Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “LEAD FREE SOLDER”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Lead-free solders: issues of toxicity, availability and impacts of extraction

This project set out to evaluate the critical issues of toxicity and public health effects, material availability, and the environmental impacts of raw material extraction and metal finishing, with the goal of using environmental impact as a factor in selecting feasible lead-free alloys.

toxicity lead-free solder packaging↗

Mechanical Properties and Microstructure Investigation of Lead Free Solder

While the electronics industry appears to be focusing on Sn-Ag-Cu as the alloy of choice for lead free electronics assembly, ,the exact composition varies by geographic region, supplier and user. Add to that dissolved copper and silver from the printed circuit board traces and surface finish, and there can be significant variation in the final solder joint composition. A systematic study of the mechanical and microstructural properties of Sn-Ag-Cu alloys with Ag varying from 2wt% to 4wt% and Cu varying from 0.5wt% to lSwt%, was undertaken in this research study. Different sample preparation techniques (water quenched, oil quenched and water quenched followed by reflow) were explored and the resulting microstructure compared to that of a typical reflowed lead free chip scale package (CSP) solder joint. Tensile properties (modulus, 0.2% yield strength and the ultimate tensile strength) and creep behavior of selected alloy compositions (Sn-4Ag-1 X u , Sn-4Ag-OSCu, Sn- 2Ag-1 X u , Sn-2Ag-OSCu, Sn-3.5Ag-O.SCu) were determined for three conditions: as- cast; aged for 100 hours at 125OC; and aged for 250 hours at 125OC. There was no significant difference in Young's Modulus as a function of alloy composition. After an initial decrease in modulus after 100 hours at 125"C, there was an insignificant change with further aging. The distribution of 0.2% strain yield stress and ultimate tensile strength as a function of alloy composition was more significant and decreased with aging time and temperature. The microstructures of these alloys were examined using light and scanning electron microscopy (LM and SEM) respectively and SEM based energy dispersive x-ray spectroscopy (EDS). Fracture surface and cross-section analysis were performed on the specimens after creep testing. The creep testing results and the effect of high temperature aging on mechanical properties is presented for the oil quenched samples. In general the microstructure of oil quenched specimen exhibited a eutectic region of Sn with moderately dispersed Ag3Sn intermetallic, surrounded by a dendritic Sn-rich phase. The SEM images of the fracture surface indicated the presence of a tough shear surface at the initial cavity break area and a break line in the middle of specimen along the failure direction. A hyperbolic-sine creep model was adopted and used to fit the creep experiment data. The effect on the mechanical properties by adding the quaternary element bismuth to the Sn-3.5Ag-0.8Cu alloy was measured and compared with the mechanical properties of the ternary alloys. The results of this research study provide necessary data for the modeling of solder joint reliability for a range of Sn-Ag-Cu compositions and a baseline for evaluating the effects of subsequent quaternary additions.

Wang, Qing↗

Enhanced interfacial thermal transport in pnictogen tellurides metallized with a lead-free solder alloy

Controlling thermal transport across metal–thermoelectric interfaces is essential for realizing high efficiency solid-state refrigeration and waste-heat harvesting power generation devices. Here, the authors report that pnictogen chalcogenides metallized with bilayers of Sn{sub 96.5}Ag{sub 3}Cu{sub 0.5} solder and Ni barrier exhibit tenfold higher interfacial thermal conductance Γ{sub c} than that obtained with In/Ni bilayer metallization. X-ray diffraction and x-ray spectroscopy indicate that reduced interdiffusion and diminution of interfacial SnTe formation due to Ni layer correlates with the higher Γ{sub c}. Finite element modeling of thermoelectric coolers metallized with Sn{sub 96.5}Ag{sub 3}Cu{sub 0.5}/Ni bilayers presages a temperature drop ΔT ∼ 22 K that is 40% higher than that obtained with In/Ni metallization. Our results underscore the importance of controlling chemical intermixing at solder–metal–thermoelectric interfaces to increase the effective figure of merit, and hence, the thermoelectric cooling efficiency. These findings should facilitate the design and development of lead-free metallization for pnictogen chalcogenide-based thermoelectrics.

