At least 37 records · Page 2

Ion beam sputtering of fluoropolymers

Ion beam sputter processing rates as well as pertinent characteristics of etched targets and films are described. An argon ion beam source was used to sputter etch and deposit the fluoropolymers PTFE, FEP, and CTFE. Ion beam energy, current density, and target temperature were varied to examine effects on etch and deposition rates. The ion etched fluoropolymers yield cone or spire-like surface structures which vary depending upon the type of polymer, ion beam power density, etch time, and target temperature. Sputter target and film characteristics documented by spectral transmittance measurements, X-ray diffraction, ESCA, and SEM photomicrographs are included.

Sovey, J. S.↗

Thermosetting Fluoropolymer Foams

New process makes fluoropolymer foams with controllable amounts of inert-gas fillings in foam cells. Thermosetting fluoropolymers do not require foaming additives leaving undesirable residues and do not have to be molded and sintered at temperatures of about 240 to 400 degree C. Consequently, better for use with electronic or other parts sensitive to high temperatures or residues. Uses include coatings, electrical insulation, and structural parts.

Lee, Sheng Yen↗

Degradation Of Fluoropolymers by O(3P)

Three reports describe experimental studies of degradation of some fluoropolymers (and few nonfluorinated polymers) by monatomic oxygen in 3P state. Studies motivated by need to develop polymeric coats to protect some components of spacecraft against highly reactive O(3P) atmosphere at typical low Earth orbital altitudes. Results indicate fully fluorinated polymers most resistant to oxidation, while cross-linked (but otherwise fully fluorinated) fluoropolymers most resistant to etching.

Wydeven, Theodore↗

Performance characterization of EURECA retroreflectors with fluoropolymer-filled SiO(x) protective coatings

Aluminized corner-cube polymethylmethacrylate retroreflectors were coated with 92% SiO(x) - 8% fluoropolymer (by volume) and flown on the EURECA spacecraft. The fluoropolymer-filled SiO(x) protective coating was found to be durable to atomic oxygen when exposed in a ground-based plasma asher to an anticipated mission fluence of 2x10(exp 20) atoms/cm(exp 2). Unprotected retroreflector surfaces were found to develop highly diffuse reflectance characteristics, thus inhibiting their use for laser retroreflector purposes. A noncontacting retroreflector optical characterization system was constructed and used to measure the optical retroreflection characteristics of the following retroreflector materials: uncoated unexposed, coated unexposed, both uncoated and coated ground laboratory atomic oxygen exposed, and coated exposed to space atomic oxygen on the EURECA spacecraft. A comparison of the optical characterizations is presented.

Banks, Bruce A.↗

X-ray Photoelectron Spectroscopy Study of Argon-Plasma-Treated Fluoropolymers

Films of poly(tetrafluoroethylene) (PTFE) and of a tetrafluoroethylene-perfluoroalkyl vinyl ether (approximately 49:1) copolymer (PFA) were exposed to a radio-frequency argon plasma and then examined by X-ray photoelectron spectroscopy (XPS). The use of fluoropolymer films nearly free of surface hydrocarbon contamination as well as the use of a monochromatized X-ray source for XPS removed two factors contributing to conflicting reports on the effect of exposure time on the fluorine-to-carbon (F/C) and oxygen-to-carbon (O/C) ratios for several Ar-plasma-treated fluoropolymers. Contrary to literature indications, a common pattern was found for PTFE and PFA: a moderate decrease in F/C ratio (from 1.99 to 1.40, and from 1.97 to 1.57, respectively), together with a moderate increase in O/C ratio (from negligible to about 0.10, and from 0.012 to about O.10, respectively) at very short exposures, after which the F/C ratios remained essentially constant on prolonged exposures, while the O/C ratios for PTFE and PFA leveled off at 0.11 and 0.15, respectively. The XPS C(sub 1s), spectra for these polymers exposed to the Ar plasma for 20 min were similar and presented, besides a prominent peak at 292.0 eV (CF2,) and a minor peak at 294.0 or 294.1 eV (CF3), a composite band of four curve-resolved peaks (approximately 285-290 eV) representing various CH, CC, CO, CN, and CF functionalities.

Golub, Morton A.↗

Concerning Apparent Similarity of Structures of Fluoropolymer Surfaces Exposed to an Argon Plasma or Argon Ion Beam

X-ray photoelectron spectroscopy (XPS) C(sub 1s) spectra of fluoropolymers exposed to either an argon plasma or argon ion beam show remarkable similarity, implying that the surface-modification reactions for these two processes likely proceed through comparable mechanisms, revolving predominantly ion-surface interactions. The importance of working with a monochromatized x-ray source for XPS analysis of the surface-modified fluoropolymers is once again emphasized.

