Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ARC welding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Effects of Mars Atmosphere on Arc Welds: Phase 2

Gas tungsten arc welding (GTAW) is a vital fusion welding process widely used throughout the aerospace industry. Its use may be critical for the repair or manufacture of systems, rockets, or facilities on the Martian surface. Aluminum alloy AA2219-T87 and titanium alloy Ti-6Al-4V butt welds have been investigated for weldability and weld properties in a simulated Martian gas environment. The resulting simulated Martian welds were compared to welds made in a terrestrial atmosphere, all of which used argon shielding gas. It was found that GTAW is a process that may be used in a Martian gas environment, not accounting for pressure and gravitational effects, as long as adequate argon shielding gas is used to protect the weld metal. Simulated Martian welds exhibited higher hardness in all cases and higher tensile strength in the case of AA2219-T87. This has been attributed to the absorption of carbon into the fusion zone, causing carbide precipitates to form. These precipitates may act to pin dislocations upon tensile testing of AA2219-T87. Dissolved carbon may have also led to carburization, which may have caused the increase in hardness within the fusion zone of the welds. Based on the results of this experiment and other similar experiments, GTAW appears to be a promising process for welding in a Martian gas environment. Additional funding and experimentation is necessary to determine the effects of the low pressure and low gravity environment found on Mars on GTAW.

Courtright, Z. S.↗

Gas arc constriction for plasma arc welding

A welding torch for plasma arc welding apparatus has an inert gas applied circumferentially about the arc column externally of the constricting nozzle so as to apply a constricting force on the arc after it has exited the nozzle orifice and downstream of the auxiliary shielding gas. The constricting inert gas is supplied to a plenum chamber about the body of the torch and exits through a series of circumferentially disposed orifices in an annular wall forming a closure at the forward end of the constricting gas plenum chamber. The constricting force of the circumferential gas flow about the arc concentrates and focuses the arc column into a more narrow and dense column of energy after exiting the nozzle orifice so that the arc better retains its energy density prior to contacting the workpiece.

McGee, William F.↗

Multi-Pass Hybrid Laser Arc Welding of Alloy 740H

The presentation reviews the progress made toward reducing the joining time of an advanced nickel-based alloy, Alloy 740H by a factor of two using a novel two step fusion welding approach. In the first step, a high powered laser is used to rapidly join thick weld groove lands (~10-12 mm thick) during a single pass. Hybrid laser arc welding (HLAW) is then used to fill the remaining weld groove and complete the joint. This sequential process also utilizes laser wobble in both steps to reduce welding defects and refine the weld microstructure to obtain improved properties compared to conventional gas tungsten or gas metal arc welds, GTAW and GMAW, respectively. The creep behavior of laser-only thick weld groove land welds and HLAW welds were found to be the same or slightly improved compared to conventional GMAW or GTAW welds in this alloy. Creep tests have been started to verify the long-term creep behavior (~10,000 hrs) of these welds. Modeling results on deep penetration laser welding are presented and the initial simulations of laser welding with laser wobble are shown. The next phase of the project will combine the two processes to make complete welds - deep penetration laser welds of thick weld groove lands followed by rapid filling of the remaining weld groove by HLAW - in thick plates (32 mm thick) Alloy 740H plate and entails development of narrow weld groove welding to further decrease the joining time of this alloy.

36 MATERIALS SCIENCE↗

Plasma arc welding weld imaging

A welding torch for plasma arc welding apparatus has a transparent shield cup disposed about the constricting nozzle, the cup including a small outwardly extending polished lip. A guide tube extends externally of the torch and has a free end adjacent to the lip. First and second optical fiber bundle assemblies are supported within the guide tube. Light from a strobe light is transmitted along one of the assemblies to the free end and through the lip onto the weld site. A lens is positioned in the guide tube adjacent to the second assembly and focuses images of the weld site onto the end of the fiber bundle of the second assembly and these images are transmitted along the second assembly to a video camera so that the weld site may be viewed continuously for monitoring the welding process.

Rybicki, Daniel J.↗

Closed circuit TV system automatically guides welding arc

Closed circuit television /CCTV/ system automatically guides a welding torch to position the welding arc accurately along weld seams. Digital counting and logic techniques incorporated in the control circuitry, ensure performance reliability.

