At least 37 records · Page 2

Spiral Orbit Tribometry: Evaluation of Three Liquid Lubricants in Vacuum - 2

The coefficients of friction and relative degradation rates of three lubricants run in the boundary regime in vacuum are evaluated in a Spiral Orbit Tribometer. This tribometer subjected the lubricants to rolling contact conditions similar to those found in angular contact ball bearings. A multiply alkylated cyclopentane (MAC) hydrocarbon lubricant suffered degradation at a rate almost two orders of magnitude less than the degradation rate of two perfluoropolyalkylether (PFPE) lubricants.

Pepper, Stephen V.↗

The ball bearing as a rheological test device

An angular-contact ball bearing provides an easily obtainable, precise mechanical system for rheological tests on thin films under high pressure. The test conditions are by definition similar to those found in practice. Accessible independent variables include size, pressure, bulk temperature, roughness, adsorbed surfactant, fluid type, fluid quantity, fluid supply rate, film thickness, entrainment velocity, transit time, and combined strain. Easily measured or inferred variables include slip, changes in film thickness with time (transients), strain rate, lubricant elastic modulus (thin film, high pressure), tractive force, lubricant chemical degradation rate, and lubricant degradation product. Methods for setting and obtaining these quantities in a bearing are discussed, together with experimental limitations on them.

Kingsbury, E.↗

Nonmetallic materials handbook. Volume 2: Epoxy and silicone materials

Chemical and physical property test data obtained during qualification and receiving inspection testing of nonmetallic materials for the Viking Mars Lander program is presented. Thermochemical data showing degradation as a function of temperature from room temperature through 773 K is included. These data include activation energies for thermal degradation, rate constants, and exo- and/or endotherms. Thermal degradations carried out under vacuum include mass spectral data taken simultaneously during the decomposition. Many materials have supporting data such as condensation rates of degassed products and isothermal weight loss. Changes in mechanical, electrical, and thermal properties after exposure to 408 K in nitrogen for times ranging from 380 to 570 hours are included for many materials.

Podlaseck, S. E.↗

Evaluation of Commercial Automotive-Grade BME Capacitors

Three Ni-BaTiO3 ceramic capacitor lots with the same specification (chip size, capacitance, and rated voltage) and the same reliability level, made by three different manufacturers, were degraded using highly accelerated life stress testing (HALST) with the same temperature and applied voltage conditions. The reliability, as characterized by mean time to failure (MTTF), differed by more than one order of magnitude among the capacitor lots. A theoretical model based on the existence of depletion layers at grain boundaries and the entrapment of oxygen vacancies has been proposed to explain the MTTF difference among these BME capacitors. It is the conclusion of this model that reliability will not be improved simply by increasing the insulation resistance of a BME capacitor. Indeed, Ni-BaTiO3 ceramic capacitors with a smaller degradation rate constant K will always give rise to a longer reliability life

capacitor↗

Evaluation of Commercial Automotive-Grade BME Capacitors

Three Ni-BaTiO3 ceramic capacitor lots with the same specification (chip size, capacitance, and rated voltage) and the same reliability level, made by three different manufacturers, were degraded using highly accelerated life stress testing (HALST) with the same temperature and applied voltage conditions. The reliability, as characterized by mean time to failure (MTTF), differed by more than one order of magnitude among the capacitor lots. A theoretical model based on the existence of depletion layers at grain boundaries and the entrapment of oxygen vacancies has been proposed to explain the MTTF difference among these BME capacitors. It is the conclusion of this model that reliability will not be improved simply by increasing the insulation resistance of a BME capacitor. Indeed, Ni-BaTiO3 ceramic capacitors with a smaller degradation rate constant K will always give rise to a longer reliability life.

reliability↗

Study of toluene stability for an Organic Rankine Cycle (ORC) space-based power system

The design, fabrication, assembly, and endurance operation of a dynamic test loop, built to evaluate the thermal stability of a proposed Organic Rankine Cycle (ORC) working fluid, is discussed. The test fluid, toluene, was circulated through a heater, simulated turbine, regenerator, condenser and pump to duplicate an actual ORC system. The maximum nominal fluid temperature, 750 F, was at the turbine simulator inlet. Samples of noncondensible gases and liquid toluene were taken periodically during the test. The samples were analyzed to identify the degradation products formed and the quantity of these products. From these data it was possible to determine the degradation rate of the working fluid and the generation rate of noncondensible gases. A further goal of this work was to relate the degradation observed in the dynamic operating loop to degradation obtained in isothermal capsule tests. This relationship was the basis for estimating the power loop degradation in the Space Station Organic Rankine Cycle system.

