In situ investigation of high-pressure hydrogen-induced swelling in elastomers and its correlation with material properties

The resistance of elastomeric materials to high-pressure hydrogen-induced damage is essential for ensuring the reliability of hydrogen infrastructure. Here, in this study, we systematically investigated the swelling behavior and hydrogen transport properties of four elastomer types – EPDM, NBR, FKM, and HNBR – using a custom in-situ view cell system capable of real-time monitoring during decompression from pressures up to 96.5 MPa. Each elastomer was formulated with and without fillers and plasticizers to assess the effects of formulation on swelling response. Thermal desorption analysis (TDA) was employed to determine equilibrium hydrogen content and diffusion coefficients, providing insight into gas uptake and mobility within each material. Correlation analyses using Pearson and Spearman coefficients revealed that the diffusion coefficient showed a stronger relationship with swelling behavior than hydrogen content, highlighting the dominant role of hydrogen mobility. Filled elastomers, particularly those with carbon black, consistently showed reduced swelling due to enhanced stiffness and reduced diffusivity. These results deepen our understanding of diffuso-mechanical interactions in elastomers and support the rational design of sealing materials for high-pressure hydrogen systems.

EPDM

Development of procedures for calculating stiffness and damping of elastomers in engineering applications, part 6

An elastomer damper was designed, tested, and compared with the performance of a hydraulic damper for a power transmission shaft. The six button Viton-70 damper was designed so that the elastomer damper or the hydraulic damper could be activated without upsetting the imbalance condition of the assembly. This permitted a direct comparison of damper effectiveness. The elastomer damper consistently performed better than the hydraulic mount and permitted stable operation of the power transmission shaft to speeds higher than obtained with the squeeze film damper. Tests were performed on shear specimens of Viton-79, Buna-N, EPDM, and Neoprene to determine performance limitations imposed by strain, temperature, and frequency. Frequencies of between 110 Hz and 1100 Hz were surveyed with imposed strains between 0.0005 and 0.08 at temperatures of 32 C, 66 C, and 80 C. A set of design curves was generated in a unified format for each of the elastomer materials.

Rieger, A.

Elastomer damper performance - A comparison with a squeeze film for a supercritical power transmission shaft

This paper describes the design and testing of an elastomer damper on a super-critical power transmission shaft. The elastomers were designed to provide acceptable operation through the fourth bending mode and to control synchronous as well as nonsynchronous vibration throughout the operating range. The design of the elastomer was such that it could be incorporated into the system as a replacement for a squeeze-film damper without a reassembly, which could have altered the imbalance of the shaft. This provided a direct comparison of the elastomer and squeeze-film dampers without having to assess the effect of shaft imbalance changes.

Zorzi, E. S.

Mechanical design handbook for elastomers

A comprehensive guide for the design of elastomer dampers for application in rotating machinery is presented. Theoretical discussions, a step by step procedure for the design of elastomer dampers, and detailed examples of actual elastomer damper applications are included. Dynamic and general physical properties of elastomers are discussed along with measurement techniques.

Darlow, M.

Addition polyimide adhesives containing ATBN and silicone elastomers

A study was conducted to determine the effects of added elastomers on the thermal stability, adhesive strength, and fracture toughness of LARC-13, a high-temperature addition polyimide adhesive. Various butadiene/acrylonitrile and silicon elastomers were incorporated into the polyimide resin either as physical polyblends, or by chemically reacting the elastomers with the polyimide backbone. Adhesive single lap-shear and T-peel strengths were measured before and after ageing at elevated temperature. A tapered double-cantilever beam specimen was used to determine the fracture toughness of the elastomer-modified polyimide adhesives.

Saint Clair, A. K.

Elastomer-toughened polyimide adhesives

A study has been conducted to determine the effects of added elastomers on the Tg, thermal stability, adhesive strength, and fracture toughness of LARC-13, a high-temperature addition polyimide adhesive. Various butadiene/acrylonitrile and silicone elastomers were incorporated into the polyimide resin (1) as physical polyblends, and (2) by chemically reacting the elastomers with the polyimide backbone. Adhesive single lap-shear and T-peel strengths were measured before and after aging at elevated temperature. A tapered double-cantilever beam specimen was used to determine the fracture toughness of the elastomer-modified polyimide adhesives.

Saint Clair, A. K.

