Quad- Chart - Development of Ultra Dense Edge Interconnects for Die to Die Connections Based on Immersion Solder Bridging.
Abstract not provided.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
The goal of this project was to study the combined effects of die design, proper internal cooling and efficient die lubricants on die life. The project targeted improvements in die casting insert life by: Optimized Die Design for Reduced Surface Temperature: The life of die casting dies is significantly shorter when the die is exposed to elevated temperature for significant periods of time. Any die operated under conditions leading to surface temperature in excess of 1050oF undergoes structural changes that reduce its strength. Optimized die design can improve die life significantly. This improvement can be accomplished by means of cooling lines, baffles and bubblers in the die. A key objective of the project was to establish criteria for the minimal distance of the cooling lines from the surface. This effort was supported with alloys and machining by BohlerUddeholm, Dunn Steel, HH Stark and Rex Buckeye. In plant testing and evaluation was conducted as in-kind cost share at St. Clair Die Casting. The Uddeholm Dievar steel evaluated in this program showed superior resistance to thermal fatigue resistance. Based on the experimental evidence, cooling lines could be placed as close as 0.5"Â from the surface. Die Life Extension by Optimized Die Lubrication: The life of die casting dies is affected by additions made to its surface with the proper lubricants. These lubricants will protect the surface from the considerable temperature peaks that occur when the molten melt enters the die. Dies will reach a significantly higher temperature without this lubricant being applied. The amount and type of the lubricant are critical variables in the die casting process. However, these lubricants must not corrode the die surface. This effort was supported with alloys and machining by BohlerUddeholm, Dunn Steel, HH Stark and Rex Buckeye. In plant testing and evaluation was conducted as in-kind cost share at St. Clair Die Casting. Chem- Trend participated in the program with die lubricants and technical support. Experiments conducted with these lubricants demonstrated good protection of the substrate steel. Graphite and boron nitride used as benchmarks are capable of completely eliminating soldering and washout. However, because of cost and environmental considerations these materials are not widely used in industry. The best water-based die lubricants evaluated in this program were capable of providing similar protection from soldering and washout. In addition to improved part quality and higher production rates, improving die casting processes to preserve the life of the inserts will result in energy savings and a reduction in environmental wastes. Improving die life by means of optimized cooling line placement, baffles and bubblers in the die will allow for reduced die temperatures during processing, saving energy associated with production. The utilization of optimized die lubricants will also reduce heat requirements in addition to reducing waste associated with soldering and washout. This new technology was predicted to result in an average energy savings of 1.1 trillion BTU's/year over a 10 year period. Current (2012) annual energy saving estimates, based on commercial introduction in 2010, a market penetration of 70% by 2020 is 1.26 trillion BTU's/year. Along with these energy savings, reduction of scrap and improvement in casting yield will result in a reduction of the environmental emissions associated with the melting and pouring of the metal which will be saved as a result of this technology. The average annual estimate of CO2 reduction per year through 2020 is 0.025 Million Metric Tons of Carbon Equivalent (MM TCE).
An elevated temperature forming die apparatus comprising a lower die part having a first upper surface positioned to engage a lower surface of a first region of such a workpiece, an upper die part supported for reciprocal motion relative to the lower die part, the upper die part having a lower surface that engages an upper surface of a second region of a sheet material workpiece, heaters in thermal communication with the die parts, and a third die part having an upper surface that engages a lower surface of the second region of a sheet material workpiece whose first portion is positioned between the upper and lower die parts, the third die part being supported for reciprocal motion relative to the upper die part such that closure of the upper die part along the first stroke portion against the third die part will clamp the first portion of the workpiece between the upper and third die parts, and the third die part being supported for reciprocal motion relative to the lower die part such that, once the first portion of a workpiece has been clamped between the upper and third die parts a draw region of the workpiece extending adjacent an interface between the first and second portions of the workpiece can be drawn by displacing the lower die part relative to the clamped-together upper and third die parts along a second portion of the die set stroke.
