Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “LLZO solid-state electrolyte”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Developing cathode infiltration processes for all-solid-state bilayer LLZO cells

To realize the bilayer architecture of lithium lanthanum zirconate (LLZO) for application in solid-state batteries (SSBs), the scaffold structure must be optimized, and effective cathode infiltration strategies must be established. In this study, we fabricate a modified bilayer LLZO using a sacrificial layer to enhance surface porosity, and systematically investigate various cathode infiltration techniques to fill the scaffold with oxide cathode active materials (CAM). Structural characterizations showed that the sacrificial layer significantly increased open surface porosity, enabling the surface of the scaffold to be filled with CAM. To further increase infiltration depth, applying vacuum or vibration was compared, with the full-depth infiltration achieved using a sonicator-based vibration. Full cells prepared using the modified bilayer LLZO and vibration-assisted technique demonstrated successful operation. This work demonstrates a practical and scalable approach for engineering bilayer LLZO structures and integrating oxide cathodes into porous scaffolds, offering a promising pathway toward high-performance solid-state batteries.

Bilayer↗

Heterogeneous doping via nanoscale coating impacts the mechanics of Li intrusion in brittle solid electrolytes

Lithium dendrite intrusion in solid-state batteries limits fast charging and causes short-circuiting, yet the underlying regulating mechanisms are not well-understood. Here, in this work, we discover that heterogeneous Ag + doping dramatically affects lithium intrusion into Li 6.6 La 3 Zr 1.6 Ta 0.4 O 12 (LLZO), a brittle solid electrolyte. Nanoscale Ag + doping is achieved by thermally annealing a 3-nm-thick metallic coating on LLZO, inducing Ag–Li ion exchange and Ag diffusion into grains and grain boundaries. Density functional theory calculations and experimental characterization show negligible impact on the electronic properties and surface wettability from Ag + incorporation. Mechanically, nanoindentation experiments show a fivefold increase in the mechanical force required to fracture the surface Ag + -doped LLZO, indicating substantial doping-induced surface toughening. Operando microprobe scanning electron microscopy experiments show that the Ag + -doped LLZO surface exhibits improved lithium plating at >250 mA cm −2 and an electroplating diameter that is expanded by over fourfold, even under an extreme indentation stress of 3 GPa. This demonstrates enhanced defect tolerance in LLZO, rather than electronic or adhesion effects. Our study reveals a chemo-mechanical mechanism via surface heterogeneous doping, complementing present bulk design rules to minimize mechanical failures in solid-state batteries.

36 MATERIALS SCIENCE↗

Improved interfacial li-ion transport in composite polymer electrolytes via surface modification of LLZO

Composite polymer electrolytes that incorporate ceramic fillers in a polymer matrix offer mechanical strength and flexibility as solid electrolytes for lithium metal batteries. However, fast Li + transport between polymer and Li + -conductive filler phases is not a simple achievement due to high barriers for Li + exchange across the interphase. This study demonstrates how modification of Li 7 La 3 Zr 2 O 12 (LLZO) nanofiller surfaces with silane chemistries influences Li + transport at local and global electrolyte scales. Anhydrous reactions covalently link amine-functionalized silanes [(3-aminopropyl)triethoxysilane (APTES)] to LLZO nanoparticles, which protects LLZO in air. APTES functionalization lowers the poly (ethylene oxide) (PEO)-LLZO interphase resistance to half that of unmodified LLZO and increases effective Li + transference number, while insulating Al 2 O 3 completely blocks ion exchange and lowers transference number and conductivity in PEO-lithium bis(trifluoromethanesulfonyl)imide (LiTFSI)-LLZO composites. Modeling an inner resistive interphase between LLZO and PEO surrounded by an outer conductive interphase explains non-linear conductivity trends. Solid-state 7 Li & 6 Li nuclear magnetic resonance shows Li + only exchanges between PEO-LiTFSI and some LLZO interphase, with no appreciable Li + transport through bulk LLZO. Surface functionalization is a promising path toward lowering the polymer-ceramic interphase resistance. This work demonstrates that local changes in Li + transport affect macroscopic performance, highlighting the intricate relationships between all interfaces in inherently heterogeneous composite polymer electrolytes.

