Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CLINKER”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Evaluation of P{sub 2}O{sub 5} distribution inside the main clinker minerals by the application of EPMA method

The formation of Portland clinker phases has taken place in thermodynamically non-equilibrium state between macro-oxides CaO, SiO{sub 2}, Al{sub 2}O{sub 3}, Fe{sub 2}O{sub 3} and MgO from raw meal and P{sub 2}O{sub 5} from bone meal. The paper deals with the study of clinker minerals as solid solutions with P{sub 2}O{sub 5} during the clinkerization of raw mixture containing bone meal (BM). The ash of BM has contributed as a raw material to the formation of different clinker phases. Electron probe microanalysis (EPMA) method was used to determine the preferential distribution of P{sub 2}O{sub 5} inside calcium silicate phases and its influence upon C{sub 2}S/C{sub 3}S ratio. Basing on these results, composition of solid solution of C{sub 2}S and C{sub 3}S was established.

36 MATERIALS SCIENCE↗

Producing cement clinker assemblages in the system: CaO-SiO2-Al2O3-SO3-CaCl2-MgO

Highlights: • Alinite formation conditions are optimised. • Ye'elimite and alinite cannot be simultaneously produced. • Ternesite and chlormayenite are compatible at 1150 °C. • Alite is formed at a reduced temperature of 1300 °C. • Wadalite and chlorellestadite can incorporate chloride in cement clinker assemblages. The cement industry is carbon-intensive, and the valorisation of industrial side-streams/residuals for use as alternative raw materials can enable the cement industry to reduce its carbon footprint as well as promote resource efficiency. Apart from key clinker ingredients such as CaO, Al{sub 2}O{sub 3}, and SiO{sub 2}, industrial residues can also contain MgO, CaCl{sub 2}, and SO{sub 3}. Therefore, this study investigates the formation of cement clinker assemblages in the system CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-SO{sub 3}-CaCl{sub 2}-MgO at temperatures ranging between 1100 and 1300 °C. The production of a clinker composed mainly of alinite and ye'elimite is first attempted; it is found that these phases cannot be simultaneously produced. Ternesite is also not compatible with alinite under the conditions studied. Wadalite is compatible with both ye'elimite and ternesite, while ternesite is also compatible with chlormayenite at 1150 °C. Additionally, the low-temperature formation of alite was also observed with the presence of CaCl{sub 2} in the raw-material mix.

36 MATERIALS SCIENCE↗

Aluminum-rich belite sulfoaluminate cements: Clinkering and early age hydration

Belite sulfoaluminate (BSA) cements have been proposed as environmentally friendly building materials, as their production may release up to 35% less CO{sub 2} into the atmosphere when compared to ordinary Portland cements. Here, we discuss the laboratory production of three aluminum-rich BSA clinkers with nominal mineralogical compositions in the range C{sub 2}S (50-60%), C{sub 4}A{sub 3}$ (20-30%), CA (10%) and C{sub 12}A{sub 7} (10%). Using thermogravimetry, differential thermal analysis, high temperature microscopy, and X-ray powder diffraction with Rietveld quantitative phase analysis, we found that burning for 15 min at 1350 deg. C was the optimal procedure, in these experimental conditions, for obtaining the highest amount of C{sub 4}A{sub 3}$, i.e. a value as close as possible to the nominal composition. Under these experimental conditions, three different BSA clinkers, nominally with 20, 30 and 30 wt.% of C{sub 4}A{sub 3}$, had 19.6, 27.1 and 27.7 wt.%, C{sub 4}A{sub 3}$ respectively, as determined by Rietveld analysis. We also studied the complex hydration process of BSA cements prepared by mixing BSA clinkers and gypsum. We present a methodology to establish the phase assemblage evolution of BSA cement pastes with time, including amorphous phases and free water. The methodology is based on Rietveld quantitative phase analysis of synchrotron and laboratory X-ray powder diffraction data coupled with chemical constraints. A parallel calorimetric study is also reported. It is shown that the beta-C{sub 2}S phase is more reactive in aluminum-rich BSA cements than in standard belite cements. On the other hand, C{sub 4}A{sub 3}$ reacts faster than the belite phases. The gypsum ratio in the cement is also shown to be an important factor in the phase evolution.

