Use of Ethylene Carbonate Free Ester Solvent Systems with Alternative Lithium Salts for Improved Low-Temperature Performance in NCM622∣∣ Graphite Li-ion Batteries

An investigation of alternative lithium salts, lithium tetrafluoroborate (LiBF 4 ), lithium difluoro(oxalato)borate (LiDFOB) and lithium hexafluorophosphate (LiPF 6 ), in novel ester-based (methyl acetate/fluoroethylene carbonate- MA/FEC or methyl propionate/fluoroethylene carbonate- MP/FEC) electrolyte formulations has been conducted in LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622)/graphite cells to improve low temperature cycling performance of lithium ion batteries at −20 °C. Improved low temperature performance was observed with all the lithium salts in MA/FEC electrolyte while comparable room temperature (25 °C) capacities were observed with LiPF 6 salt only. Detailed ex-situ analysis of surface films generated with LiBF 4 , LiDFOB and LiPF 6 in ester-based electrolytes reveals that the solid electrolyte interphase (SEI) is predominately composed of lithium salt decompaction products and addition of 10% FEC (by volume%) may not be sufficient at forming a protective SEI.

25 ENERGY STORAGE↗

Understanding and Mitigating the Dissolution and Delamination Issues Encountered with High-Voltage LiNi 0.5 Mn 1.5 O 4

In our initial study on the high-voltage 5 V cobalt-free spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode, we discovered a severe delamination issue in the laminates when cycled at a high upper cut-off voltage (UCV) of 4.95 V, especially when a large cell format was used. This delamination problem prompted us to investigate further by studying the transition metal (TM) dissolution mechanism of cobalt-free LNMO cathodes, and as a comparison, some cobalt-containing lithium nickel manganese cobalt oxides (NMC) cathodes, as the leachates from the soaking experiment might be the culprit for the delamination. Unlike other previous reports, we are interested in the intrinsic stability of the cathode in the presence of a baseline Gen2 electrolyte consisting of 1.2 M of LiPF 6 in ethylene carbonate/ethyl methyl carbonate (EC/EMC), similar to a storage condition. The electrode laminates (transition metal oxides, transition metal oxides, TMOs, coated on an Al current collector with a loading level of around 2.5 mAh/cm 2 ) or the TMO powders (pure commercial quality spinel LNMO, NMC, etc.) were stored in the baseline solution, and the transition metal dissolution was studied through nuclear magnetic resonance, such as 1 H NMR, 19 F NMR, scanning electron microscope (SEM), X-ray photoelectron spectroscopy (XPS) and inductively coupled plasma mass spectrometry (ICP-MS). Significant electrolyte decomposition was observed and could be the cause that leads to the TM dissolution of LNMO. To address this TM dissolution, additives were introduced into the baseline electrolyte, effectively alleviating the issue of TM dissolution. The results suggest that the observed delamination is caused by electrolyte decompositions that lead to etching, and additives such as lithium difluorooxalato borate and p-toluenesulfonyl isocyanate can alleviate this issue by forming a firm cathode electrolyte interface. This study provides a new perspective on cell degradation induced by electrode/electrolyte interactions under storage conditions.

25 ENERGY STORAGE↗

Electrolytes Containing Triethyl Phosphate Solubilized Lithium Nitrate for Improved Silicon Anode Performance

An electrolyte consisting of lithium nitrate (LiNO3) and lithium difluoro(oxalato)borate (LiDFOB) in ethylene carbonate (EC), ethylmethyl carbonate (EMC), and triethyl phosphate (TEP) is used to improve the long-term cycling stability of silicon anodes. TEP was selected for its ability to dissolve LiNO 3 in carbonates to a concentration of ~0.2 M. The large amount of LiNO 3 combined with the LiDFOB salt leads to a capacity retention of 87.1% after one hundred cycles due to the formation of a relatively stable solid electrolyte interphase (SEI). Ex-situ surface analysis reveals that the SEI consists of oxalates, lithium alkyl carbonates, borates, and nitrate reduction products. By selecting two components which are preferentially reduced (LiNO 3 and LiDFOB), the SEI is able to inhibit continuous solvent decomposition and allows for improved electrochemical cycling for pure silicon anodes.

