Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Inconel”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Elevated temperature mechanical properties of Inconel 617 surface oxide using nanoindentation

Inconel 617 is a principal candidate material for helium gas cooled very-high-temperature reactors with outlet temperatures of 700–950 °C. Recent findings showed that this alloy develops unique surface oxide layers especially at high temperature (HT) helium environment with distinctive wear, friction and contact properties. This study investigates the elevated temperature mechanical properties of Inconel 617 top surface layers aged in HT helium environment. Nanoindentation technique is used to obtain load-displacement graphs of the alloy top surface oxide in temperatures ranging from 25 °C up to 600 °C. In addition, using finite element analysis along with an iterative regression technique, a semi-numerical method is developed to further measure and quantify the material parameters and, in particular, time-independent and creep characteristics of the oxide. Although Young's modulus of the oxide is found to be relatively close to the bulk for the tested temperatures, the yield strength and hardness, in comparison to the bulk material, increase significantly as the material is oxidized after aging. The oxide exhibits significant softening as the temperature increases to 600 °C. Unlike the bulk material, diffusion through the grains is found to be the dominant creep mechanism for the oxide. Considerable difference between the mechanical properties of the oxide and the bulk material shows the need for accurate measurements of near surface mechanical properties, if reliable predictive contact and tribological models are sought at elevated temperatures.

36 MATERIALS SCIENCE↗

Microstructure, stored energy, and stability of H/He-filled nanocavities in low temperature irradiated Inconel 718

The microstructure, trapped transmutation gases, stored energy, and mechanical behavior of samples from an irradiated Inconel 718 proton beam window were characterized using transmission electron microcopy, thermal desorption spectrometry (TDS), differential scanning calorimetry (DSC), and tensile testing. In the as-irradiated condition the microstructure contained a high number density of 1–3 nm gas-filled nanocavities. Emissions of trapped gases, H and He, during TDS correlated with peaks of the energy release curves from DSC examinations, which suggest these gases were likely stored in highly stable defect traps. The stored energy from radiation damage saturated at doses of a few dpa and did not increase with increasing radiation dose, but the amount of stored H and He increased with increasing dose. Effects of post-irradiation annealing were studied as well. After exposure to 700 °C, the nanocavities grew only slightly to 2–4 nm in diameter, but after exposure to 900 °C, the cavities grew to 10–20 nm in diameter and electron energy-loss spectroscopy showed these cavities contained a core of He surrounded by a shell of H. Further, this study demonstrated that the irradiation defect structures containing H and He were remarkably stable during irradiation and after exposure up to 700 °C. The effect of the irradiation temperature, defect mobility, and interaction of H, He, and irradiation defects on mechanical behavior provides insight into the processes responsible for the unusual recovery in ductility with increasing radiation dose observed in Inconel 718 after high energy proton and spallation neutron irradiation.

36 MATERIALS SCIENCE↗

Self-welding of Inconel 617 under high-pressure-high-temperature conditions for nuclear reactors

In response to continuously declining availability of fossil fuels, nuclear power has become an important alternative source of power generation. Growing application of nuclear power has relieved the shortage of electricity. However, it is also accompanied with new drawbacks, such as radioactive waste, and potential catastrophic consequences in case of major accidents. For nuclear power plants, severe accidents mostly originate from the reactor, making the reliability of the reactor of paramount importance to the overall safety of a nuclear power plant. Massive heat generation through nuclear fission/fusion and heat exchange render the whole reactor operating at extremely high temperatures (i.e., 900–1000 °C), which, in conjunction with large load from subsystems/ components made of special heavy alloys, renders the reactor under the risk of self-welding, a phenomenon that could lead to strong bonding between components and paralyze the operability of the nuclear reactor. This paper investigates the self-welding behavior of Inconel 617, a primary candidate nickel alloy for key components of the next generation gas cooled nuclear plant, inside a controlled atmospheric furnace with preset static load, simulating the high-pressure high-temperature conditions inside nuclear reactors. Therefore, test results show that Inconel 617 experiences self-welding through common oxide zone at the interface, and it has remarkable bonding strength, requiring 4114 N (57.15 MPa) and 4338 N (60.25 MPa) to break apart a mated sample pair, under an apparent contact pressure of 0.341 MPa after 50-h aging, in helium and air atmospheres, respectively. The higher oxygen presence in air results in slightly stronger oxide bond at the interface, compared to helium, and the bond strength increases with dwell time.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

