At least 343 records · Page 19

Creep and Creep-Fatigue of Alloy 617 Weldments

Alloy 617 is the primary candidate material for the heat exchanger of a very high temperature gas cooled reactor intended to operate up to 950°C. While this alloy is currently qualified in the ASME Boiler and Pressure Vessel Code for non-nuclear construction, it is not currently allowed for use in nuclear designs. A draft Code Case to qualify Alloy 617 for nuclear pressure boundary applications was submitted in 1992, but was withdrawn prior to approval. Prior to withdrawal of the draft, comments were received indicating that there was insufficient knowledge of the creep and creep-fatigue behavior of Alloy 617 welds. In this report the results of recent experiments and analysis of the creep-rupture behavior of Alloy 617 welds prepared using the gas tungsten arc process with Alloy 617 filler wire. Low cycle fatigue and creep-fatigue properties of weldments are also discussed. The experiments cover a range of temperatures from 750 to 1000°C to support development of a new Code Case to qualify the material for elevated temperature nuclear design. Properties of the welded material are compared to results of extensive characterization of solution annealed plate base metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Bending fatigue of electron-beam-welded foils. Application to a hydrodynamic air bearing in the Chrysler/DOE upgraded automotive gas tubine engine

A hydrodynamic air bearing with a compliment surface is used in the gas generator of an upgraded automotive gas turbine engine. In the prototype design, the compliant surface is a thin foil spot welded at one end to the bearing cartridge. During operation, the foil failed along the line of spot welds which acted as a series of stress concentrators. Because of its higher degree of geometric uniformity, electron beam welding of the foil was selected as an alternative to spot welding. Room temperature bending fatigue tests were conducted to determine the fatigue resistance of the electron beam welded foils. Equations were determined relating cycles to crack initiation and cycles to failure to nominal total strain range. A scaling procedure is presented for estimating the reduction in cyclic life when the foil is at its normal operating temperature of 260 C (500 F).

Saltsman, J. F.↗

Hot-cracking studies of Inconel 718 weld- heat-affected zones

Hot ductility tests, gas-tungsten-arc fillerless fusion tests, and circle patch-weld-restraint tests were conducted on Inconel 718 to better understand and correlate the weldability /resistance to hot cracking/ of the alloy. A correlation of the test results with composition, heat-treat condition, grain size, and microstructure was made.

Thompson, E. G.↗

Effect of Welding Processes on the Microstructure, Mechanical Properties and Residual Stresses of Plain 9Cr-1Mo Steel Weld Joints

9Cr-1Mo steel designated as P9 is widely used in the construction of power plants and high-temperature applications. It is chosen for fabricating hexcan fuel subassembly wrapper components of fast breeder reactors. Arc welding processes are generally used for fabricating 9Cr-1Mo steel weld joints. A-TIG welding process is increasingly being adopted by the industries. In the present study, shielded metal arc (SMA), tungsten inert gas (TIG) and A-TIG welding processes are used for fabricating the 9Cr-1Mo steel weld joints of 10 mm thickness. Effect of the above welding processes on the microstructure evolution, mechanical properties and residual stresses of the weld joints has been studied in detail. All the three weld joints exhibited comparable strength and ductility values. 9Cr-1Mo steel weld joint fabricated by SMAW process exhibited lower impact toughness values caused by coarser grain size and inclusions. 9Cr-1Mo steel weld joint fabricated by TIG welding exhibited higher toughness due to finer grain size, while the weld joint fabricated by A-TIG welding process exhibited adequate toughness values. SMA steel weld joint exhibited compressive residual stresses in the weld metal and HAZ, while TIG and A-TIG weld joint exhibited tensile residual stresses in the weld metal and HAZ.

36 MATERIALS SCIENCE↗

2017 Accomplishments – Tritium Aging Studies on Stainless Steel Weldments and Heat-Affected Zones

In this study, the combined effects tritium and decay helium in forged and welded Types 304L and 21-6-9 stainless steels were studied. To measure these effects, fracture mechanic specimens were thermally precharged with tritium and aged for approximately 17 years to build in decay helium from tritium decay prior to testing. The results are compared to earlier measurements on the same alloys and weldments (4-5, 8-9). In support of Enhanced Surveillance, “Tritium Effects on Materials”, the fracture toughness properties of long-aged tritium-charged stainless-steel base metals and weldments were measured and compared to earlier measurements. The fracture-toughness data were measured by thermally precharging as-forged and as-welded specimens with tritium gas at 34.5 MPa and 350°C and aging for approximately 17 years to build-in decay helium prior to testing. These data result from the longest aged specimens ever tested in the history of the tritium effects programs at Savannah River and the fracture toughness values measured were the lowest ever recorded for tritium-exposed stainless steel. For Type 21-6-9 stainless steel, fracture toughness values were reduced to less than 2-4% of the as-forged values to 41 lbs / in specimens that contained more than 1300 appm helium from tritium decay. The fracture toughness properties of long-aged weldments were also measured. The fracture toughness reductions were not as severe because the specimens did not retain as much tritium from the charging and aging as did the base metals. For Type 304L weldments, the specimens in this study contained approximately 600 appm helium and their fracture toughness values averaged 750 lbs / in. The results for other steels and weldments are reported and additional tests will be conducted during FY18.

