At least 343 records · Page 19

Heat treatment study of the SiC/Ti-15-3 composite system

The oxidation and aging behaviors of a continuous fiber SiC/Ti-15V-3Cr-3Sn-3Al composite (SiC/Ti-15-3) were investigated. The aging characteristic of the composite were compared with those of the unreinforced Ti-15-3 matrix material, which was processed in the same manner as the composite. Various age hardened conditions of both the unreinforced matrix and the composite were evaluated by using optical microscopy, hardness measurements, and room temperature tensile tests (unreinforced matrix only). The Ti-15-3 material formed a thick surface oxide at temperature at or above 550 C when heat treated in air. The in situ composite matrix was softer than the unreinforced matrix for equivalent aging conditions. Both materials hardened to a maximum, then softened during overaging. The temperature at which peak aging occurred was approx. 450 C for both the in situ composite matrix and the unreinforced matrix. The room temperature elastic modulus and ultimate tensile strength of the unreinforced matrix varied as a function of aging treatment and paralleled the hardness behavior. The modulus and tensile strength showed little response to aging up to temperatures of 300 C; however, these properties increased after aging at 550 C. Aging at temperatures above 550 C resulted in a decrease in the modulus and tensile strength. The failure strain was a function of the precipitation state and of the amount of oxidation resulting from the heat treatment. Aging in air at the higher temperatures (greater than 550 C) caused the formation of a thick oxide layer and reduced the ductility. Aging in vacuum at these temperatures resulted in significantly higher ductilities. Long term exposures at 700 C caused the formation of a large grain boundary alpha-phase which reduced the ductility, even though the specimens were heat treated in vacuum.

Lerch, Bradley A.↗

Influence of interfacial shear strength on the mechanical properties of SiC fiber reinforced reaction-bonded silicon nitride matrix composites

The influence of fiber/matrix interface microstructure and interfacial shear strength on the mechanical properties of a fiber-reinforced ceramic composite was evaluated. The composite consisted of approximately 30 vol percent uniaxially aligned 142 microns diameter SiC fibers (Textron SCS-6) in a reaction-bonded Si3N4 matrix (SiC/RBSN). The interface microstructure was varied by controlling the composite fabrication conditions and by heat treating the composite in an oxidizing environment. Interfacial shear strength was determined by the matrix crack spacing method. The results of microstructural examination indicate that the carbon-rich coating provided with the as-produced SiC fibers was stable in composites fabricated at 1200 C in a nitrogen or in a nitrogen plus 4 percent hydrogen mixture for 40 hr. However this coating degraded in composites fabricated at 1350 C in N2 + 4 percent H2 for 40 and 72 hr and also in composites heat treated in an oxidizing environment at 600 C for 100 hr after fabrication at 1200 C in a nitrogen. It was determined that degradation occurred by carbon removal which in turn had a strong influence on interfacial shear strength and other mechanical properties. Specifically, as the carbon coating was removed, the composite interfacial shear strength, primary elastic modulus, first matrix cracking stress, and ultimate tensile strength decreased, but the first matrix cracking strain remained nearly the same.

Bhatt, Ramakrishna T.↗

An investigation of the thermal cycling damage of 25 vol. pct SiCw/alumina ceramic matrix composite

An investigation was made of the thermal cycling damage of a 25 vol pct SiC whisker/alumina (SiCw/Al2O3) composite. Thermal cycling tests were conducted by subjecting a composite specimen to two different fluidized beds. After thermal cycling the composite specimens were subjected to elastic modulus and effective fracture toughness measurements. The thermal cycled specimens were investigated with SEM and TEM studies. It was found that this composite has a relatively high resistance to thermal cycling.

Armstrong, William D.↗

Intercalated graphite fiber composites as EMI shields in aerospace structures

The requirements for electromagnetic interference (EMI) shielding in aerospace structures are complicated over that of ground structures by their weight limitations. As a result, the best EMI shielding materials must blend low density, high strength, and high elastic modulus with high shielding ability. In addition, fabrication considerations including penetrations and joints play a major role. The EMI shielding properties are calculated for shields formed from pristine and intercalated graphite fiber/epoxy composites and compared to preliminary experimental results and to shields made from aluminum. Calculations indicate that EMI shields could be fabricated from intercalated graphite composites which would have less than 12 percent of the mass of conventional aluminum shields, based on mechanical properties and shielding properties alone.

Gaier, James R.↗

Mechanical strength and thermophysical properties of PM212: A high temperature self-lubricating powder metallurgy composite

A powder metallurgy composite, PM212, composed of metal bonded chromium carbide and solid lubricants is shown to be self-lubricating to a maximum application temperature of 900 C. The high temperature compressive strength, tensile strength, thermal expansion and thermal conductivity data needed to design PM212 sliding contact bearings and seals are reported for sintered and isostatically pressed (HIPed) versions of PM212. Other properties presented are room temperature density, hardness, and elastic modulus. In general, both versions appear to have adequate strength to be considered as sliding contact bearing materials, but the HIPed version, which is fully dense, is much stronger than the sintered version which contains about 20 percent pore volume. The sintered material is less costly to make, but the HIPed version is better where high compressive strength is important.