25 ENERGY STORAGE↗

Methods for Quantitative Thermal Analysis of Lithium Solid-State and Beyond Battery Safety

The use of differential scanning calorimetry (DSC) to measure the thermal behavior of individual components and electrolyte/electrode combinations is common. However, here we focus on DSC tests on an anode, cathode, and electrolyte (ACE) component combination over a temperature range that includes many of the phase transitions and key reactions (i.e., to 500 °C) that contribute to thermal runaway. This method can help quantify the complex reaction network in a full cell, thereby informing potential safety issues. Here, we used DSC heat flow data from a solid-state Li 0.43 CoO 2 +C+PVDF | LLZO | Li metal ACE sample and its components to quantify key factors affecting results. We focused on three areas: (1) ACE sample preparation and assembly in DSC pans, (2) DSC measurement parameters, and (3) heat flow analysis. Key points include the choice of component ratios (e.g., commercially relevant N:P capacity ratio), the importance of conductive carbon and binder, type of pan used, DSC ramp rate, and integration method used when dealing with broad and overlapping exothermic peaks. This work deepens the scientific basis and best practices for obtaining heat flow data from ACE samples for early-stage evaluation of solid-state and beyond battery safety.

25 ENERGY STORAGE↗

Understanding the Influence of Li 7 La 3 Zr 2 O 12 Nanofibers on Critical Current Density and Coulombic Efficiency in Composite Polymer Electrolytes

Composite polymer electrolytes (CPEs)are attractive materials for solid-state lithium metal batteries, owing to their high ionic conductivity from ceramic ionic conductors and flexibility from polymer components. As with all lithium metal batteries, however, CPEs face the challenge of dendrite formation and propagation. Not only does this lower the critical current density (CCD) before cell shorting, but the uncontrolled growth of lithium deposits may limit Coulombic efficiency (CE) by creating dead lithium. Here, we present a fundamental study on how the ceramic components of CPEs influence these characteristics. CPE membranes based on poly-(ethylene oxide) and lithium bis-(trifluoro methane sulfonyl)-imide(PEO-LiTFSI) with Li 7 La 3 Zr 2 O 12 (LLZO) nanofibers were fabricated with industrially relevant roll-to-roll manufacturing techniques. Galvanostatic cycling with lithium symmetric cells shows that the CCD can be tripled by including 50 wt % LLZO, but half-cell cycling reveals that this comes at the cost of CE. Varying the LLZO loading shows that even a small amount of LLZO drastically lowers the CE, from 88% at 0 wt % LLZO to 77% at just 2 wt % LLZO. Mesoscale modeling reveals that the increase in CCD cannot be explained by an increase in the macroscopic or microscopic stiffness of the electrolyte; only the microstructure of the LLZO nanofibers in the PEO-LiTFSI matrix slows dendrite growth by presenting physical barriers that the dendrites must push or grow around. This tortuous lithium growth mechanism around the LLZO is corroborated with mass spectrometry imaging. In conclusion, this work highlights important elements to consider in the design of CPEs for high-efficiency lithium metal batteries.

36 MATERIALS SCIENCE↗

Nanoscale Ion Transport Enhances Conductivity in Solid Polymer-Ceramic Lithium Electrolytes

The predictive design of flexible and solvent-free polymer electrolytes for solid-state batteries requires an understanding of the fundamental principles governing the ion transport. In this work, we establish a correlation among the composite structures, polymer segmental dynamics, and lithium ion (Li + ) transport in a ceramic-polymer composite. Elucidating this structure–property relationship will allow tailoring of the Li + conductivity by optimizing the macroscopic electrochemical stability of the electrolyte. The ion dissociation from the slow polymer segmental dynamics was found to be enhanced by controlling the morphology and functionality of the polymer/ceramic interface. The chemical structure of the Li + salt in the composite electrolyte was correlated with the size of the ionic cluster domains, the conductivity mechanism, and the electrochemical stability of the electrolyte. Polyethylene oxide (PEO) filled with lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) or lithium bis(fluorosulfonyl) imide (LiFSI) salts was used as a matrix. A garnet electrolyte, aluminum substituted lithium lanthanum zirconium oxide (Al-LLZO) with a planar geometry, was used for the ceramic nanoparticle moieties. Further, the dynamics of the strongly bound and highly mobile Li + were investigated using dielectric relaxation spectroscopy. The incorporation of the Al-LLZO platelets increased the number density of more mobile Li + . The structure of the nanoscale ion-agglomeration was investigated by small-angle X-ray scattering, while molecular dynamics (MD) simulation studies were conducted to obtain the fundamental mechanism of the decorrelation of the Li + in the LiTFSI and LiFSI salts from the long PEO chain.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Riddle of Dark LLZO: Cobalt Diffusion in Garnet Separators of Solid‐State Lithium Batteries