36 MATERIALS SCIENCE↗

Reduction of porosity in aluminum weldments

Method is described for elimination of porosity of aluminum weldments by replacing polyvinyl chloride tubing (used to connect welder to gas source, and is permeable to moisture at high humidity) with copper tubing. In addition liquid argon gas is used at weld stations.

Lee, W. S.↗

Fabrication of experimental three-meter space telescope primary and secondary mirror support structure

The fabrication of prototype titanium alloy primary and secondary mirror support structures for a proposed experimental three-meter space telescope is discussed. The structure was fabricated entirely of Ti-6Al-4V tubing and plate. Fabrication included the development of procedures including welding, forming, and machining. Most of the structures was fabricated by gas-shielding tungsten-arc (GTA) welding with several major components fabricated by high frequency resistance (HFR) welding.

Mishler, H. W.↗

Heater for Combustible-Gas Tanks

Proposed heater for pressurizing hydrogen, oxygen, or another combustible liquid or gas sealed in immersion cup in pressurized tank. Firmly supported in finned cup, coiled rod transfers heat through liquid metal to gas tank. Heater assembly welded or bolted to tank flange.

Ingle, Walter B.↗

Utilization of a bipolar lead acid battery for the advanced launch system

The development of a battery comprised of bipolar lead acid modules is discussed. The battery is designed to satisfy the requirements of the Advanced Launch System (ALS). The battery will have the following design features: (1) conventional lead acid chemistry; (2) thin electrode/active materials; (3) a thin separator; (4) sealed construction (gas recombinant); and (5) welded plastic frames for the external seal.

Gentry, William O.↗

Assessing Gaseous Hydrogen Assisted Fatigue Crack Growth Susceptibility of Pipeline Steel Weld Fusion Zones and Heat Affected Zones

The objective of this work was twofold: (1) measure reliable fatigue crack growth relationships for X65 steel and its girth weld in high-pressure hydrogen gas to enable structural integrity assessments of hydrogen pipelines, and (2) evaluate the hydrogen accelerated fatigue crack growth susceptibility of the weld fusion zone and heat-affected zone relative to the base metal. Fatigue crack growth relationships (da/dN versus ΔK) were measured for girth welded X65 pipeline steel in high pressure hydrogen gas (21 MPa) and in air. Hydrogen assisted fatigue crack growth was observed for the base metal (BM), fusion zone (FZ), and heat-affected zone (HAZ), and was manifested through crack growth rates reaching nearly an order of magnitude acceleration over rates in air. Addditionally, at higher ΔK values, crack growth rates of BM, FZ, and HAZ were coincident; however, at lower ΔK, the fatigue crack growth relationships exhibited some divergence with the fusion zone having the highest crack growth rates. These relative fatigue crack growth rates in the BM, FZ, and HAZ were provisional, however, since both crack closure and residual stress contributed to the crack-tip driving force in specimens extracted from the HAZ. Despite the relatively high applied R-ratio (R = 0.5), crack closure was detected in the heat affected zone tests, in contrast to the absence of crack closure in the base metal tests. Crack closure corrections were performed using the adjusted compliance ratio method and the effect of residual stress on K max was determined by the crack-compliance method. Crack-tip driving forces that account for closure and residual stress effects were quantified as a weighted function of ΔK and K max (i.e., K norm ), and the resulting da/dN versus K norm relationships showed that the HAZ exhibited higher hydrogen accelerated fatigue crack growth rates than the BM at lower K norm values.