As a net shape process, die casting is intrinsically efficient and improvements in energy efficiency are strongly dependent on design and process improvements that reduce scrap rates so that more of the total consumed energy goes into acceptable, usable castings. A casting that is distorted and fails to meet specified dimensional requirements is typically remelted but this still results in a decrease in process yield, lost productivity, and increased energy consumption. This work focuses on developing, and expanding the use of, computer modeling methods that can be used to improve the dimensional accuracy of die castings and produce die designs and machine/die setups that reduce rejection rates due to dimensional issues. A major factor contributing to the dimensional inaccuracy of the casting is the elastic deformations of the die cavity caused by the thermo mechanical loads the dies are subjected to during normal operation. Although thermal and die cavity filling simulation are widely used in the industry, structural modeling of the die, particularly for managing part distortion, is not yet widely practiced. This may be due in part to the need to have a thorough understanding of the physical phenomenon involved in die distortion and the mathematical theory employed in the numerical models to efficiently model the die distortion phenomenon. Therefore, two of the goals of this work are to assist in efforts to expand the use of structural modeling and related technologies in the die casting industry by 1) providing a detailed modeling guideline and tutorial for those interested in developing the necessary skills and capability and 2) by developing simple meta-models that capture the results and experience gained from several years of die distortion research and can be used to predict key distortion phenomena of relevance to a die caster with a minimum of background and without the need for simulations. These objectives were met. A detailed modeling tutorial was provided to NADCA for distribution to the industry. Power law based meta-models for predicting machine tie bar loading and for predicting maximum parting surface separation were successfully developed and tested against simulation results for a wide range of machines and experimental data. The models proved to be remarkably accurate, certainly well within the requirements for practical application. In addition to making die structural modeling more accessible, the work advanced the state-of-the-art by developing improved modeling of cavity pressure effects, which is typically modeled as a hydrostatic boundary condition, and performing a systematic analysis of the influence of ejector die design variables on die deflection and parting plane separation. This cavity pressure modeling objective met with less than complete success due to the limits of current finite element based fluid structure interaction analysis methods, but an improved representation of the casting/die interface was accomplished using a combination of solid and shell elements in the finite element model. This approximation enabled good prediction of final part distortion verified with a comprehensive evaluation of the dimensions of test castings produced with a design experiment. An extra deliverable of the experimental work was development of high temperature mechanical properties for the A380 die casting alloy. The ejector side design objective was met and the results were incorporated into the metamodels described above. This new technology was predicted to result in an average energy savings of 2.03 trillion BTU's/year over a 10 year period. Current (2011) annual energy saving estimates over a ten year period, based on commercial introduction in 2009, a market penetration of 70% by 2014 is 4.26 trillion BTU's/year by 2019. Along with these energy savings, reduction of scrap and improvement in casting yield will result in a reduction of the environmental emissions associated with the melting and pouring of the metal which will be saved as a result of this technology. The average annual estimate of CO2 reduction per year through 2020 is 0.085 Million Metric Tons of Carbon Equivalent (MM TCE).
Compaction dies used to create europium oxide and tantalum control plates were modeled using ANSYS 11.0. Two-piece designs were considered in order to make the dies easier to assemble than the five-piece dies that were previously used. The two areas of concern were the stresses at the interior corner of the die cavity and the distortion of the cavity wall due to the interference fit between the two pieces and the pressure exerted on the die during the compaction process. A successful die design would have stresses less than the yield stress of the material and a maximum wall distortion on the order of 0.0001 in. Design factors that were investigated include the inner corner radius, the value of the interference fit, the compaction force, the size of the cavity, and the outer radius and geometry of the outer ring. The results show that for the europium oxide die, a 0.01 in. diameter wire can be used to create the cavity, leading to a 0.0055 in. radius corner, if the radial interference fit is 0.003 in. For the tantalum die, the same wire can be used with a radial interference fit of 0.001 in. Also, for the europium oxide die with a 0.003 in. interference fit, it is possible to use a wire with a diameter of 0.006 in. for the wire burning process. Adding a 10% safety factor to the compaction force tends to lead to conservative estimates of the stresses but not for the wall distortion. However, when the 10% safety factor is removed, the wall distortion is not affected enough to discard the design. Finally, regarding the europium oxide die, when the cavity walls are increased by 0.002 in. per side or the outer ring is made to the same geometry as the tantalum die, all the stresses and wall distortions are within the desired range. Thus, the recommendation is to use a 0.006 in. diameter wire and a 0.003 in. interference fit for the europium oxide die and a 0.01 in. diameter wire and a 0.001 in. interference fit for the tantalum die. The dies can also be made to have the same outer geometry if desired.
Highlights: • A selective chemical etching method has been developed for removal of metallization layers on ultrathin Si dies for three-point bending test. • The complex elastoplastic stress distribution in the die is simplified to an elastic stress distribution. • The die sidewall fracture strength can be determined using the standard three-point bending tensile stress equation. • The characteristic fracture strengths of ultrathin Si dies were correlated to the laser-induced microstructures of the die sidewall. - Abstract: The sidewall fracture strength of ultrathin Si dies with frontside and backside metallization layers cannot be determined directly from three-point bending (3PB) test. The complex 3PB elastoplastic stress distribution makes it difficult to determine the die sidewall fracture strength by analytical method or finite element analysis due to various theoretical and practical constraints. In this work, a selective chemical etching method has been developed for complete removal of the frontside and backside metallization layers on the ultrathin die without affecting the critical microstructure and strength of the die sidewall induced by laser dicing. By removing all the metallization layers on the die, the complex 3PB elastoplastic stress distribution is simplified to an elastic stress distribution. This enables a straightforward calculation of the die sidewall fracture strength using the standard 3PB tensile stress equation for a homogeneous linear elastic material with a rectangular cross section. Two chemical etchants were evaluated and found to be suitable but FeCl{sub 3} is preferred because of the much faster etching time. With this improved 3PB test method, the effect of nanosecond laser dicing on ultrathin Si dies with backside Cu layer was investigated. The die frontside and backside characteristic fracture strengths of ultrathin Si dies with varying backside Cu thickness were determined and correlated to TEM analyses of the compositions and microstructures at the fracture origins.