25 ENERGY STORAGE↗

Performance Improvement of Lithium Metal Batteries Enabled By LiBF 3 CN as a New Electrolyte Additive

A newly synthesized electrolyte additive, lithium trifluoro(cyano) borate (LiBF 3 CN), has been investigated for electrochemical performance improvement of lithium metal batteries. The LiBF 3 CN has a structure where one fluorine atom of BF 4 – is substituted with a cyano group (–CN) prepared by the reaction of boron trifluoride etherate with lithium cyanide. The electrochemical performance in symmetric Li/Li cells and NCM523/Li cells is significantly improved upon the incorporation of LiBF 3 CN as an electrolyte additive into a carbonate-based electrolyte. Extensive characterization of the deposited lithium metal reveals that a thin (≈20 nm) and robust SEI composed of LiN x O y , Li 3 N and Li 2 O is formed by the reductive decomposition of the LiBF 3 CN additive, which plays an important role in decreasing the resistance and stabilizing lithium deposition/stripping. The insight into the substitution effect of a functional group obtained from this work provides guidance for the design of new electrolyte additives.

25 ENERGY STORAGE↗

Mitigating Calendar Aging in Si-NMC Batteries with Advanced Dual-Salt Glyme Electrolytes

In addressing the critical challenge of calendar aging in silicon (Si)-based lithium-ion batteries, this study introduces a groundbreaking strategy utilizing glyme-type dual-salt electrolytes (lithium bis(trifluoromethanesulfonyl)imide [LiTFSI] and lithium difluoro(oxalato)borate [LiDFOB]). These electrolytes are demonstrated to significantly mitigate parasitic reactions and capacity loss in Si-NMC (lithium nickel manganese cobalt oxide) full cells, especially when compared with traditional carbonate-based electrolytes. Further, our exhaustive mechanistic analysis reveals that such electrolytes not only preserve the integrity of the Si anode but also improve the cathode/electrolyte interphases (CEI) through the formation of a conformal coating on the high-voltage cathode surface. This dual-salt approach, enhanced by the addition of a phosphate additive, effectively decelerates calendar aging, marking a substantial advance in the quest for durable and reliable Si-based energy storage technologies. The findings underscore the vital role of electrolyte composition in extending the calendar life of Si batteries, offering an alternative avenue toward maximizing the performance and longevity of next-generation Li-Si batteries.

36 MATERIALS SCIENCE↗

Seamless aperture and length enlargement of single crystalline materials for high-energy laser applications

An optically seamless method for increasing the aperture or length of nonlinear materials has been developed, which is suitable for optics in high energy laser systems and other applications. Differences between aperture and length scaling are analyzed. Bonding of component pairs of a nonlinear crystal, lithium tri-borate, is experimentally demonstrated by GAMDAN Optics Inc. and tested at the Laboratory of Laser Energetics at the University of Rochester. Here, a bonded crystal is shown to deliver beam quality and second harmonic conversion efficiency that is equivalent to that of a monolithic crystal of similar dimensions.

aperture scaling↗

Succinonitrile-Lithium Salt Complexes as Solid Catholytes for LLZO-Based Solid-State Batteries

The thermal and electrochemical properties of several succinonitrile (SN)-based organic ionic plastic crystals (OIPCs) containing lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), lithium bis(oxalate) borate (LiBOB) or mixtures of the two salts, were investigated with the goal of determining which is most promising for use as a catholyte in solid-state lithium batteries. The best combination of properties for this use was found for the mixture containing 3 mol% LiTFSI and 2 mol% LiBOB in SN. Based on these observations, several solid-state cells containing Al-substituted Li 7 La 3 Zr 2 O 12 separators with composite cathodes consisting of LiNi 0.33 Mn 0.33 Co 0.33 O 2 (NMC111), carbon black, and the succinonitrile-salt mixtures were assembled and cycled at room temperature, without exogenous pressure, using a simple design.

25 ENERGY STORAGE↗

The Evaluation of Triphenyl Phosphate as a Flame Retardant Additive to Improve the Safety of Lithium-Ion Battery Electrolytes

With the intent of improving the safety characteristics of lithium ion cells, electrolytes containing flame retardant additives have been investigated. A number of triphenyl phosphate-containing electrolytes were evaluated in both coin cells and experimental three electrode lithium-ion cells (containing reference electrodes). A number of chemistries were investigated, including MCMB carbon/LiNi(0.8)Co(0.2)O2 (NCO), graphite/LiNi(0.8)Co(0.15)Al(0.05)O2 (NCA), Li/Li(Li(0.17)Ni(0.25)Mn(0.58))O2, Li/LiNiMnCoO2 (NMC) and graphite/LiNiMnCoO2 (NMC), to study the effect that different electrolyte compositions have upon performance. A wide range of TPP-containing electrolytes were demonstrated to have good compatibility with the C/NCO, C/NCA, and Li/NMC systems, however, poor performance was initially observed with the high voltage C/NMC system. This necessitated the development of improved electrolytes with stabilizing additives, leading to formulations containing lithium bis(oxalato)borate (LiBOB) that displayed substantially improved performance.

