At least 343 records · Page 19

Performance of Alumina-Forming Austenitic Steels, Fe-base and Ni-base alloys exposed to metal dusting environments

A series of conventional Fe- and Ni- base, chromia- and alumina- forming alloys, and a newly developed creep-resistant, alumina-forming austenitic steel were developed and its performance relative to conventional Fe- and Ni-based chromia-forming alloys was evaluated in metal dusting environments with a range of water vapor contents. Five 500h experiments have been performed at 650 C with different water vapor contents and total pressures. Without water vapor, the Ni-base alloys showed greater resistance to metal dusting than the Fe-base alloys, including AFA. However, with 10-28% water vapor, more protective behavior was observed with the higher-alloyed materials and only small mass changes were observed. Longer exposure times are in progress to further differentiate performance.

36 MATERIALS SCIENCE↗

Improvements in Low-Frequency, Ultrasonic Phased-Array Evaluation for Thick Section Cast Austenitic Stainless Steel Piping Components

Research is being conducted for the U.S. Nuclear Regulatory Commission (NRC) at the Pacific Northwest National Laboratory (PNNL) to assess the effectiveness and reliability of advanced nondestructive examination (NDE) methods for the inspection of light water reactor (LWR) components. A primary objective of this work is to evaluate various NDE methods to assess their ability to detect, localize, and size cracks in coarse-grained steel components. This particular study focused on the evaluation of custom-designed, low-frequency (500 kHz) phased-array (PA) probes for examining welds in thick-section cast austenitic stainless steel (CASS) piping. In addition, research was conducted to observe ultrasonic sound field propagation effects from known coarse-grained microstructures found in parent CASS material. The study was conducted on a variety of thick-wall, coarse-grained CASS specimens that were previously inspected by an older generation 500-kHz PA-UT probe and acquisition instrument configuration. This comparative study describes the impact of the new PA probe design on flaw detection and sizing in a low signal-to-noise environment. The set of Pressurized Water Reactor Owners Group (PWROG) CASS specimens examined in this study are greater than 50.8-mm (2.0-in.) thick with documented flaws and microstructures. These specimens are on loan to PNNL from the Electric Power Research Institute (EPRI) NDE Center in Charlotte, North Carolina. The flaws contained within these specimens are thermal fatigue cracks (TFC) or mechanical fatigue cracks (MFC) and range from 13% to 42% in through-wall extent. In addition, ultrasonic signal continuity was evaluated on two CASS parent material ring sections by examining the edge-of-pipe response (corner geometry) for regions of signal loss.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Phased Array Ultrasonic Sound Field Mapping through Large-Bore Coarse Grained Cast Austenitic Stainless Steel (CASS) Components

A sound field beam mapping exercise was conducted to assist in understanding the effects of coarse-grained microstructures found in cast austenitic stainless steel (CASS) materials on acoustic longitudinal wave propagation. Ultrasonic laboratory measurements were made on three specimens representing four different grain structures. Phased array (PA) probes were fixed on each specimen surface and excited in the longitudinal mode at specific angles while a point receiver was scanned in a raster pattern over the end of the specimen, generating a transmitted sound field image. Three probes operating at nominal frequencies of 0.5, 0.8, and 1.0 MHz were used. A 6.4 mm (0.25-in.) thick slice was removed from the specimen end and beam mapping was repeated three times, yielding four full sets of beam images. Data were collected both with a constant part path for each configuration (probe, specimen and slice, angle, etc.) and with a variable part path (fixed position on the surface). The base specimens and slices were then polished and etched to reveal measureable grain microstructures that were compared to the sound field interactions and scattering effects seen in the collected data.

cast austenitic stainless steel↗

Ultrasonic Sound Field Mapping Through Coarse Grained Cast Austenitic Stainless Steel Components

The Pacific Northwest National Laboratory (PNNL) has been involved with nondestructive examination (NDE) of coarse-grained cast austenitic stainless steel (CASS) components for over 30 years. More recent work has focused on mapping the ultrasonic sound fields generated by low-frequency phased array probes that are typically used for the evaluation of CASS materials for flaw detection and characterization. The casting process results in the formation of large grained material microstructures that are nonhomogeneous and anisotropic. The propagation of ultrasonic energy for examination of these materials results in scattering, partitioning and redirection of these sound fields. The work reported here provides an assessment of sound field formation in these materials and provides recommendations on ultrasonic inspection parameters for flaw detection in CASS components.