Havens, Vance↗

Dust Abrasion Damage on Martian Solar Arrays: Experimental Investigation and Opportunity Rover Performance Analysis

Here we investigate the effects of erosion and weathering that occur on III-V cover-glass interconnected cells (CICs) after exposure to Mars dust storm conditions. The durability of these materials in a Martian environment is not well characterized so we perform analogous experimentation. To replicate the dust impingement, test coupons were placed in an enclosure and sandblasted with Mars dust simulant. We show the J-V response dependency on both incident angle and exposure times. We find that the simulated Martian dust storm often results in damage to the anti-reflective coating and subsequent reduced short circuit current. Reduction in the open circuit voltage is observed, likely caused by structural damage to the crystal lattice after CIC fracture. We employ data-driven modeling to determine a performance degradation rate that is consistent with zero within uncertainty. We also quantify the soiling contribution and power degradation of the photovoltaic cells on Mars through analysis of 4.95 Martian years of report-out power conditions from the Opportunity rover. We find that atmospheric dust suspended due to a weather event does not result in instantaneous settled dust on the PV cells. We calculate via autocorrelation function that the dust settling rate is approximately 21 Sols from atmospheric dust suspension. The findings presented here deliver a realistic approximation for the insolation values and subsequent PV power expected over time on the Martian surface thus informing future dust abatement systems.

McMillon-Brown, Lyndsey↗

Dust Abrasion Damage on Martian Solar Arrays: Experimental Investigation and Opportunity Rover Performance Analysis

Here we investigate the effects of erosion and weathering that occur on III-V cover-glass interconnected cells (CICs) after exposure to Mars dust storm conditions. The durability of these materials in a Martian environment is not well characterized so we perform analogous experimentation. To replicate the dust impingement, test coupons were placed in an enclosure and sandblasted with Mars dust simulant. We show the J-V response dependency on both incident angle and exposure times. We find that the simulated Martian dust storm often results in damage to the anti-reflective coating and subsequent reduced short circuit current. Reduction in the open circuit voltage is observed, likely caused by structural damage to the crystal lattice after CIC fracture. We employ data-driven modeling to determine a performance degradation rate that is consistent with zero within uncertainty. We also quantify the soiling contribution and power degradation of the photovoltaic cells on Mars through analysis of 4.95 Martian years of report-out power conditions from the Opportunity rover. We find that atmospheric dust suspended due to a weather event does not result in instantaneous settled dust on the PV cells. We calculate via autocorrelation function that the dust settling rate is approximately 21 Sols from atmospheric dust suspension. The findings presented here deliver a realistic approximation for the insolation values and subsequent PV power expected over time on the Martian surface thus informing future dust abatement systems.

