Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Effects of via-conductor geometry in the electromigration failure of Al:Cu wires

Electromigration (EM) experiments conducted using two types of via/plug to conductor alignment indicate a geometrical dependence of electromigration failure in Al:Cu conductors. The resistance vs time curves show distinctive steps when the alignment is parallel. This is explained by a successive loss of conductivity through the plug due to void formation. In the perpendicular via/conductor arrangement, resistance increases by smaller and closely spaced steps. EM experiments without vias, found that the conductor life under stress increases by at least an order of magnitude. Kinetic studies at four temperatures between 180-240 C found activation energies to be 1.0 plus or minus 0.1eV.

Al:Cu accelerated testing electromigration activat↗

Flow through negatively charged, nanoporous membranes separates Li + and K + due to induced electromigration

Flow through negatively charged nanopores separates Li + and K + with selectivities of up to 70 and Li + passages from 20% to above 100%. Remarkably, both the Li + /K + selectivity and Li + passage initially increase with flow rate, breaking the permeability/selectivity trade-off. Modelling demonstrates that flow through the membranes creates electric fields that retard transport of cations. Selectivity increases with flow rate because the K + electromigration velocity exceeds its convective velocity, but for Li + electromigration is weaker than convection. Here, modelling also shows the importance of controlling concentration polarization. With further work, related separations might provide highly pure Li salts for battery manufacturing.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electromigration study of copper lines on steps prepared by a plasma-based etch process

The electromigration phenomenon of the copper line etched with a plasma-based process over the SiN{sub x} step has been investigated. Two important factors, i.e., the dielectric topography and the stress temperature, were examined using the accelerated isothermal electromigration method. The activation energy of 0.73 eV to 0.89 eV indicates two possible mass transport pathways: interfacial and copper surface diffusions. The copper line on the SiN{sub x} step has a shorter lifetime and a smaller activation energy than the copper line on the flat surface has. For the former, voids were formed at the cusp region and perpendicular to the current flow direction. For the latter, voids were formed in series and parallel to the current flow direction. The ''neck'' structure at the cusp region, which is a result of the inappropriate etching condition, further decreased the lifetime and the activation energy. The lifetime of the ''neck-free'' copper line over the SiN{sub x} step was estimated to be 7.1 x 10{sup 9} s under the high-speed IC operation condition. The thermal stress mismatch between the copper layer and TiW barrier layer as well as the underneath dielectric layer facilitated the void formation. The step effect on the lifetime was reduced when the test temperature was high because of the change of the local stress. In summary, the topography and the test temperature are critical factors for the copper line's lifetime.

36 MATERIALS SCIENCE↗

Lattice dependent motion of voids during electromigration

The influence of the crystal lattice configuration to electromigration processes, e.g., void formation and propagation, is investigated in suitable test structures. They are fabricated out of self-assembled, bi-crystalline Ag islands, grown epitaxially on a clean Si(111) surface. The {mu}m-wide and approximately 100 nm thick Ag islands are a composition of a Ag(001) and a Ag(111) part. By focused ion beam milling, they are structured into wires with a single grain boundary, the orientation of which can be chosen arbitrarily. In-situ scanning electron microscopy (SEM) allows to capture an image sequence during electrical stressing and monitors the development of voids and hillocks in time. To visualize the position and motion of voids, we calculate void maps using a threshold algorithm. Most of the information from the SEM image sequence is compressed into one single image. Our present electromigration studies are based on in-situ SEM investigations for three different lattice configurations: Ag(001) (with electron current flow in [110] direction), Ag(111) (with electron current flow in [112] direction), and additionally 90 Ring-Operator rotated Ag(111) (with electron current flow in [110] direction). Our experimental results show that not only the formation and shape but also the motion direction of voids strongly depends on the crystal orientation.