Method of bonding plasticized elastomer to metal and articles produced thereby

Plasticized elastomer was securely bonded to a metal surface by interposing between the adhesive-coated metal surface and the elastomer sheet of material obtained by combining adhesive with a portion of the elastomer that was treated to remove plasticizers therefrom and heating the assembly in a mold under pressure. The sheet material is made up by dissolving a portion of the plasticized elastomer in an organic solvent, casting the solution, exposing it to a vacuum to remove the solvent and plasticizers, dissolving the deplasticized material in liquid adhesive and casting and drying the resulting liquid.

White, W. T.

Mechanical Design Handbook for Elastomers

Mechanical Design Handbook for Elastomers reviews state of art in elastomer-damper technology with particular emphasis on applications of highspeed rotor dampers. Self-contained reference but includes some theoretical discussion to help reader understand how and why dampers used for rotating machines. Handbook presents step-by-step procedure for design of elastomer dampers and detailed examples of actual elastomer damper applications.

Darlow, M.

Electrostrictive Graft Elastomers

An electrostrictive graft elastomer has a backbone molecule which is a non-crystallizable, flexible macromolecular chain and a grafted polymer forming polar graft moieties with backbone molecules. The polar graft moieties have been rotated by an applied electric field, e.g., into substantial polar alignment. The rotation is sustained until the electric field is removed. In another embodiment, a process for producing strain in an elastomer includes: (a) providing a graft elastomer having a backbone molecule which is a non-crystallizable, flexible macromolecular chain and a grafted polymer forming polar graft moieties with backbone molecules; and (b) applying an electric field to the graft elastomer to rotate the polar graft moieties, e.g., into substantial polar alignment.

Su, Ji

Characteristics of Elastomer Seals Exposed to Space Environments

A universal docking and berthing system is being developed by the National Aeronautics and Space Administration (NASA) to support all future space exploration missions to low-Earth orbit (LEO), to the Moon, and to Mars. The Low Impact Docking System (LIDS) is being designed to operate using a seal-on-seal configuration in numerous space environments, each having unique exposures to temperature, solar radiation, reactive elements, debris, and mission duration. As the LIDS seal is likely to be manufactured from an elastomeric material, performance evaluation of elastomers after exposure to atomic oxygen (AO) and ultraviolet radiation (UV) was conducted, of which the work presented herein was a part. Each of the three candidate silicone elastomer compounds investigated, including Esterline ELA-SA-401, and Parker Hannifin S0383-70 and S0899-50, was characterized as a low outgassing compound, per ASTM E595, having percent total mass loss (TML) less than 1.0 percent and collected volatile condensable materials (CVCM) less than 0.1 percent. Each compound was compatible with the LIDS operating environment of -50 to 50 C. The seal characteristics presented include compression set, elastomer-to-elastomer adhesion, and o-ring leakage rate. The ELA-SA-401 compound had the lowest variation in compression set with temperature. The S0383-70 compound exhibited the lowest compression set after exposure to AO and UV. The adhesion for all of the compounds was significantly reduced after exposure to AO and was further decreased after exposure to AO and UV. The leakage rates of o-ring specimens showed modest increases after exposure to AO. The leakage rates after exposure to AO and UV were increased by factors of up to 600 when compared to specimens in the as-received condition.

Daniels, Christopher C.

Elastomer Reinforced with Carbon Nanotubes

Elastomers are reinforced with functionalized, single-walled carbon nanotubes (SWNTs) giving them high-breaking strain levels and low densities. Cross-linked elastomers are prepared using amine-terminated, poly(dimethylsiloxane) (PDMS), with an average molecular weight of 5,000 daltons, and a functionalized SWNT. Cross-link densities, estimated on the basis of swelling data in toluene (a dispersing solvent) indicated that the polymer underwent cross-linking at the ends of the chains. This thermally initiated cross-linking was found to occur only in the presence of the aryl alcohol functionalized SWNTs. The cross-link could have been via a hydrogen-bonding mechanism between the amine and the free hydroxyl group, or via attack of the amine on the ester linage to form an amide. Tensile properties examined at room temperature indicate a three-fold increase in the tensile modulus of the elastomer, with rupture and failure of the elastomer occurring at a strain of 6.5.

Hudson, Jared L.