McMillon-Brown, Lyndsey↗

Maximum Sample Temperature for Mars Sample Return: A Historical Perspective

Since the first Mars Sample Return (MSR) report published by the Jet Propulsion Laboratory (JPL) in 1974 [1], a series of panels, reports, and white papers have recognized the importance of sample temperature and offered an informed sample maximum temperature (henceforth SMT) limit for returning martian samples to Earth. The Mars Sample Handling and Requirements Panel (MSHARP, 1999) stated that "[t]he main issue in sample preservation is temperature" [2]. More recently, the Mars Exploration Program Analysis Group (MEPAG)'s "Science Priorities for Mars Sample Return" report (2008), declared that "[s]ignificant loss, particularly to biological studies, occurs if samples reach +50C for three hours", whereby "scientific objectives related to life goals could be seriously compromised" [3]. By contrast, the Mars 2020 mission has adopted a SMT of +60C as spelled out in Beaty et al., 2016 [4]. Samples will be collected and then deposited on the surface in sealed tubes for possible retrieval and return to Earth. Beaty et al. [4] calculates that the samples will experience maximum temperatures of ~+30 to +60C, depending on latitude. At present, there is no mission requirement for the measurement/data logging of sample temperature during this period. We will explore the history of martian SMTs, as they have been recorded since 1974 [1], effectively representing input across multiple generations of Mars scientists. Ten separate publications present SMTs for MSR samples [1-10]. One report [10] is for a mission concept specifically designed to exclude life detection investigations, and recommended an SMT of 50C. Another did not specify a temperature, recommending "Mars ambient temperature" [5]. Of the remaining eight, SMTs are given as: -30C [1], -20C [3], 60C [4], -73 to 41C depending on sample type [6], -40C [7], -43 to 13C depending on type [2,8], and -33C [9]. If we restrict the temperatures to samples highlighted in the Mars 2020 mission goals, i.e. organics-bearing and sedimentary rocks, then the average SMT is -28+/-39C (n=8). Applying a Dixon's Q Test at P=0.05 (two-tailed), the 60C SMT [4] fails with Q=0.602 versus Qcrit=0.526. Excluding the outlier produces an average SMT of -40+/-17C (n=7). Therefore, the average SMT expressed by the Mars science community over the past 44 years (two generations) is a sample temperature no greater than -40C. The difference in chemical reaction rates between this average SMT and Beaty et al [4] can be estimated using the Arrhenius equation. Assuming a generic chemical reaction with an activation energy of 50 kJ/mol and a pre-exponential factor invariant with temperature, this reaction will proceed 2300x faster at 60C than at -40C. To illustrate the effects of the increased reaction rate, consider 10 ppb of alanine in a Mars 2020 cache, and assume that it becomes unmeasurable if it degrades to 1 ppb, as per the Mars 2020 Organic Contamination Panel contamination limits [11]. If we illustrate the effect with an arbitrary degradation rate such that the alanine will become undetectable in ten years at -40C, then the same 10 ppb alanine degrades beyond detectability in only 38 days at 60C. Further research is required to quantify expected analyte losses in the cached samples due to thermal processing.

Fries, Marc↗

Bioreactor perfusion system for the long-term maintenance of tissue-engineered skeletal muscle organoids

Three-dimensional skeletal muscle organ-like structures (organoids) formed in tissue culture by fusion of proliferating myoblasts into parallel networks of long, unbranched myofibers provide an in vivo-like model for examining the effects of growth factors, tension, and space flight on muscle cell growth and metabolism. To determine the feasibility of maintaining either avian or mammalian muscle organoids in a commercial perfusion bioreactor system, we measured metabolism, protein turnover. and autocrine/paracrine growth factor release rates. Medium glucose was metabolized at a constant rate in both low-serum- and serum-free media for up to 30 d. Total organoid noncollagenous protein and DNA content decreased approximately 22-28% (P < 0.05) over a 13-d period. Total protein synthesis rates could be determined accurately in the bioreactors for up to 30 h and total protein degradation rates could be measured for up to 3 wk. Special fixation and storage conditions necessary for space flight studies were validated as part of the studies. For example, the anabolic autocrine/paracrine skeletal muscle growth factors prostaglandin F2alpha (PGF2alpha) and insulin-like growth factor-1 (IGF-1) could be measured accurately in collected media fractions, even after storage at 37 degrees C for up to 10 d. In contrast, creatine kinase activity (a marker of cell damage) in collected media fractions was unreliable. These results provide initial benchmarks for long-term ex vivo studies of tissue-engineered skeletal muscle.

NASA Discipline Musculoskeletal↗

Topics in electrochemical degradation of photovoltaic modules

Electrochemical degradation of photovoltaic modules was examined. It is found that the extent of electrochemical damage is dependent on the integrated leakage current. The PV electrochemical degradation mechanisms in the two polarities are different: (1) degradation rates in the two polarities are of the same order of magnitude; (2) center tapped grounded arrays are a preferred system configuration to minimize electrochemical degradation. The use of thicker pottant layers and polymer substrate films to reduce equilibrium leakage current values is suggested. A metallized substrate layer, if used, should be isolated from the pottant and the frame by polyester layers, and EVA modules appear to be consistent with 30 year life allocation levels for electrochemical damage. Temperature acceleration factors are well behaved and moderately well understood; humidity acceleration factors vary radically with module construction and materials and require additional research.

