Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “DPA”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

[Redesign of the Spacesuit Long Life Battery and the Personal Life Support System Battery]

This fall I was working on two different projects that culminated into a redesign of the spacesuit LLB (long life battery). I also did some work on the PLSS (personal life support system) battery with EC. My first project was redlining the work instruction for completing DPAs (destructive physical analysis) on battery cells in the department. The purpose of this document is to create a standard process and ensure that the data in the same way no matter who carries out the analysis. I observed three DPAs, conducted one with help, and conducted two on my own all while taking notes on the procedure. These notes were used to write the final work instruction that will become is the department standard. My second project continued the work of the summer co-op before me. I was testing aluminum heat sinks for their ability to provide good thermal conduction and structural support during a thermal runaway event. The heat sinks were designed by the summer intern but there was not much time for testing before he left. We ran tests with a heater on the bottom of a trigger cell to try to drive thermal runaway and ensure that it will not propagate to adjacent cells. We also ran heat-to-vent tests in an oven to see if the assembly provided structural support and prevented sidewall rupture during thermal runaway. These tests were carried out at ESTA (energy systems test area) and are providing very promising results that safe, high performing (greater than 180 Wh/kg) designs are possible. My main project was a redesign of the LLB battery. Another summer intern did some testing and concluded that there was no simple fix to mitigate thermal runaway propagation hazards in the current design. The only option was a clean sheet redesign of the battery. I was given a volume and ideal energy density and the rest of the design was up to me. First, I created new heat sink banks in Creo using the information gathered in the metal heat sink tests from the summer intern. After this, I made capture plates to hold the cells in place and I worked on nickel bussings for the electrical connections between the cells. Finally, I designed the test box enclosure that included sections for flame arresting materials. The battery brick design, which is the heart of the battery, promises to become the first for a manned spacecraft application to achieve greater than 180 Wh/kg. My work in redlining the DPA work instructions will also be used in selecting the cells for the battery. We had a few options of cells that would provide the necessary power output and needed to make a choice. We repeatedly charged and discharged cells for around a month until they went through 100 lifecycles. The plan is to compare the DPA results on fresh and cycled cells from each manufacturer to see if cycling introduces any differences. After the complete LLB design was approved, the parts were ordered and testing should begin the first week of December. Some of my side projects included working on the CAD data for the PLSS with EC and attending the NASA Aerospace Battery Workshop in Huntsville. I was also a member of the Tours and Lectures Committee for the USRA and Pathways interns. I coordinated Apollo Evening and was on the committee for touring KSC and seeing an Atlas 5 launch. I really enjoyed my time at JSC and I would like to continue working for NASA or another aerospace company in the future. I have worked other internships prior to this, but I think the heavy research and development focus is the best fit for me. I originally thought I would need to go to grad school to work in an environment like this, but I now see it is possible with a bachelor’s degree and hard work. I would like to go into the workforce and maybe continue my education with night classes.

Scharf, Stephanie↗

Development of standardized specifications for screening space level integrated circuits and semiconductors

Standardized methods are established for screening of JAN B microcircuits and JANTXV semiconductor components for space mission or other critical applications when JAN S devices are not available. General specifications are provided which outline the DPA (destructive physical analysis), environmental, electrical, and data requirements for screening of various component technologies. This standard was developed for Air Force Space Division, and is available for use by other DOD agencies, NASA, and space systems contractors for establishing common screening methods for electronic components.

Source record↗

Oligomerization reactions of deoxyribonucleotides on montmorillonite clay - The effect of mononucleotide structure on phosphodiester bond formation

The formation of oligomers from deoxynucleotides, catalyzed by Na(+)-montmorillonite, was investigated with special attention given to the effect of the monomer structure on the phosphodiester bond formation. It was found that adenine deoxynucleotides bind more strongly to montmorillonite than do the corresponding ribonucleotides and thymidine nucleotides. Tetramers of 2-prime-dpA were detected in the reaction of 2-prime-d-5-prime-AMP with a water-soluble carbodiimide EDAC in the presence of Na(+)-montmorillonite, illustrating the possible role of minerals in the formation of biopolymers on the primitive earth.