42 ENGINEERING↗

Rapid Solidification of Sn-Cu-Al Alloys for High-Reliability, Lead-Free Solder: Part I. Microstructural Characterization of Rapidly Solidified Solders

Particles of Cu x Al y in Sn-Cu-Al solders have previously been shown to nucleate the Cu 6 Sn 5 phase during solidification. In this study, the number and size of Cu 6 Sn 5 nucleation sites were controlled through the particle size refinement of Cu x Al y via rapid solidification processing and controlled cooling in a differential scanning calorimeter. Cooling rates spanning eight orders of magnitude were used to refine the average Cu x Al y and Cu 6 Sn 5 particle sizes down to submicron ranges. The average particle sizes, particle size distributions, and morphologies in the microstructures were analyzed as a function of alloy composition and cooling rate. Deep etching of the samples revealed the three-dimensional microstructures and illuminated the epitaxial and morphological relationships between the Cu x Al y and Cu 6 Sn 5 phases. Transitions in the Cu 6 Sn 5 particle morphologies from faceted rods to nonfaceted, equiaxed particles were observed as a function of both cooling rate and composition. Initial solidification cooling rates within the range of 10 3 to 10 4 °C/s were found to be optimal for realizing particle size refinement and maintaining the Cu x Al y /Cu 6 Sn 5 nucleant relationship. In addition, little evidence of the formation or decomposition of the ternary-β phase in the solidified alloys was noted. As a result, solidification pathways omitting the formation of the ternary-β phase agreed well with observed room temperature microstructures.

36 MATERIALS SCIENCE↗

Study on the Reliability of Carbon Nanotube-Reinforced Sn-58Bi Lead-Free Solder Joints

The wettability, microstructure and mechanical properties of multi-walled carbon nanotube (CNT)-reinforced Sn-58Bi composite solder joints were investigated. The results indicate that the wettability of the Sn-58Bi solder is improved and the growth of interfacial intermetallic (IMC) compounds for solder joints is restrained by CNTs. The thickness of the IMC layers is decreased with increasing CNTs concentration. The microstructure of the Sn-58Bi composite solders is refined, the maximum tensile strength and shear strength are obtained by adding the optimum CNTs content about 0.01 wt.%. However, excessive content of CNTs addition can deteriorate the properties. The creep rupture life of Sn-58Bi solder joint and Sn-58Bi-0.01CNTs solder joint is decreased with increasing load, temperature and current density. The average creep rupture life of Sn-58Bi-0.01CNTs composite solder joint is 60% higher than that of the plain solder joint.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Corrosion and Electrochemical Behavior of Sn-2Ag-0.5Cu Lead-Free Solders Solidified with Magnet Stirring

In this study, permanent magnet stirring (PMS) was applied to modify the crystallographic texture and corrosion resistance of Sn-2Ag-0.5Cu (SAC205) solders. The results indicate that PMS transforms the lamellar structure into equiaxed grains. Following the initiation corrosion process, the crystallographic texture shows a new class of grains that consists of single-crystal morphology with {111}{sub Sn} facets before applying PMS. This could result in severe corrosion of β-Sn crystals with non-uniform corrosion rate caused by the orientation effect of (111). The corrosion rate for SAC205 solder, measured by immersion tests in 3.5% NaCl solution at 25 °C, was significantly decreased from 31 to 8 mpy after applying PMS. This change in corrosion resistance of SAC205 solder can be attributed to the improved anodic and cathodic reaction activities caused by the modification of microstructure and crystallographic texture. The mechanism of pitting and sequential corrosion events is fully explained and discussed.

36 MATERIALS SCIENCE↗

Suppressing tin whisker growth in lead-free solders and platings

A process of irradiation Sn containing Pb-free solder to mitigate whisker formation and growth thereon is provided. The use of gamma radiation such as cobalt-60 has been applied to a substrate of Sn on copper has been found to change the morphology of the crystalline whisker growth to a more truncated hillock pattern. The change in morphology greatly reduces the tendency of whiskers to contribute to electrical short-circuits being used as a Pb-free solder system on a copper substrate.

36 MATERIALS SCIENCE↗

Working with Consortia - Advanced Packaging Reliability

Description: Support the responsible NASA official for lead-free solder evaluation. Serve as the NASA technical liaison to the NASA/DoD Pb-free Project. Assure NASA areas of interest are included in JG-PP follow-on work. Support NASA/DoD telcons and face-to-face meetings. Update MSFC lead-free solder lessons learned report. FY10 plans: - Reliability data on lead-free solder applications for various part lead finishes and board finishes. - Update lead-free solder risks and risk mitigation strategies for NASA. - Evaluate lead-free alloy/lead-free finish reliability in design application. - Status CAVE project on Pb-free solder aging effects. - Compile the LTESE flight and bench data.