Abstract Solid‐state batteries (SSBs) with a Li 7 La 3 Zr 2 O 12 (LLZO) garnet electrolyte are attracting much attention as robust and safe alternative to conventional lithium‐ion batteries. Technical challenges in the practical implementation of garnet SSBs are related to the need for high‐temperature sintering, which often leads to undesirable chemical reactions with the cathode material. While these reactions are well understood for composite cathodes, very little is known about similar processes between cathode and separator during battery fabrication. This work focuses on understanding the processes between the composite LiCoO 2 ‐LLZO cathode and the LLZO separator and how they affect the battery performance. The extensive diffusion of Co‐ions within LLZO, which leads to the often‐observed LLZO darkening, is shown to have a significant impact on ionic conductivity, electronic conductivity, and dendrite stability of the separator. Experimental data coupled with large‐scale molecular dynamics simulations uncover the diffusion mechanism for Co‐ions and identify secondary phases that form during these interactions. In addition to extensive Co‐ion diffusion within the grains, a non‐uniform segregation of Co‐ions at grain boundaries is found leading to the formation of three distinct Co‐containing phases. This work offers a general approach to studying the fundamental ion diffusion processes that occur during the fabrication of oxide SSBs.

electrochemical properties↗

Room-temperature fabrication of garnet-type solid-electrolyte: Optimizing particle size for high ionic conductivity

Dense and uniform Li 6.25 Al 0.25 La 3 Zr 2 O 12 (Al-doped LLZO) solid-electrolyte film of ~24 µm thickness is successfully fabricated by room temperature aerosol deposition (AD) method. The process optimization study revealed that careful control of particle size and morphology is one of critical determinants in the development of a compact AD membrane. Notably, our method facilitated an impressive ionic conductivity of approximately 10 –5 S cm –1 , bypassing the necessity for post-annealing processes, a milestone in itself. However, it is hypothesized that the attained conductivity is somewhat restrained by factors such as smaller grain size and potential surface degradation due to moisture exposure during fabrication, indicating avenues for further research. Looking forward, detailed investigations into the film's microstructure and its impact on transport properties will be a focal point, alongside potential enhancements through post-annealing and particle coating strategies. Finally, this research hints at a promising trajectory for the development of high-efficiency solid-state battery technology.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ion Size Effects on the Thermodynamic, Kinetic, and Mechanical Properties during Ion Exchange in Solid-State Electrolytes

Ion exchange offers a pathway to impose residual compressive stresses to mitigate the electro-chemo-mechanical cracking of solid-state electrolytes such as lithium lanthanum zirconium oxide. This study uses a coupled multiscale framework (integrating density functional theory (DFT), molecular dynamics (MD), and continuum modeling) to examine how exchange ion size influences stress, diffusion, fracture toughness, and electronic properties. Larger isovalent ions (Na + , Ag + , K + ) were exchanged with Li + , with DFT confirming their preference for octahedral 96h sites and a linear relationship between ion size and chemical free expansion coefficient. MD simulations reveal stress and concentration effects on exchange ion diffusivity at elevated temperatures, with Na + and Ag + maintaining favorable mobility while K + showing concentration-dependent clustering. Continuum modeling predicts the range of fracture strength improvements and the required ion exchange concentration profile. It was shown that a 5% surface exchange concentration can induce ∼0.6 GPa of surface compressive stress using Na + and ∼1.0 GPa of surface compressive stress using Ag + . On the other hand, larger ion exchange species may penalize Li + diffusivity by increasing the activation volume and activation energy. Interestingly, Na + has a negligible penalty on Li-ion diffusivity. The room temperature Li + ion diffusivity is reduced by ∼40% with Ag + ion exchange. Electronic band structure analysis shows no size-dependent change in the bandgap, though Ag + introduces localized defect states near the valence band maximum. This study highlights ion size as a key factor in optimizing LLZO properties, offering a framework to improve the solid-state battery performance.