An Alternative Casting Technique to Improve the Creep Resistance of Cast INCONEL Alloy 740H

The increasing performance requirements of power plant designs, such as advanced-ultra supercritical (A-USC), require the use of Ni-based superalloys to replace high-strength, ferritic-martensitic steels for components subjected to temperatures above 898 K (625 °C) and for austenitic stainless steels components at temperatures above 973 K (700 °C). To date, commercial Ni-based superalloy INCONEL 740H has been shown to be appropriate for use in A-USC power plants as boiler components in a wrought product. However, large complex components in boilers as well as other casings in the turbine and valve chest require castings of a thick-wall nature. Using the alloy in its cast form would be significantly valuable in terms of range of component size, geometry and complexity. Previous investigations revealed short creep lives from cast INCONEL alloy 740H. Here in this investigation, an alternative casting route that utilized a melt procedure resulting in a fine-grain casting, and in conjunction with a computationally optimized homogenization heat treatment, not only controlled the grain size and grain boundary structure but minimized chemistry variability and segregation. A primarily equiaxed and homogenous grain size distribution was obtained from this approach with better repartition of M 23 C 6 carbides along the grain boundaries. Furthermore, better than 38 pct increase was obtained for this material in comparison to the creep life obtained from the best performing conventionally cast material. More importantly, the fine-grain homogenized (FGH) casting route resulted in the Larson–Miller plot for this material that coincided with that of wrought alloy 740. At low creep stresses (with a test still in progress), the FGH casting is resulting in higher values of the LMP than the wrought alloy.

36 MATERIALS SCIENCE↗

Laser powder bed fusion of Inconel 718 on 316 stainless steel

The joining of Inconel 718 and 316 stainless steel has notable industrial importance. However, traditional arc-welding has many issues. In particular, the formation of the detrimental Nb-rich Laves phase in the heat affected zone can promote crack initiation and propagation, which leads to poor mechanical properties. The small heat input and the rapid solidification of laser powder bed fusion (PBF) has the potential to suppress this problem. Despite the infancy of the multi-material PBF, it is of interest to investigate the relationship among the process parameter, the microstructure at the materials joining point, and the mechanical performance. In this study, we used high-speed x-ray imaging to in-situ monitor the printing of Inconel 718 tracks on a 316H SS substrate via laser powder bed fusion, followed by post-build characterization and testing with SEM, XRD and nanoindentation. We observed that a higher linear energy density resulted in a more diffused interface and a smaller compositional gradient, but as a trade-off, generated more keyhole pores and thermal cracks. Furthermore, we also showed that the built layer exhibited chemical inhomogeneity at two length scales: a tens-of-mu m-scale compositional vortex due to the melt flow, and a sub-mu m-scale Nb-rich dendritic structure due to the non-equilibrium solidification that led to the formation of the Laves phase. It was inferred that the chemical inhomogeneity may benefit the mechanical properties at the interface by providing more interlocking between the two materials and also by limiting the effect of the brittle Laves phase to potentially short range.

36 MATERIALS SCIENCE↗

An investigation into the effects of cyclic strain rate on the high cycle and very high cycle fatigue behaviors of wrought and additively manufactured Inconel 718

Additive Manufacturing (AM) has increasingly been used to fabricate parts in aerospace applications, which may require service lives beyond ten-million cycles due to the imposed high loading frequencies. Understanding the very high cycle fatigue (VHCF) behavior of these additive manufactured (AM) parts is an important step towards their design and qualification processes. This study focuses on the high cycle fatigue (HCF) and VHCF behaviors of both wrought and laser beam-powder bed fusion (LB-PBF) fabricated Inconel 718 in machined/polished surface condition, emphasizing on the influence of test frequency (i.e., cyclic strain rate). Uniaxial, fully-reversed force- and stress-controlled fatigue tests were conducted utilizing a servo-hydraulic and an ultrasonic test system operating at 5 Hz and 20 kHz, respectively, on wrought as well as LB-PBF vertically and diagonally built specimens. Fatigue cracks in the majority of the specimens were found to initiate from intra-granular slip bands near or at the surface, which gives rise to strong anisotropy in fatigue resistance in LB-PBF specimens due to the presence of columnar grains along the build directions. Longer fatigue lives were obtained at 20 kHz, which was ascribed to possibly lower-than-intended stresses applied in the ultrasonic tests. The corrected stress-life fatigue data at 20 kHz were found to converge to the one obtained from conventional testing at 5 Hz, implying no effect of cyclic strain rate on the fatigue behavior of Inconel 718 regardless of the fabrication process. The findings of this work confirm the use of ultrasonic fatigue testing to expedite generation of AM materials data to keep up with the current demand; however, the applied stress may need to be corrected.