Golub, Morton A.↗

Fluoropolymer Films Deposited by Argon Ion-Beam Sputtering of Polytetrafluoroethylene

The FT-IR, XPS and UV spectra of fluoropolymer films (SPTFE-I) deposited by argon ion-beam sputtering of polytetrafluoroethylene (PTFE) were obtained and compared with prior corresponding spectra of fluoropolymer films (SPTFE-P) deposited by argon rf plasma sputtering of PTFE. Although the F/C ratios for SPTFE-I and -P (1.63 and 1.51) were similar, their structures were quite different in that there was a much higher concentration of CF2 groups in SPTFE-I than in SPTFE-P, ca. 61 and 33% of the total carbon contents, respectively. The FT-IR spectra reflect that difference, that for SPTFE-I showing a distinct doublet at 1210 and 1150 per centimeter while that for SPTFE-P presents a broad, featureless band at ca. 1250 per centimeter. The absorbance of the 1210-per centimeter band in SPTFE-I was proportional to the thickness of the film, in the range of 50-400 nanometers. The SPTFE-I was more transparent in the UV than SPTFE-P at comparable thickness. The mechanism for SPTFE-I formation likely involves "chopping off" of oligomeric segments of PTFE as an accompaniment to "plasma" polymerization of TFE monomer or other fluorocarbon fragments generated in situ from PTFE on impact with energetic Ar ions. Data are presented for SPTFE-I deposits and the associated Ar(+) bombarded PTFE targets where a fresh target was used for each run or a single target was used for a sequence of runs.

Golub, Morton A.↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material’s degradation modes and the backsheets’ field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics).

41 EE - Solar Energy Technologies Office (EE-4S)↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics). This presentation focuses on gloss, FTIR, and breakdown voltage measurements. Results for MiMo power, grayness from EL imaging, optical micrscopy, and specimen morphology (on extraction when cut from MiMos) is also presented.

backsheet↗

3D-Printable Fluoropolymer Gas Diffusion Layers for CO 2 Electroreduction

The electrosynthesis of value-added multicarbon products from CO 2 is a promising strategy to shift chemical production away from fossil fuels. Particularly important is the rational design of gas diffusion electrode (GDE) assemblies to react selectively, at scale, and at high rates. However, the understanding of the gas diffusion layer (GDL) in these assemblies is limited for the CO 2 reduction reaction (CO 2 RR): particularly important, but incompletely understood, is how the GDL modulates product distributions of catalysts operating in high current density regimes > 300 mA cm -2 . Here, 3D-printable fluoropolymer GDLs with tunable microporosity and structure are reported and probe the effects of permeance, microstructural porosity, macrostructure, and surface morphology. Under a given choice of applied electrochemical potential and electrolyte, a 100× increase in the C 2 H 4 :CO ratio due to GDL surface morphology design over a homogeneously porous equivalent and a 1.8× increase in the C 2 H 4 partial current density due to a pyramidal macrostructure are observed. Overall, these findings offer routes to improve CO 2 RR GDEs as a platform for 3D catalyst design.

36 MATERIALS SCIENCE↗

BACKFLIP: Identification of Materials and Changes Upon Aging of Emerging Fluoropolymer-Free and Industry-Benchmark PV Backsheets

Extending lifetimes of photovoltaic (PV) modules and decreasing manufacturing and decommissioning costs are motivating research of novel PV module backsheet materials. Backsheet integrity is critical to the safety and performance of a PV module, however, the polymeric materials are often vulnerable to environmental degradation. The long-term durability of emerging polyolefin (PO) materials is being examined to inform regarding the possible replacement of laminated backsheets containing polyethylene terephthalate (PET) cores and fluoropolymer protective inner/outer layers. This study compares traditional PET-based backsheets with novel, co-extruded, and recyclable PO-based backsheets after being subjected to hygrometric and UV photolytic accelerated weathering. A large set of characterization methods will compare physical, chemical, structural, mechanical, and insulating properties of these backsheets and the resulting mini-module (MiMo) PV performances. The study of chemical composition, glass- and phase-transition temperatures, degree of crystallinity, and crystalline structure are described here.

mini-module↗

HALAR fluoropolymer: A versatile insulation material

Research directed toward developing materials for the wire and cable industry has resulted in a new product, E-CTFE copolymer, which has an outstanding combination of electrical, thermal, and mechanical properties. The properties of E-CTFE are discussed and compared with those of other commercial fluoropolymers. Particular attention is given to the utility of E-CTFE as a wire and cable insulation.