36 MATERIALS SCIENCE↗

Electromigration induced Kirkendall void growth in Sn-3.5Ag/Cu solder joints

Effects of electric current flow on the Kirkendall void formation at solder joints were investigated using Sn-3.5Ag/Cu joints specially designed to have localized nucleation of Kirkendall voids at the Cu{sub 3}Sn/Cu interface. Under the current density of 1 × 10{sup 4} A/cm{sup 2}, kinetics of Kirkendall void growth and intermetallic compound thickening were affected by the electromigration (EM), and both showed the polarity effect. Cu{sub 6}Sn{sub 5} showed a strong susceptibility to the polarity effect, while Cu{sub 3}Sn did not. The electromigration force induced additional tensile (or compressive) stress at the cathode (or anode), which accelerated (or decelerated) the void growth. From the measurements of the fraction of void at the Cu{sub 3}Sn/Cu interface on SEM micrographs and analysis of the kinetics of void growth, the magnitude of the local stress induced by EM was estimated to be 9 MPa at the anode and −7 MPa at the cathode.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Fast electromigration crack in nanoscale aluminum film

The current-induced breakage of 20 nm thin aluminum layers deposited onto capacitor grade polypropylene (PP) films is experimentally studied. Biexponential current pulses of different amplitude (10–15 A) and duration (0.1–1 μs) were applied to the samples. Breakage occurred after fast development of electromigrating ∼200 nm-wide cracks with initial propagation velocity of ∼1 m/s under a high current density of ∼10{sup 12 }A/m{sup 2}. The cracks stopped when their lengths reached 250–450 μm. This behavior is explained by the balance of electromigration and stress-induced atomic fluxes.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

1/f noise measurements for faster evaluation of electromigration in advanced microelectronics interconnections

The use of 1/f noise measurements is explored for the purpose of finding faster techniques for electromigration (EM) characterization in advanced microelectronic interconnects, which also enable a better understanding of its underlying physical mechanisms. Three different applications of 1/f noise for EM characterization are explored. First, whether 1/f noise measurements during EM stress can serve as an early indicator of EM damage. Second, whether the current dependence of the noise power spectral density (PSD) can be used for a qualitative comparison of the defect concentration of different interconnects and consequently also their EM lifetime t50. Third, whether the activation energies obtained from the temperature dependence of the 1/f noise PSD correspond to the activation energies found by means of classic EM tests. In this paper, the 1/f noise technique has been used to assess and compare the EM properties of various advanced integration schemes and different materials, as they are being explored by the industry to enable advanced interconnect scaling. More concrete, different types of copper interconnects and one type of tungsten interconnect are compared. The 1/f noise measurements confirm the excellent electromigration properties of tungsten and demonstrate a dependence of the EM failure mechanism on copper grain size and distribution, where grain boundary diffusion is found to be a dominant failure mechanism.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Temperature control in wafer-level testing of large multi-segment electromigration test structures

The paper describes two methods for maintaining a constant metallization temperature throughout a wafer-level isothermal electromigration test of large multisegment test structures where Joule-heating is high and chip to chuck thermal contact is poor. In the first method, an initial calibration of Joule heating versus metal temperature is carried out. During the isothermal electromigration test, the Joule heating is continuously monitored and the chuck temperature is adjusted based on the calibration results to maintain a constant metal temperature. In the second method, temperature sensors are fabricated on the chip and then the sensors are used to monitor the chip temperature directly. The chuck temperature is then adjusted as needed.

Zamani, Nasser↗

Designing Accelerated Tests Of Electromigration

Method for design of accelerated tests of electromigration (as in microscopic conductors in integrated circuits) based partly on simplified mathematical model of electromigration and partly on error analysis. Objective to determine quickly operating life of tested components under normal operating conditions by extrapolation from lifetime measurements at operating stresses greater than normal. Involves compromise between reducing testing time by increasing stresses and reducing uncertainty in extrapolated lifetime by decreasing stresses.

