Pristine Interface between Lithium Lanthanum Zirconate and Lithium Manganese Oxide by Pulsed Laser Deposition

Solid state lithium-ion batteries have garnered increasing interest in recent years due to several potential advantages over liquid-electrolyte based systems. The possibility of integrating the lithium garnet oxide, Li 6.75 La 3 Zr 1.75 Ta 0.25 O 12 (LLZTO), with the high voltage cathode, spinel Li x Mn 2 O 4 (LMO), is evaluated here. Thin film bilayer structures are prepared by pulsed laser deposition on MgO (001) substrates and characterized by x-ray diffraction and transmission electron microscopy. The LLZTO is grown by an alternating layer-by-layer deposition of LLZTO and Li 3 N and subsequently annealed for several hours at 575 °C to promote crystallinity. Growth of crystalline LMO with a pristine interface to LLZTO is achieved by gentle heat treatment (500 °C) to remove surface carbonate from the electrolyte and by cathode growth at a low temperature of 250 °C. Higher temperature depositions (330 – 450 °C) result in reaction between the two materials and the appearance of Li 2 MnO 3 , which may be in part due to the presence of excess lithium in the electrolyte layer. Because fully lithiated LiMn 2 O 4 has a voltage of ≈3.7 V versus Li+/Li, the observation of a well-defined interface, free of impurity phases and with no interdiffusion of elements, indicates LLZTO is stable to at least 3.7 V.

Garnet LLZO↗

3D LiMn 2 O 4 nThin Film Deposited by ALD: A Road toward High-Capacity Electrode for 3D Li-Ion Microbatteries

Miniaturized electronics suffer from a lack of energy autonomy. In that context, the fabrication of lithium-ion solid-state microbatteries with high performance is mandatory for powering the next generation of portable electronic devices. Here, the fabrication of a thin film positive electrode for 3D Li-ion microbatteries made by the atomic layer deposition (ALD) method and in situ lithiation step is demonstrated. The 3D electrodes based on spinel LiMn 2 O 4 films operate at high working potential (4.1 V vs Li/Li + ) and are capable of delivering a remarkable surface capacity (approximate to 180 mu Ah cm -2 ) at low C-rate while maintaining more than 40 mu Ah cm -2 at C/2 (time constant = 2 h). Both the thickness of the electrode material and the 3D gain of the template are carefully tuned to maximize the electrode performance. Further, advanced characterization techniques such as transmission electron and X-ray transmission microscopies are proposed as perfect tools to study the conformality of the deposited films and the interfaces between each layer: no interdiffusion or segregation are observed. This work represents a major issue towards the fabrication of 3D-lithiated electrode by ALD-without any prelithiation step by electrochemical technique-making it an attractive solution for the fabrication of 3D Li-ion solid-state microbatteries with semiconductor processing methods.

3D Li-ion micro-batteries↗

Long-term cyclability of Li 4 Ti 5 O 12 /LiMn 2 O 4 cells using carbonate-based electrolytes for behind-the-meter storage applications

Li 4 Ti 5 O 12 /LiMn 2 O 4 (LTO/LMO) chemistry was evaluated as a potential candidate for behind-the-meter storage (BTMS) applications. Its long-term cycle performance at 45 °C was tested using ethylene carbonate (EC) and propylene carbonate (PC) solvent electrolytes. Over 1000 cycles, LTO/LMO cells exhibited ~80% capacity retention and Coulombic efficiency higher than 99.96%. Electrochemical test results showed the major degradation mode of LTO/LMO cells arises from continuous electrolyte decomposition at the LTO anode and loss of Li inventory. EC and PC electrolytes created distinct surface layers, where the EC reduction products were more effective in passivating the LTO electrode surface. Dissolution and migration of Mn from the cathode was probed as Mn 2+ species distributed throughout the surface layer at the anode. By utilizing a prelithiated LTO electrode, the LTO/LMO cell performance was significantly enhanced with EC electrolyte. On the other hand, PC electrolyte resulted in accelerated electrolyte decomposition at the lithiated LTO surface due to the lack of surface passivation. Thus, mitigating parasitic reactions at the LTO electrode is the key to developing successful LTO/LMO cells.

25 ENERGY STORAGE↗

Thermally Aged Li–Mn–O Cathode with Stabilized Hybrid Cation and Anion Redox

Though low-cost and environmentally friendly, Li–Mn–O cathodes suffer from low energy density. Although synthesized Li 4 Mn 5 O 12 -like overlithiated spinel cathode with reversible hybrid anion- and cation-redox (HACR) activities has a high initial capacity, it degrades rapidly due to oxygen loss and side-reaction-induced electrolyte decomposition. In this study, we develop a two-step heat treatment to promote local decomposition as Li 4 Mn 5 O 12 → 2LiMn 2 O 4 + Li 2 MnO 3 + 1/2 O 2 ↑, which releases near-surface reactive oxygen that is harmful to cycling stability. The produced nanocomposite delivers a high discharge capacity of 225 mAh/g and energy density of over 700 Wh/kg at active-material level at a current density of 100 mA/g between 1.8 to 4.7 V. Benefiting from suppressed oxygen loss and side reactions, 80% capacity retention is achieved after 214 cycles in half cells. With industrially acceptable electrolyte amount (6 g/Ah), full cells paired with Li 4 Ti 5 O 12 anode have a good retention over 100 cycles.

25 ENERGY STORAGE↗