36 MATERIALS SCIENCE↗

Thermal Stir Welding Development at Marshall Space Flight Center

Solid state welding processes have become the focus of welding process development at NASA's Marshall Space Flight Center. Unlike fusion weld processes such as tungsten inert gas (TIG), variable polarity plasma arc (VPPA), electron beam (EB), etc., solid state welding processes do not melt the material during welding. The resultant microstructure can be characterized as a dynamically recrystallized morphology much different than the casted, dentritic structure typical of fusion weld processes. The primary benefits of solid state processes over fusion weld processes include superior mechanic properties and the elimination of thermal distortion and residual stresses. These solid state processes attributes have profoundly influenced the direction of advanced welding research and development within the NASA agency. Thermal Stir Welding (TSW) is a new solid state welding process being developed at the Marshall Space Flight Center. Unlike friction stir welding, the heating, stirring and forging elements of the weld process can be decoupled for independent control. An induction coil induces energy into a workpiece to attain a desired plastic temperature. An independently controlled stir rod, captured within non-rotating containment plates, then stirs the plasticized material followed by forging plates/rollers that work the stirred weld joint. The independent control (decoupling) of heating, stirring and forging allows, theoretically, for the precision control of microstructure morphology. The TSW process is being used to evaluate the solid state joining of Haynes 230 for ARES J-2X applications. It is also being developed for 500-in (12.5 mm) thick commercially pure grade 2 titanium for navy applications. Other interests include Inconel 718 and stainless steel. This presentation will provide metallurgical and mechanical property data for these high melting temperature alloys.

Ding, Robert J.↗

Cold Trap Replacement Project Report

This report documents the replacement of the Mechanisms Engineering Test Loop (METL) cold trap. The work involved preparation of the facility to replace the cold trap, removal of the existing welded cold trap from the sodium purification circuit, installation of a new replacement cold trap, completion of associated welds and examinations, restoration of instrumentation and heaters, and controlled return of the cold trap circuit to service. The replacement represented a significant maintenance evolution because the cold trap is an integral welded component of the sodium system. As a result, the work required coordinated control of sodium chemistry, deliberate formation of freeze plugs, inert gas management, precision cutting and welding, and a staged reheating and refill sequence. The activity was executed using procedural controls intended to protect personnel, preserve system cleanliness, and maintain the integrity of the sodium boundary throughout the work. This report provides a narrative summary of the milestone, including the purpose of the work, the pre-job system condition, the major field activities performed, observations made during execution, and the resulting post-work condition of the METL cold trap circuit.

42 ENGINEERING↗

Calibration Check For Programmed Welding Robot

Preweld calibration check helps to ensure welding torch on computer-controlled welding robot mounted properly, right gas cup selected, and length of extension of electrode adjusted correctly. Performed by operator just before dry run for each set of parts welded. Procedure takes 2 to 3 minutes and enables correction of errors before parts or equipment damaged.

Sliwinski, Karen E.↗

The variable polarity plasma arc welding process: Its application to the Space Shuttle external tank

The technical history of the variable polarity plasma arc (VPPA) welding process being introduced as a partial replacement for the gas shielded tungsten arc process in assembly welding of the space shuttle external tank is described. Interim results of the weld strength qualification studies, and plans for further work on the implementation of the VPPA process are included.

Nunes, A. C., Jr.↗

Spinarc gas tungsten arc torch holder

Semiautomatic welding torch enables operator to control arc length, torch angle, and spring tension when welding small diameter aluminum tubing. Tungsten is preset for the weld to make arc initiation easier and to eliminate searching for the joint through a dark welding lens.

Brace, D. F.↗

An experimental investigation of the effectiveness of Ar-CO 2 shielding gas mixture for the wire arc additive process

Wire arc additive manufacturing (AM) is the process by which a large, metallic structure is built layer-by-layer using a welding arc to melt a wire feedstock. A novel opportunity exists to alter the shielding gas composition to fabricate distinct geometrical features without altering the other AM parameters. In this paper, shielding gases with varied concentrations of Argon (Ar) and CO 2 was used to deposit three distinct geometric shapes (walls, infill, and overhang) using a wire-based additive manufacturing system utilizing the gas metal arc welding (GMAW) surface tension transfer (STT) process. Computer-aided design (CAD) models were sliced with a custom-built slicer, and the sliced algorithm was converted into optimal robotic toolpaths. A custom virtual instrument (VI) was built in LabVIEW to compare the temperature profiles on the surface during each deposition process. After each deposition, the geometric features were scanned, and the surface waviness value was evaluated. Tensile and Charpy impact coupons were extracted from the wall geometries in the longitudinal and transverse directions and tested. The results indicated that a higher CO 2 content produced higher melt pool temperatures to an extent, while lower contents of CO 2 resulted in a dimensionally accurate geometry. The data also indicated that the 2%/98% CO 2 /Ar blend produced scatter in tensile strength and the analysis of variance (ANOVA) shows significant difference. However, the intermediate range of CO 2 (5–10%) resulted in uniform tensile properties. Altogether, these results indicate that a 5%/95% CO 2 /Ar blend is the ideal shielding gas for lowering process temperatures and improving mechanical properties in wire arc additive manufacturing using the gas metal arc welding surface tension transfer process. Additionally, varying concentrations of Ar/CO 2 can be used within the same part in order to modify the local properties or process parameters such as strength, toughness, temperature, or dimensional features. This may improve overall manufacturing quality without sacrificing specific properties.