Mon, G. R.↗

Growth factor involvement in tension-induced skeletal muscle growth

Long-term manned space travel will require a better understanding of skeletal muscle atrophy which results from microgravity. Astronaut strength and dexterity must be maintained for normal mission operations and for emergency situations. Although exercise in space slows the rate of muscle loss, it does not prevent it. A biochemical understanding of how gravity/tension/exercise help to maintain muscle size by altering protein synthesis and/or degradation rate should ultimately allow pharmacological intervention to prevent muscle atrophy in microgravity. The overall objective is to examine some of the basic biochemical processes involved in tension-induced muscle growth. With an experimental in vitro system, the role of exogenous and endogenous muscle growth factors in mechanically stimulated muscle growth are examined. Differentiated avian skeletal myofibers can be 'exercised' in tissue culture using a newly developed dynamic mechanical cell stimulator device which simulates different muscle activity patterns. Patterns of mechanical activity which significantly affect muscle growth and metabolic characteristics were found. Both exogenous and endogenous growth factors are essential for tension-induced muscle growth. Exogenous growth factors found in serum, such as insulin, insulin-like growth factors, and steroids, are important regulators of muscle protein turnover rates and mechanically-induced muscle growth. Endogenous growth factors are synthesized and released into the culture medium when muscle cells are mechanically stimulated. At least one family of mechanically induced endogenous factors, the prostaglandins, help to regulate the rates of protein turnover in muscle cells. Endogenously synthesized IGF-1 is another. The interaction of muscle mechanical activity and these growth factors in the regulation of muscle protein turnover rates with our in vitro model system is studied.

Vandenburgh, Herman H.↗

Non-gassing nickel-cadmium battery electrodes and cells

Supposedly long-lived nickel-cadmium batteries often fail due to severe gassing on charge. In order to increase the lives of such cells attempts are being made to construct nongassing positive and negative electrodes. The gassing characteristics of both electrodes in negative limited cells were determined as a function of charge rate, charge temperature, and loading. Cycle life tests, up to 70 cycles, of some of the cells show they operate in a nongassing manner with very low degradation rates.

Luksha, E.↗

Reliability Issues with PME and BME Ceramic Capacitors

This work is a review of reliability issues specific for low-voltage precious metal electrode (PME) and base metal electrode (BME) multilayer ceramic capacitors (MLCC). A special attention is given to degradation and failures in capacitors with defects, in particular with cracks. Temperature and voltage reliability acceleration factors have been calculated based on approximation of distributions of degradation rates of leakage currents using a general log-linear Weibull model. Results show a substantial difference in behavior of BME and PME capacitors with defects. Mechanisms of degradation and failures in humid and dry environments and risks of overstressing capacitors during highly accelerated life testing (HALT) are discussed.

Teverovsky, Alexander↗

Vacuum and ultraviolet radiation effects on binders and pigments for spacecraft thermal control coatings

An evaluation of several silicone resin binders and powdered inorganic pigments for potential use in spacecraft thermal-control paint formulations is presented. The pigments were selected on the basis of a hypothesis relating the heat of formation of a compound to the compound's resistance to ultra-radiation-induced degradation. Reflectance measurements were made in situ to determine degradation rates due to ultraviolet radiation. The tested polydimethylsiloxane resins were not significantly affected by long exposures to ultraviolet radiation. All the pigments, which were dispersed in a polydimethylsiloxane resin, were degraded by ultraviolet radiation as determined by an increase of solar absorptance. For the materials evaluated in this study, no evidence was found to indicate that pigments with high heats of formation were resistant to ultraviolet degradation.

Progar, D. J.↗

Interference susceptibility measurements for an MSK satellite communication link

The results are presented of measurements of the degradation of an MSK satellite link due to modulated and CW (unmodulated) interference. These measurements were made using a hardware based satellite communication link simulator at NASA-Lewis. The results indicate the amount of bit error rate degradation caused by CW interference as a function of frequency and power level, and the degradation caused by adjacent channel and cochannel modulated interference as a function of interference power level. Results were obtained for both the uplink case (including satellite nonlinearity) and the downlink case (linear channel).

Kerczewski, Robert J.↗

Interference susceptibility measurements for an MSK satellite communication link

The results are presented of measurements of the degradation of an MSK satellite link due to modulated and CW (unmodulated) interference. These measurements were made using a hardware based satellite communication link simulator at NASA-Lewis. The results indicate the amount of bit error rate degradation caused by CW interference as a function of frequency and power level, and the degradation caused by adjacent channel and cochannel modulated interference as a function of interference power level. Results were obtained for both the uplink case (including satellite nonlinearity) and the downlink case (linear channel).

Kerczewski, Robert J.↗