Ferris, James P.↗

Destructive physical analysis results of Ni/H2 cells cycled in LEO regime

Six 48-Ah individual pressure vessel (IPV) Ni/H2 cells containing 26 and 31 percent KOH electrolyte were life cycle tested in low Earth orbit. All three cells containing 31 percent KOH failed (3729, 4165, and 11,355 cycles), while those with 26 percent KOH were cycled over 14,000 times in the continuing test. Destructive physical analysis (DPA) of the failed cells included visual inspections, measurements of electrode thickness, scanning electron microscopy, chemical analysis, and measurements of nickel electrode capacity in an electrolyte flooded cell. The cycling failure was due to a decrease of nickel electrode capacity. As possible causes of the capacity decrease, researchers observed electrode expansion, rupture, and corrosion of the nickel electrode substrate, active material redistribution, and accumulation of electrochemically undischargeable active material with cycling.

Lim, Hong S.↗

Report of investigations into charge cadmium reactivity: Nickel-cadmium cell ESD 91-86

In Aug. 1990, a presentation was given at the 25th Ann. IECEC meeting on the results of Destructive Physical Analysis (DPA) on two successive sets of Ni-Cd cells. The cells were of two different separator types, Pellon 2505 and 2536. One cell of each separator type was analyzed on two occasions; the first pair were analyzed to establish baseline data on essentially new cells; the second pair were analyzed after the cells had been on charge-discharge cycling for a year in connection with a satellite simulation study. The gas composition found in the cells, the absence of charged cadmium in the analytical data, and the appearance of dried out portions on the Cd plates in the one year cell S/N 7 which used Pellon 2505 as its separator material, were questions which arose. These concerns are answered and the observational results are clarified.

Lewis, Harlan L.↗

Destructive physical analysis results of Ni/H2 cells cycled in LEO regime

Six 48-Ah individual pressure vessel (IPV) Ni/H2 cells containing 26 and 31 percent KOH electrolyte were life cycle tested in low earth orbit. All three cells containing 31 percent KOH failed (3729, 4165, and 11,355 cycles), while those with 26 percent KOH were cycled over 14,000 times in the continuing test. Destructive physical analysis (DPA) of the failed cells included visual inspections, measurements of electrode thickness, scanning electron microscopy, chemical analysis, and measurements of nickel electrode capacity in an electrolyte flooded cell. The cycling failure was due to a decrease of nickel electrode capacity. As possible causes of the capacity decrease, researchers observed electrode expansion, rupture, and corrosion of the nickel electrode substrate, active material redistribution, and accumulation of electrochemically undischargeable active material with cycling.

Lim, Hong S.↗

Special tests and destructive physical analyses as used by the Aerospace Corporation with nickel-hydrogen cells

The destructive physical analysis (DPA) of electrochemical devices is an important part of the overall test. Specific tests were developed to investigate the degradation mode or the failure mechanism that surfaces during the course of a cell being assembled, acceptance tested, and life-cycle tested. The tests that have been developed are peculiar to the cell chemistry under investigation. Tests are often developed by an individual or group of researchers as a result of their particular interest in an unresolved failure mechanism or degradation mode. A series of production, operational, and storage issues that were addressed by the Electrochemistry Group at The Aerospace Corporation are addressed. As a result of these investigations, as well as associated research studies carried out to develop a clearer understanding of the nickel oxyhydroxide electrode, a series of unique and useful specialized tests were developed. Some of these special tests were assembled to describe the methods that were found to be particularly useful in resolving a wide spectrum of manufacturing, operational, and storage issues related to nickel-hydrogen cells. The general methodology of these tests is given here with references listed to provide the reader with a more detailed understanding of the tests. The tests are classified according to the sequencing, starting with the impregnation of the nickel plaque material and culminating with the storage of completed cells. The details of the wet chemical procedures that were found to be useful because of their accuracy and reproducibility are given. The equations used to make the appropriate calculations are listed.

Zimmerman, A. H.↗

Analysis for nickel (3 and 4) in positive plates from nickel-cadmium cells

The NASA-Goddard procedure for destructive physical analysis (DPA) of nickel-cadmium cells contains a method for analysis of residual charged nickel as NiOOH in the positive plates at complete cell discharge, also known as nickel precharge. In the method, the Ni(III) is treated with an excess of an Fe(II) reducing agent and then back titrated with permanganate. The Ni(III) content is the difference between Fe(II) equivalents and permanganate equivalents. Problems have arisen in analysis at NAVSURFWARCENDIV, Crane because for many types of cells, particularly AA-size and some 'space-qualified' cells, zero or negative Ni(III) contents are recorded for which the manufacturer claims 3-5 percent precharge. Our approach to this problem was to reexamine the procedure for the source of error, and correct it or develop an alternative method.