Ultrasonic, Phased Array, Cast Austenitic Stainles↗

Characterization of high performance austenitic and ODS alloys for SCWR conditions

High temperature oxidation resistance is of critical importance for the in-reactor components of the European supercritical water reactor (SCWR) concept. To consider candidate materials for this purpose, selected austenitic steels, iron based ODS (Oxide Dispersion Strengthened) alloys and one Ni alloy have been tested by exposure to supercritical water at 650 deg. C/25 MPa up to 2000 h. Results of observed mass change, oxide thickness and composition after exposure are shown and discussed regarding implications for long term oxidation performance. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Mesoscale Modeling of Dislocation Cell Structure Evolution and Radiation-Induced Segregation in Additively Manufactured Austenitic Stainless Steel

Structural alloys under irradiation develop radiation-induced segregation (RIS) at point defect sinks, which lead to undesired changes in the alloy's properties. Additively manufactured austenitic stainless steels are expected to yield a distinct response to irradiation damage owing to their unique as-printed dislocation cell structure. In this talk, we present the development of a mesoscale model for dislocation cell structure evolution coupled with RIS using the MOOSE framework. The evolution of network dislocations within spatially distinct cells and cell walls are modeled using climb-mediated edge annihilation and generation processes. Starting with initial microstructures of as-printed non-equilibrium segregations at dislocation cell walls, our 2D and 3D simulations explore the effects of irradiation temperature, dose rate, dislocation sink bias, and specimen thickness on microstructure evolution. The results will be compared against experimental characterizations of in-situ and ex-situ ion-irradiated samples, and the implications of evolving cell structure on irradiation damage response will be discussed.

additive manufacturing↗

Plastic Deformation Processes Accompanying Stress Corrosion Crack Propagation in Irradiated Austenitic Steels

During stress corrosion crack propagation, stress values in the crack tip vicinity often exceed material yield stress limit. Plastic deformation processes may accompany and influence cracking. Here, stress corrosion crack propagation and deformation mechanisms were investigated using EBSD analysis. The investigated material was 304L Ti-enriched austenitic stainless steel irradiated to 10.4 dpa at 320°C in the BOR-60 fast reactor. Crack growth tests were conducted in a simulated Normal Water Chemistry (NWC) environment in the temperature range 288–320 °C using compact tension specimens. By analyzing crack trajectory and grain structure in the crack vicinity, it was established that grain orientation with respect to the acting stress direction was not a key factor controlling crack propagation. No crystallographic orientation susceptible to cracking was identified. Also, EBSD analysis revealed strong inhomogeneity in plastic strain distribution along the crack path. Most crack-adjacent grains remained virtually strain-free whereas few grains experienced strong plastic strain. These areas were presumed to be “plastic bridges” or “ductile ligaments.”

Gussev, Maxim N↗

Increasing the Upper Temperature Oxidation Limit of Alumina Forming Austenitic Stainless Steels in Air with Water Vapor

A family of alumina-forming austenitic (AFA) stainless steels is under development for use in aggressive oxidizing conditions from {approx}600-900 C. These alloys exhibit promising mechanical properties but oxidation resistance in air with water vapor environments is currently limited to {approx}800 C due to a transition from external protective alumina scale formation to internal oxidation of aluminum with increasing temperature. The oxidation behavior of a series of AFA alloys was systematically studied as a function of Cr, Si, Al, C, and B additions in an effort to provide a basis to increase the upper-temperature oxidation limit. Oxidation exposures were conducted in air with 10% water vapor environments from 800-1000 C, with post oxidation characterization of the 900 C exposed samples by electron probe microanalysis (EPMA), scanning and transmission electron microscopy, and photo-stimulated luminescence spectroscopy (PSLS). Increased levels of Al, C, and B additions were found to increase the upper-temperature oxidation limit in air with water vapor to between 950 and 1000 C. These findings are discussed in terms of alloy microstructure and possible gettering of hydrogen from water vapor at second phase carbide and boride precipitates.

08 HYDROGEN↗

Development of 1100 °C Capable Alumina-Forming Austenitic Alloys

Recently dalumina-forming austenitic (AFA) alloys based on ~12–32 weight % (wt%) Ni have been developed and offer an attractive combination of oxidation resistance and creep resistance at relatively low alloy cost. But, they exhibit a transition to internal oxidation and nitridation of Al above ~750–950 °C depending on composition and exposure environment. In order to identify AFA compositions capable of higher-temperature operation for applications such as ethylene cracking, the oxidation behavior of a series of developmental, as-cast nominal Fe–(25–45)Ni–(10–25)Cr–(4–5)Al–1Si–0.15Hf–0.07Y–0.01B wt% base alloys with and without Nb, Ti, and C additions was evaluated at 1100 °C in air with 10% water vapor. Furthermore, we observed protective alumina scale formation at levels of 35Ni, 25Cr, and 4Al with additions of Nb and C, indicating promise for 1100°C capable cast AFA alloys.