Jagad, Harsh D. [Brown Univ., Providence, RI (Unit↗

Identifying Bounds of Inorganic Content in Solventless Processing of Hybrid Solid Electrolytes

Solid-state lithium batteries require safe, robust electrolytes to enable higher energy densities and improved safety over conventional cells. Hybrid polymer–ceramic electrolytes are a promising solution, combining the processability of polymers with the high ionic conductivity and mechanical strength of inorganic fillers. In this work, we demonstrate a solventless, UV-curing method to produce hybrid solid electrolytes using a poly(ethylene glycol) dimethyl ether (PEGDME)-based photocurable matrix incorporating Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 (LAGP) or Li 7 La 3 Zr 2 O 12 (LLZO) ceramic electrolyte. Inorganic filler loadings up to ∼55 wt.% could be successfully incorporated via this process which was the highest inorganic content at which the slurry remains processable and cured into a uniform film. The resulting UV-cured composite electrolytes remain flexible and exhibit room-temperature ionic conductivities on the order of 10 −4 S·cm −1 , along with notably improved lithium-ion transference numbers compared to conventional polymer electrolytes. Similar performance and processing limits were observed for both LAGP and LLZO, indicating that ceramic filler chemistry does not significantly affect the UV-curing process or the electrolyte's ion transport properties in this regime. Eliminating solvents from fabrication not only simplifies processing and mitigates environmental concerns but also enables higher solid contents that enhance mechanical strength and help suppress lithium dendrite formation. In conclusion, this scalable approach thus paves the way for manufacturing robust composite solid electrolytes for next-generation solid-state batteries (SSBs).

Batteries↗

Highly disordered amorphous Li-battery electrolytes

"Medium-entropy" highly disordered amorphous Li garnets, with ≥4 unique local bonding units (LBUs), hold promise for use as solid-state electrolytes in hybrid or all-solid-state batteries owing to their grain-boundary-free nature and low-temperature synthesis requirement. Through this work, we resolved the local structure of amorphous Li garnet and understood their implication for Li dynamics. These medium-entropy amorphous structures possess unique characteristics with edge- and face-sharing LBUs, not conforming to the classic Zachariasen glass formation rules, and can be synthesized in a wide but processing-friendly temperature range (<680°C). Within these amorphous structures, Li and Zr are identified as the network formers and La as network modifier, with maxima in Li dynamics observed for smaller Li-O and Zr-O coordination; this structure understanding serves as a baseline for identifying additional network formers to further modulate Li transport. In conclusion, our insight provides fundamental guidelines for the structure and phase design for amorphous Li garnets and paves the way for their integration in next-generation batteries.

25 ENERGY STORAGE↗

Electro-Chemo-Mechanical Evolution at the Garnet Solid Electrolyte–Cathode Interface

Solid-state batteries promise higher energy density and improved safety compared with lithium-ion batteries. However, electro-chemomechanical instabilities at the solid electrolyte interface with the cathode and the anode hinder their large scale implementation. Here, in this study, we focus on resolving electro-chemo-mechanical instability mechanisms and their onset conditions between a state-of-the-art cathode, LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622), and the garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte. We used thin-film NMC622 on LLZO pellets to place the interfacial region within the detection depth of the X-ray characterization techniques. The experimental probes of the near-interface region included in operando X-ray absorption spectroscopy and ex situ focused ion beam scanning electron microscopy. Electrochemical degradation was not observable during cycling at room temperature with 4.3 V versus Li/Li + charge voltage cutoff, or with stepwise potentiostatic hold up to 4.1 V versus Li/Li + . In contrast, secondary phases including reduced transition metal species (Ni 2+ , Co 2+ ) were found after cycling up to 4.3 V versus Li/Li + at 80 °C and during potentiostatic hold at 4.3 V versus Li/Li + (Ni 2+ ). Intergranular cracks between NMC622 grains and delamination at the NMC622|LLZO interface occurred readily after the first charge. These interface reaction products and mechanical failure lowered the capacity and cell efficiency due to partial loss of the NMC622 phase, partial loss of contact at the interface, and a higher polarization resistance. Electrochemical instability between delithiated NMC622 and LLZO could be mitigated by using a low charge voltage cutoff or cycling at lower temperature. Ways to engineer the mechanical properties to avoid crack deflection and delamination at the interface are also discussed for enhancing mechanical stability.