Buehler, Martin G.↗

An analytical solution of the solution-diffusion-electromigration equations reproduces trends in ion rejections during nanofiltration of mixed electrolytes

Here, this paper develops an analytical solution to the equations governing the solution-diffusion-electromigration transport of the ions from two salts that contain a common ion. The analytical expressions, which rely on constant ion permeances, readily enable simple spreadsheet computations of the permeate ion concentrations in nanofiltration (NF). Despite the model simplicity, calculations of ion rejections as a function of transmembrane volume fluxes, feed-solution compositions, and permeance values reproduce experimental trends, with ion permeances as the only adjustable parameters. For example, with solutions containing dissolved MA and M 2 B, when the membrane permeance to B 2– is much lower than the permeances to A – and M + , plots of A – rejection versus transmembrane volume flux show the negative minimum that is often characteristic of NF. Moreover, B 2– rejection increases with increasing MA in the feed solution, reflecting a decreasing electric field in the membrane. The analytical solution also enables spreadsheet computations of electric fields in membrane separation layers and effectively models experimental data for intrinsic rejections as a function of transmembrane volume flow. Interestingly, the model suggests that with sufficiently high permeances of A – (relative to M + ), at certain feed compositions the A – /B 2– selectivity may increase without bound as a function of volume flow. Otherwise, this selectivity does not vary greatly with feed composition and quickly reaches a limit as the volume flow increases. Despite the simplifying approximation of constant ion permeances, using only a few adjustable parameters this model readily reveals trends in NF ion rejections and may help to identify the desired ion permeances or solution compositions for specific separations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Explaining an unusual electromigration behavior—A comprehensive experimental and theoretical analysis using finite element method

In metallic interconnects, it is generally assumed that electromigration (EM) failure location is independent of the applied electrical current and always occurs at the highest-current-density area. Our experiments show otherwise. We designed an Al interconnect that alters its failure location by only varying the applied current density. The failure occurs near the high for a current above 2 × 10 7 A/cm 2 , but at a location with 59% of the maximum for lower current densities. Thermoreflectance thermal imaging is employed to gather time-dependent high-resolution spatial temperature distributions of the Al interconnect during EM. More importantly, we propose a computationally inexpensive 2D finite element method that tracks EM evolution in time and matches well with the observations from different experimental conditions. A detailed analysis covering the major driving forces of EM is carried out to understand the complex physics behind EM. The atomic depletion rate contributed by each force is quantitatively studied. By examining the results from every tested experimental condition, the model reveals that the temperature gradient is the key reason causing atomic depletion near the failure location. Graphical illustrations and qualitative analysis are provided to intuitively show the key findings of our work.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

In-situ study of electromigration-induced grain rotation in Pb-free solder joint by synchrotron microdiffraction

The rotation of Sn grains in Pb-free flip chip solder joints hasn't been reported in literature so far although it has been observed in Sn strips. In this letter, we report the detailed study of the grain orientation evolution induced by electromigration by synchrotron based white beam X-ray microdiffraction. It is found that the grains in solder joint rotate more slowly than in Sn strip even under higher current density. On the other hand, based on our estimation, the reorientation of the grains in solder joints also results in the reduction of electric resistivity, similar to the case of Sn strip. We will also discuss the reason why the electric resistance decreases much more in strips than in the Sn-based solders, and the different driving force for the grain growth in solder joint and in thin film interconnect lines.

36 MATERIALS SCIENCE↗

Microstructure evolution of Ag–8Au–3Pd alloy wire during electromigration

As the continuous shrinkage of the interconnect line width in microelectronics devices, there is a growing concern about the electromigration (EM) failure of bonding wire. In addition, an innovative Ag–8Au–3Pd alloy wire has shown promise as an economical substitute for gold wire interconnects due to the cost pressure of gold in the last decade. In present study of the Ag–8Au–3Pd alloy wire, the surface diffusion occupied the dominant position during EM failure, and the activation energy was found to be 0.61 eV. In order to reveal the failure mechanism, the cross-sections of the Ag–8Au–3Pd alloy wire during EM were prepared by focused ion beam (FIB) micro-machining for electron backscatter diffraction (EBSD) analysis. The microstructure evolution of the Ag–8Au–3Pd alloy wire was characterized by the grain size and grain boundary. As a result, the EM failure originates in the atom transportation, which causes grain size increasing and atom diffusion on the wire surface. - Highlights: • The activation energy of Ag–8Au–3Pd alloy wire was obtained as 0.61 eV. • During EM, the silver atoms diffused from negative to the positive terminal on the wire surface. • The microstructure (grain size and grain boundary) was characterized by FIB-EBSD. • During EM, the atom transportation was found to cause grain size growth and atom diffusion on the wire surface.

