At least 343 records · Page 19

Spatiotemporal mapping of microscopic strains and defects to reveal Li-dendrite-induced failure in all-solid-state batteries

Solid-state electrolytes (SSEs) are key to the success and reliability of all-solid-state lithium batteries, potentially enabling improvements in terms of safety and energy density over state-of-the-art lithium-ion batteries. However, there are several critical challenges to their implementation, including the interfacial instability stemming from the dynamic interaction of as-formed dendritic lithium during cycling. Here, we emphasize the importance of studying the spatial distribution and temporal evolution of strains and defects in crystalline solid-state electrolytes at the micro-scale, and how this affects dendrite growth. A proof-of-principle study is demonstrated using the synchrotron radiation based micro Laue X-ray diffraction method, and a custom-developed in-situ cycling device. Defects and residual strains are mapped, and the evolution of intragranular misorientation is observed. The feasibility of using this technique is discussed, and recommendations for micro-strain engineering to address the Li/SSEs interfacial issues are given. Additionally, work directions are pointed out with the consideration of combining multi-techniques for “poly-therapy”.

36 MATERIALS SCIENCE↗

Sulfur Solutions: Advancing High Voltage and High Energy Lithium Batteries with Organosulfur Electrolytes

Achieving energy densities exceeding 350 Wh kg -1 while operating at elevated voltages (>4.5 V vs Li/Li + ) is attainable through judicious selection of electrochemical pairs at the cathode and anode. However, current state-of-the-art electrolytes exhibit limited stability when exposed to systems operating at or above 4.3 V. This limitation contributes to the degradation of electrode materials and raises critical safety concerns, impeding the commercialization of such systems. Consequently, there has been a notable surge in research efforts aimed at developing innovative electrolyte compositions capable of supporting high-voltage lithium-ion batteries (LIBs). A substantial portion of this research has focused on the family of organosulfur molecules, which possess high oxidative stability. Organosulfur salts also facilitate the formation of dense, ionically conductive solid electrolyte interfaces (SEI) and demonstrate excellent solubility. This article provides a comprehensive overview of the field of organosulfur electrolyte components for their applications in energy storage, encompassing solvents, alternative conducting salts, and additives. It emphasizes the idea that the deliberate design of electrolyte compositions is instrumental in controlling electrode passivation, with organosulfur-based structures historically proving advantageous in every aspect of the electrolyte. Crucially, it should be noted that many of these components are commercially available, holding significant implications for industrial applications.

25 ENERGY STORAGE↗

All‐Solid‐State Lithium–Sulfur Batteries of High Cycling Stability and Rate Capability Enabled by a Self‐Lithiated Sn‐C Interlayer

Abstract All‐solid‐state lithium–sulfur batteries (ASSLSBs) have attracted intense interest due to their high theoretical energy density and intrinsic safety. However, constructing durable lithium (Li) metal anodes with high cycling efficiency in ASSLSBs remains challenging due to poor interface stability. Here, a compositionally stable, self‐lithiated tin (Sn)‐carbon (C) composite interlayer (LSCI) between Li anode and solid‐state electrolyte (SSE), capable of homogenizing Li‐ion transport across the interlayer, mitigating decomposition of SSE, and enhancing electrochemical/structural stability of interface, is developed for ASSLSBs. The LSCI‐mediated Li metal anode enables stable Li plating/stripping over 7000 h without Li dendrite penetration. The ASSLSBs equipped with LSCI thus exhibit excellent cycling stability of over 300 cycles (capacity retention of ≈80%) under low applied pressure (<8 MPa) and demonstrate improved rate capability even at 3C. The enhanced electrochemical performance and corresponding insights of the designed LSCI broaden the spectrum of advanced interlayers for interface manipulation, advancing the practical application of ASSLSBs.

Ye, Lei↗

Degradation of Lithium Iron Phosphate Sulfide Solid-State Batteries by Conductive Interfaces

The superionic solid-state argyrodite electrolyte Li 6 PS 5 Br can improve lithium and lithium-ion batteries' safety and energy density. Despite many reports validating the conductivity of this electrolyte, it still suffers from passivating electrode degradation mechanisms. At first analysis, lithium iron phosphate (LFP) should be more thermodynamically stable in contact with sulfide electrolytes. However, without substantial improvements to interfacial engineering, we find that LFP is not inherently stable against Li 6 PS 5 Br. We hypothesize argyrodite oxidation favorably competes with LFPAs delithiation, insulating the electrolyte-electrode interface and causing large overpotential losses. We show that compared to LiNi x Mn y Co z O 2 , LFP has no actual electrochemical stability advantage despite operating at a lower voltage. We utilize tender energy XAS and XPS to show that chemical reactions occur between LFP and the Li 6 PS 5 Br solid electrolyte and these reactions are exacerbated by cycling. We also show that electrochemical degradation occurs at the interface between the solid electrolyte ion conductor and any electron conductor, namely the active material and carbon additives. We further demonstrate that LiNbO 3 cathode coatings on LFP can delay electrochemical degradation by electronically insulating the LFP-sulfide electrolyte interface but not prevent its occurrence at the carbon-electrolyte interface.