rechargable batteries↗

Electrolytes with Improved Safety Developed for High Specific Energy Li-Ion Cells with Si-Based Anodes

A number of electrolyte formulations that have improved safety characteristics have been developed for use with high capacity silicon-based anodes. To improve the compatibility with Si-based anodes, a number of technical approaches have been employed, including: (1) the use of mono-fluoroethylene carbonate (FEC) in conjunction with, or in lieu of, ethylene carbonate (EC), (2) the use of high proportions of fluorinated co-solvents, (3) the use of vinylene carbonate (VC) to stabilize the Si/C electrode, and (4) the use of lithium bis(oxalato)borate (LiBOB) to improve the compatibility of the electrolyte when Si/C electrodes are used in conjunction with high voltage cathodes. Candidate electrolytes were studied in Li/Si-C and Si-C/ Li(MnNiCo)O2 (NMC) coin cells, as well as in larger Si-C/NMC three-electrode cells equipped with lithium reference electrodes. In summary, many electrolytes that contain triphenyl phosphate (TPP), which is used as a flame retardant additive up to concentrations of 15 volume percent, and possess FEC as a co-solvent have been demonstrated to outperform the all-carbonate baseline electrolytes when evaluated in Si-C/ Li(MnNiCo)O2 cells.

Silicon-Based Anode↗

Use of Additives to Improve Performance of Methyl Butyrate-Based Lithium-Ion Electrolytes

This work addresses the need for robust rechargeable batteries that can operate well over a wide temperature range. To this end, a number of electrolyte formulations have been developed that incorporate the use of electrolyte additives to improve the high-temperature resilience, low-temperature power capability, and life characteristics of methyl butyrate-based electrolyte solutions. These electrolyte additives include mono-fluoroethylene carbonate (FEC), lithium oxalate, vinylene carbonate (VC), and lithium bis(oxalato)borate (LiBOB), which have been shown to result in improved high-temperature resilience of all carbonate-based electrolytes. Improved performance has been demonstrated of Li-ion cells with methyl butyrate-based electrolytes, including 1.20M LiPF6 in EC+EMC+MB (20:20:60 v/v %); 1.20M LiPF6 in EC+EMC+MB (20:20:60 v/v %) + 2% FEC; 1.20M LiPF6 in EC+EMC+MB (20:20:60 v/v %) + 4% FEC; 1.20M LiPF6 in EC+EMC+MB (20:20:60 v/v %) + lithium oxalate; 1.20M LiPF6 in EC+EMC+MB (20:20:60 v/v %) + 2% VC; and 1.20M LiPF6 in EC+EMC+MB (20:20:60 v/v %) + 0.10M LiBOB. These electrolytes have been shown to improve performance in MCMB-LiNiCoO2 and graphite-LiNi1/3Co1/3Mn1/3O2 experimental Li-ion cells. A number of LiPF6-based mixed carbonate electrolyte formulations have been developed that contain ester co-solvents, which have been optimized for operation at low temperature, while still providing reasonable performance at high temperature. For example, a number of ester co-solvents were investigated, including methyl propionate (MP), ethyl propionate (EP), methyl butyrate (MB), ethyl butyrate (EB), propyl butyrate (PB), and butyl butyrate (BB) in multi-component electrolytes of the following composition: 1.0M LiPF6 in ethylene carbonate (EC) + ethyl methyl carbonate (EMC) + X (20:60:20 v/v %) [where X = ester co-solvent]. ["Optimized Car bon ate and Ester-Based Li-Ion Electrolytes", NASA Tech Briefs, Vol. 32, No. 4 (April 2008), p. 56.] Focusing upon improved rate capability at low temperatures (i.e., 20 to 40 C), this approach was optimized further, resulting in the development of 1.20M LiPF6 in EC+EMC+MP (20:20:60 v/v %) and 1.20M LiPF6 in EC+EMC+EB (20:20:60 v/v %), which were demonstrated to operate well over a wide temperature range in MCMB-LiNiCoAlO2 and Li4Ti5O12(-)LiNiCoAlO2 prototype cells.

