Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “LITHIUM METAL”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Sorption of atmospheric gases by bulk lithium metal

Lithium conditioning of plasma facing components has enhanced the performance of several fusion devices. Elemental lithium will react with air during maintenance activities and with residual gases (H 2 O, CO, CO 2 ) in the vacuum vessel during operations. We have used a mass balance (microgram sensitivity) to measure the mass gain of lithium samples during exposure of a ~1 cm 2 surface to ambient and dry synthetic air. For ambient air, we found an initial mass gain of several mg/h declining to less than 1 mg/h after an hour and decreasing by an order of magnitude after 24 h. A 9 mg sample achieved a final mass gain corresponding to complete conversion to Li 2 CO 3 after 5 days. Exposure to dry air resulted in a 30 times lower initial rate of mass gain. The results have implications for the chemical state of lithium plasma facing surfaces and for safe handling of lithium coated components.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Failure Mechanism of Fast-Charged Lithium Metal Batteries in Liquid Electrolyte

In recent years, lithium anode has re-attracted broad interest because of the necessity of employing lithium metal in the next-generation battery technologies such as lithium sulfur (Li-S) and lithium oxygen (Li-O2) batteries. Fast capacity degradation and safety issue associated with rechargeable lithium metal batteries have been reported, although the fundamental understanding on the failure mechanism of lithium metal at high charge rate is still under debate due to the complicated interfacial chemistry between lithium metal and electrolyte. Herein, we demonstrate that, at high current density, the quick growth of porous solid electrolyte interphase towards bulk lithium, instead of towards the separator, dramatically builds up the cell impedance that directly leads to the cell failure. Understanding the lithium metal failure mechanism is very critical to gauge the various approaches used to address the stability and safety issues associated with lithium metal anode. Otherwise, all cells will fail quickly at high rates before the observation of any positive effects that might be brought from adopting the new strategies to protect lithium.

Environmental Molecular Sciences Laboratory↗

Hybrid Lithium-Sulfur Batteries with an Advanced Gel Cathode and Stabilized Lithium-Metal Anode

The insulating nature of sulfur, polysulfide shuttle effect, and lithium metal deterioration cause a decrease in practical energy density and fast capacity fade in lithium-sulfur batteries. Here, we present an integrated strategy for the development of hybrid Li-S batteries based on a gel sulfur cathode, a solid electrolyte, and a protective anolyte composed of highly-concentrated salt electrolyte containing mixed additives. The dense solid electrolyte completely blocks polysulfide diffusion, and also makes it possible to investigate the cathode and anode independently. This gel cathode effectively traps the polysulfide active material while maintaining a low electrolyte to sulfur ratio (E/S) of 5.2 mL/g. The anolyte effectively protects the Li metal and suppresses the consumption of liquid electrolyte, enabling stable long-term cycling for over 700 hours in Li symmetric cells. This advanced design can simultaneously suppress the polysulfide shuttle, protect Li metal, and reduce the liquid electrolyte usage. The assembled hybrid batteries exhibit remarkably stable cycling performance over 300 cycles with high capacity. Finally, surface-sensitive techniques were carried out to directly visualize and to probe the interphase formed on the surface of the LAGP pellet, which may help stabilize the solid-liquid interface.

25 ENERGY STORAGE↗

A Cation-Tethered Flowable Polymeric Interface for Enabling Stable Deposition of Metallic Lithium

A fundamental challenge, shared across many energy storage devices, is the complexity of electrochemistry at the electrode–electrolyte interfaces that impacts the Coulombic efficiency, operational rate capability, and lifetime. Specifically, in energy-dense lithium metal batteries, the charging/discharging process results in structural heterogeneities of the metal anode, leading to battery failure by short-circuit and capacity fade. In this work, we take advantage of organic cations with lower reduction potential than lithium to build an electrically responsive polymer interface that not only adapts to morphological perturbations during electrodeposition and stripping but also modulates the lithium ion migration pathways to eliminate surface roughening. As a result, we find that this concept can enable prolonging the long-term cycling of a high-voltage lithium metal battery by at least twofold compared to bare lithium metal.