25 ENERGY STORAGE↗

Chemo-Mechanical Behavior and Stability of High-Loading Cathodes in Solid-State Batteries

Solid-state batteries can offer higher energy density and improved safety compared to lithium ion batteries, which use flammable liquid electrolytes. Increasing the ratio of cathode active materials in composite cathodes enhances the energy density and reduces manufacturing costs. Changes in the ratio of cathode active materials alter the microstructure and chemo-mechanical response of a cathode during operation. Understanding the relationship between composition, microstructure, and chemo-mechanical interactions is critical for optimizing solid-state cathodes. Here, in this study, we engineered composite cathodes with varying ratios of LiNi 0.8 Co 0.1 Mn 0.1 O 2 and Li 6 PS 5 Cl to systematically investigate the role of microstructural evolution in long-term chemo-mechanical transformations. Chemo-mechanical stresses resulting from the volume changes of the cathode active materials led to degradation mechanisms, such as fracture and interfacial delamination. Active material fracture and delamination led to underutilization of active material and significant capacity decay during cycling. Coatings that suppress active material-active material interactions during cycling may aid in suppressing the generation of local stress hotspots.

36 MATERIALS SCIENCE↗

Understanding the Reactivity of a Thin Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 Solid–State Electrolyte toward Metallic Lithium Anode

The thickness of solid-state electrolytes (SSEs) significantly affects the energy density and safety performance of all-solid-state lithium batteries. However, a sufficient understanding of the reactivity toward lithium metal of ultrathin SSEs (<100 μm) based on NASICON remains lacking. Herein, for the first time, a self-standing and ultrathin (70 μm) NASICON-type Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 (LAGP) electrolyte via a scalable solution process is developed, and X-ray photoelectron spectroscopy reveals that changes in LAGP at the metastable Li-LAGP interface during battery operation is temperature dependent. Severe germanium reduction and decrease in LAGP particle size are detected at the Li-LAGP interface at elevated temperature. As a result, oriented plating of lithium metal on its preferred (110) face occurs during in situ X-ray diffraction cycling.

25 ENERGY STORAGE↗

Determination of the structure of lithium niobosilicate glasses by molecular dynamics simulation with a new Nb-O potential

A partial charge empirical potential for the Nb-O pair has been developed based on existing parameters of other pairs in a Teter potential to enable molecular dynamics simulations of both lithium niobate crystal and lithium niobosilicate glasses. The developed potential is capable of describing structural features of lithium niobosilicate glasses in a wide composition range, including niobium coordination number and bond length, density, bond angle distribution, polyhedral distribution and fraction of bridging oxygen. Furthermore, the results obtained using this new potential show good agreement with experimental data of density and structure from Raman spectroscopy of lithium niobosilicate glasses and X-ray absorption spectroscopy near Nb K-edge.

36 MATERIALS SCIENCE↗

Large Local Currents in a Lithium-Ion Battery during Rest after Fast Charging

Increasing electric vehicle (EV) adoption requires lithium-ion batteries that can be charged quickly and safely. Some EV batteries have caught on fire despite being neither charged nor discharged. While the lithium that plates on graphite during fast charging affects battery safety, so do the internal ionic currents that can occur when the battery is at rest after charging. These currents are difficult to quantify; the external current that can readily be measured is zero. Here we study a graphite electrode at rest after 6C fast charging using operando X-ray microtomography. We quantify spatially resolved current density distributions that originate at plated lithium and end in underlithiated graphite particles. The average current densities decrease from 1.5 to 0.5 mA cm -2 in about 20 min after charging is stopped. Surprisingly, the range of the stripping current density is independent of time, with outliers above 20 mA cm -2 . In conclusion, the persistence of outliers provides a clue as to the origin of catastrophic failure in batteries at rest.