Smart, Marshall C.↗

Improved Performance of Silicon-Containing Anodes with Organic Solvent-Solubilized Lithium Nitrate

Three different organic solvents (dimethylacetamide (DMAc), dimethylformamide (DMF), and dimethyl sulfoxide (DMSO)) were used to improve the solubility of LiNO 3 in a standard carbonate-based electrolyte with lithium difluoro(oxalato)borate (LiDFOB) as the salt. Together, the LiDFOB and organic-solvent solubilized LiNO 3 preferentially reduce on the surface of silicon-containing anodes to create an SEI rich in oxalates, nitrate decomposition species, and B-F species. The improved stability of the SEI throughout the first 100 cycles results in silicon and silicon/graphite composite anodes with better capacity retention than observed with standard electrolytes or fluoroethylene carbonate (FEC) containing electrolytes. This study demonstrates the feasibility of the use of non-traditional electrolyte solvents in the improvement and optimization of lithium ion-battery electrolytes.

25 ENERGY STORAGE↗

Modulating physicochemical interfaces enables li-rich oxides based ceramic solid-state li batteries under ambient conditions

Li-rich layered oxides exhibit promising potential applications in high-energy-density solid-state lithium metal batteries. Nevertheless, the strong oxidative oxygen species generate at high voltage, which poses great challenges to positive electrode-side interface stability. Herein, a robust in-situ polymerization gel polymer electrolyte with bifunctional additives is designed for interface modification. These additives, include lithium difluoro(oxalate) borate and LiPO 2 F 2 , regulate the Li + chemical environment in gel polymer electrolyte to enhance crosslink density without residual oligomer, which reduce gas generation and suppress contact loss, thus avoiding interfacial impedance divergence. Concurrently, the designed gel polymer electrolyte enables a wide electrochemical stability window (up to 4.7 V) and a high Li + transference number (0.82). Additionally, the additives induced F- and B-rich inorganic cathode-electrolyte interphase inhibits side reactions and oxygen/transition metal loss effectively, stabilizing the chemical interface. The as-constructed Li-rich layered oxides-based ceramic solid-state lithium metal batteries with gel polymer electrolyte interface modification exert a high discharge capacity of 276.5 mAh g -1 at 30 °C without external pressure, delivering a retention of 81.7% after 100 cycles at 25 mA g -1 during 2.0-4.7 V. This work provides a guideline for developing high-voltage solid-state lithium metal batteries via interfacial design.

Hu, Xinchao [Xiamen University (China)]↗

Novel Low-Temperature Electrolyte Using Isoxazole as the Main Solvent for Lithium-Ion Batteries

A novel electrolyte system with an excellent low temperature performance for lithium-ion batteries (LIBs) has been developed and studied. It was discovered for the first time, in this work, that when isoxazole (IZ) was used as the main solvent, the ionic conductivity of the electrolyte for LIBs is more than doubled in a temperature range between -20 and 20 °C compared to the baseline electrolyte using ethylene carbonate–ethyl methyl carbonate as solvents. To solve the problem of solvent cointercalation into the graphite anode and/or electrolyte decomposition, the lithium difluoro(oxalato)borate (LiDFOB) salt and fluoroethylene carbonate (FEC) additive were used to form a stable solid electrolyte interphase on the surface of the graphite anode. Benefitting from the high ionic conductivity at low temperature, cells using a new electrolyte with 1 M LiDFOB in FEC/IZ (1:10, vol %) solvents demonstrated a very high reversible capacity of 187.5 mAh g -1 at -20 °C, while the baseline electrolyte only delivered a reversible capacity of 23.1 mAh g -1 .

25 ENERGY STORAGE↗

Influence of Electrolyte Additives on Interfacial Stability of Manganese-Rich Lithium-Ion Battery Cathodes

Affordable, long-lasting energy storage has become critical to support increased electricity demand in recent years. Cobalt-free, lithium- and manganese-rich lithium nickel manganese oxide (LMR-NM) cathodes stand to reduce cost and supply-chain concerns associated with traditional cobalt-containing cathodes for lithium-ion batteries by leveraging more earth-abundant materials; however, they have shown issues with long-term cycling stability. Here, we investigate lithium difluoro(oxalate)borate (LiDFOB), tris(trimethylsilyl) phosphite (TMSPi), and vinylene carbonate (VC) electrolyte additives for their ability to improve cycling performance of LMR-NM (0.3 Li 2 MnO 3 + 0.7 LiMn 0.5 Ni 0.5 0 2 ) cells. Cryogenic scanning transmission electron microscopy (cryo-STEM) with electron energy loss spectroscopy enables the construction of a structure–function relationship between cathode electrolyte interphase (CEI) characteristics and the electrochemical performance of cells aged with these additives. We find the combination of 2 wt % TMSPi + 1 wt % LiDFOB performs better than any single additive, achieving a 28% improvement in specific capacity over the baseline electrolyte after long-term cycling. We attribute this to LiDFOB mitigating Mn ion dissolution, with cryo-STEM showing Mn stabilized up to the CEI surface, coupled with improved CEI structure and chemistry enabled by TMSPi, evidenced by a moderately thick (∼7–15 nm) CEI that appears to protect against further electrolyte reactions with the particle. These results, achieved through site-specific nanoscale characterization, directly reveal mechanisms through which electrolyte engineering can improve the performance of earth-abundant cathodes, enabling informed development of more affordable and reliable batteries to meet future energy storage needs.