Effects of Hypervelocity Impacts on Silicone Elastomer Seals and Mating Aluminum Surfaces

While in space silicone based elastomer seals planned for use on NASA's Crew Exploration Vehicle (CEV) are exposed to threats from micrometeoroids and orbital debris (MMOD). An understanding of these threats is required to assess risks to the crew, the CEV orbiter, and missions. An Earth based campaign of hypervelocity impacts on small scale seal rings has been done to help estimate MMOD threats to the primary docking seal being developed for the Low Impact Docking System (LIDS). LIDS is being developed to enable the CEV to dock to the ISS (International Space Station) or to Altair (NASA's next lunar lander). The silicone seal on LIDS seals against aluminum alloy flanges on ISS or Altair. Since the integrity of a seal depends on both sealing surfaces, aluminum targets were also impacted. The variables considered in this study included projectile mass, density, speed, incidence angle, seal materials, and target surface treatments and coatings. Most of the impacts used a velocity near 8 km/s and spherical aluminum projectiles (density = 2.7 g/cubic centimeter), however, a few tests were done near 5.6 km/s. Tests were also performed using projectile densities of 7.7, 2.79, 2.5 or 1.14 g/cubic centimeter. Projectile incidence angles examined included 0 degrees, 45 degrees , and 60 degrees from normal to the plane of the target. Elastomer compounds impacted include Parker's S0383-70 and Esterline's ELA-SA-401 in the as received condition, or after an atomic oxygen treatment. Bare, anodized and nickel coated aluminum targets were tested simulating the candidate mating seal surface materials. After impact, seals and aluminum plates were leak tested: damaged seals were tested against an undamaged aluminum plate; and undamaged seals were placed at various locations over craters in aluminum plates. It has been shown that silicone elastomer seals can withstand an impressive level of damage before leaking beyond allowable limits. In general on the tests performed to date, the diameter of the crater in either the elastomer, or the aluminum, must be at least as big as 80% to 90% of width of the bulb of the seal before significant leakage occurs.

deGroh, Henry C., III

Effects of Hypervelocity Impacts on Silicone Elastomer Seals and Mating Aluminum Surfaces

While in space silicone based elastomer seals planned for use on NASA's Crew Exploration Vehicle (CEV) are exposed to threats from micrometeoroids and orbital debris (MMOD). An understanding of these threats is required to assess risks to the crew, the CEV orbiter, and missions. An Earth based campaign of hypervelocity impacts on small scale seal rings has been done to help estimate MMOD threats to the primary docking seal being developed for the Low Impact Docking System (LIDS). LIDS is being developed to enable the CEV to dock to the ISS (International Space Station) or to Altair (NASA's next lunar lander). The silicone seal on LIDS seals against aluminum alloy flanges on ISS or Altair. Since the integrity of a seal depends on both sealing surfaces, aluminum targets were also impacted. The variables considered in this study included projectile mass, density, speed, incidence angle, seal materials, and target surface treatments and coatings. Most of the impacts used a velocity near 8 km/s and spherical aluminum projectiles (density = 2.7 g/cubic cm), however, a few tests were done near 5.6 km/s. Tests were also performed using projectile densities of 7.7, 2.79, 2.5 or 1.14 g/cubic cm. Projectile incidence angles examined included 0 deg, 45 deg, and 60 deg from normal to the plane of the target. Elastomer compounds impacted include Parker's S0383-70 and Esterline's ELA-SA-401 in the as received condition, or after an atomic oxygen treatment. Bare, anodized and nickel coated aluminum targets were tested simulating the candidate mating seal surface materials. After impact, seals and aluminum plates were leak tested: damaged seals were tested against an undamaged aluminum plate; and undamaged seals were placed at various locations over craters in aluminum plates. It has been shown that silicone elastomer seals can withstand an impressive level of damage before leaking beyond allowable limits. In general on the tests performed to date, the diameter of the crater in either the elastomer, or the aluminum, must be at least as big as 80% to 90% of width of the bulb of the seal before significant leakage occurs.

deGroh, Henry C., III

Use of VUV Radiation to Control Elastomer Seal Adhesion

Due to their wide operating temperatures and low leakage rates, silicone elastomers are the only class of flight qualified elastomer materials that currently meet NASA's needs for various seal applications, which include docking and hatch seals for future space exploration vehicles. However, silicone elastomers are naturally sticky and exhibit sizeable adhesion when mated against metals and other silicone surfaces. This undesirable adhesion can make undocking spacecraft or opening a hatch problematic. Two approaches that can be used to reduce seal adhesion include use of grease or, application of low doses of atomic oxygen (AO). This paper investigates a third approach: the application of light doses of vacuum ultraviolet (VUV) radiation. Presented are the adhesion and leakage characteristics of S0383-70 silicone elastomer exposed to various VUV doses in the 115 to 200 nm wavelength range. The data indicate that adhesion is expected to be less than the target threshold maximum of 2 lb/in(exp2) after about 1 J/cm(exp2) of VUV exposure for seal-to-metal configurations and after 2 J/cm(exp2) for seal-to-seal configurations with no significant damage, or increase in seal leakage. This paper shows that VUV, without AO or grease, can be an effective means to reduce adhesion to the desired levels necessary for space seals with minimal change in seal leak rates.