36 MATERIALS SCIENCE↗

Stability of ternesite and the production at scale of ternesite-based clinkers

A method to synthesize high-purity ternesite is presented and the importance of reaction volume is highlighted; a brief description of the product morphology is also presented. Thermodynamic data for ternesite are derived and the limits of ternesite stability are then explored. An upper temperature stability limit of ≈ 1290 °C at 1 atm is determined; however, this temperature is dependent on the fugacity of the volatile components in the atmosphere. Thermodynamic predictions confirm that belite and ternesite rich calcium sulfoaluminate clinkers can be readily produced in a single stage process at temperatures above 1200 °C provided the atmosphere and temperature are controlled. To demonstrate this control at larger scales, a conventional 7.4-meter rotary kiln has been used to produce ≈ 20 kg of ternesite-containing clinkers. This demonstrates the usefulness of thermodynamic modelling as it has enabled ternesite-based clinkers to be readily produced at scale in a single-stage process using existing equipment without major modifications.

36 MATERIALS SCIENCE↗

Effect of ZnO on the whiteness of white Portland cement clinker

The addition of ZnO to significantly improve the Hunter whiteness of white Portland cement (WPC) clinkers is introduced in this paper. The effects of ZnO on the whiteness of WPC were studied by chroma analysis, X-ray diffraction (XRD), the Rietveld method, hydration heat measurements and SEM-EDS. The results showed that adding ZnO increased the visible light reflectance, increased the brightness (L{sup ⁎}), and reduced the yellowness (b{sup ⁎}) of WPC clinker with high Fe{sub 2}O{sub 3}. Therefore, ZnO can increase the whiteness of WPC clinker. Zn was mainly distributed in the amorphous phase and unquantifiable crystalline phase (ACn), and then dissolved in the silicate phase. ZnO stabilized R-C{sub 3}S, reduced the crystallization of C{sub 3}A, and increased the ACn content. ZnO increased the amount of Fe in the ACn and minerals, thereby reducing the formation of C{sub 4}AF and improving whiteness. ZnO increased the accumulated heat of hydration but prolonged the induction period. This method provides a new approach for the WPC industry to broaden sources of raw materials and improve product quality.

36 MATERIALS SCIENCE↗

Boosting the use of bauxite residue (red mud) in cement - Production of an Fe-rich calciumsulfoaluminate-ferrite clinker and characterisation of the hydration

Highlights: • Incorporation of 35 wt% of bauxite residue for production of CSAF clinker • Thermochemical calculations as suitable tool for predicting phase assemblage • Hydration of the cement was found to be accelerated in contrast to other CSA cements. • High early compressive strengths of 40 MPa In the present work, calciumsulfoaluminate-ferrite clinker was produced using 35 wt% of bauxite residue in combination with alumina, clay, limestone and gypsum. At a temperature of 1300 °C, the hydraulic phases ye'elimite, ferrite and C{sub 2}S were formed. Computed thermochemical predictions were a significantly better match for the real mineralogy than modified Bogue equations. Hydration of the clinker led to the formation of ettringite and monosulfate, resulting in compressive strengths of 17 MPa after 28d. Compressive strengths of 40 MPa after 2d, and 28d-strengths exceeding 50 MPa, were reached in blends with 10 wt% of anhydrite. The strength development was due to the rapid formation of ettringite, mainly originating from ye'elimite, which did not convert to AFm phases and led to a compact microstructure. Only when the ye'elimite dissolution decreased, did the ferrite phase react. In pastes with additional sulfates, ferrite hydration led to the formation of ettringite and to hydrogarnet. Cement nomenclature is used in this work.{sup 1}.

36 MATERIALS SCIENCE↗

Sulphate resistance of low‐clinker engineered cementitious composites examined by MicroXRF imaging