25 ENERGY STORAGE↗

Li 8 MnO 6 : A Novel Cathode Material with Only Anionic Redox

In Li-excess transition-metal-oxide cathode materials, anionic oxygen redox can offer high capacity and high voltages, although peroxo and superoxo species may cause oxygen loss, poor cycling performance, and capacity fading. Previous work showed that undesirable formation of peroxide and superoxide bonds is controlled to some extent by Mn substitution, and the present work uses density functional calculations to examine the reasons for this by studying the anionic redox mechanism Li 8 MnO 6 . This material is obtained by substituting Mn for Sn in Li 8 SnO 6 or for Zr in Li 8 ZrO 6 , and we also compare to previous work on those materials. The calculations predict that Li 8 MnO 6 is stable at room temperature (with a band gap of 3.19 eV as calculated HSE06 and 1.82 eV as calculated with the less reliable with PBE+U), and they elucidate the chemical and structural effects involved in the inhibition of oxygen release in this cathode. Throughout the whole delithiation process, only O 2- ions are oxidized. The directional Mn-O bonds formed from unfilled 3d orbitals effectively inhibit the formation of O-O bonds, and the layered structure is maintained even after removing 3 Li per Li 8 MnO 6 formula unit. The calculated average voltage for removal of 3 Li is 3.69 V by HSE06, and the corresponding capacity is 389 mAh/g. The high voltage of oxygen anionic redox and the high capacity result in a high energy density of 1436 Wh/kg. The Li-ion diffusion barrier for the dominant interlayer diffusion path along the c-axis is 0.57 eV by PBE+U. Finally, these results help us to understand the oxygen redox mechanism in a new lithium-rich Li 8 MnO 6 cathode material and contribute to the design of high-energy-density lithium-ion-battery cathode materials with favorable electrochemical properties based on anionic oxygen redox.

Li8MnO6↗

A multiscale model to understand the interface chemistry, contacts, and dynamics during lithium stripping

A reversible Li-metal electrode, paired with a solid electrolyte, is critical for attaining higher energy density and safer batteries beyond the current lithium-ion cells. A stable stripping process may be even harder to attain as the stripping process will remove Li-atoms from the surface, and naturally reduce surface contact area, if not self-corrected by other mechanisms, such as diffusion and plastic deformation under an applied external stack pressure. Here, we capture these mechanisms occurring at multiple length- and time- scales, i.e., interface interactions, vacancy hopping, and plastic deformation, by integrating density functional theory (DFT) simulations, kinetic Monte Carlo (KMC), and continuum finite element method (FEM). By assuming the self-affine nature of multiscale contacts, we predict the steady-state contact area as a function of stripping current density, interface wettability, and stack pressure. We further estimate the exponential increase of overpotential due to contact area loss to maintain the same stripping current density. We demonstrate that a lithiophilic interface requires less stack pressure to reach the same steady-state contact area fraction than a lithiophobic interface. A “tolerable steady-state” contact area loss for maintaining stable stripping is estimated at 20 %, corresponding to a 10 % increase in overpotential. To constrain contact loss within the tolerance, the required stack pressure is 0.1, 0.5, and 2 times the yield strength of lithium metal for three distinct interfaces, lithiophilic Li/lithium oxide(Li2O), Li/lithium lanthanum zirconium oxide(LLZO), and lithiophoblic Li/lithium fluoride(LiF), respectively. The modeling results agree with experiments on the impact of the stack pressure quantitatively, while the discrepancy in stripping rate sensitivity is attributed to the simplifying interface interaction in our simulations. Overall, this multiscale simulation framework demonstrates the importance of electrochemical-mechanical coupling in understanding the dynamics of the Li/SE interface during stripping.

Feng, Min↗

A polymeric composite protective layer for stable Li metal anodes

Lithium (Li) metal is a promising anode for high-performance secondary lithium batteries with high energy density due to its highest theoretical specific capacity and lowest electrochemical potential among anode materials. However, the dendritic growth and detrimental reactions with electrolyte during Li plating raise safety concerns and lead to premature failure. Herein, we report that a homogeneous nanocomposite protective layer, prepared by uniformly dispersing AlPO 4 nanoparticles into the vinylidene fluoride-co-hexafluoropropylene matrix, can effectively prevent dendrite growth and lead to superior cycling performance due to synergistic influence of homogeneous Li plating and electronic insulation of polymeric layer. The results reveal that the protected Li anode is able to sustain repeated Li plating/stripping for >750 cycles under a high current density of 3 mA cm -2 and under a practical specific capacity of 2 mAh cm -2 . Moreover, full-cell Li-ion battery is constructed by using LiFePO 4 and protected Li as a cathode and anode, respectively, rendering a stable capacity after 400 charge/discharge cycles. The current work presents a promising approach to stabilize Li metal anodes for next-generation Li secondary batteries.