Stephans, D. L.↗

Sensing the gas metal arc welding process

Control of gas metal arc welding (GMAW) requires real-time sensing of the process. Three sensing techniques for GMAW are being developed at the Idaho National Engineering Laboratory (INEL). These are (1) noncontacting ultrasonic sensing using a laser/EMAT (electromagnetic acoustic transducer) to detect defects in the solidified weld on a pass-by-pass basis, (2) integrated optical sensing using a CCD camera and a laser stripe to obtain cooling rate and weld bead geometry information, and (3) monitoring fluctuations in digitized welding voltage data to detect the mode of metal droplet transfer and assure that the desired mass input is achieved.

Carlson, N. M.↗

Quarterly Management Document – FY21, 4th Quarter, Multi-pass Hybrid Laser Arc Welding of Alloy 740H

This report summarizes the progress made on reducing the joining time for thick plates of Alloy 740H. Modeling of deep penetration laser welding of Alloy 740H continues with the goal of explaining cracking in the weld that is observed in experimental laser welds in this alloy. Experimental work was also performed to understand factors influencing hybrid laser arc weld quality as a function of the arc and laser parameters. Laser welds and hybrid laser arc welds have been made using best practices up this point in the project. Welded materials have been sent to a commercial vendor to make creep specimens and perform short term creep tests to help evaluate the quality of the welds that have been made so far.

36 MATERIALS SCIENCE↗

Gas tungsten arc welding in a microgravity environment: Work done on GAS payload G-169

GAS payload G-169 is discussed. G-169 contains a computer-controlled Gas Tungsten Arc Welder. The equipment design, problem analysis, and problem solutions are presented. Analysis of data gathered from other microgravity arc welding and terrestrial Gas Tungsten Arc Welding (GTAW) experiments are discussed in relation to the predicted results for the GTAW to be performed in microgravity with payload G-169.

Welcher, Blake A.↗

Melting Efficiency During Plasma Arc Welding

A series of partial penetration Variable Polarity Plasma Arc welds were made at equal power but various combinations of current and voltage on 2219 aluminum. Arc Efficiency was measured calorimetrically and ranged between 48% and 66%. Melting efficiency depends on the weld pool shape. Increased current increases the melting efficiency as it increases the depth to width ratio of the weld pool. Higher currents are thought to raise arc pressure and depress the liquid at the bottom of the weld pool causing a more nearly two dimensional heat flow condition.

McClure, J.C.↗

Preventing Arc Welding From Damaging Electronics

Shielding technique developed to protect sensitive electronic equipment from damage due to electromagnetic disturbances produced by arc welding. Established acceptable alternative in instances in which electronic equipment cannot be removed prior to arc welding. Guidelines established for open, unshielded welds. Procedure applicable to robotics or computer-aided manufacturing.

Sargent, Noel↗

Automated Variable-Polarity Plasma-Arc Welding

Variable-polarity plasma-arc methods produces better welds at lower cost than gas-shielded tungsten-arc welding in assemblies. Weld porosity very low and costs of joint preparation, depeaking, inspection, and weld repair minimized.

Numes, A. C., Jr.↗

Plasma arc welding repair of space flight hardware

Repair and refurbishment of flight and test hardware can extend the useful life of very expensive components. A technique to weld repair the main combustion chamber of space shuttle main engines has been developed. The technique uses the plasma arc welding process and active cooling to seal cracks and pinholes in the hot-gas wall of the main combustion chamber liner. The liner hot-gas wall is made of NARloyZ, a copper alloy previously thought to be unweldable using conventional arc welding processes. The process must provide extensive heat input to melt the high conductivity NARloyZ while protecting the delicate structure of the surrounding material. The higher energy density of the plasma arc process provides the necessary heat input while active water cooling protects the surrounding structure. The welding process is precisely controlled using a computerized robotic welding system.