Lewis, Harlan L.↗

Destructive Physical Analysis of Flight- and Ground-Tested Sodium-Sulfur Cells

Destructive physical analysis (DPA) was used to study the effects of microgravity on the sulfur electrode in sodium-sulfur cells. The cells examined in this work were provided by the Air Force Research Laboratory (AFRL) from their program on sodium-sulfur technology. The Naval Research Laboratory (NRL) provided electrical characterization of the flight-tested and ground-tested cells.

Wasz, Margot L.↗

NIST Efforts to Quality-Assure Gunpowder Measurements

In the past few years, the National Institute for Standards and Technology (NIST) has been promoting the idea of quantitatively determining the additives in smokeless gunpowder using micellar capillary electrophoresis as a means of investigating the criminal use of hand guns and pipe bombs. As a part of this effort, we have evaluated both supercritical fluid and ultrasonic solvent extractions for the quantitative recovery of nitroglycerin (NG), diphenylamine (DPA), N-nitrosodiphenylamine (NnDPA), and ethyl centralite (EC) from gunpowder. Recoveries were evaluated by repeat extraction and matrix spiking experiments. The final extraction protocol provides greater than 95 percent recoveries. To help other researches validate their own analytical method for additive determinations, NIST is exploring the development of a standard reference material, Additives in Smokeless Gunpowder. The evaluated method is being applied to two double-base (NG-containing) powders, one stabilized with diphenylamine and the other with ethyl centralite. As part of this reference material development effort, we are conducting an interlaboratory comparison exercise among the forensic and military gunpowder measurement community.

MacCrehan, William A.↗

COTS Ceramic Chip Capacitors: An Evaluation of the Parts and Assurance Methodologies

This viewgraph presentation profiles an experiment to evaluate the suitability of commercial off-the-shelf (COTS) ceramic chip capacitors for NASA spaceflight applications. The experiment included: 1) Voltage Conditioning ('Burn-In'); 2) Highly Accelerated Life Test (HALT); 3) Destructive Physical Analysis (DPA); 4) Ultimate Voltage Breakdown Strength. The presentation includes results for each of the capacitors used in the experiment.

Sampson, Michael J.↗

Current methods and advances in bone densitometry

Bone mass is the primary, although not the only, determinant of fracture. Over the past few years a number of noninvasive techniques have been developed to more sensitively quantitate bone mass. These include single and dual photon absorptiometry (SPA and DPA), single and dual X-ray absorptiometry (SXA and DXA) and quantitative computed tomography (QCT). While differing in anatomic sites measured and in their estimates of precision, accuracy, and fracture discrimination, all of these methods provide clinically useful measurements of skeletal status. It is the intent of this review to discuss the pros and cons of these techniques and to present the new applications of ultrasound (US) and magnetic resonance (MRI) in the detection and management of osteoporosis.

Review, Academic↗

Quantitative computed tomography for spinal mineral assessment: current status

Quantitative CT (QCT) is an established method for the noninvasive assessment of bone mineral content in the vertebral spongiosum and other anatomic locations. The potential strengths of QCT relative to dual photon absorptiometry (DPA) are its capability for precise three-dimensional anatomic localization providing a direct density measurement and its capability for spatial separation of highly responsive cancellous bone from less responsive cortical bone. The extraction of this quantitative information from the CT image, however, requires sophisticated calibration and positioning techniques and careful technical monitoring.