25 ENERGY STORAGE↗

Good Practice for Safe Handling of Lithium Metal Anode and High Energy Rechargeable Lithium Metal Batteries

High-energy rechargeable lithium metal batteries have been intensively revisited in recent years. Since more researchers started to use pouch cell as the platform to study the fundamentals at relevant scales, safe testing and handling of lithium metal and high-energy lithium metal batteries have become critical. Cautions and safety procedures are needed when handling cycled pouch cells with pulverized lithium particles inside. From cell design, electrode preparation, cell fabrication to testing procedure, this work aims to discuss all possible root causes that may initiate cell internal shorting and raise safety concerns. Safe transfer and disposal of cycled pouch cells are also discussed. The insights provided in this article are applicable for the research on high-energy lithium-ion batteries as well and may inspire more safety strategies to accelerate research innovation by using large-format batteries as the testing vehicle and conduct the research safely.

25 ENERGY STORAGE↗

Lithium-coated polymeric matrix as a minimum volume-change and dendrite-free lithium metal anode

Lithium metal is the ideal anode for the next generation of high-energy-density batteries. Nevertheless, dendrite growth, side reactions and infinite relative volume change have prevented it from practical applications. Here, we demonstrate a promising metallic lithium anode design by infusing molten lithium into a polymeric matrix. The electrospun polyimide employed is stable against highly reactive molten lithium and, via a conformal layer of zinc oxide coating to render the surface lithiophilic, molten lithium can be drawn into the matrix, affording a nano-porous lithium electrode. Importantly, the polymeric backbone enables uniform lithium stripping/plating, which successfully confines lithium within the matrix, realizing minimum volume change and effective dendrite suppression. The porous electrode reduces the effective current density; thus, flat voltage profiles and stable cycling of more than 100 cycles is achieved even at a high current density of 5 mA cm -2 in both carbonate and ether electrolyte. Furthermore, the advantages of the porous, polymeric matrix provide important insights into the design principles of lithium metal anodes.

36 MATERIALS SCIENCE↗

Understanding the Reactivity of a Thin Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 Solid–State Electrolyte toward Metallic Lithium Anode

The thickness of solid-state electrolytes (SSEs) significantly affects the energy density and safety performance of all-solid-state lithium batteries. However, a sufficient understanding of the reactivity toward lithium metal of ultrathin SSEs (<100 μm) based on NASICON remains lacking. Herein, for the first time, a self-standing and ultrathin (70 μm) NASICON-type Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 (LAGP) electrolyte via a scalable solution process is developed, and X-ray photoelectron spectroscopy reveals that changes in LAGP at the metastable Li-LAGP interface during battery operation is temperature dependent. Severe germanium reduction and decrease in LAGP particle size are detected at the Li-LAGP interface at elevated temperature. As a result, oriented plating of lithium metal on its preferred (110) face occurs during in situ X-ray diffraction cycling.

25 ENERGY STORAGE↗

Size Effects of Micro-Pattern on Lithium Metal Surface on the Electrochemical Performance of Lithium Metal Secondary Batteries.

Two micro-patterns of different sizes (50 and 80 gm) are designed to have equivalent capacities of 1.06 and 2.44 mAh cm(-2) by building a computational battery model. After preparing two stamps each possessing a micro pattern design, the corresponding pattern is properly imprinted on the surface of 100 mu m lithium metal, which is confirmed by scanning electron microscopy. When both micro-patterned lithium metals are electrochemically reduced and oxidized up to 1 mAh cm(-2) in Li/Li symmetric cells at 1 or 2 mA cm(-2), the 80 mu m-patterned lithium shows a more stabilized lower overpotential during long-term cycling than the 50 mu m-patterned and bare lithium, probably due to the lithium anchoring effect and a larger empty volume in the patterns. Additionally, an overflow of lithium deposits is easily observed in the 50 mu m-patterned lithium metal, while the 80 mu m-patterned lithium metal holds most of the lithium deposits within the patterns. When both micro-patterned lithium metals are assembled to full cells with a LiNi0.6Co0.2Mn0.2O2 cathode of 2 mAh cm(-2), the 80 mu m-patterned lithium metal shows much better electrochemical performances with stable plating/stripping behavior within the patterns.