36 MATERIALS SCIENCE↗

In situ synchrotron study of electromigration induced grain rotations in Sn solder joints

In this paper we report an in situ study of the early stage of microstructure evolution induced by electromigration in a Pb-free β-Sn based solder joint by synchrotron polychromatic X-ray microdiffraction. With this technique, crystal orientation evolution is monitored at intragranular levels with high spatial and angular resolution. During the entire experiment, no crystal growth is detected, and rigid grain rotation is observed only in the two grains within the current crowding region, where high density and divergence of electric current occur. Theoretical calculation indicates that the trend of electrical resistance drop still holds under the present conditions in the grain with high electrical resistivity, while the other grain with low resistivity reorients to align its a-axis more parallel with the ones of its neighboring grains. A detailed study of dislocation densities and subgrain boundaries suggests that grain rotation in β-Sn, unlike grain rotation in high melting temperature metals which undergo displacive deformation, is accomplished via diffusional process mainly, due to the high homologous temperature.

36 MATERIALS SCIENCE↗

Electrochemical strain microscopy with blocking electrodes: The role of electromigration and diffusion

Electrochemical strains are a ubiquitous feature of solid state ionic devices ranging from ion batteries and fuel cells to electroresistive and memristive memories. We proposed a scanning probe microscopy (SPM) based approach, referred as electrochemical strain microscopy (ESM), for probing local ionic flows and electrochemical reactions in solids based on bias-strain coupling. In ESM, the sharp SPM tip concentrates the electric field in a small (10-50 nm) region of material, inducing interfacial electrochemical processes and ionic flows. Furthermore, we use the resultant electrochemical strains to determine it from dynamic surface displacement and provide information on local electrochemical functionality. We also analyze image formation mechanism in ESM for a special case of mixed electronic-ionic conductor with blocking tip electrode, and determine frequency dependence of response, role of diffusion and electromigration effects, and resolution and detection limits.

36 MATERIALS SCIENCE↗

Investigation of electromigration in In{sub 2}Se{sub 3} nanowire for phase change memory devices

The decomposition of In{sub 2}Se{sub 3} nanowire phase change memory devices during current-driving operation was investigated. The devices were subjected to thermal/electrical stress with current density and electric field during the reset operation at 0.24–0.38 MA/cm{sup 2} and 5.3–6.4 kV/cm, respectively. After multiple operation cycles, a change in morphology and composition of the In{sub 2}Se{sub 3} nanowire was observed and led to the device failure. The transmission electron microscopy and energy dispersive analysis indicate that electromigration causes the catastrophic failure by void formation where In atoms migrate toward the cathode and Se atoms migrate toward the anode depending on their electronegativities.

36 MATERIALS SCIENCE↗

Electromigration-induced back stress in critical solder length for three-dimensional integrated circuits

Because of the miniaturization of electronic devices, the reliability of electromigration has become a major concern when shrinking the solder dimensions in flip-chip joints. Fast reaction between solders and electrodes causes intermetallic compounds (IMCs) to form, which grow rapidly and occupy entire joints when solder volumes decrease. In this study, U-grooves were fabricated on Si chips as test vehicles. An electrode-solder-electrode sandwich structure was fabricated by using lithography and electroplating. Gaps exhibiting well-defined dimensions were filled with Sn3.5Ag solders. The gaps between the copper electrodes in the test sample were limited to less than 15 μm to simulate microbumps. The samples were stressed at various current densities at 100 °C, 125 °C, and 150 °C. The morphological changes of the IMCs were observed, and the dimensions of the IMCs were measured to determine the kinetic growth of IMCs. Therefore, this study focused on the influence of back stress caused by microstructural evolution in microbumps.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