25 ENERGY STORAGE↗

Thermal runaway mechanism of lithium-ion battery with LiNi 0.8 Mn 0.1 Co 0.1 O 2 cathode materials

Battery safety is critical to the application of lithium-ion batteries, especially for high energy density battery applied in electric vehicles. In this paper, the thermal runaway mechanism of LiNi 0.8 Co 0.1 Mn 0.1 O 2 based lithium-ion battery is illustrated. And the reaction between cathode and flammable electrolyte is proved as the trigger of the thermal runaway accident. In detail, with differential scanning calorimeter tests for battery components, the material combination contributing to thermal runaway was decoupled. Characterization with synchrotron X-ray diffraction and transmission electron microscopy with in-situ heating proved that the vigorous exothermic reaction is initiated by the liberated oxygen species. The pulse of highly active oxygen species reacted quickly with the electrolyte, accompanied with tremendous heat release, which accelerated the phase transformation of charged cathode. Also, the mechanism is verified by a confirmatory experiment when the highly active oxygen species were trapped by anion receptor, the phase transformation of the charged cathode was inhibited. Clarifying the thermal runaway mechanism of LiNi 0.8 Co 0.1 Mn 0.1 based lithium-ion battery may light the way to battery chemistries of both high energy density and high safety.

25 ENERGY STORAGE↗

Working Principle of an Ionic Liquid Interlayer During Pressureless Lithium Stripping on Li 6.25 Al 0.25 La 3 Zr 2 O 12 (LLZO) Garnet‐Type Solid Electrolyte

Abstract Solid‐state‐batteries employing lithium metal anodes promise high theoretical energy and power densities. However, morphological instability occurring at the lithium/solid–electrolyte interface when stripping and plating lithium during cell cycling needs to be mitigated. Vacancy diffusion in lithium metal is not sufficiently fast to prevent pore formation at the interface above a certain current density during stripping. Applied pressure of several MPa can prevent pore formation, but this is not conducive to practical application. This work investigates the concept of ionic liquids as “self‐adjusting” interlayers to compensate morphological changes of the lithium anode while avoiding the use of external pressure. A clear improvement of the lithium dissolution process is observed as it is possible to continuously strip more than 70 μm lithium (i. e., 15 mAh cm −2 charge) without the need for external pressure during assembly and electrochemical testing of the system. The impedance of the investigated electrodes is analyzed in detail, and contributions of the different interfaces are evaluated. The conclusions are corroborated with morphology studies using cryo‐FIB‐SEM and chemical analysis using XPS. This improves the understanding of the impedance response and lithium stripping in electrodes employing liquid interlayers, acting as a stepping‐stone for future optimization.

Fuchs, Till↗

Investigation of Structure and Transport in Li-Doped Ionic Liquid Electrolytes: [pyr14][TFSI], [pyr13][FSI] and [EMIM][BF4]

Ionic liquid electrolytes have been proposed as a means of improving the safety and cycling behavior of advanced lithium batteries; however, the properties of these electrolytes under high lithium doping are poorly understood. Here, we employ both polarizable molecular dynamics simulation and experiment to investigate the structure, thermodynamics and transport of three potential electrolytes, N-methyl-Nbutylpyrrolidinium bis(trifluoromethylsufonyl)imide ([pyr14][TFSI]), N- methyl-Npropylpyrrolidinium bis(fluorosufonyl)imide ([pyr13][FSI]), and 1-ethyl-3-- methylimidazolium boron tetrafluoride ([EMIM][BF4]), as a function of Li-salt concentration and temperature. Structurally, Li(+) is shown to be solvated by three anion neighbors in [pyr14][TFSI] and four anion neighbors in both [pyr13][FSI] and [EMIM][BF4], and at all levels of x(sub Li) we find the presence of lithium aggregates. Furthermore, the computed density, diffusion, viscosity, and ionic conductivity show excellent agreement with experimental data. While the diffusion and viscosity exhibit a systematic decrease and increase, respectively, with increasing x(sub Li), the contribution of Li(+) to ionic conductivity increases until reaching a saturation doping level of x(sub Li) is approximately 0.10. Comparatively, the Li(+) conductivity of [pyr14][TFSI] is an order of magnitude lower than that of the other liquids, which range between 0.1 - 0.3 mS/cm. The differences in Li(+) transport are reflected in the residence times of Li(+) with the anions, which are revealed to be much larger for [pyr14][TFSI] (up to 100 ns at the highest doping levels) than in either [EMIM][BF4] or [pyr13][FSI]. Finally, we comment on the relative kinetics of Li(+) transport in each liquid and we present strong evidence for transport through anion exchange (hopping) as opposed to the net motion of Li(+) with its solvation shell (vehicular).