lithium metal↗

Effect of the dielectric constant of a liquid electrolyte on lithium metal anodes

Lithium metal is considered one of the most promising anode materials for realizing high volumetric and gravimetric energy density, owing to the high specific capacity (~3860 mAh g -1 ) and the low electrochemical potential of lithium (-3.04 V vs. the standard hydrogen electrode). However, undesirable dendritic lithium growth and corresponding instability of the solid electrolyte interphase prevent safe and long-term use of lithium metal anodes. Here, this paper presents a simple electrolyte approach to enhance the performance of lithium metal batteries by tuning the dielectric constant of the liquid electrolyte. Electrolyte formulations are designed by changing the concentration of ethylene carbonate to have various dielectric constants. This study confirms that high ethylene carbonate content in a liquid electrolyte enhances the cycling performance of lithium metal batteries because the electric field intensity applied to the electrolyte is reduced in relation to the polarization of the electrolyte and thus allows smooth lithium plating and formation of a stable solid electrolyte interphase. Lastly, we believe that this approach provides an important concept for electrolyte system design suitable to lithium metal batteries.

25 ENERGY STORAGE↗

Development of lithium ion conducting interface between lithium metal and a lithium ion conducting ceramic using block polymers

The lithium-air (Li-air) technology developed by EDF uses an air electrode which works with an aqueous electrolyte, which prevent the use of unprotected lithium metal electrode. A Li+ ionic conductor glass ceramic is used to separate the aqueous electrolyte compartment from the negative lithium electrode. However, this glass-ceramic is not stable in contact with lithium, it is thus necessary to add a protective buffer layer. In another hand, this protection should ideally resist to lithium dendritic growth. It is in this context that this research project which has as goal the development of a protective buffer layer based on block copolymer electrolytes (BCE) between the lithium metal and the lithium ionic conductor ceramic, for lithium-air battery. In a first part, the BCE is studied in lithium-lithium symmetric cells, in order to determine their electrochemical properties such as ionic conductivity, steady state transference number, and finally their resistance to dendritic growth during cycling. Several characterization techniques were employed and especially hard X-ray micro-tomography to analyze the lithium morphology before and after cycling. For single-ion BCE, we expect to suppress dendritic growth, however, we report here for the first time, the visualization of a homogeneous growth of lithium but the formation of dense lithium objects. In another part, the composite BCE-ceramic is studied by electrochemical impedance spectroscopy (EIS). The cycling of lithium-composite-lithium symmetric cells and the analysis of the EIS measurement after each cycle permit to determine if the dendrites have cross the protective layer and are in contact with the ceramic. Besides, the quantification of the polarization loss at the interface polymer-ceramic is evaluated by polarization experiments. This contribution is found to be small.

36 MATERIALS SCIENCE↗

Magnetic Field-Suppressed Lithium Dendrite Growth for Stable Lithium-Metal Batteries

Lithium metal is the most attractive anode material due to its extremely high specific capacity, minimum potential, and low density. However, uncontrollable growth of lithium dendrite results in severe safety and cycling stability concerns, which hinders the application in next generation secondary batteries. In this paper, a new and facile method imposing a magnetic field to lithium metal anodes is proposed. That is, the lithium ions suffering Lorentz force due to the electromagnetic fields are put into spiral motion causing magnetohydrodynamics (MHD) effect. This MHD effect can effectively promote mass transfer and uniform distribution of lithium ions to suppress the dendrite growth as well as obtain uniform and compact lithium deposition. The results show that the lithium metal electrodes within the magnetic field exhibit excellent cycling and rate performance in a symmetrical battery. Additionally, full batteries using limited lithium metal as anodes and commercial LiFePO 4 as cathodes show improved performance within the magnetic field. In summary, a new and facile strategy of suppressing lithium dendrites using the MHD effect by imposing a magnetic field is proposed, which may be generalized to other advanced alkali metal batteries.