Edwards, Phillip M.↗

High-toughness graphite/epoxy composite material experiment

The experiment was designed to measure the effect of near-space exposure on mechanical properties of specially toughened 5208/T300 graphite-epoxy composites. The properties measured are elastic modulus, strength, and fracture toughness. Specimens were mounted on an external frame during the time of the LDEF mission. Specimen variables include angle of adjacent plies and fraction of interlaminar contact, which is controlled by the fraction of finely spaced holes in Mylar film placed between the prepreg monolayers of the composite.

Felbeck, David K.↗

Ultrasonic evaluation of oxidation and reduction effects on the elastic behavior and global microstructure of YBa2Cu3O7-x

Ultrasonic velocity measurement techniques were used to evaluate the effects of oxidation and reduction on the elastic properties, global microstructure and oxygen content of the YBa2Cu3O(7-x) ceramic superconductor for samples ranging from 70 to 90 pct. of theoretical density. Bulk density, velocity, and elastic modulus generally increased with increasing oxygen content upon oxidation, and this behavior was reversible. Velocity image patterns were similar after oxidation and reduction treatments for a 90 pct. dense sample, although the velocity value at any given point on the sample was changed following the treatments. The unchanging pattern correlated with destructive measurements showing that the spatial pore distribution (fraction and size) was not measurably altered after the treatments. Changes in superconducting behavior, crystal structure, and grain structure were observed consistent with changes in oxygen content.

Roth, Don J.↗

Ultrasonic velocity technique for monitoring property changes in fiber-reinforced ceramic matrix composites

A technique for measuring ultrasonic velocity was used to monitor changes that occur during processing and heat treatment of a SiC/RBSM composite. Results indicated that correlations exist between the ultrasonic velocity data and elastic modulus and interfacial shear strength data determined from mechanical tests. The ultrasonic velocity data can differentiate strength. The advantages and potential of this nondestructive evaluation method for fiber reinforced ceramic matrix composite applications are discussed.

Kautz, Harold E.↗

Probabilistic analysis of structures involving random stress-strain behavior

The present methodology for analysis of structures with random stress strain behavior characterizes the uniaxial stress-strain curve in terms of (1) elastic modulus, (2) engineering stress at initial yield, (3) initial plastic-hardening slope, (4) engineering stress at point of ultimate load, and (5) engineering strain at point of ultimate load. The methodology is incorporated into the Numerical Evaluation of Stochastic Structures Under Stress code for probabilistic structural analysis. The illustrative problem of a thick cylinder under internal pressure, where both the internal pressure and the stress-strain curve are random, is addressed by means of the code. The response value is the cumulative distribution function of the equivalent plastic strain at the inner radius.

Millwater, H. R.↗

Ultrasonic velocity technique for monitoring property changes in fiber-reinforced ceramic matrix composites

A technique for measuring ultrasonic velocity was used to monitor changes that occur during processing and heat treatment of a SiC/RBSM composite. Results indicated that correlations exist between the ultrasonic velocity data and elastic modulus and interfacial shear strength data determined from mechanical tests. The ultrasonic velocity data can differentiate strength. The advantages and potential of this nondestructive evaluation method for fiber reinfoced ceramic matrix composite applications are discussed.

Kautz, H. E.↗

Polycrystalline SiC fibers from organosilicon polymers

Various organosilicon polymers have been converted into small diameter, fine-grained silicon carbide fibers by melt spinning, crosslinking, and pyrolyzing to greater than 1600 C. The high pyrolysis temperature densifies the fiber and causes CO evolution which removes nearly all oxygen. An additive prevents the loss of strength normally associated with such treatments. Silicon carbide fibres with up to 2.6 GPa (380 ksi) tensile strength, greater than 420 GPa (greater than 60 Msi) elastic modulus, and 3.1-3.2 mg/cu m density have been prepared via this process. Their microstructure consists of greater than 95 wt pct B-SiC crystallites averaging 30-40 nm diameter, with varying amounts of graphitic carbon between the SiC grains. Under inert conditions, the fibers can be thermally aged at least 12 h/1800 C with minimal change in properties.

Lipowitz, Jonathan↗

Tribological evaluation of an Al2O3-SiO2 ceramic fiber candidate for high temperature sliding seals

A test program to determine the relative sliding durability of an alumina-silica candidate ceramic fiber for high temperature sliding seal applications as described. This work represents the first reporting of the sliding durability of this material system. Pin-on-disk tests were used to evaluate the potential seal material by sliding a tow or bundle of the candidate ceramic fiber against a superalloy test disk. Friction was measured during the tests and fiber wear, indicated by the extent of fibers broken in the tow or bundle, was measured at the end of each test. Test variables studied included ambient temperatures from 25 C to 900 C, loads from 1.3 to 21.2 Newtons, and sliding velocities from 0.025 to 0.25 m/sec. In addition, the effects of fiber diameter, elastic modulus, and a pretest fiber heat treatment on friction and wear were measured. In most cases, wear increased with temperature. Friction ranged from about 0.36 at 500 C and low velocity (0.025 m/s) to over 1.1 at 900 C and high velocity (0.25 m/s). The pretest fiber heat treatment, which caused significant durability reductions for alumina-boria-silica ceramic fibers tested previously, had little effect on the alumina-silica fibers tested here. These results indicate that the alumina-silica (Al2O3-SiO2) fiber is a good candidate material system for high temperature sliding seal applications.