36 MATERIALS SCIENCE↗

Demonstration of the Reproducibility Challenges in the Sintering Behavior of Lithium‐Stuffed Garnets in Scaling up Synthesis

Lithium-stuffed garnets, such as Li 7 La 3 Zr 2 O 12 (LLZO), are promising candidates for next-generation solid-state batteries because of their high room-temperature ionic conductivity and chemical stability against lithium metal anodes, which are crucial for achieving higher energy density. However, realizing LLZO's potential in practical devices requires synthesis methods that can be scaled reliably to large batch sizes for manufacturing. Herein, we investigate the sintering reproducibility of LLZO synthesized at larger scales using ultrasonic spray pyrolysis, a cost-effective and scalable synthesis route. Two 100 g batches of Al-doped LLZO are prepared and their sintering behavior is examined in detail. Both Al-LLZO batches contain over 90 wt.% cubic-phase LLZO, and both batches exhibit room temperature conductivities greater than 1 × 10 −4 S cm −1 at a relative density above 0.8. However, variations in secondary phases and subtle differences in Al content lead to significant differences in densification and microstructure. These results demonstrate that LLZO's sintering behavior is highly sensitive to small changes in secondary phases and Al content, creating reproducibility challenges when moving from laboratory- to manufacturing-scale synthesis.

36 MATERIALS SCIENCE↗

Li Stripping Behavior of Anode‐Free Solid‐State Batteries Under Intermittent‐Current Discharge Conditions

Anode‐free manufacturing holds promise to enable high energy densities and lower Lithium (Li)‐metal solid‐state batteries (LMSSBs). Nevertheless, in contrast to thick Li foil (>50 µm), the stripping capacity of in situ‐formed Li (10–30 µm) is limited due to diminished creep flow, resulting in reduced accessible capacity. This study explores the correlation between stripping capacity and surface roughness of garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte. The results reveal that stripping capacity can be enhanced through the surface modification of solid electrolytes. Additionally, this study scrutinizes the stripping behavior of in situ Li under intermittent‐current discharge conditions, which are more relevant to the operational conditions of electric vehicles (EVs). It is demonstrated that, when compared to constant‐current stripping, intermittent‐current stripping effectively suppresses void formation and enhances the stripping capacity of in situ Li by 40%. It is considered that the intermittent current inhibits the accumulation of Li vacancies, thereby delaying the void formation. These findings provide valuable insights into the development of high‐performance anode‐free LMSSBs for EVs.

25 ENERGY STORAGE↗

Particle‐Size‐Dependent Lithium‐Ion Transport in PEO/LLZO Composite Electrolytes

Lithium-metal batteries with solid electrolytes can deliver higher energy density and improved safety than conventional Li-ion batteries. Among solid electrolyte candidates, polymer/ceramic composite electrolytes are attractive because they combine polymer flexibility with the high ionic conductivity of ceramics. However, whether ceramic fillers synergistically reduce polarization losses in the polymer matrix remains unclear. A central unknown is the critical polymer/ceramic interfacial resistance (Rint,crit), below which adding ceramics lowers electrolyte overpotential. Here, we present the first macroscale model framework to quantify R int,crit for composite electrolytes based on polyethylene oxide (PEO) and Ta-doped Li 7 La 3 Zr 2 O 12 (LLZO). A 1D model for DC-polarization of tri-layer cells (PEO-LiTFSI/LLZO/PEO-LiTFSI) shows that LLZO surface functionalization reduces the PEO/LLZO interfacial resistance, consistent with electrochemical impedance measurements. Extending to a 2D composite model, we show notably that Rint,crit scales linearly with LLZO particle diameter and shifts toward experimentally accessible values (e.g., 28.8 Ωcm 2 ) as particle size increases. At fixed ceramic volume fraction, larger LLZO particles reduce the number of interfacial crossings, driving more current through the ceramic phase and lowering concentration polarization. In contrast, R int,crit is largely independent of ceramic volume fraction. These results demonstrate that ceramic filler-size engineering can enable synergistic, energy-efficient transport in polymer/ceramic composite electrolytes.

25 ENERGY STORAGE↗

Probing degradation at solid-state battery interfaces using machine-learning interatomic potential