deGroh, Henry C., III

Using Digital Image Correlation for Quantifying Load Induced in Elastomers at Cryogenic Temperatures

Elastomers have glass transition temperatures (TG) that are well below room temperature. Below this temperature, elastomers can suddenly exhibit significantly different mechanical properties than those exhibited at warmer temperatures. A unique test was developed to measure the induced load generated by elastomers that have been gripped on both ends and cooled to cryogenic temperatures. The test simulates a space flight critical component that will result in loss of vehicle if the elastomer separates from the gripped end. Digital image correlation (DIC) was used to measure the strain on the material surface and the displacement of the grips during testing. Two cameras were mounted on an isolated tripod to capture images through optical glass fitted on the thermal chamber. DIC measurements were used to measure the elastic modulus, coefficient of thermal expansion, and the loads at the gripped ends, above and below the TG. There was nearly no load developed while the temperature was above the TG but loads rapidly increased two orders of magnitude as the temperature dropped below the TG.

Matlock Mennu

Evaluation of a Conductive Elastomer Seal for Spacecraft

An electrically conductive elastomer was evaluated as a material candidate for a spacecraft seal. The elastomer used electrically conductive constituents as a means to reduce the resistance between mating interfaces of a sealed joint to meet spacecraft electrical bonding requirements. The compound's outgassing levels were compared against published NASA requirements. The compound was formed into a hollow O-ring seal and its compression set was measured. The O-ring seal was placed into an interface and the electrical resistance and leak rate were quantified. The amount of force required to fully compress the test article in the sealing interface and the force needed to separate the joint were also measured. The outgassing and resistance measurements were below the maximum allowable levels. The room temperature compression set and leak rates were fairly high when compared against other typical spacecraft seal materials, but were not excessive. The compression and adhesion forces were desirably low. Overall, the performance of the elastomer compound was sufficient to be considered for future spacecraft seal applications.

elastomer

Effects of high-pressure hydrogen exposure on filler-elastomer adhesion

Elastomers are known to gain enhanced mechanical properties through compounding with nanosized filler particles such as silica or carbon black. Filler dispersion and filler-polymer interfacial strength are key contributing factors to this improvement. The interfacial strength is critical to part lifetime in pressurized gas sealing applications such as O-rings, where weak binding between the filler particle and polymer matrix can lead to internal void structures. With the aim to build a fundamental understanding of precursors to pressurized hydrogen-induced failure in elastomers, we use all-atom molecular dynamics simulations to study the impact of hydrogen oversaturation on filler-polymer interaction strength. We systematically study the interface between a commonly used elastomer, ethylene-propylene-diene monomer (EPDM) and silica by varying gas concentration, crosslink density, and surface chemistry. Our simulations predict that decompression leads to a localization of excess gas near the interface. In conclusion, we demonstrate that this localized gas can weaken interfacial adhesion and quantify the interaction using thermodynamic approaches.

EPDM

Measuring thermal curing induced shrinkage of material extrusion based additive manufacturing silicone elastomer lattices by X-ray computed tomography

Thermal curing induces shrinkage in material extrusion based additive manufacturing silicone elastomer samples, resulting in discrepancies between as printed and final geometries. Knowing the extent to which the samples change in shape and size allows us to make appropriate modifications to the printing design to better control the geometry of the samples. We present an X-ray computed tomography (CT) based approach to determine filament-level shrinkage due to thermal curing of silicone elastomer samples printed with direct ink writing (DIW). The approach relies on custom-designed build plates that are resistant to the elevated curing temperatures and that have sufficiently distinct X-ray absorption characteristics from the silicone elastomer to ensure adequate segmentation of the latter in X-ray imaging data. We implement the approach to evaluate shrinkage in DIW ‘log pile’ samples with three distinct strand arrangements and demonstrate of how filament-level information can be extracted from the X-ray CT data.

Additive manufacturing