Hoffman, David S.↗

Plasma arc welding repair of space flight hardware

A technique to weld repair the main combustion chamber of Space Shuttle Main Engines has been developed. The technique uses the plasma arc welding process and active cooling to seal cracks and pinholes in the hot-gas wall of the main combustion chamber liner. The liner hot-gas wall is made of NARloy-Z, a copper alloy previously thought to be unweldable using conventional arc welding processes. The process must provide extensive heat input to melt the high conductivity NARloy-Z while protecting the delicate structure of the surrounding material. The higher energy density of the plasma arc process provides the necessary heat input while active water cooling protects the surrounding structure. The welding process is precisely controlled using a computerized robotic welding system.

Hoffman, David S.↗

More About Arc-Welding Process for Making Carbon Nanotubes

High-quality batches of carbon nanotubes are produced at relatively low cost in a modified atmospheric-pressure electric-arc welding process that does not include the use of metal catalysts. What would normally be a welding rod and a weldment are replaced by an amorphous carbon anode rod and a wider, hollow graphite cathode rod. Both electrodes are water-cooled. The cathode is immersed in ice water to about 0.5 cm from the surface. The system is shielded from air by flowing helium during arcing. As the anode is consumed during arcing at 20 to 25 A, it is lowered to maintain it at an approximately constant distance above the cathode. The process causes carbon nanotubes to form on the lowest 5 cm of the anode. The arcing process is continued until the anode has been lowered to a specified height. The nanotube-containing material is then harvested. The additional information contained in the instant report consists mostly of illustrations of carbon nanotubes and a schematic diagram of the arc-welding setup, as modified for the production of carbon nanotubes.

Benavides, Jeanette M.↗

Quarterly Management Document – FY22, 3rd Quarter, Multi-pass Hybrid Laser Arc Welding of Alloy 740H

During the 3rd quarter of FY22, progress was made on modeling and simulation of deep penetration laser welding of Alloy 740H. Advances in the modeling of residual stress development arising from the calculated temperature field of the solidifying weld pool were made to understand the development of solidification cracking. Additionally, preliminary modeling of the temperature field within the weld pool of a wobbling laser heat source was performed. The maximum temperature of the weld pool was found to vary with time. These result will allow modeling of deep penetration laser welding using a wobbling laser to mitigate weld defects and cracking. Also, additional characterization of hybrid laser arc welds indicated that these welds were not defect-free as originally thought and the current HLA welds would not be acceptable under criteria outlined in the ASME Boiler and Pressure Vessel Code, Section IX. Therefore, additional welding trails with variation of the welding parameters and HLA welding configurations are required to produce welds acceptable under the Section IX criteria. It was shown that considerable reduction of HLAW defects had been achieved with each successive welding campaign. Therefore additional variation of HLAW parameters may still yield the desired defect-free welds, however, options for alternate HLAW configurations as well as plate preheating are outlined as contingency plans to obtain suitable welds. These additional (unplanned) HLAW trial may prevent subsequent milestones from being achieved within the original budget.

36 MATERIALS SCIENCE↗

Arc Weld Robotic Arm & Enclosure Seismic Anchorage in B226

The Arc Weld Robotic Arm & Enclosure is adequately anchored by the details shown on sheets SKS-01 through SKS-03. Two different Hilti anchors have been provided to allow for installation flexibility. Existing documentation shows that the existing enclosure base has been anchored with 5/8”Ø Kwik Bolt TZ’s. As a result, it is believed that the existing holes are sized for that 5/8”Ø anchor. The first option is to install a 5/8”Ø Kwik Bolt TZ2, similarly to the existing conditions. The second option is to use a threaded insert anchor. Since the largest allowable diameter of HIS-N insert is 1/2”Ø based on the slab thickness, 2”x2” square plate washers with a 9/16”Ø hole will need to be installed on the top of the existing enclosure base plates to reduce the diameter of the existing holes. This is required for the anchorage to provide proper restraint in a seismic event.

42 ENGINEERING↗

Submerged arc welding of heavy plate

The submerged arc process is particularly suitable for heavy plate welding because of its ability to combine very high deposit rates along with excellent quality. It does these things without the smoke and spatter often accompanying other processes. It is available today in several forms that are pointed to the fabricators of heavy sections with long, short or round about welds. Tandem arc full automatic equipment is particularly suitable for those long heavy welds where speed and deposit rate are of the first order. An attachment called long stick-out which makes use of the IR drop on long electrode extensions can be included on this equipment to increase deposition rates 50% or more.

Wilson, R. A.↗