Abstract Engineered cementitious composites (ECC) are a class of high‐performing fibre‐reinforced cementitious materials recognised for their increased ductility and durability compared to conventional cement‐based materials, owing to their autogenously controlled tight crack widths, even when subjected to high strains. To reduce ECC's environmental impact, this research examines the use of a low‐clinker binder − limestone‐calcined clay cement (LC3) − as an alternative to portland cement (PC), along with fly ash to further reduce the clinker proportion and the embodied CO 2 of the formulations. In conventional concrete, LC3 hydrates to a denser microstructure resulting from the synergistic reaction between limestone and calcined clay. At the lower water contents typical of ECC and with the presence of fly ash, the influence of the binder composition on the microstructure is difficult to anticipate. To examine the influence of these compositional variables on microstructure, permeability and durability, the sulphate resistance of LC3‐based ECC is explored. Specifically, the ECC‐LC3 blends are designed with high clinker replacement rate of 75% by mass of binder and contain either conventional fly ash or reclaimed fly ash at 50% by mass of binder. Expansion of ECC‐LC3 samples subjected to standard sodium sulphate test conditions was measured up to 12 months and the depth of penetration of sulphates into the ECC‐LC3 of varying compositions was quantified using micro‐X‐Ray Fluorescence (microXRF) imaging and modelling. The expansion results show that the ECC‐LC3 formulations performed better than the PC samples and can provide adequate resistance to external sulphate attack, even when reclaimed fly ashes are used in place of the conventional ash. In addition, the shallow penetration of sulphate into these cementitious composites demonstrates the low diffusion coefficients values that were determined using the quantitative data from MicroXRF imaging.

Microscopy↗

Utilization of municipal solid waste incineration fly ash for sulfoaluminate cement clinker production

Highlights: > The replacement can be taken up to 30% of MSWI fly ash in the raw mix. > The novelty compositional parameters were defined, their optimum values were determined. > Expansive property of SAC is strongly depended on gypsum content. > Three leaching test methods are used to assess the environmental impact. - Abstract: The feasibility of partially substituting raw materials with municipal solid waste incineration (MSWI) fly ash in sulfoaluminate cement (SAC) clinker production was investigated by X-ray diffraction (XRD), compressive strength and free expansion ratio testing. Three different leaching tests were used to assess the environmental impact of the produced material. Experimental results show that the replacement of MSWI fly ash could be taken up to 30% in the raw mixes. The good quality SAC clinkers are obtained by controlling the compositional parameters at alkalinity modulus (C{sub m}) around 1.05, alumina-sulfur ratio (P) around 2.5, alumina-silica ratio (N) around 2.0{approx}3.0 and firing the raw mixes at 1250 deg. C for 2 h. The compressive strengths of SAC are high in early age while that develop slowly in later age. Results also show that the expansive properties of SAC are strongly depended on the gypsum content. Leaching studies of toxic elements in the hydrated SAC-based system reveal that all the investigated elements are well bounded in the clinker minerals or immobilized by the hydration products. Although some limited positive results indicate that the SAC prepared from MSWI fly ash would present no immediate thread to the environment, the long-term toxicity leaching behavior needs to be further studied.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Natural fluorapatite as a raw material for Portland clinker

The present work focuses on the mineralogy and the reactivity of clinkers made from the integration of natural fluorapatite in the raw meals with percentages ranging from 0 up to15%. The samples were characterized by infrared spectrometry, X-ray diffraction and microscopy techniques. The distribution of phosphorous and fluorine into clinkers minerals was determined by MEB/EDS mapping. The mineralogical composition was determined by XRD/Rietveld and the samples reactivity followed by isothermal microcalorimetry. It has been found that fluorine stabilizes C{sub 3}S and β-C{sub 2}S which still are found with high levels of P{sub 2}O{sub 5}. Cements obtained from up to 8% natural fluorapatite incorporation still present acceptable properties. Natural fluorapatite could have an important potential as decarbonised source of CaO contributing to decrease the CO{sub 2} emission in cement industry.

36 MATERIALS SCIENCE↗

Hydration behavior of cements with reduced clinker factor in mixture with sulfoaluminate binder

CO{sub 2} regulation and raw material availability will strongly influence the future cement market and a wider use of composite cements containing limestone and pozzolan or slag is expected. In the present paper, the possibility to combine Portland cements (PCs) with reduced clinker factor with sulfoaluminate cement (CSA), is explored. Low Portland clinker cements are prepared in laboratory using different supplementary cementitious materials (limestone, slag, pozzolan and fly ash) and mixed with a sulfoaluminate cement: the hydration behavior of the resulting binders is investigated up to 90 days through a multi-technique approach involving X-ray diffraction, differential scanning calorimetry and nuclear magnetic resonance spectroscopy. Understanding the interaction mechanisms between SCMs and CSA/PC blends will support the development of innovative high performing binders based on CEM III or CEM V, or even on new standardized CEM II. Results highlight that slag is particularly suitable promoting late strength development.