Solid-state batteries featuring fast ion-conducting solid electrolytes are promising next-generation energy storage technologies, yet challenges remain for practical deployment due to electro-chemo-mechanical instabilities at solid-solid interfaces. These interfaces, which include homogeneous/internal interfaces such as grain boundaries (GBs) and heterogeneous/external interfaces between solid-electrolyte and electrode materials, can impede Li-ion transport, deteriorate performance, and eventually lead to cell failure. Here, in this study, we leverage large-scale molecular simulations, enabled by validated machine-learning interatomic potentials, to directly probe the onset of interfacial degradation at the garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid-electrolyte/LiCoO 2 (LCO) cathode interface. By surveying different interfacial geometries and compositions, it is found that Li-deficient interfaces can lead to severe interfacial disordering with cation mixing and Co interdiffusion from LCO into LLZO. By contrast, Li-sufficient interfaces are less disordered, although elemental segregation with local ordering is observed. As a consequence of Co interdiffusion, Co-rich regions are formed at the GBs of LLZO due to cation segregation and trapping effects. This behavior is independent of the GB tilting axis, degree of disorder at the GBs, and Co concentration, which implies Co clustering at GBs is a general phenomenon in polycrystalline LLZO and can dictate its overall transport and mechanical properties. Our findings elucidate the underlying fundamental mechanisms that give rise to experimentally observed physicochemical properties and provide guidelines for interface design that can mitigate interfacial degradation and improve cycling performance.

25 ENERGY STORAGE↗

Electrochemical Oxidation in Garnet-Type Solid Electrolyte by Formation of Point Defects

All-solid-state batteries hold greater promise for improving safety and energy density over conventional battery technology employing organic liquid electrolytes. One of the required features of a Li + conducting solid electrolyte is electrochemical stability, attained thermodynamically or kinetically, within the targeted operating voltage and temperature ranges. Therefore, understanding of the oxidative or reductive degradation mechanism is important to allow the design of stable solid electrolyte materials. This work contributes to building an understanding of the oxidative degradation mechanism in lithium solid electrolytes at cell operating conditions. Here, we have focused on resolving the oxidative decomposition mechanism of Al-doped lithium garnet Li 6.28 Al 0.24 La 3 Zr 2 O 12 (LLZO) as a state-of-the-art inorganic ceramic electrolyte. By combining experimental and computational analyses, we show that oxidation of LLZO occurs by simultaneous loss of oxygen and lithium from the structure, resulting in substoichiometric LLZO, at a moderate temperature (80 °C) and a high electrode potential (4.3 V vs Li/Li + ). Based on X-ray absorption and diffraction analyses, we find that the zirconium coordination shells in LLZO contract while the crystal structure experiences positive chemical strain upon electrochemical oxidation. The results from ex situ structural characterization of both the local structure and crystal symmetry are supported by a substoichiometric LLZO with lithium and oxygen vacancies, modeled by density functional theory (DFT) calculations. These chemical and structural changes in LLZO suppress effective lithium-ion conductivity by an order of magnitude. Formation of lithium and oxygen vacancies in LLZO upon electrochemical oxidation is different from prior thermodynamic predictions of phase decomposition of LLZO. The difference here is that the experiments were conducted at near-room temperature, which can hinder the kinetics of phase separation, and thus, the resultant LLZO solid electrolyte is still single-phase but substoichiometric in Li and O. In conclusion, these findings contribute an important degradation mechanism of the electrolyte, relevant for practical operational conditions of solid-state batteries.

36 MATERIALS SCIENCE↗

Nanoscale Miscibility in In Situ Polymerized Hybrid Electrolytes Speeds Up Ion Dynamics and Enables Stable Cycling of Li Metal Batteries

While the potential use of copolymerized electrolytes in Li metal batteries is subject to intense investigation, the fundamental understanding of the nanoscale domain formation and its effect on Li + transport is still lacking. In this study, we investigated the correlation between the Li + transport mechanism and the miscibility of monomers in polymer blend electrolytes derived from the in situ copolymerization of methyl methacrylate (MMA) and vinylene carbonate (VC) in the presence of polyethylene glycol dimethyl ether (PEGDME) plasticizer and bis(trifluoromethanesulfonyl)imide (LiTFSI) salt. The addition of a polar short chain plasticizer reduced the dynamic and structural heterogeneities of the electrolyte. Small-angle X-ray scattering (SAXS) measurements and coarse-grained molecular dynamics (MD) simulations were used to investigate the nanoscale structure of the electrolytes. The distribution of relaxation times corresponding to the three distinct diffusion mechanisms of the free and interfacial Li + ions at the copolymer/plasticizer and electrolyte/SEI boundaries was analyzed in a broad temperature range to elucidate the Li + transport mechanism. Furthermore, the chemical composition of the SEI and the contribution of a ceramic lithium lanthanum zirconium oxide (LLZO, Li 7 La 3 Zr 2 O 12 ) phase on the interfacial resistance, salt degradation, and SEI stability were studied by X-ray photoelectron spectroscopy (XPS) depth profile analysis and electrochemical testing.

Li metal↗