Dellacorte, Christopher↗

High-toughness graphite/epoxy composite material experiment

This experiment was designed to measure the effect of near space exposure on three mechanical properties of specially toughened 5208/T300 graphite/epoxy composite materials. The properties measured are elastic modulus, strength, and fracture toughness. Six toughness specimens and nine tensile specimens were mounted on an external frame during the time of the Long Duration Exposure Facility (LDEF) mission. Three identical sets of specimens were manufactured at the outset: the flight set, a zero time non-flight set, and a total time non-flight set. To date, two toughness specimens and three strength and modulus specimens have been tested from each of the three groups.

Felbeck, David K.↗

High-toughness graphite/epoxy composite material experiment

This LDEF experiment was designed to measure the effects of near-earth exposure on graphite/epoxy composites over a range of properties. All of the specimens were 8 plies thick, with one of two different cross-ply angles and with one of four different values of bonding fraction between plies. The mechanical properties of interest are toughness, strength, and elastic modulus. Six toughness specimens and nine strength/modulus specimens were manufactured and flown.

Felbeck, David K.↗

Elevated temperature axial and torsional fatigue behavior of Haynes 188

The results of high-temperature axial and torsional low-cycle fatigue experiments performed on Haynes 188, a wrought cobalt-base superalloy, are reported. Fatigue tests were performed at 760 C in air on thin-walled tubular specimens at various ranges under strain control. Data are also presented for coefficient of thermal expansion, elastic modulus, and shear modulus at various temperatures from room to 1000 C, and monotonic and cyclic stress-strain curves in tension and in shear at 760 C. The data set is used to evaluate several multiaxial fatigue life models (most were originally developed for room temperature multiaxial life prediction) including von Mises equivalent strain range (ASME boiler and pressure vessel code), Manson-Halford, Modified Multiaxiality Factor (proposed here), Modified Smith-Watson-Topper, and Fatemi-Socie-Kurath. At von Mises equivalent strain ranges (the torsional strain range divided by the square root of 3, taking the Poisson's ratio to be 0.5), torsionally strained specimens lasted, on average, factors of 2 to 3 times longer than axially strained specimens. The Modified Multiaxiality Factor approach shows promise as a useful method of estimating torsional fatigue life from axial fatigue data at high temperatures. Several difficulties arose with the specimen geometry and extensometry used in these experiments. Cracking at extensometer probe indentations was a problem at smaller strain ranges. Also, as the largest axial and torsional strain range fatigue tests neared completion, a small amount of specimen buckling was observed.

Bonacuse, Peter J.↗

Anodized aluminum coatings for thermal control. II - Environmental effects and cracking

The environmental effects of thermal cycling and humidity on coating cracking are examined. Experimental measurements of thermal deflection were used to calculate values for the thermal expansion coefficient and the in situ elastic modulus of an anodized aluminum. The thermal expansion coefficient is found to be approximately the same as for alumina in bulk form. The modulus in atmospheres with less than 100 ppm water is about 12,500 ksi. Two sets of experiments are used to study cracking directly during thermal excursions: one determines the minimum temperature (Tc) at which cracks first appear during a single heating cycle and the other involves rapid thermal cycling (RTC) between fixed T max and T min values. Fatigue models for describing initiation of the first crack and the development of multiple cracking are presented, which can be used as the basis for prediction of LEO cracking.

Mcclung, R. C.↗

Tensile strain measurements of ceramic fibers using scanning laser acoustic microscopy

A noncontacting technique using scanning laser acoustic microscopy for making in situ tensile strain measurements of small diameter fibers was implemented for the tensile strain analysis of individual Nicalon SiC fibers (nominal diameter 15 microns). Stress vs strain curves for the fibers were plotted from the experimental data. The mean elastic modulus of the fibers was determined to be 185.3 GPa. Similar measurements were made for Carborundum SiC fibers (nominal diameter 28 microns) and Saphikon sapphire fibers (nominal diameter 140 microns).

Kent, Renee M.↗

Discontinuously reinforced intermetallic matrix composites via XD synthesis

A review is given of recent results obtained for discontinuously reinforced intermetallic matrix composites produced using the XD process. Intermetallic matrices investigated include NiAl, multiphase NiAl + Ni2AlTi, CoAl, near-gamma titanium aluminides, and Ll2 trialuminides containing minor amounts of second phase. Such mechanical properties as low and high temperature strength, compressive and tensile creep, elastic modulus, ambient ductility, and fracture toughness are discussed as functions of reinforcement size, shape, and volume fraction. Microstructures before and after deformation are examined and correlated with measured properties. An observation of interest in many of the systems examined is 'dispersion weakening' at high temperatures and high strain rates. This behavior is not specific to the XD process; rather similar observations have been reported in other discontinuous composites. Proposed mechanisms for this behavior are presented.

Kumar, K. S.↗