36 MATERIALS SCIENCE↗

Formulation of low clinker blended cements and concrete with enhanced fresh and hardened properties

Blended cements appear as the most promising way to massively produce cements with reduced environmental footprints. However, considering the generally lower early mechanical performance of highly blended cements, chemical admixtures are increasingly relied upon to increase early strength. However, in many cases this can negatively impact other properties as rheology and durability. This paper proposes an approach to formulate low clinker cements and concrete using moderate alkali activation or gypsum to enhance early and long-term compressive strength, without inducing excessive alkali-silica reaction (ASR) expansion. It examines blended cements containing burnt oil shale along with limestone and fly ash or slag as supplementary cementitious materials. It optimizes the combination of polycarboxylate ether (PCE) superplasticizers with the strength enhancers. Along with the use of Ca(NO{sub 3}){sub 2} to drive PCE adsorption, this provides good rheology control, increased early and long-term compressive strength, as well as acceptable ASR expansion in cements with only 50% clinker.

36 MATERIALS SCIENCE↗

Carbon-Enhanced Cement Clinker

A clinker for use in cement manufacturing includes a cement clinker mixture having crystals of an element that is less electronegative than carbon and carbon bonded to at least a portion of the crystals.

Abney, Morgan Barrera↗

Reaction kinetics during early hydration of calcined phyllosilicates in clinker-free model systems

Investigations of nearly pure, calcined phyllosilicates (“meta-phyllosilicates”) in clinker-free model systems were performed in presence and absence of sulfate. Calorimetric investigations show a pronounced reaction during the early reaction period only for metakaolin. Quantitative in situ X-ray diffraction reveals calcium silicate hydrate formation in the systems with metakaolin and metaillite, but not in those with metamuscovite. Ettringite crystallizes in all systems containing sulfate, where only the metakaolin system reaches the maximum ettringite content possible. The amount of aluminum ions released from 2:1 meta-phyllosilicates seems to be insufficient to reach the maximum content. Differences in portlandite dissolution and bound water indicate adsorption effects of calcium or calcium – sulfate ion pair complexes on surfaces of the calcined clay particles. Thus, the chemical as well as the physical influence of the meta-phyllosilicates must be considered to predict the reaction kinetics of calcined clays during early hydration.

36 MATERIALS SCIENCE↗

Characterization using thermomechanical and differential thermal analysis of the sinterization of Portland clinker doped with CaF{sub 2}

In this work, the sintering process of Portland cement was studied by combining thermomechanical analysis (TMA) and differential thermal analysis (DTA), together with X-ray diffraction (XRD) and scanning electron microscopy (SEM). Thermal analysis results employing both techniques indicted that phase transformations appeared at lower temperatures when CaF{sub 2} was incorporated in the raw materials. Besides, it was observed at high temperature that in some phase transformations TMA conducts to better resolution compared with the DTA measurements. Furthermore, mechanical properties and X-ray diffraction patterns corroborate the TMA and DTA results, corroborating that the final amount of alite (Ca{sub 3}SiO{sub 5}) is higher when a certain amount of CaF{sub 2} was present during the clinkerization process.

36 MATERIALS SCIENCE↗

Nanostructural evolution of Al(OH)3 gel formed by the cubic and orthorhombic ye'elimite clinkers of calcium sulfoaluminate cements in an ultra-wide hydration temperature range

This paper investigated the influence of hydration temperature on the nanostructure of the AH{sub 3} phase formed in calcium sulfoaluminate cements. Orthorhombic ye'elimite (st-ye'elimite) and cubic ye'elimite (ss-ye'elimite) were hydrated in an ultra-wide temperature range (5–220 °C). Results showed that the AH{sub 3} phase formed by ss-ye'elimite was always microcrystalline in nature at various curing temperatures (5–130 °C), and transformed into the AlOOH phase at 150 °C and above. However, the AH{sub 3} phase formed by st-ye'elimite grew from a microcrystal to a favorable crystal as the temperature increased, and transformed into the AlOOH phase at 170 °C and above. The nanostructure of hydration products was further investigated using TEM/SAED analysis together with FE-SEM images, directly evidencing that the formed AFm-12 phase was single-crystal in nature, and the formed AH{sub 3} phase was microcrystalline at low temperatures and grew into single-crystal hexagonal prisms with the preferred growth direction along [001] direction at high temperatures.

36 MATERIALS SCIENCE↗