lithium batteries↗

The Pulsed Fission-Fusion (PUFF) Concept for Deep Space Exploration and Terrestrial Power Generation

This team is exploring a modified Z-pinch geometry as a propulsion system, imploding a liner of liquid lithium onto a pellet containing both fission and fusion fuel. The plasma resulting from the fission and fusion burn expands against a magnetic nozzle, for propulsion, or a magnetic confinement system, for terrestrial power generation. There is considerable synergy in the concept; the lithium acts as a temporary virtual cathode, and adds reaction mass for propulsion. Further, the lithium acts as a radiation shield against generated neutrons and gamma rays. Finally, the density profile of the column can be tailored using the lithium sheath. Recent theoretical and experimental developments (e.g. tailored density profile in the fuel injection, shear stabilization, and magnetic shear stabilization) have had great success in mitigating instabilities that have plagued previous fusion efforts. This paper will review the work in evaluating the pellet sizes and z-pinch conditions for optimal PuFF propulsion. Trades of pellet size and composition with z-pinch power levels and conditions for the tamper and lithium implosion are evaluated. Current models, both theoretical and computational, show that a z-pinch can ignite a small (~1 cm radius) fission-fusion target with significant yield. Comparison is made between pure fission and boosted fission targets. Performance is shown for crewed spacecraft for high speed Mars round trip missions and near interstellar robotic missions. The PuFF concept also offers a solution for terrestrial power production. PuFF can, with recycling of the effluent, achieve near 100% burnup of fission fuel, providing a very attractive power source with minimal waste. The small size of PuFF relative to today's plants enables a more distributed power network and less exposure to natural or man-made disruptions.

Adams, Robert↗

Rational Design of Weakly‐Solvating Molecules for Salt‐In‐Pre‐Ionic‐Liquid Electrolytes for Li Metal Batteries

Lithium metal batteries (LMBs) promise step‐changes in energy densities but suffer from poor cycle life due to unstable electrolyte‐lithium interfaces. Conventional carbonate electrolytes exhibit excessive lithium‐ion solvation and low oxidative stability, leading to rapid capacity loss. Herein, we report a rationally designed weakly‐solvating cyclic sulfonamide, 1‐trifluoromethanesulfonyl)amide pyrrolidine (TFMSPyr), which integrates an electron‐withdrawing trifluoromethanesulfonyl functional group at pyrrolidinic‐N. TFMSPyr acts as a pre‐ionic‐liquid solvent that forms intrinsically localized, anion‐dominated solvation, coupling molecular architecture, solvation topology, and transport dynamics. As a result, LiFSI based salt‐in‐pre‐ionic‐liquid (SIPIL) electrolytes exhibit high lithium‐ion transference number, oxidative stability > 5 V versus Li/Li + and anion‐derived solid electrolyte interphases (SEI). Li||Cu cells with SIPIL deliver a first cycle Coulombic efficiency (CE) of ≈ 99% with average CE of 99.2% for 100 cycles, and lithium half‐cells with lithium iron phosphate (LFP) cathode exhibit 82% capacity retention after 400 cycles with CE of 99.98%. In anode‐free full cells, 95% of initial capacity is retained after 63 cycles with an average CE of 99.5%. These results demonstrate that molecular engineering of solvents offers a powerful pathway to stabilize lithium metal interfaces and enable practical Anodeless LMBs.

25 ENERGY STORAGE↗

Aligning lithium metal battery research and development across academia and industry

Successful integration of metallic lithium anodes into secondary batteries could enhance energy density and enable new forms of electrified transportation. However, the outlook for widespread lithium metal adoption in energy storage devices remains mixed. This comes in part from existing gaps in our understanding of the relationships connecting the initial state of lithium, its evolution with cycling, and end-of-life state. It remains important to develop standardized protocols for material and cell characterization, cycling performance, safety, and recycling procedures for lithium metal-based batteries. In February 2023 a cohort of scientists and engineers from academia, national laboratories, and industry gathered to converge on a list of critical challenges and action items to provide better understanding of lithium metal evolution and to enhance academic, governmental, and industrial partnerships to address these challenges. Here, we highlight the major discussion topics revolving around the manufacturing of lithium metal, its related metrology and integration into battery form factors, and best practices testing its electrochemical performance relevant to automotive applications. We introduce a power-controlled discharge testing protocol for research and development cells, in alignment between major automotive stakeholders, that may reveal lithium metal battery dynamics closer to practical driving behavior.

25 ENERGY STORAGE↗