36 MATERIALS SCIENCE↗

Dose and dose rate effects on the microstructural and mechanical stability of long-range ordered precipitates in Inconel 718

Nickel-based alloys offer exceptional mechanical properties and corrosion resistance for various applications in extreme environments such as high neutron flux, temperature, and stress. Precipitates, resulting from thermal treatments, increase the strength and creep resistance of these alloys. Here, heavy ion irradiation is shown to destabilize the γ' and γ" precipitates in Inconel 718 nickel-based alloy by disordering and dissolution processes. Transmission electron microscopy and atom probe tomography reveal that the disordering and dissolution rates of the precipitates are proportional to both irradiation dose and dose rate. Irradiation induced disordering occurs at a higher rate than the dissolution. From analyzing the hardening contributions, microscale mechanical results suggest radiation-induced disordering is responsible for the majority of the softening response at low dose. In addition, low dose radiation-induced disordering results in strain localization and is believed to be the primary cause for the drastic degradation of uniform elongation and toughness in irradiated Inconel 718.

36 MATERIALS SCIENCE↗

Growth and Performance of High-Quality SWCNT Forests on Inconel Foils as Lithium-Ion Battery Anodes

Large-scale production of vertically aligned single-walled carbon nanotubes (VA-SWCNTs) on metal foils promises to enable technological advancements in many fields, from functional composites to energy storage to thermal interfaces. In this work, we demonstrate growth of high-quality (G/D > 6, average diameters ~ 2–3 nm, densities > 10 12 cm –2 ) VA-SWCNTs on Inconel metal for use as a lithium-ion battery (LIB) anode. Scale-up of SWCNT growth on Inconel 625 to 100 cm 2 exhibits nearly invariant CNT structural properties, even when synthesis is performed near atmospheric pressure, and this robustness is attributed to a growth kinetic regime dominated by the carbon precursor diffusion in the bulk gas mixture. SWCNT forests produced on large-area metal substrates at close to atmospheric pressure possess a combination of structural features that are among the best demonstrated so far in the literature for growth on metal foils. Leveraging these achievements for energy applications, we demonstrate a VA-SWCNT LIB anode with capacity >1200 mAh/g at 1.0C and stable cycling beyond 300 cycles. Furthermore, this robust synthesis of high-quality VA-SWCNTs on metal foils presents a promising route toward mass production of high-performance CNT devices for a broad range of applications.

Energy↗

3D Printing of Inconel 718 with Enhanced Boron Composition as a Novel Solar Absorber Tube Material in the Concentrated Solar Power (CSP) System

The growing demands for elevated efficiency in the solar energy industry led researchers to focus on the development of functional solar absorber tube material in concentrated solar power (CSP) systems, when molten salts are adopted as the heat transfer fluid. In this study, the typical solar absorber tube material, Inconel 718, was enhanced with boron to achieve a higher solar absorptivity in the visible light spectrum. Combined with an additive manufacturing (AM) method, the boron composition exceeded the traditional manufacturing limit of 60 ppm without microstructural defects. The boron-enhanced Inconel 718 exhibited a high solar absorptivity of nearly 90 % while maintaining a high thermal cycle fatigue resistance after thermal cycling treatment between 550°C and 720°C. The boron composition was increased to the manufacturing failure point, and the effects of different boron compositions on mechanical properties, microstructure, and optical properties were studied. The provided microstructure-property map in this study delivers high potentials of functional AM-printed alloy material in CSP applications.

13 HYDRO ENERGY↗

Inconel 718 Oxide Coating Process for Mu2e Target Redesign

A method of growing an oxide coating on Inconel 718 samples was investigated to increase the emissivity of the redesigned Inconel Mu2e production target. Microscopy and emissivity measurements of a range of samples indicate excellent performance.