Lumbar Vertebrae/radiography↗

Light Weight Design Nickel-Alkaline Cells Using Fiber Electrodes

Using fiber electrode technology, currently produced by Bekaert Corporation (Bekaert), Electro Energy, Inc., (EEI) Mobile Energy Products Group (formerly, Eagle-Picher Technologies, LLC., Power Systems Department) in Colorado Springs, CO has demonstrated that it is feasible to manufacture flight weight nickel-hydrogen cells having about twice the specific energy (80 vs. 40 watt-hr/kg) as state-of-the-art nickel-hydrogen cells that are flown on geosynchronous communications satellites. Although lithium-ion battery technology has made large in-roads to replace the nickel-alkaline technology (nickel-cadmium, nickel-metal hydride), the technology offered here competes with lithium-ion weight and offers alternatives not present in the lithium-ion chemistry such as ability to undergo continuous overcharge, reversal on discharge and sustain rate capability sufficient to start automotive and aircraft engines at subzero temperatures. In development to date seven 50 ampere-hour nickel-hydrogen have been constructed, acceptance tested and briefly tested in a low earth orbit (LEO) cycle regime. The effort was jointly funded by Electro Energy, Inc. and NASA Glenn Research Center, Cleveland, OH. Five of the seven cells have been shipped to NASA GRC for further cycle testing. Two of the cells experienced failure due to internal short circuits during initial cycle testing at EEL Destructive Physical Analysis (DPA) of one of the cells has shown the failure mode to be due to inadequate hydrogen catalyst electrodes that were not capacity balanced with the higher energy density nickel oxide electrodes. In the investigators opinion, rebuild of the cells using proper electrode balance would result in cells that could sustain over 30,000 cycles at moderate depths-of-discharge in a LEO regime or endure over 20 years of geosynchronous orbit (GEO) cycling while realizing a two-fold increase in specific energy for the battery or a 1.1 kg weight savings per 50 ampere-hour cell. Additional information is included in the original extended abstract.

Pickett, David F.↗

Status of JPL Li-Ion Cell Development Program

None given. This is a series of viewgraphs from a visual presentation to the workshop. From outline: JPL program overview; low temperature studies; cycle life studies; destructive physical analysis (DPA) of cycled cells; prototype cell development; summary of accomplishment.

JPL LI-Ion Program low temperature studies cycle l↗

Reliability Evaluation of Au/Al Wire Bonds in Commercial Microcircuits

The slide presentation provides an overview of research related to problems in quality evaluation in the mechanisms of wire bond degradation. Case studies presented examine the evaluation of reliability of hermetic and plastic microcircuits with suspected poor wire bonding. The authors conclude that in the cases when destructive physical analysis (DPA) or design evaluation indicate possible problems with wire bonding, a wire bond qualification testing may be required. This test should include high temperature storage (175 degrees C to 200 decrees C) of the parts with periodic measurements of contact resistances followed by internal examination and wire pull or ball sear testing.

Teverovsky, Alexander↗

Apparatus and method for automated monitoring of airborne bacterial spores

An apparatus and method for automated monitoring of airborne bacterial spores. The apparatus is provided with an air sampler, a surface for capturing airborne spores, a thermal lysis unit to release DPA from bacterial spores, a source of lanthanide ions, and a spectrometer for excitation and detection of the characteristic fluorescence of the aromatic molecules in bacterial spores complexed with lanthanide ions. In accordance with the method: computer-programmed steps allow for automation of the apparatus for the monitoring of airborne bacterial spores.

Ponce, Adrian↗

Li-Ion Batteries for Space Applications: High Specific Energy and Wide-Operating Temperature

Compared to the conventional Ni-Co oxides (with or without AI additions), the NMC (1/3:1/3:1/3) cathode provides marginal improvement in specific capacity. However, some of the formulations based on the solid solutions of layered Li2Mn03 and LiM02 (M = Mn0.5Ni0.5} have shown capacities as high as 250 mAh/g, combined with high cell voltages (4.5 V) and with the likelihood of enhanced thermal stability. Multi-component electrolytes with low EC-proportions and selected co-solvents provide significant improvement in the low temperature performance, down to -60 C, combined with the non-flammable attribute from the co-solvents. The NMC cathode shows good compatibility with the carbonate-based low temperature electrolytes. Impressive performances have been realized at low temperatures of <= 30 C. Electrolytes with high salt concentration and high EC content fare well at room temperatures, while the formulations with low EC content and low salt concentration are preferred at low temperatures. DPA studies reveal increased SEI growth on the electrodes, especially anode, upon irradiation. Performance of low temperature electrolytes in prototype cells corroborate the findings from laboratory cells.

storage↗