Robertson, A. B.↗

The Acute Inhalation Toxicity in Rats from the Pyrolysis Products of Four Fluoropolymers

Male Sprague-Dawley rats (225?250 g) were exposed to the thermal degradation products from four fluoropolymers. The three polymers containing vinylidene fluoride and hexafluoropropene (VF2/HFP) were pyrolyzed at 550? and 800?C, whereas polytetrafluoroethylene (PTFE) was pyrolyzed at 625 and 800?C. At the lower temperatures, the pyrolysate from the copolymer of vinylidene fluoride and hexafluoropropene (VF2/HFP) was less toxic than the pyrolysates from either the terpolymer of vinyidene fluoride, hexafluoropropene, and tetrafluoroethylene (VF2/HFP/TFE) or the copolymer of vinylidene fluoride and hexafluoropropene with ?additives? (VF2/HFP-A). However, the pyrolysates from the VF2/HFP-containing materials produced less toxic products than the pyrolysate from PTFE at 625?C. When the pyrolysis temperature was increased to 800?C, very little difference was noted between the pyrolysis toxicity for any of the VF2/HFP-containing polymers with the most toxic pyrolysate again produced by PTFE. Carbon monoxide levels were all sublethal. No correlation could be established between hydrolyzable fluoride levels and the lethality of the pyrolysates. Death following exposure occurred within 48 hr due to acute pulmonary edema and hemorrhage. Survival of this acute phase was followed by alveolar lymphocytic infiltration and peribronchial tissue proliferation.

Carter, V. L., Jr.↗

Flexible fluoropolymer filled protective coatings

Metal oxide films such as SiO2 are known to provide an effective barrier to the transport of moisture as well as gaseous species through polymeric films. Such thin film coatings have a tendency to crack upon flexure of the polymeric substrate. Sputter co-deposition of SiO2 with 4 to 15 percent fluoropolymers was demonstrated to produce thin films with glass-like barrier properties that have significant increases in strain to failure over pure glass films which improves their tolerance to flexure on polymeric substrates. Deposition techniques capable of producing these films on polymeric substrates are suitable for durable food packaging and oxidation/corrosion protection applications.

Banks, Bruce A.↗

Reactively Deposited Aluminum Oxide and Fluoropolymer Filled Aluminum Oxide Protective Coatings for Polymers

Reactive ion beam sputter deposition of aluminum simultaneous with low energy arrival of oxygen ions at the deposition surface enables the formation of highly transparent aluminum oxide films. Thick (12 200 A), adherent, low stress, reactively deposited aluminum oxide films were found to provide some abrasion resistance to polycarbonate substrates. The reactively deposited aluminum oxide films are also slightly more hydrophobic and more transmitting in the UV than aluminum oxide deposited from an aluminum oxide target. Simultaneous reactive sputter deposition of aluminum along with polytetrafluoroethylene (PTFE Teflon) produces fluoropolymer-filled aluminum oxide films which are lower in stress, about the same in transmittance, but more wetting than reactively deposited aluminum oxide films. Deposition properties, processes and potential applications for these coatings will be discussed.

Rutledge, Sharon K.↗

Fluoropolymer Films Deposited by RF Plasma Sputtering of Polytetrafluoroethylene Using Inert Gases

The FT-IR (Fourier Transform Infrared), UV (Ultraviolet) and XPS (X Ray Photoelectron Spectroscopy) spectra of fluoropolymer films (SPTFE) deposited by rf (radio frequency) plasma sputtering of polytetrafluoroethylene (PTFE), using Ne, Kr and Xe as sputtering gases, were obtained and compared with prior spectra for SPTFE formed using He and Ar. The F/C (fluorine / carbon) ratios for SPTFE films (1.44-1.55), obtained at a rf power of 10 W, were essentially the same for all five rare gases, there being no trend of decreasing fluorine content in the SPTFE product with increasing atomic weight of the sputtering gas - contrary to the momentum transfer notion advanced by M. E. Ryan, et al. Increasing rf power from 10 to 50 W resulted in successively lower F/C ratios for SPTFE (e.g., from 1.55 to 1.21 in the case of Xe plasma-sputtered PTFE), accompanied by sputtering of the glass reactor and deposition of fragments of sodium aluminum silicate occurring at 40 W and above. In order to achieve a "Teflon-like" SPTFE structure (i.e., products with as high a F/C ratio as possible) in a given plasma reactor, an optimum rf power must be found, which in the present case was approximately 10 W.