25 ENERGY STORAGE↗

Fast-Charging Li-Ion Battery Enabled by an Acetonitrile-Based Electrolyte

Fast charging remains a critical challenge for current-generation lithium-ion batteries (LIBs), particularly in electric vehicle applications. Here, in this study, we present a highly conductive electrolyte formulation based on a ternary solvent system consisting of acetonitrile (AN), fluoroethylene carbonate (FEC), and ethylene carbonate (EC), combined with a tailored additive, lithium difluoro­(oxalato)­borate (LiDFOB). This electrolyte demonstrates significantly enhanced ionic conductivity and a higher Li + transference number, enabling accelerated Li + transport kinetics. The synergistic effect of the solvents and the additive promotes the formation of a robust, low-resistance, inorganic-rich solid-electrolyte-interphase (SEI) that effectively passivates the graphite surface and suppresses AN decomposition. As a result, the electrolyte substantially reduces internal cell resistance and overpotential, both of which are critical for reliable fast charging. These findings highlight the essential role of rational electrolyte design in addressing the limitations of fast-charging LIBs.

Wu, Dezhen [Argonne National Laboratory (ANL), Arg↗

Improved Low Temperature Performance of Graphite/Li Cells Using Isoxazole as a Novel Cosolvent in Electrolytes

An investigation of novel electrolyte formulations to improve low temperature performance of Li/graphite half cells has been conducted. A novel electrolyte co-solvent, isoxazole (IZ), has been investigated in electrolyte systems composed of lithium difluoro(oxalato)borate (LiDFOB) in fluoroethylene carbonate (FEC) and LiDFOB in ethylene carbonate (EC). Cells containing 1 M LiDFOB FEC: IZ electrolyte have a significant improvement in capacity retention and reversible capacity at −10 °C. Ex-situ surface analysis of the cycled electrodes suggests that reduction of LiDFOB results in an oxalate rich solid electrolyte interphase (SEI). Addition of FEC, results in improved stability of the anode SEI preventing further decomposition of isoxazole solvent and improving cycling performance.

25 ENERGY STORAGE↗

Performance of a Novel In-Situ Converted Additive for High Voltage Li-ion Pouch Cells

In search for new classes of additives for high voltage NMC/graphite lithium-ion cells, the precursor additive bis(trimethylsilyl) malonate (bTMSM) is shown to be activated via a spontaneous reaction with LiPF 6 and LiBF 4 salts in carbonate-based electrolyte to form lithium tetrafluoro(malonato)phosphate (LiTFMP), and lithium difluoro(malonato)borate (LiDFMB), respectively. The reaction schemes and rates were studied via NMR spectroscopy and GCMS. The effects of LiTFMP and LiDFMB on high voltage electrochemical performance were then examined up to 4.5 V in Li[Ni 0.4 Mn 0.4 Co 0.16 ]O 2 (NMC442)/graphite and Li[Ni 0.6 Mn 0.4 Co 0.0 ]O 2 (NMC/640)/graphite pouch cells using aggressive voltage-hold cycling, long-term charge/discharge cycling, storage experiments, electrochemical impedance spectroscopy, and gas evolution measurements. While in situ converted additives suffer from gassing issues due to the presence of trimethylfluorosilane (TMSF) gas, a side product of the in situ reaction of bTMSM with LiPF 6 , the cycling and storage capability for the activated additives under study shows competitive performance and controlled impedance when compared to other well-known high voltage additives. Micro X-ray fluorescence spectroscopy (μXRF) confirmed that LiTFMP successfully minimizes the rate of transition metal deposition on the surface of graphite apparently by forming a protective agent at the cathode surface, hence allowing for improved cycling performance at high voltages.