Williams, J. [Fermilab]↗

Microstructure and 77K mechanical properties of electron beam welded Cu101- Inconel 625 joints

In developing large-scale next-generation superconducting radio frequency (SRF) linear accelerators using superconducting films on Cu, the design and development of dissimilar welding and joining metals, such as Cu to Inconel, stainless steel, and Nb, are essential. In this talk, we present the development of procedures for electron-beam welding of Cu¿Inconel 625 and evaluation of the microstructure and 77K mechanical properties of the weld and base material in the welded condition and heat treatments in the 750°C ¿950°C heat treatment range. The results will be presented in the context of developing joining techniques for low-temperature applications where high conductivity and strength, vacuum hygiene, and magnetic properties of the material need consideration. The methods presented here are being deployed to thin film SRF Cu cavities at Jefferson Lab. Acknowledgment: This material is based upon work supported by the U.S. Department of Energy, Office of Science, Office of Nuclear

Khanal, Bashu↗

Achieving High Strength and Creep Resistance in Inconel 740H Superalloy through Wire-Arc Additive Manufacturing and Thermodynamic-Guided Heat Treatment

Inconel 740H superalloy is commonly used in advanced ultra-supercritical power plants since it possesses excellent strength and creep resistance. This study investigates the microstructure and mechanical properties of Inconel 740H superalloy fabricated using wire-arc additive manufacturing. The as-printed microstructure consisted of columnar γ grains with the Laves phase and (Nb, Ti)C carbides as secondary phases. The anisotropy in grain structure increased from the bottom to the top regions, while the hardness was highest in the middle portion of the build. To guide the post-heat treatment design, thermodynamic and kinetic simulations were employed to predict the temperature and time. Complete recrystallization with the Laves phase dissolution occurred throughout the build after homogenization at 1200 °C for 2 h. The peak hardness was achieved after aging at 760 °C for 12 h with the M 23 C 6 carbides decorating the grain boundaries and γ’ precipitates in the grain interior. The yield strength (655 MPa) and ductility (29.5%) in the post-heat treated condition exceeded the design targets (620 MPa, 20%). Stress rupture tests at 750 °C showed that the high-temperature performance was at par with the wrought counterparts. The fracture mode after rupture was identified to be intergranular with the presence of grain boundary cavities along with grain boundary sliding.

36 MATERIALS SCIENCE↗

Effects of Build Orientation and Heat Treatment on Neutron Irradiation Hardening in Inconel 625 Fabricated via Laser Powder Bed Fusion

Various Inconel 625 coupons fabricated via Laser Powder Bed Fusion (L-PBF) were neutron irradiated using the inside reflector of the reactor at the University of Missouri Research Reactor (MURR). Effects of build orientation and heat treatment on neutron-induced hardening were investigated by inspecting L-PBF samples built vertically or at a 45º angle in the following heat-treated conditions: as-built (no heat treatment), 700 ºC for 1 hour, 900 ºC for 1 hour, and 1050 ºC for 1 hour. The microhardness results of L-PBF samples before and after neutron irradiation were compared with traditional wrought Inconel 625. All samples underwent an irradiation flux of 6.61 x 1013 neutrons/cm²/s for 310 hours for an estimated damage of 0.012 dpa. Results indicate that as-built L-PBF specimens are less prone to radiation hardening relative to their wrought counterparts. As-printed diagonal specimens were shown to harden by 8% as compared to 1.2% hardening in as-printed vertical specimens.

36 MATERIALS SCIENCE↗

Predicting phase transformation kinetics during metal additive manufacturing using non-isothermal Johnson-Mehl-Avrami models: Application to Inconel 718 and Ti-6Al-4V

Here, a computational model was developed to predict solid-state phase transformation kinetics within mechanical parts during metal additive manufacturing processes. This model is a modified version of the Johnson-Mehl-Avrami model for non-isothermal phase transformations that can be applied to various material systems undergoing solid-state phase transformations. Using the thermal history of an additive manufacturing fabricated mechanical part, along with the necessary thermodynamic data and kinetic information as inputs, the model outputs the history of phase fraction evolution during the build process. The model was applied to an Inconel 718 part built by powder bed fusion and a Ti-6Al-4V part built by directed energy deposition. Microstructure characterization and mechanical testing were performed for the validation of the model.