Blanche, Jim↗

Reliability of Sn/Pb and Lead-Free (SnAgCu) Solders of Surface Mounted Miniaturized Passive Components for Extreme Temperature (-185 C to +125 C) Space Missions

Surface mount electronic package test boards have been assembled using tin/lead (Sn/Pb) and lead-free (Pb-free or SnAgCu or SAC305) solders. The soldered surface mount packages include ball grid arrays (BGA), flat packs, various sizes of passive chip components, etc. They have been optically inspected after assembly and subsequently subjected to extreme temperature thermal cycling to assess their reliability or future deep space, long-term, extreme temperature environmental missions. In this study, the employed temperature range (-185oC to +125oC) covers military specifications (-55oC to +100oC), extreme old Martian (-120oC to +115oC), asteroid Nereus (-180oC to +25oC) and JUNO (-150oC to +120oC) environments. The boards were inspected at room temperature and at various intervals as a function of extreme temperature thermal cycling and bake duration. Electrical resistance measurements made at room temperature are reported and the tests to date have shown some change in resistance as a function of extreme temperature thermal cycling and some showed increase in resistance. However, the change in interconnect resistance becomes more noticeable with increasing number of thermal cycles. Further research work will be carried out to understand the reliability of packages under extreme temperature applications (-185oC to +125oC) via continuously monitoring the daisy chain resistance for BGA, Flat-packs, lead less chip packages, etc. This paper will describe the experimental reliability results of miniaturized passive components (01005, 0201, 0402, 0603, 0805, and 1206) assembled using surface mounting processes with tin-lead and lead-free solder alloys under extreme temperature environments.

extreme temperatures,↗

Age-aware solder performance models : level 2 milestone completion.

Legislated requirements and industry standards are replacing eutectic lead-tin (Pb-Sn) solders with lead-free (Pb-free) solders in future component designs and in replacements and retrofits. Since Pb-free solders have not yet seen service for long periods, their long-term behavior is poorly characterized. Because understanding the reliability of Pb-free solders is critical to supporting the next generation of circuit board designs, it is imperative that we develop, validate and exercise a solder lifetime model that can capture the thermomechanical response of Pb-free solder joints in stockpile components. To this end, an ASC Level 2 milestone was identified for fiscal year 2010: Milestone 3605: Utilize experimentally validated constitutive model for lead-free solder to simulate aging and reliability of solder joints in stockpile components. This report documents the completion of this milestone, including evidence that the milestone completion criteria were met and a summary of the milestone Program Review.

36 MATERIALS SCIENCE↗

NASA-DoD Lead-Free Electronics Project

This slide presentation reviews the current state of the lead-free electronics project. It characterizes the test articles, which were built with lead-free solder and lead-free component finishes. The tests performed and reported on are: thermal cycling, combine environments testing, mechanical shock testing, vibration testing and drop testing.

Kessel, Kurt↗

Liquid-phase diffusion bonding: Temperature effects and solute redistribution in high temperature lead-free composite solders

Liquid-phase diffusion bonding (LPDB) is being studied as the primary phenomena occurring in the development of a high temperature lead-free composite solder paste composed of gas-atomized Cu-10Ni, wt.% (Cu-11Ni, at.%) powder blended with Sn-0.7Cu-0.05Ni-0.01Ge (Sn-1.3Cu-0.1Ni-0.02Ge, at.%) Nihon-Superior SN100C solder powder. Powder compacts were used as a model system. LPDB promotes enhanced interdiffusion of the low-melting alloy matrix with the solid Cu-10Ni reinforcement powder above the matrix liquidus temperature. The initial study involved the effective intermetallic compound (IMC) compositions and microstructures that occur at varying reflow temperatures and times between 250-300°C and 30-60s, respectively. Certain reflow temperatures encourage adequate interdiffusion to form a continuous highly-conductive network throughout the composite solder joints. The diffusion of nickel, in particular, has a disperse pattern that foreshadows the possibility of a highly-conductive low-melting solder that can be successfully utilized at high temperatures.

42 ENGINEERING↗

Study of the oxidation effects on isothermal solidification based high temperature stable Pt/In/Au and Pt/In/Ag thick film interconnections on LTCC substrate

The objective of the presented paper is to determine the oxidized phase compositions of indium lead-free solders during solidification at 190 ° C under room environment with the help of X-ray diffraction (XRD) and Energy dispersive spectroscopy (EDX). Many lead-free solders alloys available oxidizes and have poor wetting properties. The oxidation of pure indium solder foil, Au, Pt, and Ag alloys were identified and investigated, in the process of isothermal solidification based solder joints construction at room environment and humidity. Both EDX and XRD characterization techniques were performed to trace out the amount of oxide levels and variety of oxide formations at solder interface respectively. The paper also aims to report the isothermal solidification technique to provide interconnections to pads on Low temperature co-fired ceramic (LTCC) substrate. It also elaborates advantages of isothermal solidification over the other methods of interconnection. Scanning electron microscope (SEM) used to identify the oxidized spots on the surface of Pt, Ag substrates and In solder. The identified oxides were reported.

36 MATERIALS SCIENCE↗