36 MATERIALS SCIENCE↗

Fireside Corrosion of Alumina-Forming Austenitic (AFA) Stainless Steels

Here, the performance of four alumina-forming austenitic alloys was tested in simulative fireside corrosion atmospheres. The alloys were exposed at 700 °C to gas atmospheres of oxygen with varying amounts of SO 2 with two deposits, one which contained Na 2 SO 4 /K 2 SO 4 /Fe 2 O 3 in a 1.5:1.5:1.0 molar ratio (SCM) and the other Na 2 SO 4 /K 2 SO 4 in a 1:1 molar ratio (M1). The specimens were placed into alumina crucibles and submerged halfway in the powder deposits. Corrosion first initiated in the region where the deposit was thinnest. In the SCM, most alloys exhibited two-stage kinetics: an initiation stage during which degradation was slow followed by a propagation stage during which degradation was rapid. Exposures in the SCM deposit showed a significant effect of alloy composition and microstructure. In the as-processed state, OC4 suffered severe scale spallation and was not protective, while OC8, which contains a higher Cr content, remained protective. The exposures with the various microstructures indicate the significance of the factor on fireside corrosion. The OC8 alloy was extremely resistant in the as-processed state but was rapidly degraded when the microstructure had been equilibrated prior to exposure. Conversely, the OCS and OCT alloys, which were borderline in the as-processed state were quite resistant after their microstructures had been equilibrated. The results indicate that corrosion resistance in these environments comes from alumina, but the alloys need more Cr and in a very accessible microstructure location to get the third-element effect to promote the alumina. The weight changes and the amount of degradation were more severe with M1 than with the SCM. Furthermore, there was more corrosion when the alkali iron trisulfates must be formed from a thermally grown iron oxide scale, than when the iron oxide was already in the deposit. In the latter case, the rate of degradation by “synergistic fluxing” was reduced.

36 MATERIALS SCIENCE↗

Effect of alloying additions on phase equilibria and creep resistance of alumina-forming austenitic stainless steels

The high-temperature creep properties of a series of alumina-forming austenitic (AFA) stainless steels based on Fe-20Ni-(12-14)Cr-(2.5-4)Al-(0.2-3.3)Nb-0.1C (weight percent) were studied. Computational thermodynamics were used to aid in the interpretation of data on microstructural stability, phase equilibria, and creep resistance. Phases of MC (M: mainly Nb), M{sub 23}C{sub 6} (M: mainly Cr), B2 [{beta}-(Ni,Fe)Al], and Laves [Fe{sub 2}(Mo,Nb)] were observed after creep-rupture testing at 750 C and 170 MPa; this was generally consistent with the thermodynamic calculations. The creep resistance increased with increasing Nb additions up to 1 wt pct in the 2.5 and 3 Al wt pct alloy series, due to the stabilization of nanoscale MC particles relative to M{sub 23}C{sub 6}. Additions of Nb greater than 1 wt pct decreased creep resistance in the alloy series due to stabilization of the Laves phase and increased amounts of undissolved, coarse MC, which effectively reduced the precipitation of nanoscale MC particles. The additions of Al also increased the creep resistance moderately due to the increase in the volume fraction of B2 phase precipitates. Calculations suggested that optimum creep resistance would be achieved at approximately 1.5 wt pct Nb in the 4 wt pct Al alloy series.

36 MATERIALS SCIENCE↗

Interrogating the Effects of Hydrogen on the Behavior of Planar Deformation Bands in Austenitic Stainless Steel

The effects of internal hydrogen on the deformation microstructures of 304L austenitic stainless steel have been characterized using electron backscattered diffraction (EBSD), transmission Kikuchi diffraction (TKD), high-resolution scanning transmission electron microscopy (HRSTEM), and nanoprobe diffraction. Samples, both thermally precharged with hydrogen and without thermal precharging, were subjected to tensile deformation of 5 and 20 pct true strain followed by multiple microscopic interrogations. Internal hydrogen produced widespread stacking faults within the as-forged initially unstrained material. While planar deformation bands developed with tensile strain in both the hydrogen-precharged and non-precharged material, the character of these bands changed with the presence of internal hydrogen. As shown by nanobeam diffraction and HRSTEM observations, in the absence of internal hydrogen, the bands were predominantly composed of twins, whereas for samples deformed in the presence of internal hydrogen, ε -martensite became more pronounced and the density of deformation bands increased. For the 20 pct strain condition, α '-martensite was observed at the intersection of ε -martensite bands in hydrogen-precharged samples, whereas in non-precharged samples α '-martensite was only observed along grain boundaries. We hypothesize that the increased prevalence of α '-martensite is a secondary effect of increased ε -martensite and deformation band density due to internal hydrogen and is not a signature of internal hydrogen itself.

