions attains a porous architecture corresponding to its multifold performance fade. This work reveals that interactions between electrolyte and cathode that result in protonation can dominate the structural reversibility/stability of bulk cathodes, and the insight sheds light for the development of future batteries.

25 ENERGY STORAGE↗