The purpose of this project was to develop a process and product which would utilize magnesium die casting and result in energy savings when compared to the baseline steel product. The specific product chosen was a side door inner panel for a mid-size car. The scope of the project included: re-design of major structural parts of the door, design and build of the tooling required to make the parts, making of parts, assembly of doors, and testing (both physical and simulation) of doors. Additional work was done on alloy development, vacuum die casting, and overcasting, all in order to improve the performance of the doors and reduce cost. The project achieved the following objectives: 1. Demonstrated ability to design a large thin-wall magnesium die casting. 2. Demonstrated ability to manufacture a large thin-wall magnesium die casting in AM60 alloy. 3. Tested via simulations and/or physical tests the mechanical behavior and corrosion behavior of magnesium die castings and/or lightweight experimental automotive side doors which incorporate a large, thin-wall, powder coated, magnesium die casting. Under some load cases, the results revealed cracking of the casting, which can be addressed with re-design and better material models for CAE analysis. No corrosion of the magnesium panel was observed. 4. Using life cycle analysis models, compared the energy consumption and global warming potential of the lightweight door with those of a conventional steel door, both during manufacture and in service. Compared to a steel door, the lightweight door requires more energy to manufacture but less energy during operation (i.e., fuel consumption when driving vehicle). Similarly, compared to a steel door, the lightweight door has higher global warming potential (GWP) during manufacture, but lower GWP during operation. 5. Compared the conventional magnesium die casting process with the “super-vacuum” die casting process. Results achieved with cast tensile bars suggest some improvement in tensile properties with vacuum casting. Plant trials with large castings revealed cavity fill issues attributed to cooling and partial solidification of metal in the shot sleeve while waiting for vacuum to be established in the die cavity. 6. Developed age-hardenable Mg-based alloys as potential alternatives to the AM60 and AZ91 alloys typically used in automotive applications. Mg-7%Al-based alloys having Sn or Sn+Si additions exhibited significant age hardening, but more work is needed to demonstrate significant improvement in tensile properties. Corrosion behavior of these alloys is between those of AM60 and AZ91 alloys. 7. Evaluated the die casting of magnesium directly onto either steel or aluminum tubes as a potential process to make large lightweight subassemblies. Samples were free of gross defects, but additional work is needed to increase the interfacial shear strength. Overall, the project demonstrated that an automotive door-in-white design incorporating a die cast magnesium inner panel and a stamped aluminum outer panel can achieve approximately 50% mass reduction compared to the stamped steel baseline door-in-white. This leads to reduced energy consumption when driving the vehicle, which should more than offset the increased embedded energy of manufacture associated with the lighter metals. However, additional design work would be needed in order to meet the mechanical performance required of a door. Development of high-strength, high-ductility magnesium alloy castings would help make this technology more attractive for potential use in the side doors on automobiles. Also, increased use of recycled magnesium and aluminum would reduce the embedded energy and greenhouse gas emissions associated with the manufacture of this type of lightweight door. Commercialization planning of the type of lightweight door technology addressed in this project would be contingent upon the doors meeting all technical performance requirements of the car maker. The specific lightweight door developed in this project didn’t meet some of those requirements, but a preliminary business case study was conducted anyhow. This study considered the ratio of cost increase to mass decrease when the lightweight door is compared to a baseline steel door. The ratio was found to be in an acceptable range for some vehicle programs, especially if the number of such vehicles to be produced is equal to or slightly less than the estimated 250,000-shot life of the die set. This would allow for the investment in the dies to be spread across many parts and thereby help minimize the cost increase.
An apparatus and method for facilitating the removal of layers from a die for an integrated circuit while maintaining the planarity of the surface of the die by avoiding rounding the corners and other edges of the die. A pocket is created in a sacrificial material, such that when the die is inserted into the pocket the edges of the die are contiguous with the walls of the pocket and a top surface of the die is coplanar with a top surface of the pocket. The sacrificial material may be the same material as the die. An adhesive substance is placed in the pocket, and the die is inserted into the pocket and against the adhesive substance which aids in retaining the die in the pocket. The layers may then be removed from the die and the sacrificial material around the die without rounding the edges of the die.