36 MATERIALS SCIENCE↗

Comparative Analysis of Austenitized Steel Microstructures Due to Induction and Conventional Heating in High Magnetic Field

While magnetic field-assisted processing shows promise in improving alloys’ mechanical properties, insufficient descriptions of heating methods hinder development of tailored processing pathways. This study investigates how induction and conventional heating affect microstructures of near-eutectoid Fe–C steel with and without 9 T magnetic field. Conventionally heated samples in field showed more austenite grain growth compared to inductively heated counterparts. Annealing twin frequency increased under field, with twin density increases not fully explained by larger grain sizes.

Hurley, Megan [University of Florida, Gainesville]↗

Improving Corrosion Resistance of 316L Austenitic Stainless Steel Using ZrO{sub 2} Sol-Gel Coating in Nitric Acid Solution

In this study, thin-film coating of zirconium oxide (ZrO{sub 2}) was prepared by sol-gel method and subsequent heat treatment process. The sol was prepared by controlled hydrolysis of zirconium tetrapropoxide using acetic acid and ethanol/acetylacetone mixture as catalyst and chelating agent, respectively, and finally deposited onto the 316L austenitic stainless steel (316L SS) using dip coating method in order to improve its corrosion resistance in nitric acid medium. The composition, structure, and morphology of the coated surface were investigated by x-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM), and atomic force microscopy (AFM). The obtained results from XRD and FTIR state the formation of tetragonal and monoclinic ZrO{sub 2} phase. Also, the obtained results from surface morphology investigation by SEM and AFM indicate the formation of smooth, homogeneous and uniform coatings on the steel substrate. Then, the corrosion behavior of stainless steel was investigated in a 1 and 10 M nitric acid solutions using electrochemical impedance spectroscopy and linear polarization test. The obtained results from these tests for ZrO{sub 2}-coated specimens indicated a considerable improvement in the corrosion resistance of 316L stainless steel by an increase in corrosion potential and transpassive potential, and a decrease in passive current density and corrosion current density. The decrease in passive current density in both the concentration of solutions was two orders of magnitude from bare to coated specimens.

36 MATERIALS SCIENCE↗

Tensile Deformation Temperature Impact on Microstructure and Mechanical Properties of AISI 316LN Austenitic Stainless Steel

Uniaxial tensile tests were conducted on AISI 316LN austenitic stainless steel from − 40 to 300 °C at a rate of 0.5 mm/min. Microstructure and mechanical properties of the deformed steel were investigated by optical, scanning and transmission electron microscopies, x-ray diffraction, and microhardness testing. The yield strength, ultimate tensile strength, elongation, and microhardness increase with the decrease in the test temperature. The tensile fracture morphology has the dimple rupture feature after low-temperature deformations and turns to a mixture of transgranular fracture and dimple fracture after high-temperature ones. The dominating deformation microstructure evolves from dislocation tangle/slip bands to large deformation twins/slip bands with temperature decrease. The deformation-induced martensite transformation can only be realized at low temperature, and its quantity increases with the decrease in the temperature.

36 MATERIALS SCIENCE↗

Effect of Boron Content on Hot Ductility and Hot Cracking Susceptibility in 316L Austenitic Stainless Steel for Welding Components

Liquation cracking may occur in the heat-affected zone during welding. Two factors influence this phenomenon: the tensile stresses generated during welding and the potential loss of ductility due to the presence of a liquid film at grain boundaries depending on their chemical composition. Gleeble hot ductility tests have been used to study the combined effect of boron content and holding time on ductility drop in the liquation temperature range of a 316L type austenitic stainless steel. It is shown that high boron contents and short holding times promote the loss of ductility in this temperature range. Secondary ion mass spectrometry has been used to correlate mechanical results to boron distribution either at grain boundaries or in the bulk. Other welding tests have been performed to confirm the influence of boron content on hot cracking sensitivity of AISI 316L stainless steels. Results indicate that cracks appear on all specimens but at different strain levels. The higher the boron content is, the more the specimen exhibits tendency to hot cracking.

36 MATERIALS SCIENCE↗

Effect of Aluminizing on the High-Temperature Oxidation Behavior of an Alumina-Forming Austenitic Stainless Steel

Due to their excellent oxidation resistance and creep resistance at elevated temperatures, alumina forming austenitic (AFA) stainless steels have emerged as potential alloys for high temperature applications. In this study, a Reactive Air Aluminizing (RAA) method was used to aluminize the surface of AFA25 stainless steel. The high temperature oxidation behavior of both as-received and aluminized AFA25 was investigated at 850 °C in dry air. The mass gain per unit area was higher for the aluminized AFA25 than for the as-received material. X-ray diffraction (XRD) analysis, scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDXS), performed on the oxide scales following the high temperature oxidation tests, confirmed the formation of alumina scale on both as-received and aluminized AFA. However, the aluminized alloy exhibited a thicker alumina scale on the surface, as well as more extensive penetration of the scale into the subsurface region of the alloy.

Rashidi, S.↗