25 ENERGY STORAGE↗

Crossover Effects of Transition‐Metal Ions on Lithium‐Metal Anode in Localized High Concentration Electrolytes

Abstract The stability of the solid–electrolyte interphase (SEI) is critical to the cycle life of lithium‐metal batteries (LMBs). While the crossover effect of transition‐metal ions from cathode to anode is extensively studied in lithium‐ion batteries with graphite anodes, its impact on LMBs remains largely unexplored. Herein, this study investigates the electrochemical and chemical properties of SEI layers formed on lithium‐metal anodes in localized high‐concentration electrolytes (LHCEs) containing dissolved transition‐metal ions (Ni 2+ , Mn 2+ , and Co 2+ ). It is demonstrated that transition‐metal ions in LHCEs reduce the coulombic efficiency (CE) and significantly degrade the cycle life of LMBs. Time‐of‐flight secondary‐ion mass spectrometry (ToF‐SIMS) reveals that SEI structures differ depending on the dissolved TM ion, with Mn 2+ and Co 2+ inducing severe destabilization, and Ni 2+ exhibiting a less severe impact. These findings underscore the detrimental effects of transition‐metal crossover effects in LMB systems.

Guo, Zezhou [Materials Science and Engineering Pro↗

Cryogenic Focused Ion Beam Characterization of Lithium Metal Anodes

Lithium metal is viewed as the ultimate battery anode because of its high theoretical capacity and low electrode potential, but its implementation has been limited by low Coulombic efficiency and dendrite formation above a critical current density. Determining the fundamental properties dictating lithium metal plating–stripping behavior is challenging because characterization techniques are limited by the sensitivity of lithium metal to damage by external probes, which regularly results in altered morphology and chemistry. Motivated by recent application of cryogenic transmission electron microscopy (cryo-TEM) to characterize lithium metal at the atomic scale, we explore the cryogenic focused ion beam (cryo-FIB) method as a quantitative tool for characterizing the bulk morphology of electrochemically deposited lithium and as a technique that enables TEM observation of Li-metal/solid-state electrolyte interfaces. Lastly, this work highlights the importance of cryo-FIB methodology for preparing sensitive battery materials and elucidates the impact of electrolyte selection on the density and morphology of plated lithium.

25 ENERGY STORAGE↗

Engineering stable interfaces for three-dimensional lithium metal anodes

Lithium metal has long been considered one of the most promising anode materials for advanced lithium batteries (for example, Li-S and Li-O 2 ), which could offer significantly improved energy density compared to state-of-the-art lithium ion batteries. Despite decades of intense research efforts, its commercialization remains limited by poor cyclability and safety concerns of lithium metal anodes. One root cause is the parasitic reaction between metallic lithium and the organic liquid electrolyte, resulting in continuous formation of an unstable solid electrolyte interphase, which consumes both active lithium and electrolyte. Until now, it has been challenging to completely shut down the parasitic reaction. We find that a thin-layer coating applied through atomic layer deposition on a hollow carbon host guides lithium deposition inside the hollow carbon sphere and simultaneously prevents electrolyte infiltration by sealing pinholes on the shell of the hollow carbon sphere. By encapsulating lithium inside the stable host, parasitic reactions are prevented, resulting in impressive cycling behavior. In conclusion, we report more than 500 cycles at a high coulombic efficiency of 99% in an ether-based electrolyte at a cycling rate of 0.5 mA/cm 2 and a cycling capacity of 1 mAh/cm 2 , which is among the most stable Li anodes reported so far.

25 ENERGY STORAGE↗