An apparatus and method for facilitating the removal of layers from a die for an integrated circuit while maintaining the planarity of the surface of the die by avoiding rounding the corners and other edges of the die. A pocket is created in a sacrificial material, such that when the die is inserted into the pocket the edges of the die are contiguous with the walls of the pocket and a top surface of the die is coplanar with a top surface of the pocket. The sacrificial material may be the same material as the die. An adhesive substance is placed in the pocket, and the die is inserted into the pocket and against the adhesive substance which aids in retaining the die in the pocket. The layers may then be removed from the die and the sacrificial material around the die without rounding the edges of the die.
ORNL/TM-2010/48 described some results from using the finite element program ANSYS to determine the design geometry for compaction dies used to create europium oxide and tantalum control plates. Because of some discrepancies between the final drawings of the parts and the TM analyses, the models were reworked and some design modifications were made. When the mesh density was increased, increasing the number of elements in the model, especially near the corners, the maximum stresses in the corners were found to be higher than in the previous study. The dies needed to be designed with inner corner radii and interference fits that would allow the necessary compression force to create the plates but not exceed the yield strength of the material. Also, modeling was done to determine the effects of loading the dies asymmetrically in the axial direction, as this would make the plate extraction process easier while increasing the stress in the corners. The results show that for the tantalum die, a diametrical interference fit of 0.0020 in. between the outer ring and the insert is acceptable, and the inner corner radius can be as small as 0.0035 in. The insert has an outer diameter of 6.150 in. The cavity in the insert is 3.4640 $\times$ 0.8086 ± 0.002 in. and the outer ring has an outer diameter of 8.150 in. The die is 2.960 in. deep. With these design parameters, the plate can be formed so that its edge is 0.500 in. from the top or the bottom of the die, and the maximum stress everywhere in the die will be less than the yield strength of the materials. For the europium oxide die, the diametrical interference fit between the outer ring and the insert must be between 0.0075 and 0.0080 in. The inner corner radius can be as small as 0.0055 in. The insert has an outer diameter of 5.960 in. The cavity in the insert is 3.4552 $\times$ 1.7246 ± 0.002 in. and the outer ring has an outer diameter of 8.150 in. The die is 3.020 in. deep. With these design parameters, the plate can be formed so that its edge is 1.225 in. from the top or the bottom of the die.
The strength of high-duty gears can be improved by carburizing and quenching processes. Quenching distortion is inevitable during the process, and it has direct effects on the precision of the gear. For spiral bevel gear with big diameter and small thickness, die quenching process is applied in the manufacturing to control the distortion in axial direction. Die quenching parameters must be optimized to minimize the distortion while considering non-uniformity of chemical compositions and loads. In this paper, material models of gear material (22CrMoH) built based on the phase transformation kinetics, static mechanical properties and phase transformation plasticity equations. Finite element analysis (FEA) models are conducted to study the whole die quenching process based on the production process. Die quenching experiments and testing of microstructures and distortions are conducted to verify the accuracy of the FEA models. The effects of loads and bottom die obliquity on the final distortion are studied to set the appropriate range and control distortion. The distortion was very sensitive to the bottom die obliquity and some part of load ranges. The distortion changes little when the load of inner die was in the range of 1.38-2.07 MPa and the load of outer die was in the range of 2.07-2.76 MPa. The distortion range is fitted the production requirements by setting the inclination angle of bottom die between 0.12° and 0.29°.
The various technologies presented herein relate to measuring a signal generated by a die-based test circuit incorporated into an IC, and utilizing the measured signal to authenticate the IC. The signal can be based upon a sensor response generated by the test circuit fabricated into the die, wherein the sensor response is based upon a property of the die material. The signal can be compared with a reference value obtained from one or more test circuit(s) respectively located on one or more reference dies, wherein the reference dies are respectively cut from different wafers, and the location at which the reference dies were cut is known. If the measured signal matches the reference value, the die is deemed to be from the same cut location as the dies from which the reference value was obtained. If the measured signal does not match the reference value, the die is not authenticated.
The various technologies presented herein relate to measuring a signal generated by a die-based test circuit incorporated into an IC and utilizing the measured signal to authenticate the IC. The signal can be based upon a sensor response generated by the test circuit fabricated into the die, wherein the sensor response is based upon a property of the die material. The signal can be compared with a reference value obtained from one or more test circuit(s) respectively located on one or more reference dies, wherein the reference dies are respectively cut from different wafers, and the location at which the reference dies were cut is known. If the measured signal matches the reference value, the die is deemed to be from the same cut location as the dies from which the reference value was obtained. If the measured signal does not match the reference value, the die is not authenticated.