36 MATERIALS SCIENCE↗

In-situ radiation response of additively manufactured modified Inconel 718 alloys

Here in this study, a novel alloy of modified Inconel 718 produced by laser powder bed fusion is studied before and after in-situ Kr irradiation up to 3 dpa at 200 and 450 °C. Before irradiation, the microstructure consists of dislocation cells having a misorientation angle less than 5° and with an average size of ~500 nm. There are also second phase particles of MC type carbides, Laves phase and oxides such as Y-O, Y-(Ti)-Al-O. While the microstructure consists of stacking fault tetrahedra, faulted and perfect loops after irradiation at 200 °C, dislocation loops are the primary defects at 450 °C. With increasing dose, the size of the defects remains similar at 200 °C while it increases at 450 °C. This has been attributed to the existence of vacancy type defects at 200 °C and the different defect transport mechanisms at different temperatures. Moreover, matrix and second phase particle compositions seem to be similar after irradiation. The sink strengths of the structures have been calculated and superior radiation resistance of this alloy has been attributed to the existence of fine cell boundaries stabilized by the second phase particles produced by additive manufacturing.

36 MATERIALS SCIENCE↗

Strain energy-based fatigue failure analyses of LB-PBF Inconel 718: Effect of build orientation

Additively manufactured Inconel 718 parts fabricated in three build orientations (horizontal, vertical, and angled at 45 degrees) are tested in fully-reversed bending fatigue mode. Damping measurements via the Impulse Excitation technique are used to assess the defects content in the microstructure and fractography analysis is performed to detect the root cause of failure. Two micro- and macro-scale methodologies of fatigue damage estimation based on the dissipated heat per cycle and the statistical estimation of micro-plastic strain energies are used to assess fatigue damage. It is shown that at a given stress level, the vertically built specimens endure the most fatigue damage before failure while the diagonally built ones sustain the least. As a result, the fatigue life is estimated for arbitrary load amplitudes via a microstructure-sensitive algorithm with acceptable accuracy as compared to the experiments.

36 MATERIALS SCIENCE↗

Process parameter translation strategies for variable directed energy deposition spot size using 316L, copper, and Inconel 625

Directed energy deposition (DED) is a form of additive manufacturing available across a variety of laser spot diameter values, often referred to as spot sizes. However, there is no method to easily transfer process parameters across discrete spot sizes, leading to DED process parameters that are equipment specific and not widely applicable. In this study, a strategy is proposed and investigated for five spot sizes that keep the areal energy density constant while varying power, feed rate, and powder flow during the deposition of 316L stainless steel. An assessment of trends in hardness and microstructure is possible due to the novel production of components of a single material across several spot sizes using a single nozzle on a single DED system. The proposed strategy was used to nullify the hardness drop during functional grading of Inconel 625 and pure copper, enabling fabrication of multi-material sample that does not compromise desirable properties. This application shows the value in establishing more efficient process parameter development and understanding spot size influences on geometric and material property flexibility, to enable a more diverse powder-based DED design space and to increase the industry adoption of DED systems.

316L↗

Synergistic effect of microstructure and defects on the initiation of fatigue cracks in additively manufactured Inconel 718

Fatigue cracks in additively manufactured (AMed) Inconel 718 (IN-718) in machined surface condition often initiate from persistent slip bands (PSBs) unlike other popular AM alloys such as 17-4 PH stainless steel or Ti-6Al-4V, where fatigue crack initiation is exclusively from volumetric defects; therefore, a competition between PSB- vs. defect- mediated crack initiation clearly exists. To shed light on the factors governing the competition, this study investigates the characteristics of cyclic strain localization, PSB formation, and crack initiation via crystal plasticity (CP) modeling of cyclic loading on polycrystalline aggregates which are then validated by experiments. In this work, a physics-based, free slip distance (FSD) dependent slip strength evolution law is proposed, which is shown to enable the CP model to simulate the heterogeneous strain distribution in IN-718. Implementing a crack initiation criterion based on strain contrast, the locations and lives for crack initiation can also be calculated. It is shown that both FSD and resolve shear stress influence the strain localization and crack initiation behaviors. The distribution of a localization parameter calculated based on the multiplication of FSD and Schmid factor within a grain is found to correlate well with the locations of PSBs. The maximum values of the localization parameters within a microstructure are shown to correlate well with the experimentally obtained crack initiation lives. The presence of volumetric defects in IN-718 generally do not impact strain localization behavior unless their size is large compared to the grain size.

42 ENGINEERING↗